730 resultados para GAAS(100)
Resumo:
We have studied the effect of molecular beam epitaxy growth conditions on the surface morphology of strained InAs/GaAs(331)A films. Our results reveal that InAs nanowires aligned along the [1 (1) over bar0] direction are formed under As-rich conditions, which is explained by the effect of anisotropic buffer layer surface roughing. Under In-rich conditions, however, the surface morphology of the InAs layers is characterized by a feature of island-pit pairs. In this case, cooperative nucleation of islands and pits can lower the activation barrier for domain growth. These results suggest that the surface morphology of strained InAs layers is highly controllable. (C) 2005 American Institute of Physics.
Resumo:
GaAs absorber was grown at low temperature (550degreesC) by metal organic chemical vapour deposition (MOCVD) and was used as an output coupler with which we realized Q-switching modelocked Yb3+-doped fibre laser. The shortest period of the envelope of the Q-switched modelocking is about 3mus. The modelocking threshold is 4.27W and the highest average output pulse power is 290 mW. The modelocking frequency is 12 MHz.
Resumo:
We have demonstrated 1.5 mum light emission from InAs quantum dots (QDs) capped with a thin GaAs layer. The extension of the emission wavelength can be assigned to the large QD height. We also investigate the effect of growth interruption on the PL properties and the shape of InAs QDs fabricated by migration-enhanced growth (MEG). Contrary to expectation, we observed a remarkable blueshift of the emission energy with the growth interruption in MEG mode. Detailed investigations reveal that the blueshift is related to the reduced island height with the growth interruption, which is confirmed by reflection high-energy electron diffraction (RHEED) patterns and atomic force microscopy (AFM) measurement results. Accordingly, the structure changes of the islands are interpreted in terms of thermodynamic and kinetic theories. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Zincblende Mn-rich Mn(Ga)As nanoclusters embedded in GaAs matrices are fabricated by in situ postgrowth annealing diluted magnetic semiconductor (Ga,Mn)As films with Mn concentration ranging from 2.6% to 8% at 650 degrees C. Magnetization measurements show that memory effect and slow magnetic relaxation, the typical characteristics of the spin-glass-like phase, occur below the blocking temperature of 45 K in samples with high Mn concentration, while for samples with low Mn concentration, ferromagnetic order remains up to 360 K. The behavior of low-temperature spin dynamics can be explained by the hierarchical model. (c) 2007 American Institute of Physics.
Resumo:
First, GaSb epilayers were grown on (001) GaAs substrates by molecular beam epitaxy. We determined that the GaSb layers had very smooth surfaces using atomic force microscopy. Then, very short period InAs/ GaSb superlattices (SLs) were grown on the GaSb buffer layer. The optical and crystalline properties of the superlattices were studied by low-temperature photoluminescence spectra and high resolution transition electron microscopy. In order to determine the interface of SLs, the samples were tested by Raman-scattering spectra at room temperature. Results indicated that the peak wavelength of SLs with clear interfaces and integrated periods is between 2.0 and 2.6 mu m. The SL interface between InAs and GaSb is InSb-like.
Resumo:
We compared two reflection-mode negative electron affinity (NEA) GaAs photocathode samples that are grown by molecular beam epitaxy with p-type beryllium doping. One sample is uniform doping, and another is gradient doping. Experimental curves of spectral response sensitivity and quantum efficiency are obtained. The thicknesses of the two cathodes are both 2.6 mu m. The integrated sensitivity of the uniform doping one is 1966 mu A/lm, and that of the gradient-doping one is 2421 mu A/lm. The escape probability and diffusion length are fitted from the spectral response curves. For the uniform-doping sample, the escape probability is 0.45 and the diffusion length is 5 mu m. For the gradient-doping sample, the escape probability is 0.55 and the diffusion length is 5.5 mu m. (c) 2007 Optical Society of America.
Resumo:
Mode gain spectrum is measured by the Fourier series expansion method for InAs/GaAs quantum-dot (QD) lasers with seven stacks of QDs at different injection currents. Gain spectra with distinctive peaks are observed at the short and long wavelengths of about 1210 nm and 1300 nm. For a QD laser with the cavity length of 1060 mu m, the peak gain of the long wavelength first increases slowly or even decreases with the injection current as the peak gain of the short wavelength increases quickly, and finally increases quickly before approaching the saturated values as the injection current further increases.
Resumo:
A photonic crystal vertical-cavity-surface-emitting laser ( PC-VCSEL) with a wavelength of about 850 nm was realized. The direct-current electrically-driven PC-VCSELs with a minimum threshold current of 2 mA and a maximum threshold current of 13.5 mA were obtained. We fabricated a series of PC-VCSEL chips whose lattice constants are in the range from 0.5 to 3 mu m with different filling factors, and found that the laser characterization depends on the lattice constant, the filling factor, the size of cavity, etc.
