205 resultados para AMMONIA CONCENTRATION
Resumo:
A new method to test the hole concentration of p-type GaN is proposed, which is carried out by analyzing the spectral response of p-n(+) structure GaN ultraviolet photodetector. It is shown that the spectral response of the photodetector changes considerably with reversed bias. It is found that the difference between photodetector's quantum efficiency at two wavelengths, i.e. 250 and 361 nm, varies remarkably with increasing reversed bias. According to the simulation calculation, the most characteristic change occurs at a reversed voltage under which the p-GaN layer starts to be completely depleted. Based on this effect the carrier concentration of p-GaN can be derived.
Resumo:
Hexagonal GaN is grown on a Si(111) substrate with AlN as a buffer layer by gas source molecular beam epitaxy (GSMBE) with ammonia. The thickness of AlN buffer is changed from 9 to 72 nm. When the thickness of AlN buffer is 36 nm, the surface morphology and crystal quality of GaN is optimal. The in-situ reflection high energy electron diffraction (RHEED) reveals that the transition to a two-dimensional growth mode of AlN is the key to the quality of GaN. However, the thickness of AlN buffer is not so critical to the residual in-plane tensile stress in GaN grown on Si(111) by GSMBE for AlN thickness between 9 to 72 nm.
Resumo:
We measured the carrier concentration distribution of gradient-doped GaAs/GqAlAs epilayers grown by molecular beam epitaxy before and after annealing at 600 degrees C, using electrochemical capacitance voltage profiling, to investigate the internal variation of transmission-mode GaAs photocathodes arising from the annealing process. The results show that the carrier concentration increased after annealing. As a result, the total band-bending energy in the gradient-doped GaAs emission layer increased by 25.24% after annealing, which improves the pbotoexcited electron movement toward the surface. On the other hand, the annealing process resulted in a worse carrier concentration discrepancy between the GaAs and the GaAlAs, which causes a lower back interface potential barrier, decreasing the amount of high-energy photoelectrons. (C) 2009 Optical Society of America
Resumo:
Gd2O3 thin films were deposited on Si (100) substrates at 650degreesC by a magnetron sputtering system under different Ar/O-2 ratios of 6:1, 4:1 and 2:1. The effect of the oxygen concentration on the properties of oxide thin films was investigated by X-ray diffraction, X-ray photoelectron spectroscopy, atomic force microscopy and capacitance-voltage (C-V)measurement. X-ray diffraction shows that the structure of oxide films changed from the monoclinic Gd2O3 phase to cubic Gd2O3 phase when the oxygen concentration increased. According to C-V measurement, the dielectric constant value of the samples deposited at different Ar/O-2 ratios is about 12. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Mn-doped ZnS nanocrystals of about 3 nm diameter were synthesized by a wet chemical method. X-ray diffraction (XRD) measurements showed that the nanocrystals have the structure of cubic zinc blende. The broadening of the XRD lines is indicative of nanomaterials. Room temperature photoluminescence (PL) spectrum of the undoped sample only exhibited a defected-related blue emission band. But for the doped samples, an orange emission from the Mn2+ T-4(1)-(6)A(1) transition was also observed, apart from the blue emission. The peak position (600 nm) of the Mn2+ emission was shifted to longer wavelength compared to that (584 nm) of bulk ZnS:Mn. With the increase of the Mn2+ concentration, the PL of ZnS:Mn was significantly enhanced. The concentration quenching effect was not observed in our experiments. Such PL phenomena were attributed to the absence of Mn2+ pairs in a single ZnS:Mn nanocrystal, considering the nonradiative energy transfer between Mn2+ ions based on the Poisson approximation. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Polycrystalline nano-grain-boundary multi-doping ZnO-based nonlinear varistors with higher concentration additives have been fabricated by sol-gel and standard solid-state reaction method, of which the best sample has a very high threshold voltage of E-b = 3300 V/mm. The effect of sintering processes, sintering temperature and sintering time, and that of additive concentration of Bi2O3 on E-b of the samples are systematically investigated. The results show that the great merit of sol-gel method is its high threshold voltage obtained by a lower sintering temperature than the solid-state reaction method. The present work also shows that five phases including solid-state sintering, rich Bi liquid phase formation and ZnO as well as other additive dissolution, ZnO grain growth, the secondary phase sufficient formation and evolution have been experienced at different sintering temperatures. The hole type defect and nonhomogeneity of the microstructure will lead to the decrease of threshold voltage, i.e., the grain size and the homogeneity of the material will be important factors and directly affect the characteristic of the varistor. The sintering characteristic and the influence of Bi2O3 content on the threshold voltage are also discussed. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
