Resumo:
We report a 1.5-mu m InGaAs/GaAs quantum well laser diode grown by molecular beam epitaxy on InGaAs metamorphic buffers. At 150 K, for a 1500 x 10 mu m(2) ridge waveguide laser, the lasing wavelength is centred at 1.508 mu m and the threshold current density is 667 A/cm(2) under pulsed operation. The pulsed lasers can operate up to 286 K.
Resumo:
We have investigated the optical properties of AlGaN grown on sapphire. It is found that two main luminescence peaks occur in the cathodoluminescence (CL) spectra of AlGaN films, and their energy separation increases with the increase of Al source flux during the growth. Spatially resolved CL investigations have shown that the line splitting is a result of variation of AlN mole fraction within the layer. The Al composition varies in both lateral and vertical direction. It is suggested that the difference in the surface mobility of Al and Ga atoms, especially, its strong influence on the initial island coalescence process and the formation of island-like regions on the uneven film surface, is responsible for the Al composition inhomogeneity. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Visible-blind p-i-n avalanche photodiodes (APDs) were fabricated with high-quality GaN epilayers deposited on c-plane sapphire substrates by metal-organic chemical vapour deposition. Due to low dislocation density and a sophisticated device fabrication process, the dark current was as small as similar to 0.05 nA under reverse bias up to 20V for devices with a large diameter of 200 mu m, which was among the largest device area for GaN-based p-i-n APDs yet reported. When the reverse bias exceeded 38V the dark current increased sharply, exhibiting a bulk avalanche field-dominated stable breakdown without microplasma formation or sidewall breakdown. With ultraviolet illumination (360 nm) an avalanche multiplication gain of 57 was achieved.
Resumo:
The defect evolution and its correlation with electrical properties of GaN films grown by metalorganic chemical vapor deposition are investigated. It is found that the dislocation density decreases gradually during the growth process, and the dislocation reduction rate in the island coalescence process is especially rapid. The changes in electron mobility of GaN with the increase of growth time are mainly dependent on the dislocations acting as scattering centers. Furthermore, the variation of carrier concentration in GaN may be related with the point defects and their clusters. The quality of GaN could be improved by suitably increasing the film thickness. (C) 2009 Elsevier B.V. All rights reserved.
The investigation on strain relaxation and double peaks in photoluminescence of InGaN/GaN MQW layers
Resumo:
Two emission peaks were observed in the low temperature photoluminescence (LTPL) spectra of an InGaN/GaN multiple quantum well (MQW) structure before and after nanopillar fabrication. After nanopillar fabrication it is found that among the two peaks the longer wavelength peak exhibits a clear blue shift and has a much stronger enhancement in LTPL intensity than the shorter one. Combined with x-ray diffraction and spatially resolved cathodoluminescence analyses, the difference induced by nanopillar fabrication is ascribed to different strain relaxation states in the lower and upper quantum well layers. It is found that the lower QW layers of the as-grown MQW which causes the longer wavelength PL peak are more strained, while the upper ones are almost fully strain-relaxed. Therefore, the nanopillar fabrication induces much less strain relaxation in the upper part of the MQW than in the lower one.
Resumo:
The leakage mechanism of GaN-based p-i-n (p-AlGaN/i-GaN/n-GaN) UV detector has been investigated. With the same dislocation density, devices made from material with higher density of V-pits on surface produce larger leakage current. SEM images show that some V-pits penetrate into i-GaN layer, sometimes even the n-GaN layer. If p-ohmic contact metal (Ni/Au) deposits in the V-pits, Schottky contact would be formed at the interface of metal and i-GaN, or form ohmic contact at the interface of metal and n-GaN. The existence of parallel Schottky junction and ohmic contact resistance enhances the leakage current greatly.
Resumo:
Mg-doped p-InGaN layers with In composition of about 10% are grown by metalorganic chemical vapor deposition (MOCVD). The effect of the annealing temperature on the p-type behavior of Mg-doped InGaN is studied. It is found that the hole concentration in p-InGaN increases with a rising annealing temperature in the range of 600 850 C, while the hole mobility remains nearly unchanged until the annealing temperature increases up to 750 C, after which it decreases. On the basis of conductive p-type InGaN growth, the p-In0.1Ga0.9N/i-In0.1Ga0.9N/n-GaN junction structure is grown and fabricated into photodiodes. The spectral responsivity of the InGaN/GaN p-i-n photodiodes shows that the peak responsivity at zero bias is in the wavelength range 350-400 nm.
