1000 resultados para infrared luminescence
Resumo:
The strong photoluminescence (PL) of SiOx:H prepared by plasma enhanced chemical vapor deposition has been systematically studied in conjunction with infrared and micro-Raman spectra. We have found that each PL spectrum is comprised of two Gaussian components, a main band and a shoulder. The main band might originate from amorphous silicon clusters embedded in die SiOx network, and its redshift with annealing temperature is due to expansion of the silicon clusters. The shoulder remains at about 835 nm in spite of the annealing temperature and possibly comes from luminescent defect centers. The enhanced PL spectra after 1170 degrees C annealing are attributed to the quantum confinement effects of nanocrystalline silicon embedded in the SiO2 matrix. (C) 1998 American Institute of Physics.
Resumo:
The microstructure, hydrogen bonding configurations and hydrogen content of high quality and stable hydrogenated amorphous silicon (a-Si:H) films prepared by a simple ''uninterrupted growth/annealing" plasma enhanced chemical vapor deposition technique have been investigated by Raman scattering and infrared absorption spectroscopy. The high stability a-Si:H films contain small amounts of a microcrystalline phase and not less hydrogen (10-16 at. %), particularly, the clustered phase hydrogen, Besides, the hydrogen distribution is very inhomogeneous. Some of these results are substantially distinct from those of conventional device-quality n-Si:H film or stable cr-Si:H films prepared by the other techniques examined to date. The stability of n-Si:H films appears to have no direct correlation with the hydrogen content or the clustered phase hydrogen concentration. The ideal n-Si:H network with high stability and low defect density is perhaps not homogeneous. (C) 1998 American Institute of Physics.
Resumo:
We analyze low-temperature Raman and photoluminescence spectra of MBE-grown GaN layers on sapphire. Strong and sharp Raman peaks are observed in the low frequency region. These peaks, which are enhanced by excitation in resonance with yellow luminescence transitions, are attributed to electronic transitions related to shallow donor levels in hexagonal GaN. It is proposed that a low frequency Raman peak at 11.7 meV is caused by a pseudo-local vibration mode related to defects involved in yellow luminescence transitions. The dependence of the photoluminescence spectra on temperature gives additional information about the residual impurities in these GaN layers.
Resumo:
AgI clusters in zeolite-Y (AgI/Y) were prepared by Ag+ exchange followed by reaction with NaI in solution. The formation of the clusters was determined by transmission electron microscopy and Auger electron spectroscopy. The clusters were uniform and even in size, 1.0-2.0 nm. The fluorescence spectrum of the clusters consists of two emission bands, which are attributed to AgI and Ag clusters, respectively. Photostimulated luminescence (PSL) is observed by stimulation at 675 or at 840 nm. The PSL spectrum of AgI/Y is consistent with the emission spectrum of Ag clusters and thus the PSL is considered to be caused by the charge transfer or carrier migration from the zeolite framework or from the AgI clusters to the Ag clusters. The appearance of PSL indicates that these materials may find application as a medium for erasable optical memory. (C) 1998 American Institute of Physics. [S0021-8979(98)02407-4].
Resumo:
Three new absorption bands, appearing around 670, 865 and 980 nm, are observed in BaFCl:Eu2+ phosphors. They are ascribed to F aggregates formed by association of F centers or by trapping of electrons to the primary F-n(+) (n = 2,3,4) centers. The growth curves of F and F-aggregated centers are similar and may be divided into three stages. The photostimulated luminescence (PSL) decays by stimulation into the absorption bands of F centers and of F aggregates are different; the former decay logarithmically and the latter decay hyperbolically. Some non-radiative processes related to F aggregates, such as electron migration, occur accompanying the PSL process, which may reduce the PSL efficiency and sensitivity of the phosphors. (C) 1997 Published by Elsevier Science Ltd. All rights reserved.
Resumo:
A novel process of room temperature ion beam sputtering deposition of vanadium oxide films and low temperature post annealing for uncooled infrared detectors was proposed in this work. VOx thin films with relatively low square resistance (70 K Omega / square) and large temperature coefficient of resistance (more than 3%/K) at room temperature were fabricated using this low temperature process which was very compatible with the process of uncooled infrared detectors based on micromachined technology. Furthermore, chemical composition and film surface have been characterized using X-ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM) respectively. The results showed that the main composition of the processed thin films was V2O5 and the thin films were in the process of crystallization.
