995 resultados para BURIED-HETEROSTRUCTURE


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fabrication of InGaAlAs MQW buried heterostructure (BH) lasers by narrow stripe selective MOVPE is demonstrated in this paper. High quality InGaAlAs MQWs were first grown by narrow stripe selective MOVPE without any etching process and assessed by analysing the cross sections and PL spectrums of the InGaAlAs MQWs. Furthermore, BHs were fabricated for the InGaAlAs MQW lasers by a developed unselective regrowth method, instead of conventional selective regrowth. The InGaAlAs MQW BH lasers exhibit good device characteristics, with a high internal differential quantum efficiency of 85% and a low internal loss of 6.7 cm(-1). Meanwhile, narrow divergence angles of the far field pattern are obtained for the fabricated lasers.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel unselective regrowth buried heterostructure (BH) long-wavelength superluminescent diode (SLD), which has a grade-strained bulk InGaAs active region, was developed by metalorganic vapor-phase epitaxy (MOVPE). The 3 dB emission spectrum bandwidth of the SLD is about 65 nm with the range from 1596 to 1661 nm at 90 mA and front 1585 to 1650 nm at 150 mA. An output power of 3.5 mW is obtained at 200 mA injection current under CW operation at room temperature. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Unselective regrowth for fabricating 1.5-mu m InGaAsP multiple-quantum well (MQW) distributed-feedback (DFB) buried heterostructure (BH) lasers is developed. The experimental results exhibit superior characteristics, such as a low threshold of 8.5 mA, high slope efficiency of 0.55 mW/mA, circular-like far-field patterns, the narrow line-width of 2.5 MHz, etc. The high performance of the devices effectively proves the feasibility of the new method to fabricate buried heterostructure lasers. (c) 2006 Society of Photo-Optical Instrumentation Engineers.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A InGaAsP/InP self-aligned, native oxidized buried heterostructure (BH) distributed feedback (DFB) laser is proposed. It is as easy to process as the ridge waveguide DFB laser and has superior performance. The current aperture can be easily controlled without selective regrowth. The laser exhibits a low threshold of 5.0 mA with 36 dB side mode suppression ratio at the emission wavelength of 1.562 mu m. It emits in a single lobe with full width at half maximum angles of 33.6 degrees and 42.6 degrees for the lateral and vertical fields, respectively. Its beam is more circular than that of the as-grown BH laser because the lower refractive index of oxide compared to the as-grown layer and results in a larger lateral optical confinement. Its characteristic temperature (T-0) is 50 K at room temperature but increases in value at the higher temperature range. (C) 2000 American Institute of Physics. [S0003-6951(00)00812-3].

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel idea of InAlAs native oxide utilized to replace the p-n-p-n thyristor blocking layer and improve the high-temperature performance of buried heterostructure InGaAsP-InP laser is first proposed and demonstrated. A characteristic temperature (T-0) of 50 K is achieved from an InA1As native oxide buried heterostructure (NOBH) InGaAsP-InP multiquantum-well laser with 1.5-mu m-wide diode leakage passage path. The threshold current and slope efficiency of NOBH laser changes from 5.6 mA, 0.23 mW/mA to 28 mA, 0.11 mW/mA with the operating temperature changing from 20 degrees C to 100 degrees C. It is comparable to conventional p-n reverse biased junction BH laser with minimized diode leakage current, and is much better than the buried ridge strip with proton implanted laterally confinement laser.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An InAlAs native oxide is used to replace the p-n reverse-biased junction in a conventional buried heterostructure InP-based laser. This technique reduces the number of regrowth steps and eliminates leakage current under high-temperature operation. The InAlAs native oxide buried heterostructure (NOBH) laser with strain-compensated InGaAsP/InP multiple quantum well active layers has a threshold current of 5.6 mA, a slope efficiency of 0.23 mW/mA, and a linear power up to 22.5 mW with a HR-coated facet. It exhibits single transverse mode with lasing wavelength at 1.532 mu m. A characteristic temperature (T-0) of 50 K is obtained from the NOBH laser with a nonoptimized oxide layer width. (C) 1998 American Institute of Physics. [S0003-6951(98)01352-7].

