We report the temperature-dependent photoluminescence and Raman spectra of In2O3 octahedrons synthesized by an evaporation condensation process. The luminescence obtained here is due to the defect-related deep level emission, which shows highly temperature-dependent behavior in 83-573 K range. Both the position as well as the intensity varies with temperature. Similarly, Raman spectroscopy in 83-303 K range shows temperature-dependent variation in peak intensity but no change in the peak position. Interestingly, the variation of intensity for different peaks is consistent with Placzek theory which invokes the possibility of temperature sensing. We demonstrate the reversibility of peak intensity with temperature for consecutive cycles and excellent stability of the octahedrons toward cryogenic temperature sensing. Overall, both the temperature-dependent photoluminescence and Raman spectra can be explored to determine temperature in the cryogenic range at micro/nano length scales. As an example, we evaluate the temperature-dependent Raman spectra of WO3 that undergoes a phase transition around 210 K and temperature-dependent luminescence of Rhodamine 6G (Rh6G) where intensity varies with temperature.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

High-kappa TiO2 thin films have been fabricated from a facile, combined sol-gel spin - coating technique on p and n type silicon substrate. XRD and Raman studies headed the existence of anatase phase of TiO2 with a small grain size of 18 nm. The refractive index `n' quantified from ellipsometry is 2.41. AFM studies suggest a high quality, pore free films with a fairly small surface roughness of 6 angstrom. The presence of Ti in its tetravalent state is confirmed by XPS analysis. The defect parameters observed at the interface of Si/TiO2 were studied by capacitance - voltage (C - V) and deep level transient spectroscopy (DLTS). The flat - band voltage (V-FB) and the density of slow interface states estimated are -0.9, -0.44 V and 5.24x10(10), 1.03x10(11) cm(-2); for the NMOS and PMOS capacitors, respectively. The activation energies, interface state densities and capture cross -sections measured by DLTS are E-V + 0.30, E-C - 0.21 eV; 8.73x10(11), 6.41x10(11) eV(-1) cm(-2) and 5.8x10(-23), 8.11x10(-23) cm(2) for the NMOS and PMOS structures, respectively. A low value of interface state density in both P-and N-MOS structures makes it a suitable alternate dielectric layer for CMOS applications. And also very low value of capture cross section for both the carriers due to the amphoteric nature of defect indicates that the traps are not aggressive recombination centers and possibly can not contribute to the device operation to a large extent. (C) 2015 Author(s).

Relevância:

80.00% 80.00%

Publicador:

Resumo:

We report our observation of a bleaching effect under an ultraviolet exposure in LiNbO3:Fe:Cu crystals. Two three-step recording-transferring-fixing schemes are proposed to record nonvolatile photorefractive holograms in such crystals. In the schemes two red laser beams and an ultraviolet illumination are used selectively to write the charge grating in the shallow-level Fe centers, to develop the charge grating in the deep-level Cu centers by transferring the charge grating in the Fe centers, and to fix only the charge grating in the Cu centers for unerasable read-out. Experimental results, verifications, and an optimal recording scheme are given. A comparison of the lithium niobate crystals of the same double-doping system of Fe:Mn, Ce:Mn, Ce:Cu, and Fe:Cu is outlined. (C) 2002 Optical Society of America.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Lattice-matched (Delta(a/a) = 1.8-3.4%) (001) LiGaO2 substrates have been employed for the first time to grow ZnO thin films by pulsed-laser deposition at 350-650 degrees C with oxygen partial pressure of 20Pa. XRD shows that a highly c-axis-oriented ZnO film can be deposited on (001) LiGaO2 substrate at 500 degrees C. AFM images reveal the surfaces of as-deposited ZnO films are smooth and root-mean-square values are 6.662, 5.765 and 6.834 nm at 350, 500 and 650 degrees C, respectively. PL spectra indicate only near-band-edge UV emission appears in the curve of ZnO film deposited at 500 degrees C. The deep-level emission of ZnO film deposited at 650 degrees C probably results from Li diffusion into the film. All the results illustrate substrate temperature plays a pretty important role in obtaining ZnO film with a high quality on LiGaO2 substrate by pulsed-laser deposition. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

