380 resultados para TRIPLET EMISSION
Resumo:
Resumo:
This paper presents a detailed PL study of Fe2+ related four zero-phonon(ZP) lines and their related phonon sidebands. Four zero-phonon transitions at approximate to 2800 cm(-1) along with the accompanying phonon sidebands extending down to 2400 cm(-1). There are ta two prominent regions in the phonon sidebands. One is ascribed to coupling to acoustic-type phonons (2700 cm(-1) region), the other is due to coupling to optic-type phonons (2500 cm(-1) region). Beside broad coupling with lattice modes, there are several groups of lines. They are ascribed to resonant modes, impurities induced gap modes and local modes.
Resumo:
The behaviors of lateral propagating modes in the aperture and the oxidized regions are investigated numerically for selectively oxidized vertical-cavity surface-emitting lasers (VCSELs). The results show that the lateral propagating modes in the oxidized region are greatly affected by the oxide layer due to its low index, the modes are divergence for the VCSELs with sufficient thick double oxide layers. So the coupling between the modes in the aperture and oxidized regions is very weak, and we can expect that the lateral spontaneous emission is greatly affected in this case. Ignoring the contribution of the lateral spontaneous emission, we calculate spontaneous emission factor by counting the total number of the guided modes in selectively oxidized VCSELs with double oxide layers. The results agree very well with the reported measurements and are inversely proportional to the lateral index step.
Resumo:
Photoluminescence (PL) from Er-implanted hydrogenated amorphous silicon suboxide (a-SiOX:H
Resumo:
nThermal processing of strained ln(0.2)Ga(0.8)As/GaAs graded-index separate confinement heterostructure single quantum well laser diodes grown by molecular beam epitaxy is investigated. It was found that rapid thermal annealing can improve the 77 K photoluminescence efficiency and electron emission from the active layer, due to removal of nonradiative centers from the InGaAs/GaAs interface. Because of the interdiffusion of Al and Ga atoms, rapid thermal annealing increases simultaneously the density of DX centers in the AlGaAs graded layer. The current stressing experiments of post-growth and annealed laser diodes are indicative of a corresponding increase in the concentration of DX centers, suggesting that DX centers may be responsible for the degradation of laser diode performance.
Resumo:
Red shifts of emission wavelength of self-organized In(Cla)As/GaAs quantum dots (QDs) covered by 3 nm thick InxGa1-xAs layer with three different In mole fractions (x = 0.1, 0.2 and 0.3, respectively) have been observed. Transmission electron microscopy images demonstrate that the stress along growth direction in the InAs dots was reduced due to introducing the InxGa1-xAs (x = 0.1, 0.2 and 0.3) covering layer instead of GaAs layer. Atomic force microscopy pictures show a smoother surface of InAs islands covered by an In0.2Ga0.8As layer. It is explained by the calculations that the redshifts of the photoluminescence (PL) spectra from the QDs covered by the InxGa1-xAs (x greater than or equal to 0.1) layers were mainly due to the reducing of the strain other than the InAs/GaAs intermixing in the InAs QDs. The temperature dependent PL spectra further confirm that the InGaAs covering layer can effectively suppress the temperature sensitivity of PL emissions. 1.3 mum emission wavelength with a very narrow linewidth of 19.2 mcV at room temperature has been obtained successfully from In,In0.5Ga0.5As/GaAs self-assembled QDs covered by a 3-nm In0.2Ga0.2As strain reducing layer. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
The InAs quantum dots (QDs) on an AlAs layer are grown on GaAs substrates by molecular beam epitaxy technique. The properties of materials and optics of such QD structures have been investigated by cross sectional transmission electron microscopy and photoluminescence (PL) techniques. It is discovered that the inhomogeneous strain filed mainly exists below InAs QDs layers in the case of no wetting layer. The full width at half maximums (FWHMs) and intensities of PL emission peaks of InAs QDs are found to be closely related to the thickness of the thin AlAs layers. The InAs QDs on an eight monolayer AlAs layer, with wide FWHMs and large integral intensity of PL emission peaks, are favorable for producing broadband QD superluminescent diodes, external-cavity QD laser with large tuning range.
Resumo:
Without introducing concentration quenching phenomenon, a few wt% of Tb3+ and Yb3+ ions were doped into a group of easily-fiberized tellurite glasses characterized by loose polyhedron structures and rich interstitial positions. Intense green upconversion emission from Tb3+ ions centered at 539 nm due to transition 5D4→7F5 was observed by direct excitation of Yb3+ ions with a laser diode at 976 nm. Optimizing the concentration ratio of Tb3+/Yb3+, a tellurite glass with composition of 80TeO2-10ZnO-10Na2O (mol%)+1.0wt% Tb2O3+3.0wt% Yb2O3 was found to present the highest green light intensity and therefore is especially suitable for efficient green fiber laser development.