Resumo:
gamma-LiAlO2 layers with a highly preferred (1 0 0) orientation were prepared by vapor transport equilibration (VTE) technique on (0 0 0 1) sapphire substrate. Microststructure of the gamma-LiAlO2 layers was studied by XRD and SEM. In the temperature range from 750 to 1100 degrees C, the residual stress in the gamma-LiAlO2 layers varied from tensile to compressive with the increase of VTE temperature, and the critical point of the change between tensile and compressive stress is around 975 degrees C. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
研究了中子辐照下钛宝石单晶体缺陷的形成及光学性能的变化。对温度梯度法(TGT)生长的钛宝石晶体进行中子辐照。中子能量为1.5MeV,剂量为4.32×10^18 neutrons/cm^2。辐照后194nm吸收峰强度增加,268nm吸收峰强度则降低。荧光谱检测中发现辐照使得420nm荧光峰强度明显降低,荧光峰位置也蓝移至414nm处。分析表明辐照使得钛宝石晶体内形成F^+缺陷,同时Ti^4+离子则转化成Ti^3+离子。辐照后的钛宝石在247C处有热释光TL出现,通过初始上升法计算出其陷阱深度为0.63eV。
Resumo:
The influence of mechanical polishing, chemo-mechanical polishing (CMP), as well as CMP and subsequent chemical etching on the properties of sapphire substrate surfaces has been studied. The sapphire substrates have been investigated by means of polarizing microscopy, atomic force microscopy (AFM). X-ray diffraction rocking curves (XRCs) and micro-Raman spectroscopy. The results show that CMP with subsequent chemically etching yields the best-quality sapphire substrate surfaces. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
最近,一种新型的掺铋发光材料引起了人们的关注。这种发光材料有长的荧光寿命(τ>200μs),在800nm激光激发下发射波长在1200~1600nm区间的超宽带荧光(荧光半高宽FWHM>200nm),其发光性质与以往文献中报道的Bi^3+或Bi^2+掺杂的发光材料的性质截然不同;光发射截面(σem)是光掺铒光纤放大器玻璃(EDFAG)的2~3倍,其σem×FWHM值是EDFAG的10倍左右,σem×τ值是掺Ti^3+蓝宝石的3倍左右。
Resumo:
通过研究提拉法生长的掺杂Ti浓度为0.2at%的LiAlO2晶体吸收光谱,荧光光谱和红外光谱,来分析此新型晶体的结构.分析发现光谱中仅出现了四价Ti离子的196nm的特征吸收峰,用235nm光激发得到384nm的特征发射峰;针对吸收光谱中660-820nm出现的四个弱小吸收峰提出了一个色心模型,从而解释了空气和富Li气氛处理后吸收峰消失的现象;对比纯LiAlO2晶体的红外光谱发现,Ti的掺入仅影响了[AlO4]键强,而[LiO4]及相关键强几乎不变;结合ICP测试估算出直径50mm,厚1mm的Ti:LiA
Resumo:
Sapphire crystals, 140 mm in diameter and 90 turn in height, have been grown by temperature gradient techniques (TGT). The growth direction of the boule was fixed by means of Lane X-ray diffraction. A prominent 204 nm absorption band in TGT-Al2O3. which does not appear in single crystals grown by Czochralski method has been studied. Analysis further substantiates the F-center model of this band. Two relatively weaker bands absorbing at 232 nm and 254 nm were ascribed to F+ centers. F-type centers concentration was determined using Smakula's equation. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Transparent polycrystalline MgO and TiO2 codoped Al2O3 ceramics were fabricated by conventional solid-state pressureless processing. The absorption, emission and excitation spectra of ( Mg, Ti : Al2O3 ceramics were measured. Owing to charge compensation of Mg2+, only UV absorption around 250nm was observed due to O2- -> Ti4+ charge transfer transitions (CT) when Ti content was low. As a result, the emission peaks of isolated Ti4+ ion located at 280-290nm and 410-420nm were observed. Besides absorption peak of V, ion, the characteristic absorption peak of V, ion centered at 490nm was observed in Mg, Ti) : Al2O3 ceramics when Ti content was high. The emission spectra of Ti3+, ion in polycrystalline Al2O3 ceramics coincide with that of Ti: Al2O3 single crystal.
