We have fabricated 1.3-mu m InAs-GaAs quantum-dot (QD) lasers with and without p-type modulation doping and their characteristics have been investigated. We find that introducing p-type doping in active regions can improve the temperature stability of 1.3-mu m InAs-GaAs QD lasers, but it does not, increase the saturation modal gain of the QD lasers. The saturation modal gain obtained from the two types of lasers is identical (17.5 cm(-1)). Moreover, the characteristic temperature increases as cavity length increases for the two types of lasers, and it improves more significantly for the lasers with p-type doping due to their higher gain.
Resumo:
The characteristics of V-defects in quaternary AlInGaN epilayers and their correlation with fluctuations of the In distribution are investigated. The geometric size of the V-defects is found to depend on the In composition of the alloy. The V-defects are nucleated within the AlInGaN layer and associated with threading dislocations. Line scan cathodoluminescence (CL) shows a redshift of the emission peak and an increase of the half width of the CL spectra as the electron beam approaches the apex of the V-defect. The total redshift decreases with decreasing In mole fraction in the alloy samples. Although the strain reduction may partially contribute to the CL redshift, indium segregation is suggested to be responsible for the V-defect formation and has a main influence on the respective optical properties. (C) 2004 American Institute Of Physics.
Resumo:
The influences of a high-temperature (HT) AlN interlayer (IL) on the phase separation in crack-free AlGaN grown on GaN have been studied. The depth-dependent cathodoluminescence (CL) spectra indicate a relatively uniform Al distribution in the growth direction, but the monochromatic CL images and the CL spectra obtained by line scan measurements reveal a lateral phase separation in AlGaN grown on relatively thick HT-AlN ILs. Moreover, when increasing the thickness of HT-AlN IL, the domain-like distribution of the AlN mole fraction in AlGaN layers is significantly enhanced through a great reduction of the domain size. The morphology of mesa-like small islands separated by V trenches in the HT-AlN IL, and the grain template formed by the coalescence of these islands during the subsequent AlGaN lateral overgrowth, are attributed to be responsible for the formation of domain-like structures in the AlGaN layer. (c) 2005 American Institute of Physics.
Resumo:
Quasi-aligned ZnO nanotubes have been grown on silicon substrates by metalorganic chemical vapor deposition without using any catalyst. Two kinds of ZnO nanotubular structures were found: Nanotubes with single walls and nanotubes with double walls. The nanotubes were grown along the [001] direction. Room-temperature photoluminescence measurements of the ZnO nanotubes indicate strong ultraviolet emission and weak green emission. A new growth mode for these ZnO nanotubes is proposed, which can be used to prepare other nanotubular structures. (c) 2005 American Institute of Physics.
Resumo:
We have successfully grown self-assembled InxGa1-xAs (x = 0.44, 0.47, 0.50) quantum dots (QDs) with high density (> 10(11)/cm(2)) by MBE. The effect of In content on the high-density QD is investigated by atomic force microscopy (AFM) and photoluminescence (PL) spectra. It is found that sample with In-mole-fraction of 0.5 shows small size fluctuation and high PL intensity. The influence of growth temperature on high-density QD is also investigated in our experiment. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The subband structure and inter-subband transition as a function of gate voltage are determined by solving the Schrodinger and Poisson equations self-consistently in an AlxGa1-xN/GaN heterostructure. Different aluminum mole fraction and thickness of AlxGa1-xN barrier are considered. Calculation results show that energy difference between the first and second subband covers a wide range (from several tens to hundreds milli-electron volt) by applying different gate voltage, which corresponds to the midinfrared and long-wave infrared wavelength scope. Furthermore, such a modulation on the subband transition energy is much more pronounced for the structure with thin barrier. When the applied positive gate voltage is increased, the triangle well formed at the interface turns to be deeper and narrower, which enhances the confinement for electrons. As a result, the overlap between electron wave function at two subbands increases, and thus the optical intersubband transition also enhances its intensity. This tendency is in good agreement with the available data in the literature. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Crack-free In0.08Al0.25Ga0.67N quaternary films, with and without thick (> 1.5 mum) high-temperature-GaN (HTGaN) interlayer, have been grown on Si(1 1 1) substrates by a low-pressure metalorganic chemical vapor deposition (MOCVD) system. Mole fractions of In and Al in quaternary alloy layers are determined by Energy dispersive spectroscopy (EDS) and Rutherford backscattering spectrometry (RBS), which are recorded as similar to8% and similar to25-27%, respectively. High-resolution X-ray diffraction (HRXRD) and room temperature photoluminescence (RT-PL) results evidence the film's single crystal structure and the existence of local In- and/or Al-rich regions. Compared with GaN film grwon on Si(1 1 1) substrate, no crack is observed in the quaternary ones. Two explanations are proposed. First, mismatch-induced strain is relaxed significantly due to gradual changes of In concentration. Second, the weak In-N bond is likely to break when the sample is cooled down to the room temperature, which is expected to favor the releasing of thermal stress. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
We have demonstrated a passively Q-switched and mode-locked Nd:YVO4 laser with an intracavity composite semiconductor saturable absorber (ICSSA). Stable Q-switched and mode-locked pulses with Q-switched envelope pulse duration of 180 ns and pulse repetition rate of 72KHz have been obtained. The maximum average output power was 1.45W at 8W incident pump power. The repetition rate of the mode-locked pulses inside the Q-switched envelope was 154 MHz. Experimental results revealed that this ICSSA was suitable for Q-switched and mode-locked solid-state lasers. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Passive mode locking of a solid-state Nd:GdVO4 laser is demonstrated. The laser is mode locked by use of a semiconductor absorber mirror (SAM). A low Nd3+ doped Nd:GdVO4 crystal is used to mitigate the thermal lens effect of the laser crystal at a high pump power. The maximum average output power is up to 6.5 W, and the pulse duration is as short as 6.2 ps. The optic-to-optic conversion efficiency is 32.5% and the repetition rate is about 110 MHz.
