406 resultados para Harmonic emission
Resumo:
The time-resolved photoluminescence and steady photoluminescence (TRPL and PL) spectra on self-assembled InAs/GaAs quantum dots (QDs) are investigated. By depositing GaAs/InAs short period superlattices (SLs), 1. 48 μtm emission is obtained at room temperature. Temperature dependent PL measurements show that the PL intensity of the emission is very steady. It decays only to half as the temperature increases from 15 K to room temperature, while at the same time, the intensity of the other emission decreases by a factor of 5 orders of magnitude. These two emissions are attributed to large-size QDs and short period superlattices (SLs), respectively. Large-size QDs are easier to capture and confine carriers,which benefits the lifetime of PL, and therefore makes the emission intensity insensitive to the temperature.
Resumo:
A kind of novel broad-band superluminescent diodes (SLDs) using graded tensile-strained bulk InGaAs is developed. The graded tensile-strained bulk InGaAs is obtained by changing only group-III trimethyl-gallium source flow during low-pressure metal organic vapor-phase epitaxy. At the injection current of 200 mA, the fabricated SLDs with such structure demonstrate full-width at half-maximum spectral width of 106 nm and the output light power of 13.6 mW, respectively.
Resumo:
In this work, The TBS glass microspheres doped with Er3+ for morphology-dependent resonances of upconversion emission were designed. The glass sample components are 25TiO(2)-27BaCO(3)-8Ba(NO3)(2)-6ZnO(2)-9CaCO(3)-5H(3)BO(3)-10SiO(2)-7water glass-3Er(2)O(3) (wt%), and the emission spectra of TBS glass and a TBS glass microsphere (about 48 mum in diameter) were measured under 633 nm excitation and discussed. The strong morphology-dependent resonances of upconversion luminescences in the microsphere were observed. The observed resonances could be assigned by using the well-known Lorenz-Mie Formalism. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
In this study, silicon nanocrystals embedded in SiO2 matrix were formed by conventional plasma enhanced chemical vapor deposition (PECVD) followed by high temperature annealing. The formation of silicon nanocrystals (nc-Si), their optical and micro-structural properties were studied using various experimental techniques, including Fourier transform infrared spectroscopy, micro-Raman spectra, high resolution transmission electron microscopy and x-ray photoelectron spectroscopy. Very strong red light emission from silicon nanocrystals at room temperature (RT) was observed. It was found that there is a strong correlation between the PL intensity and the substrate temperature, the oxygen content and the annealing temperature. When the substrate temperature decreases from 250degreesC to RT, the PL intensity increases by two orders of magnitude.
Resumo:
We have studied the spontaneous emission of polarized excitons in the GaInP/AlGaInP VCSEL from 30K to room temperature. It is observed that the spontaneous emission peak enters and leaves the resonant regime. At the resonant regime, the emission intensities of the perpendicular and horizontal polarized exciton are enhanced at different ratio to those in non-resonant regime. These experiment results are explained through the dressed exciton theory of the semiconductor microcavity device. From this theory, the intensity enhancement and the polarization dependence are understood as cooperative emission and the microcavity anisotropy.
Resumo:
Resumo:
This paper presents a detailed PL study of Fe2+ related four zero-phonon(ZP) lines and their related phonon sidebands. Four zero-phonon transitions at approximate to 2800 cm(-1) along with the accompanying phonon sidebands extending down to 2400 cm(-1). There are ta two prominent regions in the phonon sidebands. One is ascribed to coupling to acoustic-type phonons (2700 cm(-1) region), the other is due to coupling to optic-type phonons (2500 cm(-1) region). Beside broad coupling with lattice modes, there are several groups of lines. They are ascribed to resonant modes, impurities induced gap modes and local modes.
Resumo:
The behaviors of lateral propagating modes in the aperture and the oxidized regions are investigated numerically for selectively oxidized vertical-cavity surface-emitting lasers (VCSELs). The results show that the lateral propagating modes in the oxidized region are greatly affected by the oxide layer due to its low index, the modes are divergence for the VCSELs with sufficient thick double oxide layers. So the coupling between the modes in the aperture and oxidized regions is very weak, and we can expect that the lateral spontaneous emission is greatly affected in this case. Ignoring the contribution of the lateral spontaneous emission, we calculate spontaneous emission factor by counting the total number of the guided modes in selectively oxidized VCSELs with double oxide layers. The results agree very well with the reported measurements and are inversely proportional to the lateral index step.