Resumo:
We investigate plasmon excitations in a quantum wire that consists of an infinite one-dimensional array of vertically coupled InAs/GaAs strained quantum dots (QDs). The research is carried out in the framework of random-phase approximation using effective-mass theory. Our formalism is capable of studying plasmons with strong tunneling among QDs, which frustrate the conventionally adopted tight-binding approximation. Based on this formalism, a systematic study on the intraminiband or intrasubband plasmon in vertically coupled InAs/GaAs strained QDs is presented. It is found that an increase of the dot spacing will inevitably reduce the plasmon energy. In contrast, the role of dot height is relatively complex and depends on the dot spacing. The results demonstrate the possibility to engineer collective excitations in low dimensional systems by simply changing their geometric configuration.
Resumo:
Using a low temperature grown GaAs wafer as an intracavity saturable absorber, a temporal envelope duration of 11 ns of Q- switched and mode- locked ( QML) 1064 nm operation was achieved in a very simple compact plane- concave cavity Nd: YVO4 laser, it was so short that the pulses can be used as Q- switching pulses. The maximal average output power is 808 mW with the repetition rate of 25 kHz, and the corresponding peak power and energy of a single Q- switched pulse was 2.94 kW and 32.3 mu J, respectively. The mode- locked pulse trains inside the Q- switched pulse envelope had a repetition rate of 800 MHz.
Resumo:
GaAs (001) substrates are patterned by electron beam lithography and wet chemical etching to control the nucleation of InAs quantum dots (QDs). InAs dots are grown on the stripe-patterned substrates by solid source molecular beam epitaxy, A thick buffer layer is deposited on the strip pattern before the deposition of InAs. To enhance the surface diffusion length of the In atoms, InAs is deposited with low growth rate and low As pressure. The AFM images show that distinct one-dimensionally ordered InAs QDs with homogeneous size distribution are created, and the QDs preferentially nucleate along the trench. With the increasing amount of deposited InAs and the spacing of the trenches, a number of QDs are formed beside the trenches. The distribution of additional QDs is long-range ordered, always along the trenchs rather than across the spacing regions.
Resumo:
Mn ions were doped into InAs/GaAs quantum dots samples by high energy. implantation and subsequent annealing. The optical and electric properties of the samples have been studied. The photoluminescence intensity of the samples annealed rapidly is stronger than that of the samples annealed for long time. By studying the relationship between the photoluminescence peaks and the implantation dose, it can be found that the photoluminescence peaks of the quantum dots show a blueshift firstly and then move to low energy with the implantation. dose increasing. The latter change in the photoluminescence peaks is probably attributed to that Mn ions entering the InAs quantum dots, which release the strain of the quantum dots. For the samples implanted by heavy dose (annealed rapidly) and the samples annealed for long time, the resistances versus temperature curves reveal anomalous peaks around 40 K.
Resumo:
The growth of InAsxSb1-x films on (100) GaSb substrates by liquid-phase epitaxy (LPE) has been investigated and epitaxial InAs0.3Sb0.7 films with InAs0.9Sb0.09 buffer layers have been successfully obtained. The low X-ray rocking curve FHWM values of InAs0.3Sb0.7 layer shows the high quality of crystal-orientation structure. Hall measurements show that the highest electron mobility in the samples obtained is 2.9 x 10(4) cm(2) V-1 s(-1) and the carrier density is 2.78 x 10(16)cm(-3) at room temperature (RT). The In As0.3Sb0.7 films grown on (10 0) GaSb substrates exhibit excellent optical performance with a cut-off wavelength of 12 mu m. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Using micro-photoluminescence technique, we observed a new photoluminescence peak about 0.348 eV above the bandgap of GaAs (E-0). By analyzing its optical characteristics, we assigned this peak to the nonequilibrium luminescence emission from the E-0 + Delta(0) bandgap in semi-insulated GaAs, which was further verified by Raman results. The observed polarization, excitation power dependence and temperature dependence of the photoluminescence spectra from the E-0 + Delta(0) energy level were very similar to those from the E-0 of GaAs. This mainly resulted from the common conduction band around Gamma(6) that was involved in the two optical transition processes, and indicated that the optical properties of bulk GaAs were mainly determined by the intrinsic properties of the conduction band. Our results demonstrated that the micro-photoluminescence technique is a powerful tool to investigate the high energy states above the fundamental bandgap in semiconductor materials.
Resumo:
Some differences were observed between conventional molecular-beam epitaxy (MBE) and mobility enhanced epitaxy (MEE) of InAs on a vicinal GaAs(001) substrate in the variation of the number density N of the InAs islands, with additional InAs coverage (theta - theta(c)) after the critical InAs coverage theta(c) during the two- to three-dimensional (2D-3D) transition. For MBE the variation was consistent with the power law N(theta) (theta similar to theta(c))(alpha); while for MEE, the linear relation N(theta) proportional to (theta - theta(c)) was observed. The difference is discussed in terms of the randomness in the nucleation of the InAs islands.