974 resultados para Optical band gap
Resumo:
Photoluminescence (PL) of strained SiGe/Si multiple quantum wells (MQW) with flat and undulated SiGe well layers was studied at different temperature. With elevated temperature from 10K, the no-phonon (NP) peak of the SiGe layers in the flat sample has firstly a blue shift due to the dominant transition converting from bound excitons (BE) to free excitons (FE), and then has a red shift when the temperature is higher than 30K because of the narrowing of the band gap. In the undulated sample, however, monotonous blue shift was observed as the temperature was elevated from 10 K to 287 K. The thermally activated electrons, confined in Si due to type-II band alignment, leak into the SiGe crest regions, and the leakage is enhanced with the elevated temperature. It results in a blue shift of the SiGe luminescence spectra.
Resumo:
ZnS1-xTex (0.02less than or equal toxless than or equal to0.3) alloys are studied by photoluminescence under hydrostatic pressure at room temperature. Only a wide emission band is observed for each sample. Its peak energy is much lower than the corresponding band gap of alloys. These bands are ascribed to the radiative annihilation of excitons bound at Te-n(ngreater than or equal to2) isoelectronic centers. The pressure coefficients of the emission bands are smaller than those of alloy band gaps from 48% to 7%. The difference of the pressure coefficient of the emission band and the band gap increases when the binding energy of Te-n centers decreases. It seems contrary to our expectation and needs further analysis. The integrated intensities of emission bands decrease with increasing pressure due to the decreasing of the absorption coefficient associated with the Te-n centers under pressure. According to this model the Stokes shifts between the emission and absorption bands of the Te-n centers are calculated, which decrease with the increasing Te composition in alloys.
Resumo:
The GaNAs alloys have been grown by metalorganic chemical vapor deposition (MOCVD) using dimethylhydrazine (DMHv) as the nitrogen precursor, triethylgallium (TEGa) and trimethylgallium (TMGa) as the gallium precursors, respectively. Both symmetric (004) and asymmetric (1 1 5) high-resolution X-ray diffraction (HRXRD) were used to determine the nitrogen content in GaNAs layers. Secondary ion mass spectrometry (SIMS) was used to obtain the impurity content. T e influence of different Ga precursors on GaNAs quality has been investigated. Phase separation is observed in the < 1 1 5 > direction when using TMGa as the Ga precursor but not observed when using TEGa. This phenomenon should originate from the parasitic reaction between the Ga and N precursors. Furthermore. samples grown with TEGa have better quality and less impurity contamination than those with TMGa. Nitrogen content of 5.742% has been achieved using TEGa and no phase separation observed in the sample. (C) 2002 Elsevier Science B.V. All rights reserved.
Photoluminescence of AlGaAs/InGaAs/GaAs pseudomorphic HEMTs with different thickness of spacer layer
Resumo:
The photoluminescence spectra of the single delta -doped AlGaAs/InGaAs/GaAs pseudomorphic HEMTs with different thickness of spacer layer were studied. There are two peaks in the PL spectra of the structure corresponding to two sub-energy levels of the InGaAs quantum well. It was found that the photoluminescence intensity ratio of the two peaks changes with the spacer thickness of the pseudomorphic HEMTs. The reasons were discussed. The possible use of this phenomenon in optimization of pseudomorphic HEMTs was also proposed. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
Under short pulse laser excitation, we have observed an extra high-energy photoluminescence (PL) emission from GaNAs/GaAs single quantum wells (QWs). It dominates the PL spectra under high excitation and/or at high temperature. By measuring the PL dependence on both temperature and excitation power and by analyzing the time-resolved PL results, we have attributed the PL peak to the recombination of delocalized excitons in QWs. Furthermore, a competition process between localized and delocalized excitons is observed in the temperature-dependent PL spectra under the short pulse excitation. This competition is believed to be responsible for the temperature-induced S-shaped PL shift often observed in the disordered alloy semiconductor system under continuous-wave excitation. (C) 2001 American Institute of Physics.
Resumo:
Photoluminescence from a GaN0.015As0.985/GaAs quantum well has been measured at 15 K under hydrostatic pressure up to 9 GPa. Both the emissions from the GaNAs well and GaAs barrier are observed. The GaNAs-related peak shows a much weaker pressure dependence compared to that of the GaAs band gap. A group of new peaks appear in the spectra when the pressure is beyond 2.5 GPa, which is attributed to the emissions from the N isoelectronic traps in GaAs. The pressure dependence of the GaNAs-related peaks was calculated using the two-level model with the measured pressure coefficients of the GaAs band gap and N level as fitting parameters. It is found that the calculated results deviate seriously from the experimental data. An increasing of the emission intensity and the linewidth of the GaNAs-related peaks was also observed and briefly discussed. (C) 2001 American Institute of Physics.
Resumo:
The effect of ion-induced damage on GaNAs/GaAs quantum wells (QWs) grown by molecular beam epitaxy employing a DC plasma as the N source was investigated. Ion-induced damage results in: (i) an observed disappearance of pendellosung fringes in the X-ray diffraction pattern of the sample; (ii) a drastic decrease in intensity and a broadening in the full-width at half-maximum of photoluminescence spectra. It was shown that ion-induced damage strongly affected the bandedge potential fluctuations of the QWs. The bandedge potential fluctuations for the samples grown with and without ion removal magnets (IRMs) are 44 and 63 meV, respectively. It was found that the N-As atomic interdiffusion at the interfaces of the QWs was enhanced by the ion damage-induced defects. The estimated activation energies of the N-As atomic interdiffusion for the samples grown with and without IRMs are 3.34 and 1.78 eV, respectively. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
This paper is a review of research and development on semiconductor materials, which covers main scientific activities in this field. The present status acid future prospects of studies on semiconductor materials, such as silicon crystals, GaAs related III-V compound semiconductor materials and GaAs, InP and silicon based quantum well and superlattice materials, quantum wires and quantum dots materials, microcavity and photonic crystals, materials for quantum computation and wide band gap materials, are briefly discussed.
