112 resultados para wet etching
Resumo:
Silicon-on-insulator (SOI) technology offers tremendous potential for integration of optoelectronic functionson a silicon wafer. In this letter, a 1 * 1 multimode interference (MMI) Mach-Zender interferometer(MZI) thermo-optic modulator fabricated by wet-etching method is demonstrated. The modulator has anextinction ratio of -11.0 dB, extra loss of -4.9 dB and power consumption of 420 mW. The response timeis less than 30μs.
Resumo:
In this paper we report the fabrication of 1.3 mum Si-based MEMS tunable optical filter, by surface micromaching. Through wet etching of polyimide sacrificial layer, a tunable Fabry-Perot filter was successfully fabricated. We make the capacitance measurement of the prototype device, compare the experimental curve with the theoretical one, and explain the difference between them.
Resumo:
SOI based wrap-gate silicon nanowire FETs are fabricated through electron beam lithography and wet etching. Dry thermal oxidation is used to further reduce the patterned fins cross section and transfer them into nanowires. Silicon nanowire FETs with different nanowire widths varying from 60 nm to 200 nm are fabricated and the number of the nanowires contained in a channel is also varied. The on-current (I-ON) and off-current (I-OFF) of the fabricated silicon nanowire FET are 0.59 mu A and 0.19 nA respectively. The subthreshold swing (SS) and the drain induced barrier lowering are 580 mV/dec and 149 mVN respectively due to the 30 nm thick gate oxide and 1015 cm(-3) lightly doped silicon nanowire channel. The nanowire width dependence of SS is shown and attributed to the fact that the side-gate parts of a wrap gate play a more effectual role as the nanowires in a channel get narrower. It seems the nanowire number in a channel has no effect on SS because the side-gate parts fill in the space between two adjacent nanowires.
Resumo:
We demonstrate a technique based on wet chemical etching that enables quick and accurate evaluation of edge- and screw/mixed-type threading dislocations (TDs) in GaN. Large and small etch pits are formed by phosphoric acid on the etched surfaces. The large etch pits are attributed to screw/mixed TDs and the small ones to edge TDs, according to their locations on the surface and Burgers vectors of TDs. Additionally, the origin of small etch pits is confirmed by a transmission electron microscopy. The difference in the size of etch pits is discussed in view of their origin and merging. Overetching at elevated temperatures or for a long time may result in merging of individual etch pits and underestimating of the density of TDs. Wet chemical etching has also been proved efficient in revealing the distribution of TDs in epitaxial lateral overgrowth GaN.
Resumo:
于2010-11-23批量导入
Resumo:
The influence of deposition, annealing conditions, and etchants on the wet etch rate of plasma enhanced chemical vapor deposition (PECVD) silicon nitride thin film is studied. The deposition source gas flow rate and annealing temperature were varied to decrease the etch rate of SiN_x:H by HF solution. A low etch rate was achieved by increasing the SiH_4 gas flow rate or annealing temperature, or decreasing the NH_3 and N_2 gas flow rate. Concen-trated, buffered, and dilute hydrofluoric acid were utilized as etchants for SiO_2 and SiN_x:H. A high etching selectivity of SiO_2 over SiN_x:H was obtained using highly concentrated buffered HF.
Resumo:
Ion beam etching technique was used to reveal the metallograhpic microstructure and interface morphology of electroplating chromium coating, in particular, whose substrate surface layer was treated in advance by laser quenching. Chemical etchings were, also conducted for comparison. The reveal microstructures were observed and analyzed by scanning electron microscopy. The results show that ion beam etching can reveal well the whole microstructures of composite coating-substrate materials.
Resumo:
The numerical solutions of binary-phase (0, tau) gratings for one-dimensional array illuminators up to 32 are presented. Some fabrication errors, which are due to position-quantization errors, phase errors, dilation (or erosion) errors, and the side-slope error, are calculated and show that even-number array illuminators are superior to odd-number array illuminators when these fabrication errors are considered. One (0, tau) binary-phase, 8 x 16 array illuminator made with the wet-chemical-etching method is given in this paper.
