An improved 2 ×2 silicon-on-insulator Mach-Zehnder thermo-optical switch is designed and fabricated, which is based on strongly guided multimode interference couplers and single- mode phase-shifting arms. The multimode interference couplers and input/output waveguides are deeply etched to improve coupler performances and coupler-waveguide coupling efficiencies. However, shallow etching is used in the phase-shifting arms to guarantee single-mode property. The strongly guided coupler presents an attractive uniformity about 0. 03 dB and a low propagation loss of -0.6 dB. The 2× 2 switch shows an insertion loss as low as -6.8 dB, where the fiber-waveguide coupling loss of -4.3 dB is included, and the response-time is measured as short as 6.8 μs, which are much better than our previous results.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

One group of SiC films are grown on silicon-on-insulator (SOI) substrates with a series of silicon-overlayer thickness. Raman scattering spectroscopy measurement clearly indicates that a systematic trend of residual stress reduction as the silicon over-layer thickness decreases for the SOI substrates. Strain relaxation in the SiC epilayer is explained by force balance approach and near coincidence lattice model.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The simulation and analysis of S-shaped waveguide bend are presented.Bend radius larger than 30 mm assures less than 0.5 dB radiation loss for a 4-μm-wide silicon-on-insulator waveguide bend with 2-μm etch depth.Intersection angle greater than 20° provides negligible crosstalk (<-30 dB) and very low insertion loss.Any reduction in bend radius and intersection angle is at the cost of the degradation of characteristics of bent waveguide and intersecting waveguide, respectively.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A rearrangeable nonblocking thermo-optic 4×4 switching matrix,which consists of five 2×2 multimode interference-based Mach-Zehnder interferometer(MMI-MZI) switch elements,is designed and fabricated.The minimum and maximum excess loss for the matrix are 6.6 and 10.4dB,respectively.The crosstalk in the matrix is measured to be between -12 and -19.8dB.The switching speed of the matrix is less than 30μs.The power consumption for the single switch element is about 330mW.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we present simulation results of an electrooptical variable optical attenuator (VOA) inte-grated in silicon-on-insulator waveguide. The device is functionally based on free carriers absorption toachieve attenuation. Beam propagation method (BPM) and two-dimensional semiconductor device simu-lation tool PISCES-Ⅱ were used to analyze the dc and transient characteristics of the device. The devicehas a response time (including rise time and fall time) less than 200 ns, much faster than the thermoopticand micro-electromechanical systems (MEMSs) based VOAs.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Integrated multimode interference (MMI) coupler based on silicon-on-insulator(SOI) has been becoming a kind of more and more attractive device in optical systems. SiO2thin cladding layers (<1.0 μm) can be usedin SOI waveguide due to the large index step be-tween Si and SiO2, making them compatible with VLSI technology. The design and fabrica-tion of MMI optical couplers and optical switches in SOI technology are presented in thepa-per. We demonstrated the switching time of 2 × 2 MMI-MZI thermo-optical switch is less than 20 μs:

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An ultracompact 3-dB coupler is designed and fabricated in silicon-on-insulator,based on 12 line tapered multimode interference(MMI) coupler.Comparing with the conventional straigth MMI coupler,the device is-40% shorter in length.The device exhibits uniformity of 1.3dB and excess loss of 2.5dB