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The narrow stripe selective growth of the InGaAlAs bulk waveguides and InGaAlAs MQW waveguides was first investigated. Flat and clear interfaces were obtained for the selectively grown InGaAlAs waveguides under optimized growth conditions. These selectively grown InGaAlAs waveguides were covered by specific InP layers, which can keep the waveguides from being oxidized during the fabrication of devices. PL peak wavelength shifts of 70 nm for the InGaAlAs bulk waveguides and 73 nm for the InGaAlAs MQW waveguides were obtained with a small mask stripe width varying from 0 to 40 gm, and were interpreted in considering both the migration effect from the masked region (MMR) and the lateral vapor diffusion effect (LVD). The quality of the selectively grown InGaAlAs MQW waveguides was confirmed by the PL peak intensity and the PL FWHM. Using the narrow stripe selectively grown InGaAlAs MQW waveguides, then the buried heterostructure (BH) lasers were fabricated by a developed unselective regrowth method, instead of conventional selective regrowth. The InGaAlAs MQW BH lasers exhibit good performance characteristics, with a high internal differential quantum efficiency of about 85% and an internal loss of 6.7 cm(-1).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A very low CW threshold current of 1.65 mA at room temperature was obtained for an uncoated buried-heterostructure strained layer multiquantum well InGaAs-GaAs laser fabricated using hybrid molecular beam epitaxy and liquid phase epitaxy crystal growth technique. External differential quantum efficiency as high as 44.6% (0.53 mW/mA) and output power of more than 30 mW per facet were achieved in the same laser.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We have investigated a resonant refractive nonlinearity in a semiconductor waveguide by measuring intensity dependent phase shifts and bias-dependent recovery times. The measurements were performed on an optimized 750-μm-long AR coated buried heterostructure MQW p-i-n waveguide with a bandedge at 1.48 μm. Figure 1 shows the experimental arrangement. The mode-locked color center laser was tuned to 50 meV beyond the bandedge and 8 ps pulses with peak incident power up to 57 W were coupled into the waveguide. Some residual bandtail absorption remains at this wavelength and this is sufficient to cause carriers to be photogenerated and these give rise to a refractive nonlinearity, predominantly by plasma and bandfilling effects. A Fabry-Perot interferometer is used to measure the spectrum of the light which exits the waveguide. The nonlinearity within the guide causes self phase modulation (SPM) of the light and a study of the spectrum allows information to be recovered on the magnitude and recovery time of the nonlinear phase shift with a reasonable degree of accuracy. SPM spectra were recorded for a variety of pulse energies coupled into he unbiased waveguide. Figure 2 shows the resultant phase shift measured from the SPM spectra as a function of pulse energy. The relationship is a linear one, indicating that no saturation of the nonlinearity occurs for coupled pulse energies up to 230 pJ. A π phase shift, the minimum necessary for an all-optical switch, is obtained for a coupled pulse energy of 57 pJ while the maximum phase shift, 4 π, was measured for 230 pJ. The SPM spectra were highly asymmetric with pulse energy shifted to higher frequencies. Such spectra are characteristic of a slow, negative nonlinearity. This relatively slow speed is expected for the unbiased guide as the recovery time will be of the order of the recombination time of the photogenerated electrons, about 1 ns for InGaAsP material. In order to reduce the recovery time of the nonlinearity, it is necessary to remove the photogenerated carriers from the waveguide by a process other than recombination. One such technique is to apply a reverse bias to the waveguide in order to sweep the carriers out. Figure 3 shows the effect on the recovery time of the nonlinearity of applying reverse bias to the waveguide for 230 pJ coupled power. The recovery time was reduced from one much longer than the length of the pulse, estimated to be about 1 ns, at zero bias to 18 ± 3 ps for a bias voltage greater than -4 V. This compares with a value of 24 ps obtained in a bulk waveguide.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Narrow stripe selective growth of oxide-free InGaAlAs/InGaAlAs multiple quantum wells (MQWs) has been successfully performed on patterned InP substrates by ultra-low pressure MOVPE. Flat and clear interfaces were obtained for the narrow stripe selectively grown MQWs under optimized growth conditions. These selectively grown MQWs were covered by specific InP layers, which can keep the MQWs from being oxidized during the fabrication of the devices. The characteristics of selectively grown MQWs were strongly dependent on the mask stripe width. In particular, a PL peak wavelength shift of 73 nm, a PL intensity of more than 57% and a PL FWHM of less than 102 meV were observed simultaneously with a small mask stripe width varying from 0 to 40 mu m. The results were explained by considering the migration effect from the masked region (MMR) and the lateral vapour diffusion effect (LVD).

