995 resultados para CUBIC GAN
Resumo:
In our recent report, [Xu , Appl. Phys. Lett. 76, 152 (2000)], profile distributions of five elements in the GaN/sapphire system have been obtained using secondary ion-mass spectroscopy. The results suggested that a thin degenerate n(+) layer at the interface is the main source of the n-type conductivity for the whole film. The further studies in this article show that this n(+) conductivity is not only from the contribution of nitride-site oxygen (O-N), but also from the gallium-site silicon (Si-Ga) donors, with activation energies 2 meV (for O-N) and 42 meV (for Si-Ga), respectively. On the other hand, Al incorporated on the Ga sublattice reduces the concentration of compensating Ga-vacancy acceptors. The two-donor two-layer conduction, including Hall carrier concentration and mobility, has been modeled by separating the GaN film into a thin interface layer and a main bulk layer of the GaN film. The bulk layer conductivity is to be found mainly from a near-surface thin layer and is temperature dependent. Si-Ga and O-N should also be shallow donors and V-Ga-O or V-Ga-Al should be compensation sites in the bulk layer. The best fits for the Hall mobility and the Hall concentration in the bulk layer were obtained by taking the acceptor concentration N-A=1.8x10(17) cm(-3), the second donor concentration N-D2=1.0x10(18) cm(-3), and the compensation ratio C=N-A/N-D1=0.6, which is consistent with Rode's theory. Saturation of carriers and the low value of carrier mobility at low temperature can also be well explained. (C) 2001 American Institute of Physics.
Resumo:
A detailed characterisation study of GaN thin films grown by rf-plasma molecular beam epitaxy on intermediate-temperature buffer layers (ITBL) was carried out with Hall, photoluminescence (PL) and deep-level transient Fourier spectroscopy (DLTFS) techniques. The unique feature of our GaN thin films is that the GaN epitaxial layers are grown on top of a double layer that consists of an ITBL, which is grown at 690 degreesC, and a conventional low-temperature buffer layer deposited at 500 degreesC. It is observed that the electron mobility increases steadily with the thickness of the ITBL, which peaks at 377 cm(2)V(-1)S(-1) for an ITBL thickness of 800 nm. The PL also demonstrated systematic improvements with the thickness of the ITBL. The DLTFS results suggest a three-order-of-magnitude reduction in the deep level at E-c-0.40 eV in the device fabricated with the GaN films grown on an ITBL thickness of 1.25 mum in comparison with the control device without an ITBL. Our analyses indicate that the utilization of an ITBL in addition to the conventional low-temperature buffer layer leads to the relaxation of residual strain within the material, resulting in an improvement in the optoelectronic properties of the films. (C) 2002 Elsevier Science BN. All rights reserved.
Resumo:
Based on morphology observed by atomic force microscopy, a geometrical model was proposed in order to explain the statistical results obtained from morphology observation on GaN in initial growth stage. Four parameters were introduced to describe the morphology characteristics in this model. Least-square fitting of height distribution was performed. The height distribution derived from the model agreed well with that obtained from experimental records. It was also found that the model should be further advanced to understand the growth of GaN in initial growth stage. (C) 2002 Elsevier Science BY. All rights reserved.
Resumo:
High-quality and high-resistivity GaN films were grown on (0001) sapphire face by metal-organic vapour phase epitaxy. To measure the surface acoustic wave properties accurately, we deposited metallized interdigital transducers on the GaN surface. The acoustic surface wave velocity and electromechanical coupling coefficient were measured, respectively, to be 5667 m/s and 1.9% by the pulse method.
Resumo:
We report the investigation of temperature and excitation power dependence in photoluminescence spectroscopy measured in Mg-doped GaN epitaxial layers grown on sapphire by metalorganic chemical vapor deposition, The objective is to examine the effects of rapid-thermal annealing on Mg-related emissions. It is observed that the peak position of the 2.7-2.8 eV emission line is a function of the device temperature and annealing conditions, The phenomenon is attributed to Coulomb-potential fluctuations in the conduction and valence band edge and impurity levels due to the Mg-related complex dissociation. The blue shift of the 2.7-2.8 eV emission line with increasing excitation power provides clear evidence that a donor-acceptor recombination process underlies the observed emission spectrum. In addition, quenching of minor peaks at 3.2 and 3.3 eV are observed and their possible origin is discussed. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Three minutes' growth was carried out to investigate the indium-doping effect on initially grown GaN. Indium-doped and undoped samples were grown by low-pressure metalorganic vapor phase epitaxy. Atomic force microscope observation revealed that In-doping modified the morphology of the nuclei. Indium-doping also enhanced wetting between the buffer and nuclei layers, which was also supported by optical transmission. Photoluminescence suggested that indium-doping obviously enhanced band-edge related emission even in the nucleation stage. X-ray diffraction performed on samples grown for 20 minutes indicated improvement of the crystalline quality through indium-doping. The mechanism of the indium-doping effect was discussed.
