989 resultados para STIMULATED CURRENT SPECTROSCOPY
Resumo:
Thermally stimulated current (TSC) spectroscopy is attracting increasing attention as a means of materials characterization, particularly in terms of measuring slow relaxation processes in solid samples. However, wider use of the technique within the pharmaceutical field has been inhibited by difficulties associated with the interpretation of TSC data, particularly in terms of deconvoluting dipolar relaxation processes from charge distribution phenomena. Here, we present evidence that space charge and electrode contact effects may play a significant role in the generation of peaks that have thus far proved difficult to interpret. We also introduce the use of a stabilization temperature in order to control the space charge magnitude. We have studied amorphous indometacin as a model drug compound and have varied the measurement parameters (stabilization and polarization temperatures), interpreting the changes in spectral composition in terms of charge redistribution processes. More specifically, we suggested that charge drift and diffusion processes, charge injection from the electrodes and high activation energy charge redistribution processes may all contribute to the appearance of shoulders and 'spurious' peaks. We present recommendations for eliminating or reducing these effects that may allow more confident interpretation of TSC data.
Resumo:
The investigation of deep levels of argon-implanted LEC-grown semi-insulating GaAs with implantation dosages ranging from 1 x 10(11) to 1 x 10(15) cm-2 has been performed. Using a photoinduced transient-current spectroscopy (PITCS) it was demonstrated that, for implantation dosages below 1 X 10(13) cm-2, a negative peak or negative transient current (NTC) was observed in the temperature range from 330 to 350 K. The magnitude of this negative peak increased with dosage up to a level of 1 X 10(12) cm-2, beyond which it decreased with dosage. The dosage dependence of the EL3 peak height and the resistance of the specimen have also been investigated. It was observed that the variation of the EL3 peak height with dosage was similar to the variation of the magnitude of the negative peak, that is the EL3 peak height likewise increased with dosage up to 1 X 10(12) cm-2, and then decreased. The resistance of the original high-resistivity specimen dropped abruptly when the dosage reached 1 X 10(12) cm-2. This critical dosage (1 X 10(12) cm-2) was found to be a threshold for the generation of a highly disordered state.
Resumo:
Anomalous variations of d.c. electrical conductivity with temperature are observed in ammonium sulphate single crystals, suggesting a possible phase transition at 150°C. Measurements of thermally stimulated current also support these results. The mechanism of electrical conduction is explained on the basis of studies made on doped and quenched crystals.
Resumo:
Includes bibliographical references (p. 14).
Resumo:
Deep level transient spectroscopy (DLTS) and thermally stimulated current spectroscopy (TSC) have been used to investigate defects in semi-conducting and semi-insulating (SI) InP after high temperature annealing, respectively. The results indicate that the annealing in iron phosphide ambient has an obvious suppression effect of deep defects, when compared with the annealing in phosphorus ambient. A defect annihilation phenomenon has also been observed in Fe-doped SI-InP materials after annealing. Mechanism of defect formation and annihilation related to in-diffusion of iron and phosphorus is discussed. Nature of the thermally induced defects has been discussed based on the results. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Deep defects in annealed InP have been investigated by deep level transient capacitance spectroscopy (DLTS), photo induced current transient spectroscopy (PICTS) and thermally stimulated current spectroscopy (TSC). Both DLTS results of annealed semiconducting InP and PICTS and TSC results of annealed semi-insulating InP indicate that InP annealed in phosphorus ambient has five defects, while lid? annealed in iron phospbide ambient has two defects. Such a defect formation phenomenon is explained in terms of defect suppression by the iron atom diffusion process. The correlation of the defects and the nature of the defects in annealed InP are discussed based on the results.
Resumo:
As-grown Fe-doped semi-insulating InP single crystal has been converted into n-type low-resistance material after high temperature annealing. Defects in the InP materials have been studied by conventional Hall effect measurement, thermally stimulated current spectroscopy, deep level transient spectroscopy and X-ray diffraction respectively. The results indicate that Fe atoms in the InP material change from the substitutional to the interstitial sites under thermal activation. Consequently, the InP material loses its deep compensation centers which results in the change in types of conduction. The mechanism and cause of the phenomena have been analyzed through comparison of the sites of Fe atom occupation and activation in doping, diffusion and ion implantation processes of InP.
Resumo:
In this paper, we analyze and compare electrical compensation and deep level defects in semi-insulating ( SI) materials prepared by Fe-doping and high temperature annealing of undoped InP. Influence of deep level defects in the SI-InP materials on the electrical compensation has been studied thermally stimulated current spectroscopy (TSC). Electrical property of the Fe-doped SI-InP is deteriorated due to involvement of a high concentration of deep level defects in the compensation. In contrast, the concentration of deep defects is very low in high temperature annealed undoped SI-InP in which Fe acceptors formed by diffusion act as the only compensation centre to pin the Fermi level, resulting in excellent electrical performance. A more comprehensive electrical compensation model of SI-InP has been given based on the research results.
Resumo:
Deep level defects in as-grown and annealed SI-InP samples were investigated by thermally stimulated current spectroscopy. Correlations between electrical property, compensation ratio, thermal stability and deep defect concentration in SI-InP were revealed. An optimized crystal growth condition for high quality SI-InP was demonstrated based on the experimental results.
Resumo:
An apparent defect suppression effect has been observed in InP through an investigation of deep level defects in different semi-insulating (SI) InP materials. Quality improvement of SI-InP based on the defect suppression mechanism is presented.
Resumo:
Fe-doped semi-insulating (SI) InP has become semi-conducting (SC) material completely after annealing at 900 V for 10 hours. Defects in the SC and SI InP materials have been studied by deep level transient spectroscopy (DLTS) and thermally stimulated current spectroscopy (TSC) respectively. The DLTS only detected Fe acceptor related deep level defect with significant concentration, suggesting the formation of a high concentration of shallow donor in the SC-InP TSC results confirmed the nonexistence of deep level defects in the annealed SI-InP. The results demonstrate a significant influence of the thermally induced defects on the electrical properties of SI-InP. The formation mechanism and the nature of the shallow donor defect have been discussed based on the results.
Resumo:
Deep level defects in as-grown and annealed SI-InP samples were investigated by thermally stimulated current spectroscopy. Correlations between electrical property, compensation ratio, thermal stability and deep defect concentration in SI-InP were revealed. An optimized crystal growth condition for high quality SI-InP was demonstrated based on the experimental results.
Improvement of the electrical property of semi-insulating InP by suppression of compensation defects
Resumo:
Semi-insulating (SI) InP obtained by iron phosphide ambient annealing has very low concentration of deep level defects and better electrical property than SI-InP annealed in phosphorus ambient. The defect suppression phenomenon correlates with Fe diffusion and substitution in the annealing process. Analysis of the experimental result suggests that a high activation ratio of incorporated Fe in InP has an effect of defect suppression in Fe-doped and Fe-diffused SI-InP.
Resumo:
Deep defects in annealed InP have been investigated by deep level transient capacitance spectroscopy (DLTS), photo induced current transient spectroscopy (PICTS) and thermally stimulated current spectroscopy (TSC). Both DLTS results of annealed semiconducting InP and PICTS and TSC results of annealed semi-insulating InP indicate that InP annealed in phosphorus ambient has five defects, while lid? annealed in iron phospbide ambient has two defects. Such a defect formation phenomenon is explained in terms of defect suppression by the iron atom diffusion process. The correlation of the defects and the nature of the defects in annealed InP are discussed based on the results.