Resumo:
Photoluminescence (PL) from Er-implanted hydrogenated amorphous silicon suboxide (a-SiOX:H
Resumo:
nThermal processing of strained ln(0.2)Ga(0.8)As/GaAs graded-index separate confinement heterostructure single quantum well laser diodes grown by molecular beam epitaxy is investigated. It was found that rapid thermal annealing can improve the 77 K photoluminescence efficiency and electron emission from the active layer, due to removal of nonradiative centers from the InGaAs/GaAs interface. Because of the interdiffusion of Al and Ga atoms, rapid thermal annealing increases simultaneously the density of DX centers in the AlGaAs graded layer. The current stressing experiments of post-growth and annealed laser diodes are indicative of a corresponding increase in the concentration of DX centers, suggesting that DX centers may be responsible for the degradation of laser diode performance.
Resumo:
Red shifts of emission wavelength of self-organized In(Cla)As/GaAs quantum dots (QDs) covered by 3 nm thick InxGa1-xAs layer with three different In mole fractions (x = 0.1, 0.2 and 0.3, respectively) have been observed. Transmission electron microscopy images demonstrate that the stress along growth direction in the InAs dots was reduced due to introducing the InxGa1-xAs (x = 0.1, 0.2 and 0.3) covering layer instead of GaAs layer. Atomic force microscopy pictures show a smoother surface of InAs islands covered by an In0.2Ga0.8As layer. It is explained by the calculations that the redshifts of the photoluminescence (PL) spectra from the QDs covered by the InxGa1-xAs (x greater than or equal to 0.1) layers were mainly due to the reducing of the strain other than the InAs/GaAs intermixing in the InAs QDs. The temperature dependent PL spectra further confirm that the InGaAs covering layer can effectively suppress the temperature sensitivity of PL emissions. 1.3 mum emission wavelength with a very narrow linewidth of 19.2 mcV at room temperature has been obtained successfully from In,In0.5Ga0.5As/GaAs self-assembled QDs covered by a 3-nm In0.2Ga0.2As strain reducing layer. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
A novel ameliorated phase generated carrier (PGC) demodulation algorithm based on arctangent function and differential-self-multiplying (DSM) is proposed in this paper. The harmonic distortion due to nonlinearity and the stability with light intensity disturbance (LID) are investigated both theoretically and experimentally. The nonlinearity of the PGC demodulation algorithm has been analyzed and an analytical expression of the total-harmonic-distortion (THD) has been derived. Experimental results have confirmed the low harmonic distortion of the ameliorated PGC algorithm as expected by the theoretical analysis. Compared with the traditional PGC-arctan and PGC-DCM algorithm, the ameliorated PGC algorithm has a much lower THD as well as a better signal-to-noise-and-distortion (SINAD). A THD of below 0.1% and a SINAD of 60 dB have been achieved with PGC modulation depth (value) ranges from 1.5 to 3.5 rad. The stability performance with LID has also been studied. The ameliorated PGC algorithm has a much higher stability than the PGC-DCM algorithm. It can keep stable operations with LID depth as large as 26.5 dB and LID frequency as high as 1 kHz. The system employing the ameliorated PGC demodulation algorithm has a minimum detectable phase shift of 5 mu rad/root Hz @ 1 kHz, a large dynamic range of 120 dB @ 100 Hz, and a high linearity of better than 99.99%.
Resumo:
The InAs quantum dots (QDs) on an AlAs layer are grown on GaAs substrates by molecular beam epitaxy technique. The properties of materials and optics of such QD structures have been investigated by cross sectional transmission electron microscopy and photoluminescence (PL) techniques. It is discovered that the inhomogeneous strain filed mainly exists below InAs QDs layers in the case of no wetting layer. The full width at half maximums (FWHMs) and intensities of PL emission peaks of InAs QDs are found to be closely related to the thickness of the thin AlAs layers. The InAs QDs on an eight monolayer AlAs layer, with wide FWHMs and large integral intensity of PL emission peaks, are favorable for producing broadband QD superluminescent diodes, external-cavity QD laser with large tuning range.