238 resultados para Selective Oxidation
Resumo:
A macro matrix solid-phase dispersion (MSPD) method was developed to extract 266 pesticides from apple juice samples prior to gas chromatography-mass selective detection (GC-MSD) determination. A 10 g samples was mixed with 20 g diatomaceous earth. The mixture was transferred into a glass column. Pesticide residues were leached with a 160 mL hexane-dichloromethane (1:1) at 5 mL/min. Two hundred and sixty-six pesticides were divided into three groups and detected by GC-MSD under selective ion monitoring. The proposed method takes advantage of both liquid-liquid extraction and conventional MSPD methods. Application was illustrated by the analysis of 236 apple juice samples produced in Shaanxi province China mainland this year. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
We present the monolithic integration of a sampled-grating distributed Bragg reflector (SC-DBR) laser with a quantum-well electroabsorption modulator (QW-EAM) by combining ultra-low-pressure (55 mbar) selective-area-growth (SAG) metal-organic chemical vapour deposition (MOCVD) and quantum-well intermixing (QWI) for the first time. The QW-EAM and the gain section can be grown simultaneously by using SAG MOCVD technology. Meanwhile, the QWI technology offers an abrupt band-gap change between two functional sections, which reduces internal absorption loss. The experimental results show that the threshold current I-th = 62 mA, and output power reaches 3.6 mW. The wavelength tuning range covers 30 nm, and all the corresponding side mode suppression ratios are over 30 dB. The extinction ratios at available wavelength channels can reach more than 14 dB with bias of -5 V.
Resumo:
A new method for fabricating electroabsorption modulator integrated with a distributed feedback laser (EML) was proposed. With the method we fabricated a selective area growth double stack active layer EML (SAG-DSAL-EML). Through comparing with other fabrication methods of EMLs, the characters and the merits of the new method presented in this paper were discussed.
Resumo:
Narrow stripe selective MOVPE has been used to grow high quality oxide-free InGaAlAs layers on an InP substrate patterned with SiO2 masks at optimized growth conditions. Mirror-like surface morphologies and abrupt cross sections are obtained in all samples without spike growth at the mask edge. For the narrow stripe selectively grown InGaAlAs layers with a mesa width of about 1.2 mu m, a bandgap wavelength shift of 70 nm, a photoluminescence (PL) intensity of more than 80% and a PL full width at half maximum (FWHM) of less than 60 meV are obtained simultaneously with a small mask width variation from 0 to 40 mu m. The characteristics of the thickness enhancement ratio and the PL spectrum dependence on the mask width are presented and explained by considering both the migration effect from a masked region and the lateral vapour diffusion effect.
Resumo:
A distributed-feedback (DFB) laser and a high-speed electroabsorption (EA) modulator are integrated, on the basis of the selective area MOVPE growth (SAG) technique and the ridge waveguide structure, for a 10 Gbit s(-1) optical transmission system. The integrated DFB laser/EA modulator device is packaged in a compact module with a 20% optical coupling efficiency to the single-mode fibre. The typical threshold current is 15 mA, and the side-mode suppression ratio is over 40 dB with the single-mode operation at 1550 nm. The module exhibits 1.2 mW fibre output power at a laser gain current of 70 mA and a modulator bias voltage of 0 V. The 3 dB bandwidth is 12 GHz. A dynamic extinction ratio of over 10 dB has been successfully achieved under 10 Gbit s(-1) non-return to zero (NRZ) operation, and a clearly open eye diagram is obtained.
Resumo:
Resumo:
A novel integration technique has been developed using band-gap energy control of InGaAsP/InGaAsP multi-quantum-well (MQW) structures during simultaneous ultra-low-pressure (22 mbar) selective-area-growth (SAG) process in metal-organic chemical vapour deposition. A fundamental study of the controllability of band gap energy by the SAG method is performed. A large band-gap photoluminescence wavelength shift of 83nm is obtained with a small mask width variation (0-30 mu m). The method is then applied to fabricate an MQW distributed-feedback laser monolithically integrated with an electroabsorption modulator. The experimental results exhibit superior device characteristics with low threshold of 19 mA, over 24 dB extinction ratio when coupled into a single mode fibre. More than 10GHz modulation bandwidth is also achieved, which demonstrates that the ultra-low-pressure SAG technique is a promising approach for high-speed transmission photonic integrated circuits.