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We have performed a narrow stripe selective growth of oxide-free A1GaInAs waveguides on InP substrates patterned with pairs of SiO2 mask stripes under optimized growth conditions. The mask stripe width varied from 0 to 40 mu m, while the window region width between a pair of mask stripes was fixed at 1.5, 2.5 or 3.5 mu m. Flat and smooth A1GaInAs waveguides covered by specific InP layers are successfully grown on substrates patterned with different mask designs. The thickness enhancement ratio and the photoluminescence (PL) spectrum of the A1GaInAs narrow stripe waveguides are strongly dependent on the mask stripe width and the window region width. In particular, a large PL wavelength shift of 79 nm and a PL FWHM of less than 64 meV are obtained simultaneously with a small mask stripe width varying from 0 to 40 mu m when the window region width is 1.5 mu m. We present some possible interpretations of the experimental observations in considering both the migration effect from a masked region and the lateral vapour diffusion effect.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A novel in-plane bandgap energy controlling technique by ultra-low pressure (22 mbar) selective area growth (SAG) has been developed. To our knowledge, this is the lowest pressure condition during SAG process ever reported. In this work, high crystalline quality InGaAsP-InP MQWs with a photoluminescence (PL) full-width at half-maximum (FWHM) of less than 35meV are selectively grown on mask-patterned planar InP substrates by ultra-low pressure (22 mbar) metal-organic chemical vapor deposition (MOCVD). In order to study the uniformity of the MQWs grown in the selective area, novel tapered masks are designed and used. Through optimizing growth conditions, a wide wavelength shift of over 80 nm with a rather small mask width variation (0-30 mu m) is obtained. The mechanism of ultra-low pressure SAG is detailed by analyzing the effect of various mask designs and quantum well widths. This powerful technique is then applied to fabricate an electroabsorption-modulated laser (EML). Superior device characteristics are achieved, such as a low threshold current of 19mA and an output power of 7mW. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A 1.3-mu m AlGaInAs/InP buried heterostructure (BH) stripe distributed feedback laser with a novel AlInAs/InP complex-coupled grating grown by low-pressure metalorganic chemical vapor deposition (LP-MOCVD) is proposed and demonstrated. A high characteristic temperature (T-0 = 90K between 20-80 degrees C) and temperature-insensitive slope efficiency (0.25 dB drop from 20 to 80 degrees C) in 1.3 mu m AlGaInAs/InP DFB lasers was obtained by introducing AI(Ga)InAs graded-index separate-confinement heterostructure (GRINSCH) layers and a strained-compensated (SC) multi-quantum well (MQW).

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Oxide-free InGaAlAs waveguides have been grown on the InP substrates patterned with pairs of SiO2 mask stripes using narrow stripe selective MOVPE. The mask stripe width is varied from 0 to 40 pm, while the window region width between a pair of mask stripes is fixed at 1.5, 2.5 and 3.5 mu m, respectively. Smooth surface s and flat interfaces are obtained in the selectively grown InQaAlAs waveguides. There exhibit strong dependences of the thickness enhancement ratio and the photoluminescence (PL) spectrum on the mask stripe width and the window region width for the InGaAlAs wavegwdes. A large PL peak wavelength shift of 79 nm and a PL full width of at half maximum (FWHM) of less than 64 meV are obtained simultaneously. Some possible interpretations for our investigations are presented by considering both the migration effect from a masked region (MMR) and the lateral vapor diffusion effect (LVD).

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A novel unselective regrowth buried heterostructure long-wavelength superluminescent diode (SLD) with a graded composition bulk InGaAs active region is developed by metalorganic vapor phase epitaxy (MOVPE). At a 150mA injection current, the full width at half maximum of the emission spectrum of the SLD is about 72nm, ranging from 1602 to 1674nm. The emission spectrum is smooth and flat. The ripple of the spectrum is less than 0.3dB at any wavelength from 1550 to 1700nm. An output power of 4.3mW is obtained at a 200mA injection current under continuous-wave operation at room temperature. This device is suitable for the applications of light sources for gas detectors and L-band optical fiber communications.