Resumo:
Hydrogen behavior in unintentionally doped GaN epilayers on sapphire substrates grown by NH3-MBE is investigated. Firstly, we find by using nuclear reaction analysis (NRA) that with increasing hydrogen concentration the background electron concentration increases, which suggests that there exists a hydrogen-related donor in undoped GaN, Secondly, Fourier transform infrared (FTIR) absorption and X-ray photoelectron spectroscopy (XPS) reveal Further that hydrogen atom is bound to nitrogen atom in GaN with a local vibrational mode at about 3211 cm(-1) Hence, it is presumed that the hydrogen-related complex Ga. . .H-N is a hydrogen-related donor candidate partly responsible for high n-type background commonly observed in GaN films. Finally, Raman spectroscopy results of the epilayers show that ill addition to the expected compressive biaxial strain, in some cases GaN films suffer from serious tensile biaxial strain. This anomalous behavior has been well interpreted in terms of interstitial hydrogen lattice dilation. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
The influence of electric fields on surface migration of Gallium (Ga) and Nitrogen (N) adatoms is studied during GaN growth by molecular beam epitaxy (MBE). When a direct current (DC) is used to heat the sample, long distance migration of Ga adatoms and diffusion asymmetry of N adatoms at steps are observed. On the other hand, if an alternating current (AC) is used, no such preferential adatom migration is found. This effect is attributed to the effective positive charges of surface adatoms. representing an effect of electro-migration. The implications of such current-induced surface migration to GaN epitaxy are subsequently investigated. It is seen to firstly change the distribution of Ga adatoms on a growing surface, and thus make the growth to be Ga-limited at one side of the sample but N-limited at the other side. This leads to different optical qualities of the film and different morphologies of the surface. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
High-quality GaN epilayers were consistently obtained using a home-made gas-sourer MBE system on sapphire substrates. Room-temperature electron mobility of the grown GaN film is 300 cm(2)/V s with a background electron concentration as low as 2 x 10(17) cm(-3) The full-width at half-maximum of the GaN (0 0 0 2) double-crystal X-ray rocking curve is 6 arcmin. At low temperature (3.5 K), the FWHM of the: near-band-edge photoluminescence emission line is 10 meV. Furthermore, using piezoelectric effect alone with the high-quality films, two-dimensional electron gas was formed in a GaN/AlN/GaN/sapphire structure. Its room-temperature and low-temperature (77 K) electron mobility is 680 cm(2)/V s and 1700 cm(2)/V s, and the corresponding sheet electron density is 3.2 x 10(13) and 2.6 x 10(13) cm(-2), respectively. (C) 2001 Published by Elsevier Science.
Resumo:
Epitaxial growth of SiC on complex substrates was carried out at substrate temperature from 1200 degreesC to 1400 degreesC. Three kinds of new complex substrates, c-plane sapphire, AlN/sapphire, and GaN/AlN/sapphire, were used in this study. We obtained a growth rate in the range of 1-6 mum/h. Thick (6 mum) SIC epitaxial layers with no cracks were successfully obtained on AlN/sapphire and GaN/AlN/sapphire substrates. X-ray diffraction patterns have confirmed that single-crystal SiC was obtained on these complex substrates. Analysis of optical transmission spectra of the SIC grown on sapphire substrates shows the lowest-energy gap near 2.2 eV, which is the value for cubic SiC. The undoped SIC showed n-type electrical conductivity. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
GaN films were grown in pairs on two opposite c faces of Al2O3 substrate by low-pressure metal-organic vapor phase epitaxy, and studied by scanning electron microscopy and converged beam electron diffraction. It is found that GaN film on the c-Al2O3 whose c face is forward to its crystal seed has [0001] polarity, and the other film on the C-Al2O3 whose c face is backward to its crystal seed has [000 (1) over bar] polarity. (C) 2001 American Institute of Physics.
Resumo:
The effects of in situ annealing treatment in the initial growth stage and In-doping during growth of the GaN on the material properties were investigated. GaN was grown by LP-MOVPE. In situ annealing reduced the full-width at half-maximum (FWHM) of X-ray rocking curves and reduced etch pit density of GaN films. It improved the optical properties of the epilayer. Undoped and In-doped GaN films of initial growth stage were investigated. It was found that morphology and optical properties were improved in In-doped samples. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Undoped GaN epilayer on c-face (0 0 0 1) sapphire substrate has been grown by metalorganic vapor-phase epitaxy (MOVPE) in a horizontal-type low-pressure two-channel reactor. Photoluminescence (PL) as a function of temperature and excitation intensity have been systematically studied, and the competition between near band gap ultraviolet (UV) and defect-related yellow luminescence (YL) has been extensively investigated, It is revealed that the ratio of the UV-to-YL peak intensities depends strongly on the excitation intensity and the measurement temperature. The obtained results have been analyzed in comparison with the theoretical predications based on a bimolecular model. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
GaN epilayers on sapphire substrate grown by metalorganic vapor-phase epitaxy (MOVPE) in a horizontal-type low-pressure two-channel reactor were investigated. Samples were characterized by X-ray diffraction (XRD), Raman scattering, atomic force microscopy (AFM) and photoluminescence (PL) measurements. The influence of the temperature changes between low temperature (LT) deposited GaN buffer and high temperature (WT) grown GaN epilayer on crystal quality of epilayer was extensively studied. The effect of in situ thermal annealing during the growth on improving the GaN layer crystal quality was demonstrated and the possible mechanism involved in such a growth process was discussed. (C) 2001 Elsevier Science B.V. All rights reserved.