Resumo:
ZnO thin films were grown on single-crystal gamma-LiAlO2 (LAO) and sapphire (0001) substrate by pulsed laser deposition (PLD). The structural, optical and electrical properties of ZnO films were investigated. The results show that LAO is more suitable for fabricating ZnO films than sapphire substrate and the highest-quality ZnO film was attained on LAO at the substrate temperature of 550 degrees C. However, when the substrate temperature rises to 700 degrees C, lithium would diffuse from the substrate (LAO) into ZnO film which makes ZnO film on LAO becomes polycrystalline without preferred orientation, the stress in ZnO film increases dominantly and the resistivity of the film decreases exponentially. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
LiAlO2 single crystals doped with Ti at concentration 0.2 at.% are grown by the Czochralskl technique with dimensions Phi 42 x 55 mm. Ti ions in the crystal are quadrivalence proven by comparing the absorption and fluorescence spectra of pure LiAlO2 and Ti: LiAlO2. After air and Li-rich atmosphere annealing, the absorption peaks in the range of 600-800nm disappear. We conclude that 682 and 756nm absorption peaks are attributed to the V-Li and V-O absorptions, respectively. The peaks at 716nm and 798nm may stem from the V-Li(+) and F+ absorptions. The colour-centre model can be applied to explain the experimental phenomena. Ti4+-doping produces more lithium vacancies in the LiAlO2 crystal. The intensities of [LiO4] and the associated bonds remain unchanged, which improves the anti-hydrolyzation and thermal stability of LiAlO2 crystals.
Resumo:
Using vapor transport equilibration (VTE) technique we succeeded in the fabrication of single-phase gamma-LiAlO2 layer on (0001) sapphire substrate. X-ray diffraction indicated that the as-fabricated layer was highly textured with [100] orientation at proper VTE treatment temperature range from 1050 degrees C to 1100 degrees C. The main factors affecting the quality of the gamma-LiAlO2 layer were investigated by SEM and transmission spectra. These results reveal the possibility of fabricating gamma-LiAlO2 (100)//sapphire (0001) composite substrate for GaN-based epitaxial film by VTE.
Resumo:
本文研究了不同掺Ti^3+浓度对温梯法生长的Ti:Al2O3晶体吸收光谱、荧光光谱和X射线衍射光谱的影响。根据吸收光谱提出了一个色心模型。对比了样品各处420nm荧光谱,发现掺Ti^3+浓度越大,该处荧光强度越弱,同时解释了420肿处荧光峰的起源。对比了样品各处720nm处的荧光谱,发现掺Ti^3+浓度越大,该处荧光强度越强。X射线衍射谱(XRD)表明,衍射峰强度随掺Ti^3+浓度的增大而逐渐增强。
Resumo:
采用传统无压烧结工艺制备出透明性良好的掺Ti氧化铝陶瓷;测定了该陶瓷的吸收光谱、荧光光谱和激发光谱。结果表明,掺Ti氧化铝透明陶瓷样品在Mg与Ti掺入离子的摩尔比(NMg/NTi)较小时,表现出Ti^3+离子的490nm特征吸收峰,即^2T2→^2E跃迁产生的宽带吸收;NMg/NTi较大时,陶瓷样品吸收光谱中不存在Ti^3+离子吸收,其250nm处吸收为O^2-→Ti^4+的转移吸收。掺Ti氧化铝透明陶瓷样品Ti^3+离子的发射谱线与单晶的相吻合,同时Ti^3+在氧化铝陶瓷中分布很均匀,且Ti^3+浓度较
Resumo:
The annealing effects of sapphire substrates on the quality of epitaxial ZnO films grown by dc reactive magnetron sputtering were studied. The atomic steps formed on (0001) sapphire (alpha-Al2O3) substrates surface by annealing at high temperature were analyzed by atomic force microscopy. Their influence on the growth of ZnO films was examined by X-ray diffraction and photoluminescence measurements. Experimental results indicate that the film quality is strongly affected by annealing treatment of the sapphire substrate surface. The optimum annealing temperature of sapphire substrates for ZnO grown by magnetron sputtering is 1400 degrees C for 1 h in air.
Resumo:
本文采用提拉法成功地生长了钛掺杂浓度为0.1%原子分数的LiAlO2单晶体,借助光学显微镜,结合化学腐蚀法,对Ti:LiAlO2晶体(100)面空气退火前后的缺陷特征进行了研究,用AFM观测了(100)面晶片在不同温度下流动N2气氛退火过的表面形貌。结果表明:Ti:LiAlO2晶体(100)面的位错腐蚀坑是底面为平行四边形的锥形坑,位错密度约为5.0×104cm-2,900℃空气退火后晶片表面的位错腐蚀坑变大;N2退火能显著影响晶片的表面形貌,当退火温度为900℃时,晶片的均方根粗糙度(RMS)达到最低值
Resumo:
The laser-induced damage threshold (LIDT) and damage morphology of antireflection (AR) coatings on quartz and sapphire are investigated. A very interesting phenomena is found in the measurement. In the case of a single pulse laser, the LIDT of the AIR coatings on quartz is higher than that of sapphire. On the contrary, for a free-pulse laser, the LIDT of AIR coatings on sapphire is higher than that of quartz. (C) 2004 Society of Photo-Optical Instrumentation Engineers.