Resumo:
A series of systematic experiments on the growth of high quality GaNAs strained layers on GaAs (001) substrate have been carried out by using DC active Nz plasma, assisted molecular beam epitaxy. The samples of GaNAs between 3 and 200 nm thick were evaluated by double crystal X-ray diffraction (XRD) and photoluminescence (PL) measurements. PL and XRD measurements for these samples are in good agreement. Some material growth and structure parameters affecting the properties of GaNAs/GaAs heterostructure were studied; they were: (1) growth temperature of GaNAs epilayer; (2) electrical current of active N-2 plasma; (3) Nz flow rate; (4) GaNAs growth rate; (5) the thickness of GaNAs strained layer. XRD and PL measurements showed that superlattice with distinct satellite peaks up to two orders and quantum well structure with intensity at 22 meV Fourier transform infrared spectroscopy (FWHM) can be achieved in molecular beam epitaxy (MBE) system. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
Resumo:
Eu2+-doped ZnS nanoparticles with an average size of around 3 nm were prepared, and an emission band around 530 nm was observed. By heating in air at 150 degrees C, this emission decreased, while the typical sharp line emission of Eu3+ increased. This suggests that the emission around 530 nm is from intraion transition of Eu2+: In bulk ZnS:Eu2+, no intraion transition of Eu2+ was observed because the excited states of Eu2+ are degenerate with the continuum of the ZnS conduction band. We show that the band gap in ZnS:Eu2+ nanoparticles opens up due to quantum confinement, such that the conduction band of ZnS is higher than the first excited state of Eu2+, thus enabling the intraion transition of Eu2+ to occur.
Resumo:
In this letter, we investigated the effect of the buffer layer growth conditions on the secondary hexagonal phase content in cubic GaN films on GaAs(0 0 1) substrate. The reflection high-energy electron diffraction (RHEED) pattern of the low-temperature GaN buffer layers shows that both the deposition temperature and time are important in obtaining a smooth surface. Four-circle X-ray double-crystal diffraction (XRDCD) reciprocal space mapping was used to study the hexagonal phase inclusions in the cubic GaN (c-GaN) films grown on the buffer layers. The calculation of the volume contents of the hexagonal phase shows that higher temperature and longer time deposition of the buffer layer is not preferable for growing pure c-GaN film. Under optimized condition, 47 meV FWHM of near band gap emission of the c-GaN film was achieved. (C) 2000 Elsevier Science B.V. All rights reserved.
Growth and characterization of strained superlattices delta-GaNxAs1-x/GaAs by molecular beam epitaxy
Resumo:
A series of superlattices delta-GaNxAs1-x/GaAs were grown by a DC plasma-N-2-assisted molecular beam epitaxy. The evolution of the surface reconstruction during the growth has been studied with the use of in situ reflection high-energy electron diffraction. The superlattices have been characterized by high-resolution X-ray diffraction measurements. Distinct satellite peaks indicate that the superlattices are of good quality. The N compositions in strained GaNxAs1-x monolayers are obtained from the dynamical simulations of the measured X-ray diffraction patterns. The periodicity fluctuations of N composition are obtained from a kinematical method dependent on the broadening of the satellite peaks of the X-ray diffraction. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
We report the observation of the field-driven blue shift at near absorption edge in the photo-current response spectra of delta-doped Si n-i-p-i multiple quantum wells due to the widening of the effective energy gap. This phenomenon differs from the observed results in GaAs/AlGaAs and GeSi/Si superlattices, because the physical mechanisms of forming energy band in these superlattice samples are different. Our experimental results are interpreted satisfactorily by the theoretical calculation. (C) 1999 Elsevier Science Ltd. All rights reserved.
Resumo:
Photoluminescence of ZnSe, Zn0.84Mn0.16Se alloy, and ZnSe/Zn0.84Mn0.16Se superlattice (SL) have been measured in the temperature range from 10 to 300 K. It is found that the band gap of the ZnSe was smaller than that of the Zn0.84Mn0.16Se alloy at 10 K, but larger than that of the alloy at 300 K. Then the well and barrier layers of the ZnSe/Zn0.84Mn0.16Se SL would be expected to turn over at about 180 K. This type of turn over was observed in the SL sample. The turn over took place at 80 K, somewhat lower than the expected temperature. A calculation including the strain in the ZnSe/Zn0.84Mn0.16Se SL indicates that the heavy-hole bands begin crossing at 75 K, which agrees well with experimental results. [S0163-1829(99)13127-8].
Resumo:
Radiative transition in delta-doped GaAs superlattices with a weak coupling was investigted at low temperature, The experimental results show that the transitions from both electron ground state and excited state to hole state have been observed, Based on the effective mass approximation theory, the structures of energy band and photoluminescence spectra for the samples used were calculated. Comparing the experiment with theory, a good agreement was abtained.