968 resultados para Phase change films


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Device-quality a-Si:H films were prepared by glow discharge CVD with pure or H-diluted silane as well as by hot-wire CVD. The hydrogen content was varied from similar to 2 to 15 at. %. The Si-H bond absorption and its light-soaking-induced changes were studied by IR and differential IR absorption spectroscopes. The results indicate that the more stable sample exhibits an increase of the absorption at wave number similar to 2000 cm(-1), and the less stable one exhibits a decrease at similar to 2040 cm(-1) and an increase at similar to 1880 cm(-1).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

High quality hydrogenated amorphous silicon (a-Si:H) films have been prepared by a simple "uninterrupted growth/annealing" plasma enhanced chemical vapor deposition (PECVD) technique, combined with a subtle boron-compensated doping. These a-Si:H films possess a high photosensitivity over 10(6), and exhibit no degradation in photoconductivity and a low light-induced defect density after prolonged illumination. The central idea is to control the growth conditions adjacent to the critical point of phase transition from amorphous to crystalline state, and yet to locate the Fermi level close to the midgap. Our results show that the improved stability and photosensitivity of a-Si:H films prepared by this method can be mainly attributed to the formation of a more robust network structure and reduction in the precursors density of light-induced metastable defects.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A novel pulsed rapid thermal processing (PRTP) method has been used for realizing the solid-phase crystallization of amorphous silicon films prepared by PECVD. The microstructure and surface morphology of the crystallized films are investigated by X-ray diffraction (XRD) and atomic force microscopy (AFM). The results indicate that this PRTP is a suitable post-crystallization technique for fabricating large-area polycrystalline silicon films with good structural qualities such as large grain size, small lattice microstain and smooth surface morphology on low-cost substrate.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Wurtzite single crystal GaN films have been grown onto a gamma-Al2O3/Si(001) substrate in a horizontal-type low pressure MOVPE system. A thin gamma-Al2O3 layer is an intermediate layer for the growth of single crystal GaN on Si although it is only an oriented polycrystal film as shown by reflection high electron diffraction. Moreover, the oxide is not yet converted to a fully single crystal film, even at the stage of high temperature for the GaN layer as studied by transmission electron microscopy. Double crystal x-ray linewidth of (0002) peak of the 1.3 mu m sample is 54 arcmin and the films have heavy mosaic structures. A near band edge peaking at 3.4 eV at room temperature is observed by photoluminescence spectroscopy. Raman scattering does not detect any cubic phase coexistence.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

CMOS/SOS devices have lower carriers mobility and higher channel leakage current than bulk silicon CMOS devices. These mainly results from the defects of heteroepitaxial silicon film, especially from the defects near Si-Sapphire interface. This paper describes the experiment results of CMOS/SOS devices characteristics improved by a better epitaxial silicon quality which is obtained by a modified solid phase epitaxy.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Tungsten wires were introduced into a plasma-enhanced chemical vapor deposition (PECVD) system as a catalyzer: we name this technique 'hot-wire-assisted PECVD' (HW-PECVD). Under constant deposition pressure (p(g)), gas flow ratio and catalyzer position, the effects of the hot wire temperature (T-f) on the structural properties of the poly-Si films have been characterized by X-ray diffraction (XRD), Raman scattering and Fourier-transform infrared (FTIR) spectroscopy. Compared with conventional PECVD, the grain size, crystalline volume fraction (X-e) and deposition rate were all enhanced when a high T-f was used. The best poly-Si film exhibits a preferential (220) orientation, with a full width at half-maximum (FWHM) of 0.2 degrees. The Si-Si TO peak of the Raman scattering spectrum is located at 519.8 cm(-1) with a FWHM of 7.1 cm(-1). The X-c is 0.93. These improvements are mainly the result of promotion of the dissociation of SiH4 and an increase in the atomic H concentration in the gas phase. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The increased emphasis on sub-micron CMOS/SOS devices has placed a demand for high quality thin silicon on sapphire (SOS) films with thickness of the order 100-200 nm. It is demonstrated that the crystalline quality of as-grown thin SOS films by the CVD method can be greatly improved by solid phase epitaxy (SPE) process: implantation of self-silicon ions and subsequent thermal annealing. Subsequent regrowth of this amorphous layer leads to a greater improvement in silicon layer crystallinity and channel carrier mobility, evidenced, respectively, by double crystal X-ray diffraction and electrical measurements. We concluded that the thin SPE SOS films are suitable for application to high-performance CMOS circuitry. (C) 2000 Elsevier Science S.A. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fe-N films containing the Fe16N2 phase were prepared in a high-vacuum system of ion-beam-assisted deposition (IBAD). The composition and structure of the films were analysed by Auger electron spectroscopy (AES) and X-ray diffraction (XRD), respectively. Magnetic properties of the films were measured by a vibrating sample magnetometer (VSM). The phase composition of Fe-N films depend sensitively on the N/Fe atomic arrival ratio and the deposition temperature. An Fe16N2 film was deposited successfully on a GaAs (1 0 0) substrate by IBAD at a N/Fe atomic arrival ratio of 0.12. The gram-saturation magnetic moment of the Fe16N2 film obtained is 237 emu/g at room temperature, the possible cause has been analysed and discussed. Hysteresis loops of Fe16N2 have been measured, the coercive force H-c is about 120 Oe, which is much larger than the value for Fe, this means the Fe16N2 sample exhibits a large uniaxial magnetocrystalline anisotropy. (C) 1998 Elsevier Science B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We present the theoretical results of the electronic band structure of wurtzite GaN films under biaxial strains in the (11 (2) over bar2)-plane The calculations are performed by the kappa p perturbation theory approach through using the effective-mass Hamiltonian for an arbitrary direction The results show that the transition energies decrease with the biaxial strains changing from -0 5% to 0 5% For films of (11 (2) over bar2)-plane, the strains are expected to be anisotropic in the growth plane Such anisotropic strains give rise to valence band mixing which results in dramatic change in optical polarisation property The strain can also result in optical polarisation switching phenomena Finally, we discuss the applications of these properties to the (11 (2) over bar2) plane GaN based light emitting diode and lase diode