Resumo:
High-quality and nearly crack-free GaN epitaxial layer was obtained by inserting a single AlGaN interlayer between GaN epilayer and high-temperature AlN buffer layer on Si (111) substrate by metalorganic chemical vapor deposition. This paper investigates the effect of AlGaN interlayer on the structural proper-ties of the resulting GaN epilayer. It confirms from the optical microscopy and Raman scattering spectroscopy that the AlGaN interlayer has a remarkable effect on introducing relative compressive strain to the top GaN layer and preventing the formation of cracks. X-ray diffraction and transmission electron microscopy analysis reveal that a significant reduction in both screw and edge threading dislocations is achieved in GaN epilayer by the insertion of AlGaN interlayer. The process of threading dislocation reduction in both AlGaN interlayer and GaN epilayer is demonstrated.
Resumo:
The in situ optical reflectivity measurements are employed to monitor the GaN epilayer growth process above low-temperature AlN buffer layer on c-plane sapphire substrate by metalorganic chemical vapor deposition. It is found that the lateral growth of GaN islands and their coalescence is promoted in the initial growth stage if the AlN buffer layer is treated with a long annealing time and has an optimal thickness: As confirmed by atomic force microscopy observations, the quality of GaN epilayers is closely dependent on the surface morphology of AlN buffer layer, especially the grain size and nuclei density after the annealing treatment. (C) 2004 American Institute of Physics.
Resumo:
High-quality GaNAs/GaAs quantum wells with high substitutional N concentrations, grown by molecular-beam epitaxy, are demonstrated using a reduced growth rate in a range of 0.125-1 mu m/h. No phase separation is observed and the GaNAs well thickness is limited by the critical thickness. Strong room-temperature photoluminescence with a record long wavelength of 1.44 mu m is obtained from an 18-nm-thick GaN0.06As0.94/GaAs quantum well. (C) 2005 American Institute of Physics.
Resumo:
The influences of a high-temperature (HT) AlN interlayer (IL) on the phase separation in crack-free AlGaN grown on GaN have been studied. The depth-dependent cathodoluminescence (CL) spectra indicate a relatively uniform Al distribution in the growth direction, but the monochromatic CL images and the CL spectra obtained by line scan measurements reveal a lateral phase separation in AlGaN grown on relatively thick HT-AlN ILs. Moreover, when increasing the thickness of HT-AlN IL, the domain-like distribution of the AlN mole fraction in AlGaN layers is significantly enhanced through a great reduction of the domain size. The morphology of mesa-like small islands separated by V trenches in the HT-AlN IL, and the grain template formed by the coalescence of these islands during the subsequent AlGaN lateral overgrowth, are attributed to be responsible for the formation of domain-like structures in the AlGaN layer. (c) 2005 American Institute of Physics.
Resumo:
The electrical and structural properties of Mg delta-doped GaN epilayers grown by MOCVD were investigated. Compared to uniform Mg-doping GaN layers, it has been shown that the delta-doping (delta-doping) process could suppress the dislocation density and enhance the p-type performance. The influence of pre-purge step on the structural properties of GaN was also investigated. The hole concentration of p-GaN decreases when using a pre-purge step. These results can be explained convincingly using a simple model of impurity incorporation under Ga-free growth condition. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
The V/III ratio in the initial growth stage of metalorganic chemical vapor deposition has an important influence on the quality of a GaN epilayer grown on a low-temperature AIN buffer layer and c-plane sapphire substrate. A weaker yellow luminescence, a narrower half-width of the X-ray diffraction peak, and a higher electron mobility result when a lower V/III ratio is taken. The intensity of in situ optical reflectivity measurements indicates that the film surface is rougher at the beginning of GaN growth, and a longer time is needed for the islands to coalesce and for a quasi-two dimensional mode growth to start. A comparison of front- and back-illuminated photoluminescence spectra confirms that many threading dislocations are bent during the initial stage, leading to a better structural quality of the GaN layer. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Properties of the Ag/Ni/p-GaN structure at different temperatures are studied by Auger electron spectroscopy, scanning electron microscopy and high resolution x-ray diffraction. The effect of Ag in ohmic contact on the crystalline quality is investigated and the optimized value of annealing temperature is reported. The lowest specific contact resistance of 2.5 x 10(-4) Omega cm(2) is obtained at annealing temperature of 550 degrees C.
Resumo:
We demonstrate 1.25-1.29 mu m metamorphic laser diodes grown on GaAs by molecular beam epitaxy (MBE) using an alloy-graded buffer layer (GBL). Use of Be in the GBL is effective to reduce surface/interface roughness and improves optical quality. The RMS surface roughness of the optimized metamorphic laser is only two atomic monolayers for 1 x 1 mu m(2). Cross-sectional transmission electron microscopy (TEM) images confirm that most dislocations are blocked in the GBL. Ridge waveguide lasers with 4 mu m wide ridge were fabricated and characterized. The average threshold current under the pulsed excitation is in 170-200 mA for a cavity length of 0.9-1.5 mm. This value can be further reduced to about 100 mA by high-reflectivity coating. Lasers can work in an ambient temperature up to at least 50 degrees C. (c) 2006 Elsevier B.V. All rights reserved.