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A 2 x 2 Mach-Zehnder interferometer electrooptical switch integrated in silicon-on-insulator using multimode interference 3-dB couplers as splitter and combiner has been proposed and fabricated. Free carriers plasma dispersion effect was utilized to realize light modulation in silicon. Switching operation was achieved at an injection current of 358mA and which can be much reduced by optimizing the PIN structure and improving fabrication process. Extinction ratio of 7.7dB and crosstalk of 4.8dB has been observed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The authors have designed and fabricated 2x2 parabolically tapered MMI coupler with large cross-section and large space between difference ports using Silicon-on-Insulator ( SOI) technology. The devices demonstrate a minimum uniformity of 0.8dB and 30% shorter than the straight MMI coupler.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Integrated multimode interference coupler based on silicon-on-insulator has been become a kind of more and more attractive device in optical systems. Thin cladding layers (<1.0mum) can be used in SOI waveguide due to the large index step between Si and SiO2, making them compatible with the VLSI technology. Here we demonstrate the design and fabrication of multimode interference (MMI) optical couplers and optical switches in SOI technology.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Silicon-on insulator (SOI) is an attractive platform for the fabrication of optoelectronic integrated circuit. Thin cladding layers (< 1.0m) can be used in SOI waveguide due to the large index step between Si and SiO2, making them compatible with the VLSI technology. Here we demonstrate the fabrication of 1 x 4 and 2 x 2 multimode interference (MMI) coupler based on SOI technology. Performances of the devices are analyzed. The minimum excess loss of the devices is about 1.8dB. The devices show uniform power distribution.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Silicon-on-insulator (SOI) has been recognized as a promising semiconductor starting material for ICs where high speed and low power consumption are desirable, in addition to its unique applications in radiation-hardened circuits. In the present paper, three novel SOI nano-layer structures have been demonstrated. ULTRA-THIN SOI has been fabricated by separation by implantation of oxygen (SIMOX) technique at low oxygen ion energy of 45 keV and implantation dosage of 1.81017/cm2. The formed SOI layer is uniform with thickness of only 60 nm. This layer is of crystalline quality. and the interface between this layer and the buried oxide layer is very sharp, PATTERNED SOI nanostructure is illustrated by source and drain on insulator (DSOI) MOSFETs. The DSOI structure has been formed by selective oxygen ion implantation in SIMOX process. With the patterned SOI technology, the floating-body effect and self-heating effect, which occur in the conventional SOI devices, are significantly suppressed. In order to improve the total-dose irradiation hardness of SOI devices, SILICON ON INSULATING MULTILAYERS (SOIM) nano-structure is proposed. The buried insulating multilayers, which are composed of SiOx and SiNy layers, have been realized by implantation of nitride and oxygen ions into silicon in turn at different ion energies, followed by two steps of high temperature annealing process, respectively, Electric property investigation shows that the hardness to the total-dose irradiation of SOIM is remarkably superior to those of the conventional SIMOX SOI and the Bond-and-Etch-Back SOI.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

摘要: In order to improve the total-dose radiation hardness of the buried oxide of separation by implanted oxygen silicon-on-insulator wafers, nitrogen ions were implanted into the buried oxide with a dose of 10(16)cm(-2), and subsequent annealing was performed at 1100 degrees C. The effect of annealing time on the radiation hardness of the nitrogen implanted wafers has been studied by the high frequency capacitance-voltage technique. The results suggest that the improvement of the radiation hardness of the wafers can be achieved through a shorter time annealing after nitrogen implantation. The nitrogen-implanted sample with the shortest annealing time 0.5 h shows the highest tolerance to total-dose radiation. In particular, for the 1.0 and 1.5 h annealing samples, both total dose responses were unusual. After 300-krad(Si) irradiation, both the shifts of capacitance-voltage curve reached a maximum, respectively, and then decreased with increasing total dose. In addition, the wafers were analysed by the Fourier transform infrared spectroscopy technique, and some useful results have been obtained.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In the present work, a Cz-Silicon wafer is implanted with helium ions to produce a buried porous layer, and then thermally annealed in a dry oxygen atmosphere to make oxygen transport into the cavities. The formation of the buried oxide layer in the case of internal oxidation (ITOX) of the buried porous layer of cavities in the silicon sample is studied by positron beam annihilation (PBA). The cavities are formed by 15 keV He implantation at a fluence of 2 x 10(16) cm(-2) and followed by thermal annealing at 673 K for 30 min in vacuum. The internal oxidation is carried out at temperatures ranging from 1073 to 1473 K for 2 h in a dry oxygen atmosphere. The layered structures evolved in the silicon are detected by using the PBA and the thicknesses of their layers and nature are also investigated. It is found that rather high temperatures must be chosen to establish a sufficient flux of oxygen into the cavity layer. On the other hand high temperatures lead to coarsening the cavities and removing the cavity layer finally.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We experimentally demonstrate a small-size and high-speed silicon optical switch based on the free carrier plasma dispersion in silicon. Using an embedded racetrack resonator with a quality factor of 7400, the optical switch shows an extinction ratio exceeding 13 dB with a footprint of only 2.2 x 10(-3) mm(2). Moreover, a novel pre-emphasis technique is introduced to improve the optical response performance and the rise and the fall times are reduced down to 0.24 ns and 0.42 ns respectively, which are 25% and 44% lower than those without the pre-emphasis.