236 resultados para low temperature treatment
Resumo:
We realize a stable self-starting passively mode-locking all-solid-state laser by using novel GaAs mirrors as the absorber and output coupler. The GaAs mirror is grown by the technology of metal organic chemical vapour deposition at low temperature. With such an absorber as the output coupler in the laser resonator, laser pulses with duration of 42ps were generated at a repetition rate of 400MHz, corresponding to the average power of 590mW.
Resumo:
We have demonstrated stable self-starting passive mode locking in a diode-end-pumped Nd:Gd-0.8-Y0.5VO4 laser by using an In0.25Ga0.75As absorber grown at low temperature (LT In0.25Ga0.75As absorber). An In0.25Ga0.75As single-quantum-well absorber, which was grown directly on the GaAs buffer by use of the metal-organic chemical-vapor deposition technique, acts simultaneously as a passive mode-locking device and as an output coupler. Continuous-wave mode-locked pulses were obtained at 1063.5 nm. We achieved a pulse duration of 2.6 ps and an average output power of 2.15 W at a repetition rate of 96.4 MHz. (c) 2005 Optical Society of America.
Resumo:
Microcrystalline silicon thin films at different growth stages were prepared by hot wire chemical vapor deposition. Atomic force microscopy has been applied to investigate the evolution of surface topography of these films. According to the fractal analysis I it was found that, the growth of Si film deposited on glass substrate is the zero-diffused stochastic deposition; while for the film on Si substrate, it is the finite diffused deposition on the initial growth stage, and transforms to the zero-diffused stochastic deposition when the film thickness reaches a certain value. The film thickness dependence of island density shows that a maximum of island density appears at the critical film thickness for both substrates. The data of Raman spectra approve that, on the glass substrate, the a-Si: H/mu c-Si:H transition is related to the critical film thickness. Different substrate materials directly affect the surface diffusion ability of radicals, resulting in the difference of growth modes on the earlier growth stage.
Resumo:
We have investigated the effect of the thickness and layer number of the low-temperature A1N interlayer (LT-A1N IL) on the stress relaxation and the crystal quality of GaN epilayers grown on Si (111) substrate by metalorganic chemical vapor deposition. It is found that the stress decreases with the increase of the LT-AIN IL thickness, but the crystal quality of the GaN epilayer goes worse quickly when the LT-AIN IL thickness is larger than 16 nm. This is because the increase of the LT-AIN IL thickness will increase the coalescence thickness of its upper GaN layer, which sensitively affects the crystal quality of the epilayer. Using multiple LT-AIN ILs is an effective method not only to reduce the stress, but also to improve the crystal quality of the GaN epilayer. With the increase of the interlayer number, the probability that dislocations are blocked increases and the probability that dislocations are produced at interfaces decreases. Thus, dislocations in the most upper part of GaN are reduced, resulting in the improvement of the crystal quality. Finally, it is suggested that when the total thickness of the epilayer is fixed, both the thickness and the number of the LT-AIN IL should be carefully designed to reduce the stress and improve the crystal quality of the epilayer simultaneously. (c) 2004 Elsevier B.V.. All rights reserved.
Resumo:
Metalorganic chemical vapor deposition growth of InN on sapphire substrate has been investigated between 400 degrees C and 500 degrees C to seek the growth condition of InN buffer layer, i.e. the first step of realization of the two-step growth method. Ex situ characterization of the epilayers by means of atomic force microscope, scanning electron microscope and X-ray diffraction, coupled with in situ reflectance curves, has revealed different growth circumstances at these temperatures, and conclusion has been reached that the most suitable temperature for buffer growth is around 450 degrees C. In addition, the growth rate of InN at the optimized temperature with regard to different precursor flow rates is studied at length. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
GaAs absorber was grown at low temperature (550degreesC) by metal organic chemical vapour deposition (MOCVD) and was used as an output coupler with which we realized Q-switching modelocked Yb3+-doped fibre laser. The shortest period of the envelope of the Q-switched modelocking is about 3mus. The modelocking threshold is 4.27W and the highest average output pulse power is 290 mW. The modelocking frequency is 12 MHz.
Resumo:
The depth distribution of the strain-related tetragonal distortion e(T) in the GaN epilayer with low-temperature AlN interlayer (LT-AlN IL) on Si(111) substrate is investigated by Rutherford backscattering and channeling. The samples with the LT-AlN IL of 8 and 16 nm thickness are studied, which are also compared with the sample without the LT-AlN IL. For the sample with 16-nm-thick LT-AlN IL, it is found that there exists a step-down of e(T) of about 0.1% in the strain distribution. Meanwhile, the angular scan around the normal GaN <0001> axis shows a tilt difference about 0.01degrees between the two parts of GaN separated by the LT-AlN IL, which means that these two GaN layers are partially decoupled by the AlN interlayer. However, for the sample with 8-nm-thick LT-AlN IL, neither step-down of e(T) nor the decoupling phenomenon is found. The 0.01degrees decoupled angle in the sample with 16-nm-thick LT-AlN IL confirms the relaxation of the LT-AlN IL. Thus the step-down of e(T) should result from the compressive strain compensation brought by the relaxed AlN interlayer. It is concluded that the strain compensation effect will occur only when the thickness of the LT-AlN IL is beyond a critical thickness. (C) 2004 American Institute of Physics.