Resumo:
ZnO nanoparticles were synthesized in ethanolic solution using a sol-gel method. The structural and optical properties were investigated by X-ray diffraction, transmission electron microscopy, UV absorption, and photoluminescence. After annealing at 200 degrees C, the particle size is increased and the peak of defect luminescence in the visible region is changed. A yellow emission was observed in the as-prepared sample and a green emission in the annealed sample. The change of the visible emission is related to oxygen defects. Annealing in the absence of oxygen would increase oxygen vacancies. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Wafers with normal light-emitting diode structure were grown by metal organic chemical vapor deposition system. The pressure and temperature were varied during growth of buffer layer in order to grow different types of epilayers. The cathodoluminescence results show that the interface distortion of quantum well plays an important role in radiant efficiency. The electroluminescence detections indicate that the dislocations also influence the external quantum efficiency by lowering the electron injection efficiency. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
We have investigated the evolution of exciton state filling in InAs/GaAs quantum dot (QD) structures as a function of the excitation power density by using rnicro-photoluminescence spectroscopy at different temperatures. In addition to the emission bands of exciton recombination corresponding to the atom-like S, P and D, etc. shells of QDs, it was observed that some extra states V between the S and P shells, and D' between the P and D shells appear in the spectra with increasing number of excitons occupying the QDs at a certain temperature. The emergence of these inter-shell excitonic levels is power density and temperature dependent, which is an experimental demonstration of strong exciton-exciton exchange interaction, state hybridization, and coupling of a multi-exciton system in QDs. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Intense near infrared emission was observed from Al3+ and Yb3+ ions co-implanted SiO2 film on silicon. It was found that the addition of Al3+ ions could remarkably improve the photoluminescence efficiency of Yb3+-implanted SiO2 film. No excitation power saturation was observed and trivial temperature quenching factor of 2 was achieved.
Resumo:
PL properties of Er3+ doped SiOx films containing Si nanoparticles have been studied. Er3+ emission intensity does not depend strongly upon crystallinity of Si clusters. The films can yield efficient Er3+ emission.
Resumo:
In this paper, the detection wavelength and the electron-hole wave function overlap of InAs/IrxGa1-xSb type II superlattice photodetectors are numerically calculated by using the envelope function and the transfer matrix methods. The band offset is dealt with by employing the model solid theory, which already takes into account the lattice mismatch between InAs and InxGa1-xSb layers. Firstly, the detection wavelength and the wave function overlap are investigated in dependence on the InAs and InxGa1-xSb layer thicknesses, the In mole fraction, and the periodic number. The results indicate that the detection wavelength increases with increasing In mole fraction, InAs and InxGa1-xSb layer thicknesses, respectively. When increasing the periodic number, the detection wavelength first increases distinctly for small periodic numbers then increases very slightly for large period numbers. Secondly, the wave function overlap diminishes with increasing InAs and InxGa1-xSb layer thicknesses, while it enhances with increasing In mole fraction. The dependence of the wave function overlap on the periodic number shows the same trend as that of the detection wavelength on the periodic number. Moreover, for a constant detection wavelength, the wave function overlap becomes greater when the thickness ratio of the InAs over InxGa1-xSb is larger.
Resumo:
We have demonstrated a two-contact quantum well infrared photodetector (QWIP) exhibiting simultaneous photoresponse in both the mid- and the long-wavelength atmospheric windows of 3-5 mu m and of 8-12 mu m. The structure of the device was achieved by sequentially growing a mid-wavelength QWIP part followed by a long-wavelength QWIP part separated by an n-doped layer. Compared with the conventional dual-band QWIP device utilizing three ohmic contacts, our QWIP is promising to greatly facilitate two-color focal plane array (FPA) fabrication by reducing the number of the indium bumps per pixel from three to one just like a monochromatic FPA fabrication and to increase the FPA fill factor by reducing one contact per pixel; another advantage may be that this QWIP FPA boasts broadband detection capability in the two atmospheric windows while using only a monochromatic readout integrated circuit. We attributed this simultaneous broadband detection to the different distributions of the total bias voltage between the mid- and long-wavelength QWIP parts.
Resumo:
We have demonstrated a two-color quantum well infrared photodetector (QWIP) exhibiting simultaneous photoresponse with cutoff wavelengths at 11.8 and 14.5 mu m, respectively. Strong photocurrent signals are observed at temperature of 77 K. The simultaneous two-color photoresponse is achieved by utilizing a simple design by broadening the width of the quantum well and selecting an appropriate doping density. The two peaks are attributed to the intersubband transitions from the ground state to the first excited state (bound state) and to the fifth excited state (continuum state), respectively.
Resumo:
We report a period continuously tunable, efficient, mid-infrared optical parametric oscillator (OPO) based on a fan-out periodically poled MgO-doped congruent lithium niobate (PPMgLN). The OPO is pumped by a Nd:YAG laser and a maximum idler output average power of 1.65 W at 3.93 mu m is obtained with a pump average power of 10.5 W, corresponding to the conversion efficiency of about 16% from the pump to the idler. The output spectral properties of the OPO with the fan-out crystal are analyzed. The OPO is continuously tuned over 3.78-4.58 mu m (idler) when fan-out periods are changed from 27.0 to 29.4 mu m. Compared with temperature tuning, fan-out period continuous tuning has faster tuning rate and wider tuning range.