Resumo:
The effects of the carrier gas flow and water temperature on the oxidation rate for different reaction temperatures were investigated. The optimum conditions for stable oxidation were obtained. Two mechanisms of the oxidation process are revealed. One is the flow-controlling process, which is unstable. The other is the temperature-controlling process, which is stable. The stable region decreases for higher reaction temperatures. The simulation results for the stable oxidation region are also given. With optimum oxidation conditions, the stability and precision of the oxidation can be dramatically improved.
Resumo:
Wavelength tunable electro-absorption modulated distributed Bragg reflector lasers (TEMLs) are promising light source in dense wavelength division multiplexing (DWDM) optical fiber communication system due to high modulation speed, small chirp, low drive voltage, compactness and fast wavelength tuning ability. Thus, increased the transmission capacity, the functionality and the flexibility are provided. Materials with bandgap difference as large as 250nm have been integrated on the same wafer by a combined technique of selective area growth (SAG) and quantum well intermixing (QWI), which supplies a flexible and controllable platform for the need of photonic integrated circuits (PIC). A TEML has been fabricated by this technique for the first time. The component has superior characteristics as following: threshold current of 37mA, output power of 3.5mW at 100mA injection and 0V modulator bias voltage, extinction ratio of more than 20 dB with modulator reverse voltage from 0V to 2V when coupled into a single mode fiber, and wavelength tuning range of 4.4nm covering 6 100-GHz WDM channels. A clearly open eye diagram is observed when the integrated EAM is driven with a 10-Gb/s electrical NRZ signal. A good transmission characteristic is exhibited with power penalties less than 2.2 dB at a bit error ratio (BER) of 10(-10) after 44.4 km standard fiber transmission.
Resumo:
An improved selective area growth (SAG) method is proposed to better the fabrication and performance of the Electroabsorption modulated laser The typical threshold current of the EML is 18mA, and the output power is 5.6mW at EAM facet.
Resumo:
Oxide-free InGaAlAs waveguides have been grown on the InP substrates patterned with pairs of SiO2 mask stripes using narrow stripe selective MOVPE. The mask stripe width is varied from 0 to 40 pm, while the window region width between a pair of mask stripes is fixed at 1.5, 2.5 and 3.5 mu m, respectively. Smooth surface s and flat interfaces are obtained in the selectively grown InQaAlAs waveguides. There exhibit strong dependences of the thickness enhancement ratio and the photoluminescence (PL) spectrum on the mask stripe width and the window region width for the InGaAlAs wavegwdes. A large PL peak wavelength shift of 79 nm and a PL full width of at half maximum (FWHM) of less than 64 meV are obtained simultaneously. Some possible interpretations for our investigations are presented by considering both the migration effect from a masked region (MMR) and the lateral vapor diffusion effect (LVD).
Resumo:
Growth mechanism of InGaAlAs waveguides by narrow stripe selective MOVPE has been studied. Both the InGaAlAs bulk waveguides and the InGaAlAs MQW waveguides were successful grown on the patterned substrates at optimized growth conditions. The mask stripe width varied from 0 to 40 mu m, while the window region width between a pair of mask stripes was fixed 2.5 mu m. These selectively grown waveguides were covered by specific InP layers, which can keep the InGaAlAs waveguides from being oxidized during the fabrication of devices. In particular, there exhibit strong dependences of the photoluminescence (PL) spectrum on the mask stripe width for the samples. The results were explained in considering both the migration effect from a masked region (MMR) and the lateral vapor diffusion effect (LVD).
Resumo:
A novel device of tandem multiple quantum wells (MQWs) electroabsorption modulators (EAMs) monolithically integrated with DFB laser is fabricated by ultra-low-pressure (22 mbar) selective area guowth (SAG) MOCVD technique. Experimental results exhibit superior device characteristics with low threshold of 19 mX output light power of 4.5 mW and over 20 dB extinction ratio when coupled into a single mode Fiber. Moreover, over 10 GHz modulation bandwidth is developed with a driving voltage of 2 V. Using I this sinusoidal voltage driven integrated device, 10GHz repetition rate pulse with a width of 13.7 ps without any compression elements is obtained.
