Resumo:
The size and distribution of surface features of porous silicon layers have been investigated by scanning tunneling and atomic force microscopy. Pores and hillocks down to 1-2 nm size were observed, with their shape and distribution on the sample surface being influenced by crystallographic effects. The local density of electronic states show a strong increase above 2 eV, in agreement with recent theoretical predictions.
Resumo:
The photoluminescence (PL) response of porous silicon is usually in the form of a single broad peak. Recently, however, PL response with two peaks has been reported. Here we report the observation of multiple peaks in the PL spectrum of porous silicon. A simple modeling of the line shape indicates that four peaks exist within the response curve, and analysis suggests that the PL of porous silicon is derived from quantum confinement in the silicon crystallites. The line shapes can be due to either minibands within the conduction and valence bands or crystallite size variation or a combination of the two.
Resumo:
A theoretical model for the electronic structure of porous Si is presented. Three geometries of porous Si (wire with square cross section, pore with square cross section, and pore with circular cross section) along both the [001] and [110] directions are considered. It is found that the confinement geometry affects decisively the ordering of conduction-band states. Due to the quantum confinement effect, there is a mixing between the bulk X and GAMMA states, resulting in finite optical transition matrix elements, but smaller than the usual direct transition matrix elements by a factor of 10(-3). We found that the strengths of optical transitions are sensitive to the geometry of the structure. For (001) porous Si the structure with circular pores has much stronger optical transitions compared to the other two structures and it may play an important role in the observed luminescence. For this structure the energy difference between the direct and the indirect conduction-band minima is very small. Thus it is possible to observe photoluminescence from the indirect minimum at room temperature. For (110) porous Si of similar size of cross section the energy gap is smaller than that of (001) porous Si. The optical transitions for all three structures of (110) porous Si tend to be much stronger along the axis than perpendicular to the axis.
Resumo:
The microstructures in iron- and sulphur-doped InP crystals were studied using both electron microscopy and electron diffraction. A modulated structure has been found in S-doped InP crystal, where the commensurate modulations corresponded to periodicities of 0.68 nm and 0.7 nm in real space and were related to the reflections of the cubic lattice in [111] and [113BAR] directions; they were indexed as q111* = 1/2(a* + b* + c*) and q113BAR* = 1/4(-a* - b* + 3c*), respectively. Single atomic layers of iron precipitate were observed, with preferred orientations along which precipitates are formed. Simulated calculations by means of the dynamical theory of electron diffraction using models for the precipitate structure were in good agreement with our experimental results. The relation between the modulated structure and the precipitates is also discussed.
Resumo:
A low resistance and shallow ohmic contact to n-GaAs is performed by using Ge/Pd/GaAs trilayer structure and rapid thermal annealing process. The dependence of specific contact resistivity on the temperature of rapid thermal annealing is investigated. A good ohmic contact is formed after annealing at 400-500 degrees C for 60 s. The best specific contact resistivity is 1.4 x 10(-6) Omega cm(2). Auger electron spectroscopy (AES), secondary ion mass spectrometry (SIMS) and scanning electron microscopy (SEM) are used to analyze the interfacial microstructure. A strong correlation between the contact resistance and the film microstructure is observed.
Resumo:
Photoluminescence studies on porous silicon show that there are luminescence centers present in the surface states. By taking photoluminescence spectra of porous silicon with respect to temperature, a distinct peak can be observed in the temperature range 100-150 K. Both linear and nonlinear relationships were observed between excitation laser power and the photoluminescence intensity within this temperature range. In addition, there was a tendency for the photoluminescence peak to red shift at low temperature as well as at low excitation power. This is interpreted as indicating that the lower energy transition becomes dominant at low temperature and excitation power. The presence of these luminescence centers can be explained in terms of porous silicon as a mixture of silicon clusters and wires in which quantum confinement along with surface passivation would cause a mixing of Gamma and X band structure between the surface states and the bulk. This mixing would allow the formation of luminescence centers.
Resumo:
A new technique to fabricate silicon condenser microphone is presented. The technique is based on the use of oxidized porous silicon as sacrificial layer for the air gap and the heavy p~+-doping silicon of approximately 15μm thickness for the stiff backplate. The measured sensitivity of the microphone fabricated with this technique is in the range from -45dB (5.6mV/Pa) to -55dB (1.78mV/Pa) under the frequency from 500Hz to 10kHz, and shows a gradual increase at high frequency. The cut-off frequency is above 20kHz.
Resumo:
A kind of hydrogenated diphasic silicon films has been prepared by a new regime of plasma enhanced chemical vapor deposition (PECVD) near the phase transition regime from amorphous to nanocrystalline. The microstructural properties of the films have been investigated by the micro-Raman and Fourier transformed Infrared (FT-IR) spectra and atom force microscopy (AFM). The obtained Raman spectra show not only the existence of nanoscaled crystallites, but also a notable improvement in the medium-range order of the diphasic films. For the FT-IR spectra of this kind of films, it notes that there is a blueshift in the Si-H stretching mode and a redshift in the Si-H wagging mode in respect to that of typical amorphous silicon film. We discussed the reasons responsible for these phenomena by means of the phase transition, which lead to the formation of a diatomic hydrogen complex, H-2* and their congeries.
Resumo:
Photoluminescence (PL) from Er-implanted hydrogenated amorphous silicon suboxide (a-SiOX:H
Resumo:
A porous InAlAs structure was first obtained by electrochemical etching. Nano-pore arrays were formed when the In0.52Al0.48As membrane was anodized at constant voltages in an HF aqueous solution. These self-assembled structures showed evident blue-shift photoluminescence emissions. While a quantum size effect alone underestimates the blue-shift energy for a sample with a relatively large average pore wall thickness, a novel effect caused by the asymmetric etching is proposed to account for this phenomenon. The results inferred from the x-ray double crystal diffraction are in good agreement with the experimental data.