Resumo:
Using a low temperature grown GaAs wafer as an intracavity saturable absorber, a temporal envelope duration of 11 ns of Q- switched and mode- locked ( QML) 1064 nm operation was achieved in a very simple compact plane- concave cavity Nd: YVO4 laser, it was so short that the pulses can be used as Q- switching pulses. The maximal average output power is 808 mW with the repetition rate of 25 kHz, and the corresponding peak power and energy of a single Q- switched pulse was 2.94 kW and 32.3 mu J, respectively. The mode- locked pulse trains inside the Q- switched pulse envelope had a repetition rate of 800 MHz.
Resumo:
The V/III ratio in the initial growth stage of metalorganic chemical vapor deposition has an important influence on the quality of a GaN epilayer grown on a low-temperature AIN buffer layer and c-plane sapphire substrate. A weaker yellow luminescence, a narrower half-width of the X-ray diffraction peak, and a higher electron mobility result when a lower V/III ratio is taken. The intensity of in situ optical reflectivity measurements indicates that the film surface is rougher at the beginning of GaN growth, and a longer time is needed for the islands to coalesce and for a quasi-two dimensional mode growth to start. A comparison of front- and back-illuminated photoluminescence spectra confirms that many threading dislocations are bent during the initial stage, leading to a better structural quality of the GaN layer. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
We report the operation of a bidirectional picosecond pulsed ring Nd:YVO4 laser based on a low-temperature-grown semiconductor saturable absorber mirror. Except for the laser crystal, the six-mirror ring laser cavity has no intra-cavity elements such as focusing lens or mirror. The bidirectional mode locked pluses are obtained at the repetition rate of 117.5 MHz, pulse duration of 81 ps, power of 2 x 200 mW.
Resumo:
Temperature dependence of optical properties of GaInNAs/GaAs quantum wells (QWs) has been studied by photoluminescence (PL) and time-resolved PL. A rapid PL quenching is observed even at very low temperature and is of the excitation power dependence. These results strongly suggest that the non-radiative recombination process plays a very important role at low temperature. In the TRPL measurement the shape of the PL decay curve shows significant difference under different excitation powers. It is attributed to the different involvement of non-radiative recombination in the overall recombination process. The TRPL data are well fitted with the rate equation involving both the radiative and non-radiative recombination. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The temperature and pressure dependences of band-edge photo luminescence from ZnO microrods have been investigated. The energy separation between the free exciton (FX) and its first order phonon replica (FX-1LO) decreases at a rate of k(B)T with increasing temperature. The intensity ratio of the FX-1LO to the bound exciton (BX) emission is found to decrease slightly with increasing pressure. All of the exciton emission peaks show a blue shift with increasing pressure. The pressure coefficient of the FX transition, longitudinal optical (LO) phonon energy, and binding energy of BX are estimated to be 21.4, 0.5, and 0.9 meV/GPa, respectively. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
A 1.55 mu m low-temperature-grown GaAs (LT-GaAs) photodetector with a resonant-cavityenhanced structure was designed and fabricated. A LT-GaAs layer grown at 200 degrees C was used as the absorption layer. Twenty- and fifteen-pair GaAs/AlAs-distributed Bragg reflectors were grown as the bottom and top mirrors. A responsivity of 7.1 mA/W with a full width at half maximum of 4 nm was obtained at 1.61 mu m. The dark current densities are 1.28x10(-7) A/cm(2) at the bias of 0 V and 3.5x10(-5) A/cm(2) at the reverse bias of 4.0 V. The transient response measurement showed that the photocarrier lifetime in LT-GaAs is 220 fs. (c) 2006 American Institute of Physics.
Resumo:
A passively Q-switched and mode-locked diode-pumped Nd:GdVO4 laser was demonstrated using a low-temperature-grown GaAs wafer (LT-GaAs) as an intracavity saturable absorber. The maximal Q-switched mode-locked average output power was 750 mW with the Q-switched envelop having a repetition rate of 167 kHz. The mode-locked pulse trains inside the Q-switched pulse envelope had a repetition rate of similar to 790 MHz.
Resumo:
We report, for the first time to the best of our knowledge, on a passively Q-switched Nd:YVO4 laser with a GaAs absorber grown at low temperature (LT) by metal organic vapor phase expitaxy. Using the LT GaAs absorber as well as an output coupler, a passively Q-switched laser whose pulse duration is as short as 90 ns, was obtained.