Resumo:
The narrow stripe selective growth of the InGaAlAs bulk waveguides and InGaAlAs MQW waveguides was first investigated. Flat and clear interfaces were obtained for the selectively grown InGaAlAs waveguides under optimized growth conditions. These selectively grown InGaAlAs waveguides were covered by specific InP layers, which can keep the waveguides from being oxidized during the fabrication of devices. PL peak wavelength shifts of 70 nm for the InGaAlAs bulk waveguides and 73 nm for the InGaAlAs MQW waveguides were obtained with a small mask stripe width varying from 0 to 40 gm, and were interpreted in considering both the migration effect from the masked region (MMR) and the lateral vapor diffusion effect (LVD). The quality of the selectively grown InGaAlAs MQW waveguides was confirmed by the PL peak intensity and the PL FWHM. Using the narrow stripe selectively grown InGaAlAs MQW waveguides, then the buried heterostructure (BH) lasers were fabricated by a developed unselective regrowth method, instead of conventional selective regrowth. The InGaAlAs MQW BH lasers exhibit good performance characteristics, with a high internal differential quantum efficiency of about 85% and an internal loss of 6.7 cm(-1).
Resumo:
A new method has been developed to selectively fabricate nano-gap electrodes and nano-channels by conventional lithography. Based on a sacrificial spacer process, we have successfully obtained sub-100-nm nano-gap electrodes and nano-channels and further reduced the dimensions to 20 nm by shrinking the sacrificial spacer size. Our method shows good selectivity between nano-gap electrodes and nano-channels due to different sacrificial spacer etch conditions. There is no length limit for the nano-gap electrode and the nano-channel. The method reported in this paper also allows for wafer scale fabrication, high throughput, low cost, and good compatibility with modern semiconductor technology.
Resumo:
A 1.55-mu m hybrid InGaAsP-Si laser was fabricated by the selective-area metal bonding method. Two Si blocking stripes, each with an excess-metals accommodated space, were used to separate the optical coupling area and the metal bonding areas. In such a structure, the air gap between the InGaAsP structure and Si waveguide has been reduced to be negligible. The laser operates with a threshold current density of 1.7 kA/cm(2) and a slope efficiency of 0.05 W/A under pulsed-wave operation. Room-temperature continuous lasing with a maximum output power of 0.45 mW is realized.
Space-selective precipitation of Ge crystalline patterns in glasses by femtosecond laser irradiation
Resumo:
Harmonic millimeter wave (mm-wave) generation and frequency up-conversion are experimentally demonstrated using optical injection locking and Brillouin selective sideband amplification (BSSA) induced by stimulated Brillouin scattering in a 10-km single-mode fiber. By using this method, we successfully generate third-harmonic mm-wave at 27 GHz (f(LO) - 9 GHz) with single sideband (SSB) modulation and up-convert the 2GHz intermediate frequency signal into the mm-wave band with single mode modulation of the SSB modes. In addition, the mm-wave carrier obtains more than 23 dB power gain due to the BSSA. The transmission experiments show that the generated mm-wave and up-converted signals indicate strong immunity against the chromatic dispersion of the fibers.
Resumo:
A novel integration technique has been developed using band-gap energy control of InGaAsP/InGaAsP multiquantum-well (MQW) structures during simultaneous ultra-low-pressure (22 mbar) selective-area-growth (SAG) process in metal-organic chemical vapour deposition. A fundamental study of the controllability of band gap energy by the SAG method is performed. A large band-gap photoluminescence wavelength shift of 83nm is obtained with a small mask width variation (0-30μm). The method is then applied to fabricate an MQW distributed-feedback laser monolithically integrated with an electroabsorption modulator. The experimental results exhibit superior device characteristics with low threshold of 19mA, over 24 dB extinction ratio when coupled into a single mode fibre. More than 10 GHz modulation bandwidth is also achieved, which demonstrates that the ultra-low-pressure SAG technique is a promising approach for high-speed transmission photonic integrated circuits.
Resumo:
The wide stripe (ISjum) selective area growth (SAG) of InGaAsP by low pressure MOVPE is systematically investigated. The characteristics of the growth ratios,thickness enhancement factors .bandgap modulation,and composition modulation vary with the growth conditions such as mask width,growth pressure. Flux of III-group precursors are outlined and the rational mechanism behind SAG MOVPE is explained. In addition,the surface spike of the SAG InGaAsP is shown and the course of it is given by the variation of V /III .