Resumo:
The design and basic characteristics of a strained InGaAsP-InP multiple-quantum-well (MQW) DFB laser monolithically integrated with an electroabsorption modulator (EAM) by ultra-low-pressure (22 mbar) selective-area-growth (SAG) MOCVD are presented. A fundamental study of the controllability and the applicability of band-gap energy by using the SAG, method is performed. A large band-gap photoluminescence wavelength shift of 88 mn. was obtained with a small mask width variation (0-30 mu m). The technique is then applied to fabricate a high performance strained MQW EAM integrated with a DFB laser. The threshold current of 26 mA at CW operation of the device with DFB laser length of 300 mu m and EAM length of 150 mu m has been realized at a modulator bias of 0 V. The devices also exhibit 15 dB on/off ratio at an applied bias voltage of 5 V.
Resumo:
Under selective photo-excitation, the capacitance response of internal tunnelling coupling in quantum-dots-imbedded heterostructures is studied to clarify the electronic states and the number densities of electrons filling in the quantum dots (QDs). The random nature for both optical transitions and the filling in a QD assembly makes highly resolved capacitance peaks appear in the C-V characteristic after turning off the photo-excitation.
Resumo:
The exponential degradation of the photoluminescence (PL) intensity at the near-band-gap was observed in heavily doped or low-quality GaN with pristine surface under continuous helium-cadmium laser excitation. In doped GaN samples, the degradation speed increased with doping concentration. The oxidation of the surface with laser irradiation was confirmed by x-ray photoemission spectroscopy measurements. The oxidation process introduced many oxygen impurities and made an increase of the surface energy band bending implied by the shift of Ga 3d binding energy. The reason for PL degradation may lie in that these defect states act as nonradiative centers and/or the increase of the surface barrier height reduces the probability of radiative recombination.
Resumo:
The three-dimensional morphology of In(Ga)As nanostructures embedded in a GaAs matrix is investigated by combining atomic force microscopy and removal of the GaAs cap layer by selective wet etching. This method is used to investigate how the morphology of In(Ga)As quantum dots changes upon GaAs capping and subsequent in situ etching with AsBr3. A wave function calculation based on the experimentally determined morphologies suggests that quantum dots transform into quantum rings during in situ etching. (c) 2007 American Institute of Physics.
Resumo:
Fabrication of InGaAlAs MQW buried heterostructure (BH) lasers by narrow stripe selective MOVPE is demonstrated in this paper. High quality InGaAlAs MQWs were first grown by narrow stripe selective MOVPE without any etching process and assessed by analysing the cross sections and PL spectrums of the InGaAlAs MQWs. Furthermore, BHs were fabricated for the InGaAlAs MQW lasers by a developed unselective regrowth method, instead of conventional selective regrowth. The InGaAlAs MQW BH lasers exhibit good device characteristics, with a high internal differential quantum efficiency of 85% and a low internal loss of 6.7 cm(-1). Meanwhile, narrow divergence angles of the far field pattern are obtained for the fabricated lasers.
Resumo:
A buried grating structure with a selectively grown absorptive InGaAsP layer was fabricated and characterized by scanning electron microscopy and photoluminescence. The InP corrugation was etched by introducing a SiO2 mask that was more stable than a conventional photoresist mask during the etching process. Moreover, the corrugation was efficaciously preserved during the selective growth of the absorptive layer with the SiO2 mask. Though this absorptive layer was only selectively grown on the concave region of the corrugation, it has a high intensity around the peak wavelength in comparison with that of InGaAlAs multiple quantum well, which was grown on the buried grating structure.
Resumo:
The chemical properties of AlxGa1-xN surfaces exposed to air for different time periods are investigated by atomic force microscopy (AFM), photoluminescence (PL) measurement and X-ray photoelectron spectroscopy (XPS). PL and AFM results show that AlxGa1-xN samples exhibit different surface characteristics for different air-exposure times and Al contents. The XPS spectra of the Al 2p and Ga 2p core levels indicate that the peaks shifted slightly, from an Al-N to an Al-O bond and from a Ga-N to a Ga-O bond. All of these results show that the epilayer surface contains a large amount of Ga and Al oxides. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Narrow stripe selective growth of oxide-free InGaAlAs/InGaAlAs multiple quantum wells (MQWs) has been successfully performed on patterned InP substrates by ultra-low pressure MOVPE. Flat and clear interfaces were obtained for the narrow stripe selectively grown MQWs under optimized growth conditions. These selectively grown MQWs were covered by specific InP layers, which can keep the MQWs from being oxidized during the fabrication of the devices. The characteristics of selectively grown MQWs were strongly dependent on the mask stripe width. In particular, a PL peak wavelength shift of 73 nm, a PL intensity of more than 57% and a PL FWHM of less than 102 meV were observed simultaneously with a small mask stripe width varying from 0 to 40 mu m. The results were explained by considering the migration effect from the masked region (MMR) and the lateral vapour diffusion effect (LVD).