We report a new method for large-scale production of GaMnN nanowires, by annealing manganese-gallium oxide nanowires in flowing ammonia at high temperature. Microstructure analysis indicates that the GaMnN nanowires have wurtzite GaN structure without Mn precipitates or Mn-related second phases. Magnetism evolution due to nitrogen doping in manganese-gallium oxide nanowires was evaluated by magnetic measurements. Magnetic measurement reveals that the magnetization increases with the increase of nitrogen concentration. Ferromagnetic ordering exists in the GaMnN nanowires, whose Curie temperature is above room temperature. Luminescence evolution was investigated by the cathodoluminesence measurement for a single nanowire and photoluminescence measurement in a temperature range between 10 and 300 K. Experimental results indicate that optical properties can be modulated by nitrogen doping in manganese-gallium oxide nanowires. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Argon gas, as a protective environment and carrier of latent heat, has an important effect on the temperature distribution in crystals and melts. Numeric simulation is a potent tool for solving engineering problems. In this paper, the relationship between argon gas flow and oxygen concentration in silicon crystals was studied systematically. A flowing stream of argon gas is described by numeric simulation for the first time. Therefore, the results of experiments can be explained, and the optimum argon flow with the lowest oxygen concentration can be achieved. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
The growth of SiC epilayers on C-face (0 0 0 1) sapphire (alpha-Al2O3) has been performed using CVD method. We found that the quality of SiC epilayers has been improved through the nitridation of substrates by exposing them to ammonia ambient, as compared to growth on bare sapphire substrates. The single crystallinity of these layers was verified by XRD and double crystal XRD measurements. Atomic force microscopy was used to evaluate the surface morphology. Infrared reflectivity and Raman scattering measurement were carried out to investigate the phonon modes in the grown SiC. Detailed Raman analysis identified the 6H nature of the as-grown SiC films. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Depth profiles of carrier concentrations in GaMnSb/GaSb are investigated by electrochemistry capacitance-voltage profiler and electrolyte of Tiron. The carrier concentration in GaMnSb/GaSb measured by this method is coincident with the results of Hall and X-ray diffraction measurements. It is indicated that most of the Mn atoms in GaMnSb take the site of Ga, play a role of acceptors, and provide shallow acceptor level(s).
Resumo:
We have investigated the optical transitions in Ga1-yInyNxAs1-x/GaAs single and multiple quantum wells using photovoltaic measurements at room temperature. From a theoretical fit to the experimental data, the conduction band offset Q(c), electron effective mass m(e)*, and band gap energy E-g were estimated. It was found that the Q(c) is dependent on the indium concentration, but independent on the nitrogen concentration over the range x=(0-1)%. The m(e)* of GaInNAs is much greater than that of InGaAs with the same concentration of indium, and increases as the nitrogen concentration increases up to 1%. Our experimental results for the m(e)* and E-g of GaInNAs are quantitatively explained by the two-band model based on the strong interaction of the conduction band minimum with the localized N states. (C) 2001 American Institute of Physics.
Resumo:
The concentration of hydroen-indium vacancy complex VInH4 in liquid encapsulated Czochralski undoped and Fe-doped n-type InP has been studied by low-temperature infrared absorption spectroscopy. The VInH4 complex is found to be a dominant intrinsic shallow donor defect with concentrations up to similar to 10(16) cm(-3) in as-grown liquid encapsulated Czochralski InP. The concentration of the VInH4 complex is found to increase with the compensation ratio in good agreement with the proposed defect formation model of Walukiewicz [W. Walukiewicz, Phys. Rev. B 37, 4760 (1998); Appl. Phys. Lett. 54, 2094 (1989)], which predicts a Fermi-level-dependent concentration of amphoteric defects. (C) 1998 American Institute of Physics, [S0003-6951(98)04435-0].
Resumo:
It was determined that oxygen concentration in heavily Sb-doped silicon was about 40% lower than that in the lightly doped Czochralski grown silicon and decreased with increasing content of Sb by means of coincident elastic recoil detection analysis. Through thermodynamic calculation, the oxygen loss by evaporation from the free surface of melt is only due to the formation of SiO, and Sb2O3 evaporation can be neglected. The basic reason for oxygen concentration reduction in heavily Sb-doped CZSi was that oxygen solubility decreased when element Sb with larger radius doped degenerately into silicon crystal. (C) 1999 Elsevier Science B.V. All rights reserved.
Resumo:
We use nuclear reaction analysis to study hydrogen in unintentionally doped GaN, and high-concentration hydrogen, nearly 10(21) cm(-3), is detected. Accordingly, a broad but intense infrared absorption zone with a peak at 2962 cm(-1) is reported, which is tentatively assigned to the stretch mode of NH: Ga complex. The complex is assumed to be one candidate answering for background electrons in unintentionally doped GaN. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
InN films with electron concentration ranging from n similar to 10(17) to 10(20) cm(-3) grown by metal-organic chemical vapor deposition (MOCVD) and molecular beam epitaxy (MBE) were investigated by variable-temperature photoluminescence and absorption measurements. The energy positions of absorption edge as well as photoluminescence peak of these InN samples with electron concentration above 10(18) cm(-3) show a distinct S-shape temperature dependence. With a model of potential fluctuations caused by electron-impurity interactions, the behavior can be quantitatively explained in terms of exciton freeze-out in local potential minima at sufficiently low temperatures, followed by thermal redistribution of the localized excitons when the band gap shrinks with increasing temperature. The exciton localization energy sigma (loc) is found to follow the n (5/12) power relation, which testifies to the observed strong localization effects in InN with high electron concentrations.