228 resultados para semi-confined
Resumo:
The influence of the sidegate voltage on the Schottky barrier in the ion-implanted active layer via the Schottky pad on the semi-insulating GaAs substrate was observed, and the mechanism for such an influence was proposed. (C) 1996 American Institute of Physics.
Resumo:
The dynamic effect of electrons in a double quantum well under the influence of a monochromatic driving laser field is investigated. Closed-form solutions for the quasienergy and Floquet states are obtained with the help of SU(2) symmetry. For the case of weak interlevel coupling, explicit expressions of the quasienergy are presented by the use of perturbation theory, from which it is found that as long as the photon energy is not close to the tunnel splitting, the electron will be confined in an initially occupied eigenstate of the undriven system during the whole evolution process. Otherwise, it will transit between the lowest two levels in an oscillatory behavior.
Resumo:
The effect of GaAs cap layer with different thicknesses in the GaAs/In0.3Ga0.7As/GaAs heterostructure on misfit dislocation is investigated with transmission electron microscopy, and it is found that lines of misfit dislocation break up and move out of the structure when the GaAs cap layer thickness exceeds a certain amount. The breaking up and moving out of misfit dislocations, initially confined in the (001) substrate/InGaAs epilayer interface, occur mainly along the [110] direction on the interface in the structure. (C) 1995 American Institute of Physics.
Resumo:
A novel structure of spot-size converter is designed to allow low loss and large alignment tolerance between single-mode rib waveguide devices and fiber arrays theoretically. The spot-size converter consists of a tapered rib core region and a double-cladding region. Through optimizing parameters,an expanded mode field can be tightly confined in the inner cladding and thus radiation loss be reduced largely at the tapered region. The influence of refractive index and thickness of the inner cladding on coupling loss is analyzed in particular. A novel,easy method of fabricating tapered rib spot-size converter based on silicon-on-insulator material is proposed.
Resumo:
A 1.3μm low-threshold edge-emitting AlGaInAs multiple-quantum-well(MQW) laser with AlInAs-oxide confinement layers is fabricated.The Al-contained waveguide layers upper and low the active layers are oxidized as current-confined layers using wet-oxidation technique.This structure provides excellent current and optical confinement,resulting in 12.9mA of a low continuous wave threshold current and 0.47W/A of a high slope efficiency of per facet at room temperature for a 5-μm-wide current aperture.Compared with the ridge waveguide laser with the same-width ridge,the threshold current of the AlInAs-oxide confinement laser has decreased by 31.7% and the slope efficiency has increased a little.Both low threshold and high slope efficiency indicate that lateral current confinement can be realized by oxidizing AlInAs waveguide layers.The full width of half maximum angles of the Al-InAs-oxide confinement laser are 21.6° for the horizontal and 36.1° for the vertical,which demonstrate the ability of the AlInAs oxide in preventing the optical field from spreading laterally.
Resumo:
Semi-insulating (SI) InP materials have been prepared under different stoichiometric conditions, including Fe-doping in indium-rich melt and high temperature annealing undoped wafer in phosphorus and iron phosphide ambients. Deep level defects related with non-stoichiometry have been detected in the SI-InP samples. A close relationship between the material quality of electrical property and native deep defects has been revealed by a comprehensive study of defects in as-grown Fe-doped and annealed undoped SI-InP materials. Fe-doped SI-InP material with low carrier mobility and poor thermal stability contains a high concentration of deep defects with energy levels in the range of 0.1-0.4eV. The suppression of the defects by high temperature annealing undoped InP leads to the manufacture of high quality SI-InP with high mobility and good electrical uniformity. A technology for the growth of high quality SI-InP through stoichiometry control has been proposed based on the results.
Resumo:
This paper describes the high performance of narrow-beam divergence spot size converter (SSC) integrated separately confined heterostructure (SCH) LD. The upper optical confinement layer (OCL) and the butt-coupled tapered thickness waveguide were regrown simultaneously, which not only offered the separated optimization of the active region and the integrated spotsize converter, but also reduced the difficulty of the butt-joint selective regrowth. The threshold current was as low as 5.4 mA, the output power at 55 mA was 10.1 mW, the vertical and horizontal far field divergence angles were as low as 9°and 15°, and the 1-dB misalignment tolerances were 3.6 and 3.4μm, respectively.