Resumo:
Polymer deposition is a serious problem associated with the etching of fused silica by use of inductively coupled plasma (ICP) technology, and it usually prevents further etching. We report an optimized etching condition under which no polymer deposition will occur for etching fused silica with ICP technology. Under the optimized etching condition, surfaces of the fabricated fused silica gratings are smooth and clean. Etch rate of fused silica is relatively high, and it demonstrates a linear relation between etched depth and working time. Results of the diffraction of gratings fabricated under the optimized etching condition match theoretical results well. (c) 2005 Optical Society of America.
Resumo:
This paper reports on the fabrication and characterization of a ridge optical waveguide in an Er3+/Yb3+ co-doped phosphate glass. The He+ ion implantation (at energy of 2.8 MeV) is first applied onto the sample to produce a planar waveguide substrate, and then Ar+ ion beam etching (at energy of 500 eV) is carried out to construct rib stripes on the sample surface that has been deposited by a specially designed photoresist mask. According to a reconstructed refractive index profile of the waveguide cross section, the modal distribution of the waveguide is simulated by applying a computer code based on the beam propagation method, which shows reasonable agreement with the experimentally observed waveguide mode by using the end-face coupling method. Simulation of the incident He ions at 2.8 MeV penetrating into the Er3+/Yb3+ co-doped phosphate glass substrate is also performed to provide helpful information on waveguide formation.
Resumo:
gamma-LiAlO2 single crystal was successfully grown by Czochralski method. The crystal quality was characterized by X-ray rocking curve and chemical etching. The effects of air-annealing and vapor transport equilibration (VTE) on the crystal quality, etch pits and absorption spectra of LiAlO2 were also investigated in detail. The results show that the as-grown crystal has very high quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec. Dislocation density in the middle part of the crystal is as low as about 3.0 x 10(3) cm(-2). The VTE-treated slice has larger FWHM value, etch pits density and absorption coefficient as compared with those of untreated and air-annealed slices, which indicates that the crystal quality became inferior after VTE treatment. (C) 2008 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Concentration of trace elements measured by dry weight basis has become more commonly used in recent studies on cetaceans than wet weight basis, which was used more in earlier studies. Because few authors present moisture content data in their papers, it is difficult to compare the concentrations of trace elements between various studies. Therefore, we felt that it would be useful if a reference conversion factor (CF) for tissue types could be found to convert between wet weight and dry weight data on trace element concentrations. We determined the moisture contents of 14 tissues of Dall's porpoise (Phocoenoides dalli), and then, calculated the CF values for those tissues. Because the moisture content of each tissue differs from other tissues, it is necessary to use a specific CIF for each tissue rather than a general CF for several tissues. We have also found that CIF values for Dall's porpoise tissues are similar to the same tissues in other cetaceans. Therefore CF values from Dall's porpoise can be reliably used to convert between wet and dry weight concentrations for other cetacean tissues as reference data. (C) 2002 Elsevier Science Ltd. All rights reserved.
Resumo:
Sapphire substrates were nanopatterned by dry (inductively coupled plasma, ICP) etching to improve the performance of GaN-based light-emitting diodes (LEDs). GaN-based LEDs on nanopatterned sapphire substrates (NPSS) were fabricated by metal organic chemical vapor deposition (MOCVD). The characteristics of LEDs fabricated on NPSS prepared by dry etching were studied. The light output power and wall-plug efficiency of the LEDs fabricated on NPSS were greater than those of the conventional LEDs fabricated on common planar sapphire substrates when the injection currents were the same. The LEDs on NPSS and common planar sapphire substrates have similar I-V characteristics.
Resumo:
Self-assembled InAs/AlAs quantum dots embedded in a resonant tunneling diode device structure are grown by molecular beam epitaxy. Through the selective etching in a C6H8O7 center dot H2O-K3C6H5O7 center dot H2O-H2O2 buffer solution, 310 nm GaAs capping layers are removed and the InAs/AlAs quantum dots are observed by field-emission scanning electron microscopy. It is shown that as-fabricated quantum dots have a diameter of several tens of nanometers and a density of 10(10) cm(-2) order. The images taken by this means are comparable or slightly better than those of transmission electron microscopy. The undercut of the InAs/AlAs layer near the edges of mesas is detected and that verifies the reliability of the quantum dot images. The inhomogeneous oxidation of the upper AlAs barrier in H2O2 is also observed. By comparing the morphologies of the mesa edge adjacent regions and the rest areas of the sample, it is concluded that the physicochemical reaction introduced in this letter is diffusion limited.