Resumo:
Six-period 4 nm GaN/10 nm AlxGa1-xN superlattices with different Al mole fractions x were prepared on (0001) sapphire substrates by low-temperature metal-organic chemical vapor deposition. The linear electro-optic (Pockels) effect was studied by a polarization-maintaining fiber-optical Mach-Zehnder interferometer system with an incident light wavelength of 1.55 mu m. The measured electro-optic coefficients, gamma(13)=5.60 +/- 0.18 pm/V, gamma(33)=19.24 +/- 1.21 pm/V (for sample 1, x=0.3), and gamma(13)=3.09 +/- 0.48 pm/V, gamma(33)=8.94 +/- 0.36 pm/V (for sample 2, x=0.1), respectively, are about ten times larger than those of GaN bulk material. The enhancement effect in GaN/AlxGa1-xN superlattice can be attributed to the large built-in field at the interfaces, depending on the mole fraction of Al. (C) 2007 American Institute of Physics.
Resumo:
A high-power continuous wave (cw) mode-locked Nd:YVO4 solid-state laser was demonstrated by use of a semiconductor absorber mirror (SAM). The maximum average output power was 8.1 W and the optic-to-optic conversion efficiency was about 41 %. At the maximum incident pump power, the pulse width was about 8.6 ps and the repetition rate was 130 MHz. Experimental results indicated that this absorber was suitable for high power mode-locked solid-state lasers. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
We present a new way to meet the amount of strain relaxation in an InGaN quantum well layer grown on relaxed GaN by calculating and measuring its internal field. With perturbation theory, we also calculate the transition energy of InGaN/GaN SQWs as affected by internal fields. The newly reported experimental data by Graham et al. fit our calculations well on the assumption that the InGaN well layer suffered a 20% strain relaxation, we discuss the differences between our calculated results and the experimental data. Our calculation suggests that with the increase of indium mole fraction in the InGaN/GaN quantum well, the effect of polarization fields on the luminescence of the quantum well will increase. Moreover, our calculation also suggests that an increase in the quantum well width by only one monolayer can result in a large reduction in the transition energy. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The influence of defects on the responsivity of GaN Schottky barrier ultraviolet photodetectors with n(-)-GaN/n(+)-GaN layer structures is investigated. It is found that employing undoped GaN instead of Si-doped GaN as the n(-)-GaN layer brings about a higher responsivity due to a lower Ga vacancy concentration. On the other hand, the dislocations may increase the recombination of electron-hole pairs and enhance the surface recombination in the photodetectors. Employing undoped GaN and reducing the dislocation density in the n(-)-GaN layer are necessary to improve the responsivity of Schottky barrier photodetectors. (c) 2007 American Institute of Physics.
Resumo:
By using a composite semiconductor absorber and an output coupler, we demonstrated a Q-switched and mode-locked diode-pumped microchip Nd:YVO4 laser. With a 350-mu m-thick crystal, the width of the Q-switched envelope was as short as 12 ns; the repetition rate of the mode-locked pulses inside the Q-switched pulse was more than 10 GHz. The average output power was 335 mW at a maximum pump power of 1.6 W. Q-switched envelope widths of 21 and 31 ns were also achieved with crystals 0.7 and 1.0 mm thick, respectively.
Resumo:
The effect of Al incorporation on the AlGaN growth by metalorganic chemical vapor deposition is investigated. With the increase of trimethylalluminum (TMAl) flux, the crystal quality becomes worse, and the epilayer surface becomes rougher. An interesting phenomenon is that the growth rate of AlGaN decrease with increasing TMAl flux, which is opposite to the AlN growth rate dependence on the TMAl flux. All these effects are attributed to the different properties of At atoms due to the higher bond strength of Al-N compared with Ga-N, which lead to lower surface mobility and stronger competitive ability of Al atoms during the growth. The enhancement of the surface mobility of Al is especially important for improving the quality of AlGaN. (c) 2006 Elsevier B.V. All rights reserved.