ZnO films were grown on (0 0 0 1) LiNbO3 substrates by metal organic chemical vapor deposition (MOCVD). Annealing of ZnO films was performed in air for I h at 800 degrees C. The effects of annealing on the structural and optical properties of ZnO thin films on LiNbO3 substrates were investigated using X-ray diffraction (XRD), atomic force microscopy (AFM) and photoluminescence (PL) measurements. XRD patterns and AFM showed that the as-grown and the annealed ZnO films grown on LiNbO3 substrates had c-axis preferential orientation, the crystallinity of the ZnO films grown on LiNbO3 Substrates was improved, and the grain size increased by annealing. The PL spectra showed that the intensity of the UV near-band-edge peak was increased after annealing, while the intensity of visible peak (deep-level emission) decreased. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Zinc oxide (ZnO) thin films were grown on the beta-Ga2O3 (100) substrate by pulsed laser deposition (PLD). X-ray diffraction (XRD) indicated that the ZnO films are c-axis oriented. The optical and electrical properties of the films were investigated. The room temperature Photoluminescence (PL) spectrum showed a near band emission at 3.28 eV with two deep level emissions. Optical absorption indicated a visible exciton absorption at room temperature. The as-grown films had good electrical properties with the resistivities as low as 0.02 Omega cm at room temperature. Thus, beta-Ga2O3 (100) substrate is shown to be a suitable substrate for fabricating ZnO film. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

ZnO films prepared by the thermal oxidation of the ZnS films through thermal evaporation are reported. The as-deposited ZnS films have transformed to ZnO films completely at 400 degrees C. The 400-700 degrees C annealed films with a preferential c-axis (002) orientation have a hexagonal wurtzite structure. The band gap of ZnO films shifts towards longer wavelength with the increase of the annealing temperature. The relationship between the band gap energy of ZnO films and the grain size is discussed. The shift of the band gap energy can be ascribed to the quantum confinement effect in nanocrystal ZnO films. The photoluminescence spectra of ZnO films show a dominant ultraviolet emission and no deep level or trap state defect emission in the green region. It confirms the absence of interstitial zinc or oxygen vacancies in ZnO films. These results indicate that ZnO film prepared by this simple thermal oxidation method is a promising candidate for optoelectronic devices and UV laser. (c) 2005 Elsevier BN. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Surface-architecture-controlled ZnO nanowires were grown using a vapor transport method on various ZnO buffer film coated c-plane sapphire substrates with or without Au catalysts. The ZnO nanowires that were grown showed two different types of geometric properties: corrugated ZnO nanowires having a relatively smaller diameter and a strong deep-level emission photoluminescence (PL) peak and smooth ZnO nanowires having a relatively larger diameter and a weak deep-level emission PL peak. The surface morphology and size-dependent tunable electronic transport properties of the ZnO nanowires were characterized using a nanowire field effect transistor (FET) device structure. The FETs made from smooth ZnO nanowires with a larger diameter exhibited negative threshold voltages, indicating n-channel depletion-mode behavior, whereas those made from corrugated ZnO nanowires with a smaller diameter had positive threshold voltages, indicating n-channel enhancement-mode behavior.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The structure, formation energy, and energy levels of the various oxygen vacancies in Ta2O5 have been calculated using the λ phase model. The intra-layer vacancies give rise to unusual, long-range bonding rearrangements, which are different for each defect charge state. The 2-fold coordinated intra-layer vacancy is the lowest cost vacancy and forms a deep level 1.5 eV below the conduction band edge. The 3-fold intra-layer vacancy and the 2-fold inter-layer vacancy are higher cost defects, and form shallower levels. The unusual bonding rearrangements lead to low oxygen migration barriers, which are useful for resistive random access memory applications. © 2014 AIP Publishing LLC.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Hall effect, Raman scattering, photoluminescence spectroscopy (PL), optical absorption (OA), mass spectroscopy, and X-ray diffraction have been used to study bulk ZnO single crystal grown by a closed chemical vapor transport method. The results indicate that shallow donor impurities (Ga and Al) are the dominant native defects responsible for n-type conduction of the ZnO single crystal. PL and OA results suggest that the as-grown and annealed ZnO samples with poor lattice perfection exhibit strong deep level green photoluminescence and weak ultraviolet luminescence. The deep level defect in as-grown ZnO is identified to be oxygen vacancy. After high-temperature annealing, the deep level photoluminescence is suppressed in ZnO crystal with good lattice perfection. In contrast, the photoluminescence is nearly unchanged or even enhanced in ZnO crystal with grain boundary or mosaic structure. This result indicates that a trapping effect of the defect exists at the grain boundary in ZnO single crystal. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

