Metalorganic vapor-phase epitaxial growth of GaAs doped with isovalent Sb is reported. By increasing the trimethylantimony concentration during growth the total Sb concentration was varied between 1 X 10(17)-1 X 10(19) cm-3. A new deep level defect with an activation energy of the thermal emission rates of E(c) - 0.54 eV is observed. The defect concentration increases with increasing As partial pressure and with increasing Sb doping. It is also found that the EL2 concentration decreases with increasing Sb doping. The new energy level is suggested to be the 0/ + transition of the Sb(Ga) heteroantisite defect. No photocapacitance quenching effect, reflecting a metastable state as seen for EL2 (As(Ga)), is observed for Sb(Ga).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Alternating layers of Si(200 angstrom thick) and Ce(200 angstrom thick) up to 26 layers altogether were deposited by electron evaporation under ultrahigh vacuum conditions on Si(100) substrate held at 150-degrees-C. Isothermal, rapid thermal annealing has been used to react these Ce-Si multilayer films. A variety of analytical techniques has been used to study these multilayer films after annealing, and among these are Auger electron spectroscopy, Rutherford backscattering, X-ray diffraction, and high resolution transmission electron microscopy. Intermixing of these thin Ce-Si multilayer films has occurred at temperatures as low as 150-degrees-C for 2 h, when annealed. Increasing the annealing temperature from 150 to 400-degrees-C for 1 h, CeSi2 forms gradually and the completion of reaction occurs at approximately 300-400-degrees-C. During the formation of CeSi2 from 150-400-degrees-C, there is some evidence for small grains in the selected area diffraction patterns, indicating that CeSi2 crystallites were present in some regions. However, we have no conclusive evidence for the formation of epitaxial CeSi2 layers, only polycrystals were formed when reacted in the solid phase even after rapid thermal anneal at 900-degrees-C for 10 s. The formation mechanism has also been discussed in combining the results of the La-Si system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using photoemission spectroscopy and Auger electron spectroscopy, the interfacial formation process and the reactions between Al and hydrogenated amorphous Si are probed, and annealing behaviors of the Al/a-Si:H system are investigated as well. It is found that a three-dimensional growth of Al metal clusters which includes reacted Al and non-reacted metal Al occurs at the initial Al deposition time, reacted Al and Si alloyed layers exist in the Al/a-Si:H interface, and non-reacted Al makes layer-by-layer growth forming a metal Al layer on the sample surface. The interfacial reactions and element interdiffusion of Al/a-Si:H are promoted under the vacuum annealing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have studied the vertical transport and formation mechanisms of electric field domains in doped weakly-coupled GaAs/AlAs superlattices. Under hydrostatic pressure two kinds of sequential resonant tunneling are observed within the pressure range from 0 to 4.5 kbar. A transition from Gamma-Gamma to Gamma-X sequential resonant tunneling occurs at P-t approximate to 1.6 kbar. For P < P-t, the high electric field domain is formed by the Gamma-Gamma process, while for P > P-t it is preferentially formed by the Gamma-X process.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

CdS clusters in zeolite-Y have been prepared by the exchange of Cd2+ into the zeolite following by sulfurization with Na2S in solution. Blue-shifts from the bulk caused by quantum size effect and the change of absorption upon CdS loading are observed. Two absorption bands are detected for one of the sample and are assigned to the 1s-1s band and exciton transition, respectively. The exciton feature is more pronounced in the excitation spectrum than in the absorption spectrum, and the luminescence excited at the exciton band is stronger than that at the 1s-1s band. Copyright (C) 1996 Elsevier Science Ltd

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fe-N films were deposited on Si(100) and GaAs(100) substrates at room temperature by ion beam assisted deposition under various N/ Fe atomic arrival ratio, 0.09, 0.12, 0.15. The results of X-ray diffraction indicated that the film deposited at 0.12 of N/Fe arrival ratio contained a considerable fraction of the Fe16N2 phase which had grown predominantly in the [001] orientation. For the larger N/Fe arrival ratio, a martensite phase with 15 at.% nitrogen was obtained. It was found that a lower deposition temperature (<200 degrees C) was necessary for the formation of the Fe16N2 phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

PbS clusters in zeolite-Y have been prepared with the reaction of Pb2+-ion-exchanged zeolite-Y with Na2S in solution at room temperature. Their absorption spectra show dramatic blue shifts from that of the bulk PbS. Obvious change of both the absorption edges and peak positions upon PbS concentrations have been observed. These phenomena provide evidences that PbS clusters have been formed within the zeolite. The absorption spectra show featureless structure and have no tails near the absorption edges. As the PbS loading density becomes higher, the absorption bands become stronger and sharpen. Order PbS clusters lattice with high quality might be formed in the supercages of zeolite-Y. (C) 1996 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

于2010-11-23批量导入

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Deep defects in annealed InP have been investigated by deep level transient capacitance spectroscopy (DLTS), photo induced current transient spectroscopy (PICTS) and thermally stimulated current spectroscopy (TSC). Both DLTS results of annealed semiconducting InP and PICTS and TSC results of annealed semi-insulating InP indicate that InP annealed in phosphorus ambient has five defects, while lid? annealed in iron phospbide ambient has two defects. Such a defect formation phenomenon is explained in terms of defect suppression by the iron atom diffusion process. The correlation of the defects and the nature of the defects in annealed InP are discussed based on the results.