Resumo:
Properties of Fe-doped semi-insulating (SI) InP with different iron concentrations are studied by using Hall effect, current-voltage (I-V), photoluminescence spectroscopy (PL) and photocurrent spectroscopy (PC) measurements. I-V characteristics of SI InP strongly depend on Fe doping concentration. Fe doping concentration also influences optical properties and defective formation in as-grown SI InP. Band-gap narrowing phenomenon and defects in Fe doped SI InP are studied using PI and PC.
Resumo:
Semi-insulating (SI) InP wafers of 50 and 75mm in diameter can be obtained by annealing of undoped liquid encapsulated Czochralski (LEC) InP at 930 ℃ for 80h. The annealing ambient can be pure phosphorus (PP) or iron phosphide (IP). The IP-SI InP wafers have good electrical parameters and uniformity of whole wafer. However, PP-SI InP wafers exhibit poor uniformity and electrical parameters, Photoluminescence which is subtle to deep defect appears in IP-annealed semi-insulating InP. Traps in annealed SI InP are detected by the spectroscopy of photo-induced current transient. The results indicate that there are fewer traps in IP-annealed undoped SI InP than those in as-grown Fe-doped and PP-undoped SI-undoped SI InP. The formation mechanism of deep defects in annealed undoped InP is discussed.
Resumo:
国家自然科学基金
Resumo:
We have investigated the optical properties of asymmetric multiple layer stacked self-assembled InAs quantum dot with different interlayer. We found that asymmetric multiple stacked QD samples with In0.2Ga0.8As + GaAs interlayer can afford a 180nm flat spectral width with strong PL intensity compared to other samples at room temperature. We think this result is due to the introduction of In0.2Ga0.8As strain-reducing layer. Additionally, for the broad spectral width and the strong PL intensity, this structure can be a promising candidate for quantum-dot superluminescent diodes.
Resumo:
Polymorphous Si nanowires (SiNWS) have been successfully synthesized on Si wafer by plasma enhanced chemical vapor deposition (PECVD) at 440degreesC,using silane as the Si source and Au as the catalyst. To grow the polymorphous SiNWS preannealing the Si substrate with Au film at 1100 degreesC is needed. The diameters of Si nanowires range from 15 to 100 urn. The structure morphology and chemical composition of the SiNWS have been characterized by high resolution x-ray diffraction, scanning electron microscopy, transmission electron microscopy, as well as energy dispersive x-ray spectroscopy. A few interesting nanowires with Au nanoclusters uniformly distributed in the body of the wire were also produced by this technique.
Resumo:
A kind of hydrogenated diphasic silicon films has been prepared by a new regime of plasma enhanced chemical vapor deposition (PECVD) near the phase transition regime from amorphous to nanocrystalline. The microstructural properties of the films have been investigated by the micro-Raman and Fourier transformed Infrared (FT-IR) spectra and atom force microscopy (AFM). The obtained Raman spectra show not only the existence of nanoscaled crystallites, but also a notable improvement in the medium-range order of the diphasic films. For the FT-IR spectra of this kind of films, it notes that there is a blueshift in the Si-H stretching mode and a redshift in the Si-H wagging mode in respect to that of typical amorphous silicon film. We discussed the reasons responsible for these phenomena by means of the phase transition, which lead to the formation of a diatomic hydrogen complex, H-2* and their congeries.
Resumo:
The semiconductor microlasers based on the equilateral triangle resonator (ETR) can be fabricated from the edge-emitting laser wafer by dry-etching technique, and the directional emission can be obtained by connecting an output waveguide to one of the vertices of the ETR. We investigate the mode characteristics, especially the mode quality factor, for the ETR with imperfect vertices, which is inevitable in the real technique process. The numerical simulations show that the confined modes can still have a high quality factor in the ETR with imperfect vertices. We can expect that the microlasers is a suitable light source for photonic integrated circuits.
Resumo:
The semiconductor microlasers with an equilateral triangle resonator which can be fabricated by dry etching technique from the laser wafer of the edge emitting laser, are analyzed by FDTD technique and rate equations. The results show that ETR microlaser is suitable to realize single mode operation. By connecting an output waveguide to one of the vertices of the ETR, we still can get the confined modes with high quality factors. The EM microlasers are potential light sources for photonic integrated circuits.