For large size- and chemical-mismatched isovalent semiconductor alloys, such as N and Bi substitution on As sites in GaAs, isovalent defect levels or defect bands are introduced. The evolution of the defect states as a function of the alloy concentration is usually described by the popular phenomenological band anticrossing (BAC) model. Using first-principles band-structure calculations we show that at the impurity limit the N-(Bi)-induced impurity level is above (below) the conduction- (valence-) band edge of GaAs. These trends reverse at high concentration, i.e., the conduction-band edge of GaAs1-xNx becomes an N-derived state and the valence-band edge of GaAs1-xBix becomes a Bi-derived state, as expected from their band characters. We show that this band crossing phenomenon cannot be described by the popular BAC model but can be naturally explained by a simple band broadening picture.
Resumo:
The rapid thermal annealing temperature dependence of the recrystallization, Yb migration and its optical activation were studied for Yb-implanted silicon. For the annealing regime 800-1000-degrees-C, the Yb segregates both at the crystal/amorphous interface and at the surface, which is different from the usual segregation of Er at the crystal/amorphous interface, and the efficiency of optical activation also increases with annealing temperature. However, the amorphous layer regrows completely and no photoluminescence is observed after the annealing at 1200-degrees-C.
Resumo:
We report fundamental changes of the radiative recombination in a wide range of n-type and p-type GaAs after diffusion with the group-I element Li. These optical properties are found to be a bulk property and closely related to the electrical conductivity of the samples. In the Li-doped samples the radiative recombination is characterized by emissions with excitation-dependent peak positions which shift to lower energies with increasing degree of compensation and concentration of Li. These properties are shown to be in qualitative agreement with fluctuations of the electrostatic potential in strongly compensated systems. For Li-diffusion temperatures above 700-800-degrees-C semi-insulating conditions with electrical resistivity exceeding 10(7) OMEGA cm are obtained for all conducting starting materials. In this heavy Li-doping regime, the simple model of fluctuating potentials is shown to be inadequate for explaining the. experimental observations unless the number of charged impurities is reduced through complexing with Li. For samples doped with low concentrations of Li, on the other hand, the photoluminescence properties are found to be characteristic of impurity-related emissions.
Resumo:
Solid films containing phosphorus impurities were formed on p-type silicon wafer surface by traditional spin-on of commercially available dopants. The doping process is accomplished by irradiating the sample with a 308 nm XeCl pulsed excimer laser. Shallow junctions with a high concentration of doped impurities were obtained. The measured impurity profile was ''box-like'', and is very suitable for use in VLSI devices. The characteristics of the doping profile against laser fluence (energy density) and number of laser pulses were studied. From these results, it is found that the sheet resistance decreases with the laser fluence above a certain threshold, but it saturates as the energy density is further increased. The junction depth increases with the number of pulses and the laser energy density. The results suggest that this simple spin-on dopant pre-deposition technique can be used to obtain a well controlled doping profile similar to the technique using chemical vapor in pulsed laser doping process.
Resumo:
Recently, we reported successful growth of high-quality GaAs/Si epilayers by using a very thin amorphous Si film as buffer layer. In this paper, the impurity properties of this kind of GaAs/Si epilayers have been studied by using PL spectrum, SIMS and Hall measurement. Compared to a typical PL spectrum of the GaAs/Si epilayers grown by conventional two-step method, a new peak was observed in our PL spectrum at the energy of 1.462 eV, which is assigned to the band-to-silicon acceptor recombination. The SIMS analysis indicates that the silicon concentration in this kind of GaAs/Si epilayers is about 10(18) cm(-3). But its carrier concentration (about 4 x 10(17) cm(-3)) is lower than the silicon concentration. The lower carrier concentration in this kind of GaAs/Si epilayer can be interpreted both as the result of higher compensation and as the result of the formation of the donor-defect complex. We also found that the high-quality and low-Si-concentration GaAs/Si epilayers can be regrown by using this kind of GaAs/Si epilayer as substrate. The FWHM of the X-ray (004) rocking curve from this regrowth GaAs epilayer is 118 '', it is much less than that of the first growth GaAs epilayer (160 '') and other reports for the GaAs/Si epilayer grown by using conventional two-step method (similar to 200 '').
Quantum Well Intermixing of InGaAsP QWs by Impurity Free Vacancy Diffusion Using SiO_2 Encapsulation
Resumo:
Experiment on quantum well intermixing (QWI) of InGaAsP QWs by impurity free vacancy diffusion (IFVD) using SiO_2 encapsulation is reported. A maximum band gap wavelength blue-shift as large as 200nm is realized. Furthermore, an FP laser blue-shifted 21nm by QWI is fabricated with characteristics comparable with the asgrown one.
Resumo:
Properties of Fe-doped semi-insulating (SI) InP with different iron concentrations are studied by using Hall effect, current-voltage (I-V), photoluminescence spectroscopy (PL) and photocurrent spectroscopy (PC) measurements. I-V characteristics of SI InP strongly depend on Fe doping concentration. Fe doping concentration also influences optical properties and defective formation in as-grown SI InP. Band-gap narrowing phenomenon and defects in Fe doped SI InP are studied using PI and PC.
Resumo:
The free electron concentration of as-grown liquid encapsulated Czochralski (LEC) InP measured by Hall effect is much higher than the concentration of net donor impurity determined by glow discharge mass spectroscopy. Evidence of the existence of a native donor hydrogen-indium vacancy complex in LEC undoped and Fe-doped InP materials can be observed with infrared absorption spectra. The concentration increase of the donor complex correlates with the increase of ionized deep acceptor iron impurity Fe~(2+) concentration in Fe-doped semi-insulating (SI) InP. These results indicate that the hydrogen-indium vacancy complex is an important donor defect in as-grown LEC InP, and that it has significant influence on the compensation in Fe-doped SI InP.
Resumo:
于2010-11-23批量导入
Resumo:
Argon gas, as a protective environment and carrier of latent heat, has an important effect on the temperature distribution in crystals and melts. Numeric simulation is a potent tool for solving engineering problems. In this paper, the relationship between argon gas flow and oxygen concentration in silicon crystals was studied systematically. A flowing stream of argon gas is described by numeric simulation for the first time. Therefore, the results of experiments can be explained, and the optimum argon flow with the lowest oxygen concentration can be achieved. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
GaN epilayers grown on pre-nitridated (0001) sapphire substrates by metallorganic vapor phase epitaxy were investigated by wavelength dispersive X-ray spectroscopy and energy dispersive S-ray spectroscopy. Precipitates were observed to mainly consist of O impurity whose strengths were weaker than surrounding matrix. The precipitates were larger in size and distributed more sparsely and inhomogeneously in < 11-20 > directions of the epilayers grown on substrates pre-nitridated for longer periods. The larger precipitates often joined to cracks in the TEM specimens. The crack formation seems to be attributed to the compressive stress concentration at edge angles of the larger precipitates. Yellow luminescence of the epilayers was imaged by cathodoluminescence. The distribution similarity between the cathodoluminescence and the precipitates suggested that the precipitates were responsible for the yellow luminescence band. (C) 2000 Elsevier Science S.A, All rights reserved.