(110) ZnO/(001) Nb-1 wt %-doped SrTiO3 n-n type heteroepitaxial junctions were fabricated using the pulse laser deposition method. A diodelike current behavior was observed. Different from conventional p-n junctions or Schottky diodes, the diffusion voltage was found to increase with temperature. At all temperatures, the forward current was perfectly fitted on the thermionic emission model. The band bending at the interface can qualitatively explain our results, and the extracted high ideality factor at low temperatures, as well as large saturation currents, is ascribed to the deep-level-assisted tunneling current through the junction. (C) 2008 American Institute of Physics.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This letter reports on the Raman, optical and magnetic properties of FeNi co-doped ZnO nanowires prepared via a soft chemical solution method. The microstructural investigations show that the NiFe co-dopants are substituted into wurtzite ZnO nanostructure without forming any secondary phase. The co-doped nanowires show a remarkable reduction of 34 nm (267.9 meV) in the optical band gap, while suppression in the deep-level defect transition in visible luminescence. Furthermore, these nanowires exhibit ferromagnetism and an interesting low-temperature spin glass behavior, which may arise due to the presence of disorder and strong interactions of frustrated spin moments of Ni and Fe co-dopants on the ZnO lattice sites. Copyright (C) EPLA, 2009

Relevância:

80.00% 80.00%

Publicador:

Resumo:

ZnO films have been fabricated on (0 0 1), (0 1 1) and (1 1 1) SrTiO3 (STO) substrates by metal-organic chemical vapour deposition (MOCVD). It is interesting that the ZnO films on (0 0 1) and (0 1 1) STO substrates show polar and semipolar orientations, which are different from previous reports, while the same growing direction of polar ZnO with previous results is found on (1 1 1) STO. For the atomic arrangements, two orthogonal domains and a single domain are observed on (0 0 1) and (1 1 1) STO, respectively. Photoluminescence spectra show that every sample has a sharp near-band-edge emission peak at about 3.28 eV without any deep-level emission band between 1.5 and 2.8 eV, implying a high optical quality. A violet emission around 3.0 eV is observed only in ZnO films on (0 0 1) and (0 1 1) STO substrates grown at 600 degrees C, which is discussed briefly. Additionally, the semipolar ZnO does not weaken the emission efficiency along with the reduction in the polarization effect compared with polar ZnO. These results show that high-quality polar and semipolar ZnO films can be grown on STO substrates by MOCVD.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

High-density and uniform well-aligned ZnO sub-micron rods are synthesized on the silicon substrate over a large area. The morphology, and structure of the ZnO sub-micron rods are investigated by x-ray diffraction, transmission electron microscopy and Raman spectra. It is found that the ZnO sub-micron rods are of high crystal quality with the diameter in the range of 400-600 nm and the length of several micrometres long. The optical properties were studied bill photoluminescence spectra. The results show that the intensity of the ultraviolet emission at 3.3 eV is rather high, meanwhile the deep level transition centred at about 2.38 eV is weak. The free exciton emission could also be observed at low, temperature, which implies the high optical quality of the ZnO sub-micron rods. This growth technique provides one effective way to fabricate the high crystal quality ZnO nanowires array, which is very important for potential applications in the new-type optoelectronic nanodevices.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

We demonstrate the self-organized InAs quantum dots capped with thin and In0.2Al0.8As and In0.2Ga0.8As combination layers with a large ground and first excited energy separation emission at 1.35 mum at room temperature. Deep level transient spectroscopy is used to obtain quantitative information on emission activation energies and capture barriers for electrons and holes. For this system, the emission activation energies are larger than those for InAs/GaAs quantum dots. With the properties of wide energy separation and deep emission activation energies, self-organized InAs quantum dots capped with In0.2Al0.8As and In0.2Ga0.8As combination layers are one of the promising epitaxial structures of 1.3 mum quantum dot devices. (C) 2004 American Institute of Physics.