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this paper, a serial of Bi3.4Yb0.6Ti3-xVxO12 (BYTV) thin film with different V5+ contents were deposited on Pt/Ti/SiO2/Si substrates by chemical solution deposition (CSD). The crystallized phase and electrical properties of the films were investigated using X-ray diffraction, polarization hysteresis loops, leakage current-voltage, and fatigue test. From our experimental results, it can be found that the ferroelectric properties can be improved greatly using V5+-doped in Bi3.4Yb0.6Ti3O12 (BYT) thin film, compared with the reported BYT thin film. The remanent polarization was enhanced and excellent leakage current characteristic with 10(-11)A at the bias voltage of 4V, which is much lower than the BYT thin film or some reported bismuth layer-structure ferroelectric films. Fatigue test shows that the fabricated films have good anti-fatigue characteristic after 10(10) switching cycles. (c) 2008 Published by Elsevier B.V.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

ZnO films were deposited on (100) Si substrate by radio frequency magnetron sputtering. These films were irradiated at room temperature with 308 MeV Xe-ions to a fluence of 1.0 x 10(12), 1.0 x 10(13) or 1.0 x 10(14) Xe/cm(2). Then the samples were investigated using RBS, XRD, FESEM and PL analyses. The obtained experimental results showed that the deposited ZnO films were highly c-axis orientated and of high purity, 308 MeV Xe-ion irradiations could not change the c-axis oriented. The topography and PL properties of the ZnO films varied with increasing the Xe-ion irradiation fluence. For 1.0 x 10(13) or 1.0 x 10(14) Xe/cm(2) irradiated samples, surface cracks were observed. Furthermore, it was found that the 1.0 x 10(14) Xe/cm(2) irradiated sample exhibiting the strongest PL ability. The modification of structure and PL properties induced by 308 MeV Xe-ion irradiations were briefly discussed. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Experimental data are presented to show the influence of alkyl metal phosphates, Shengli resin fraction, and NaCl, on the shear viscosity of interfacial films and the stability of emulsions. It was found that the alkyl metal phosphates and the Shengli resin fraction could enhance the shear viscosity of interfacial films and the stability of emulsions. NaCl (0.01-0.03 mol L-1) could change the shear viscosity of interfacial films containing alkyl metal phosphates and the Shengli resin fraction. The shear viscosity of interfacial films containing ethyl iron phosphate and the Shengli resin fraction decreased with the increase of the concentration of NaCl. On the other hand, NaCl could decrease the stability of the emulsions. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The microenvironment of the aqueous core phase in the black soap film of cationic surfactant cetyltrimethylammonium bromide with the anionic dye Brilliant Yellow as spectral probe has been studied by UV-vis spectroscopy. Under neutral and basic conditions, the dye aggregates in the films exist as both the acid and base forms in contrast to a preference of the base form in the bulk solutions. The specific property of black soap film, that the intrinsic pH value of the aqueous core phase insensitively responds to pH changes of the bulk solution, is directly observed through UV-vis spectra.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper reports the study of protein conformational change by Au nanoparticles (AUNPs)-amplified surface plasmon resonance (SPR) spectroscopy. Taking cytochrome c (Cyt c) as an example, this paper gives a detailed description of the construction of metal-protein-metal sandwich nanostructure consisting of an Au film underlayer, a cytochrome c intermediate layer and an AuNPs upper layer. The incorporation of AuNPs into SPR biosensing results in increased SPR sensitivity to protein conformational change as demonstrated by acid denaturation of Cyt c. It suggests the conformational change of surface-confined Cyt c leads to the distance and electromagnetic coupling variations of Au film-AuNPs.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The phase behaviors of comblike block copolymer A(m+1)B(m)/homopolymer A mixtures are studied by using the random phase approximation method and real-space self-consistent field theory. From the spinodals of macrophase separation and microphase separation, we can find that the number of graft and the length of the homopolymer A have great effects on the phase behavior of the blend. For a given composition of comblike block copolymer, increasing the number of graft does not change the macrophase separation spinodal curve but decreases the microphase separation region. The addition of a small quantity of long-chain homopolymer A increases the microphase separation of comblike block copolymer/homopolymer A mixture.