272 resultados para DIFFUSION LAYERS
Resumo:
Single crystalline 3C-SiC epitaxial layers are grown on φ50mm Si wafers by a new resistively heated CVD/LPCVD system, using SiH_4, C_2H_4 and H_2 as gas precursors. X-ray diffraction and Raman scattering measurements are used to investigate the crystallinity of the grown films. Electrical properties of the epitaxial 3C-SiC layers with thickness of 1 ~ 3μm are measured by Van der Pauw method. The improved Hall mobility reaches the highest value of 470cm~2/(V·s) at the carrier concentration of 7.7 * 10~(17)cm~(-3).
Resumo:
国家自然科学基金
Resumo:
Metal-semiconductor-metal (MSM) structures were fabricated by RF-plasma-assisted MBE using different buffer layer structures. One type of buffer structure consists of an AlN high-temperature buffer layer (HTBL) and a GaN intermediate temperature buffer layer (ITBL), another buffer structure consists of just a single A IN HTBL. Systematic measurements in the flicker noise and deep level transient Fourier spectroscopy (DLTFS) measurements were used to characterize the defect properties in the films. Both the noise and DLTFS measurements indicate improved properties for devices fabricated with the use of ITBL and is attributed to the relaxation of residue strain in the epitaxial layer during growth process. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
980nm InGaAs/InGaAsP/AlGaAs strained quantum well lasers,vitta novel large optical cavity and asymmetrical claddings was fabricated bg MOCVD. Very high differential quantum efficiency elf 90% (1.15W/A) and low vertical divergence angle of 24 degrees at long cavity length were obtained for 100 mu m stripe lasers. The differential quantum efficiency is up to 94% (1.20) at cavity length of 500 mu m.
Resumo:
Open-tube Ga diffusion into a SiO2/Si structure was used for fabrication of the high speed thyristor. The advantages of open-tube Ga diffusion are as follows; it is easier to operate and easier to control the profile of the Ga concentration during processing, a clean surface, which is free from alloy spots can be obtained, this technique ensures to improve the on-state characteristics and dynamic characteristics.
Resumo:
We have designed and fabricated the visible vertical-cavity surface-emitting lasers (VCSEL's) by using metalorganic vapor phase epitaxy (MOVPE). We use the 8 lambda optical cavities with 3 quantum wells in AlGaInP/AlGaAs red VCSEL's to reduce the drift leakage current and enhance the model gain in AlGaInP active region. The structure has a p-type stack with 36 DBR pairs on the top and an n-type with 55-1/2 pairs on the bottom. Using micro-area reflectance spectrum, we try to get a better concordance between the center wavelength of DBR and the emitting wavelength of the active region. We used a component graded layer of 0.05 lambda thick (x = 0.5 similar to 0.9) at the p-type DBR AlGaAs/AlAs interface to reduce the resistance of p-type DBR. We use selective oxidation to define the current injection path. Because the oxidation rate of a thick layer is faster than a thinner one, we grown a thick AlAs layer close to the active region. In this way, we got a smaller active region for efficient confinement of injected carriers (the aperture area is 3 x 3 mu m) to reduce the threshold and, at the same time, a bigger conductive area in the DBR layers to reduce the resistance. We employ Zn doping on the p-side of the junction to improve hole injection and control the Zn dopant diffusion to get proper p-i-n junction. At room temperature, pulse operation of the laser has been achieved with the low threshold current of 0.8mA; the wavelength is about 670nm.
Resumo:
The behaviors of lateral propagating modes in the aperture and the oxidized regions are investigated numerically for selectively oxidized vertical-cavity surface-emitting lasers (VCSELs). The results show that the lateral propagating modes in the oxidized region are greatly affected by the oxide layer due to its low index, the modes are divergence for the VCSELs with sufficient thick double oxide layers. So the coupling between the modes in the aperture and oxidized regions is very weak, and we can expect that the lateral spontaneous emission is greatly affected in this case. Ignoring the contribution of the lateral spontaneous emission, we calculate spontaneous emission factor by counting the total number of the guided modes in selectively oxidized VCSELs with double oxide layers. The results agree very well with the reported measurements and are inversely proportional to the lateral index step.
Resumo:
Raman scattering measurement has been used to study the residual strains in the thin 3C-SiC/Si(001) epilayers with a variation of film thickness from 0.1 to 1.2 mu m. which were prepared by chemical vapor deposition (CVD)growth. Two methods have been exploited to figure our the residual strains and the exact LO bands. The final analyzing results show that residual strains exist in the 3C-SiC epilayers. The average stress is 1.3010 GPa, and the relative change of the lattice constant is 1.36 parts per thousand. Our measurements also show that 3C-SiC phonons are detectable even for the samples with film thickness in the range of 0.1 to 0.2 mu m. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
Resumo:
The annealing of Mg-doped GaN with Pt and Mo layers has been found to effectively improve the hole concentration of such material by more than 2 times as high as those in the same material without metal. Compared with the Ni and Mo catalysts, Pt showed good activation effect for hydrogen desorption and ohmic contact to the Ni/Au electrode. Despite the weak hydrogen desorption, Mo did not diffuse into the GaNepilayer in the annealing process, thus suppressing the carrier compensation phenomenon with respect to Ni and Pt depositions, which resulted in the high activation of Mg acceptors. For the GaN activated with the Ni, Pt, and Mo layers, the blue emission became dominant, followed by a clear peak redshift and the degradation of photoluminescence signal when compared with that of GaN without metal.
Resumo:
This work was supported by the 863 High Technology R&D Program of China (Grant Nos. 2007AA03Z402 and 2007AA03Z451), the Special Funds for Major State Basic Research Project (973 program) of China (Grant No. 2006CB604907), and the National Science Foundation of China (Grant Nos. 60506002 and 60776015). The authors express their appreciation to Dr. Tieying Yang and Prof. Huanhua Wang (Beijing Synchrotron Radiation Facility, Institute of High Energy Physics, Chinese Academy of Sciences) for XRD measurements and helpful discussions.