980 resultados para Photonic band gap
Resumo:
Radiative transition in delta-doped GaAs superlattices with and without Al0.1Ga0.9As barriers is investigated by using photoluminescence at low temperatures. The experimental results show that the transition mechanism of delta-doped superlattices is very different from that of ordinary superlattices. Emission intensity of the transition from the electron first excited state to hole states is obviously stronger than that from the electron ground state to hole states due to larger overlap integral between wavefunctions of electrons in the first excited state and hole states. Based on the effective mass theory we have calculated the self-consistent potentials, optical transition matrix elements and photoluminescence spectra for two different samples. By using this model we can explain the main optical characteristics measured. Moreover, after taking into account the bandgap renormalization energy, good agreement between experiment and theory is obtained.
Resumo:
The interfacial behavior of the single quantum well (SQW) GaAs/AlxGa1-xAs electrode in HQ/BQ and Fc/Fc(+) electrolytes was characterized respectively by studying the quantum confined Stark effect and Franz-Keldysh oscillation with electrolyte electroreflectance spectroscopy. The interaction of the surface state of the SQW electrode with redox species and its effects on the distribution of external bias at the interface of the SQW electrode are discussed.
Resumo:
Current-based microscopic defect analysis methods with optical filling techniques, namely current deep level transient spectroscopy (I-DLTS) and thermally stimulated current (TSC), have been used to study defect levels in a high resistivity silicon detector (p(+)-n-n(+)) induced by very high fluence neutron (VHFN) irradiation (1.7x10(15) n/cm(2)). As many as fourteen deep levels have been detected by I-DLTS. Arrhenius plots of the I-DLTS data have shown defects with energy levels ranging from 0.03 eV to 0.5 eV in the energy band gap. Defect concentrations of relatively shallow levels (E(t) < 0.33 eV) are in the order of 10(13)cm(-3), while those for relatively deep levels (E(t) > 0.33 eV) are in the order of 10(14) cm(-3). TSC data have shown similar defect spectra. A full depletion voltage of about 27,000 volts has been estimated by C-V measurements for the as-irradiated detector, which corresponds to an effective space charge density (N-eff) in the order of 2x10(14) cm(-3). Both detector leakage current and full depletion voltage have been observed to increase with elevated temperature annealing (ETA). The increase of the full depletion voltage corresponds to the increase of some deep levels, especially the 0.39 eV level. Results of positron annihilation spectroscopy have shown a decrease of total concentration of vacancy related defects including vacancy clusters with ETA, suggesting the breaking up of vacancy clusters as possible source of vacancies for the formation of single defects during the reverse anneal.
Resumo:
Photoluminescence of GaInP under hydrostatic pressure is investigated. The Gamma valley of disordered GaInP shifts sublinearly upwards with respect to the top of the valence band with increasing pressure and this sublinearity is caused by the nonlinear relationship between lattice constant and hydrostatic pressure. The Gamma valleys of ordered GaInP rise more slowly than that of the disordered one and the relationship between the band gap and the pressure can not be explained in the same way. Taking into account the interactions between the Gamma valley and the folded L valleys, as well as, the X valleys, the experimental pressure dependences of the band gap of ordered GaInP epilayers are calculated and fitted quite well using first order perturbation theory. The results indicate that simultaneous ordering along [111] and [100] directions can occur in ordered GaInP. (C) 1996 American Institute of Physics.
Resumo:
Photoluminescence of GaInP epilayers under hydrostatic pressure is investigated. The Gamma valley of disordered GaInP shifts sublinearly upwards with respect to the top of the valence band with increasing pressure and this sublinearity is caused by the nonlinear dependence of lattice constant on the hydrostatic pressure. The Gamma valleys of ordered GaInP epilayers rise slower than that of the disordered one. Considering the interactions between the Gamma valley and folded L and X valleys, the pressure dependence of the band gap of ordered GaInP is calculated and fitted. The results demonstrate that not only ordering along [111] directions but also sometimes simultaneous ordering along [111] and [100] directions can occur in ordered GaInP. (C) 1996 American Institute of Physics.
Resumo:
Electrical, structural and reaction characteristics of In-based ohmic contacts to n-GaAs were studied. Attempts were made to form a low-band-gap interfacial phase of InGaAs to reduce the barrier height at the metal/semiconductor junction, thus yielding low-resistance, highly reliable contacts. The contacts were fabricated by e-beam sputtering Ni, NiIn and Ge targets on VPE-grown n(+)-GaAs film (approximate to 1 mu m, 2 x 10(18) cm(-3)) in ultrahigh vacuum as the structure of Ni(200 Angstrom)/NiIn(100 Angstrom)/Ge(40 Angstrom)/n(+)-GaAs/SI-GaAs, followed by rapid thermal annealing at various temperatures (500-900 degrees C). In this structure, a very thin layer of Ge was employed to play the role of heavily doping donors and diffusion limiters between In and the GaAs substrate. Indium was deposited by sputtering NiIn alloy instead of pure In in order to ensure In atoms to be distributed uniformly in the substrate; nickel was chosen to consume the excess indium and form a high-temperature alloy of Ni3In. The lowest specific contact resistivity (rho(c)) of (1.5 +/- 0.5)x 10(-6) cm(2) measured by the Transmission Line Method (TLM) was obtained after annealing at 700 degrees C for 10 s. Auger sputtering depth profile and Transmission Electron Microscopy (TEM) were used to analyze the interfacial microstructure. By correlating the interfacial microstructure to the electronical properties, InxGa1-xAs phases with a large fractional area grown epitaxially on GaAs were found to be essential for reduction of the contact resistance.
Resumo:
An LCAO scheme (linear combination of atomic orbitals) taking into account ten atomic orbitals (s-, p-, and d-type) is used to calculate the electronic structure of a vacancy present in the core of the reconstructed 90 degrees partial dislocation in silicon. The levels in the band gap are extracted using Lanczos' algorithm and a continued fraction representation of the local density of states. The three-fold degenerate stale of the ideal vacancy is split into three levels with energies 0.26, 1.1, and 1.9 eV measured from the valence band edge.
Resumo:
The electronic structure and magnetism of eskolaite are studied by using first-principles calculations where the on-site Coulomb interaction and the exchange interaction are taken into account and the LSDA+U method is used.The calculated energies of magnetic configurations are very well fitted by the Heisenberg Hamiltonian with interactions in five neighbour shells; interaction with two nearest neighbours is found to be dominant. The Neel temperature is calculated in the spin-3/2 pair-cluster approximation. It is found that the measurements are in good agreement with for the values of U and J that are close to those obtained within the constrained occupation method.The band gap is of the Mott-Hubbard type.
Resumo:
The transitions of E0 ,E0 +A0, and E+ in dilute GaAs(1-x) Nx alloys with x = 0.10% ,0.22% ,0.36% ,and 0.62% are observed by micro-photoluminescence. Resonant Raman scattering results further confirm that they are from the intrinsic emissions in the studied dilute GaAsN alloys rather than some localized exciton emissions in the GaAsN alloys. The results show that the nitrogen-induced E E+ and E0 + A0 transitions in GaAsN alloys intersect at a nitrogen content of about 0.16%. It is demonstrated that a small amount of isoelectronic doping combined with micro-photoluminescence allows direct observation of above band gap transitions that are not usually accessible in photoluminescence.
Quantum Well Intermixing of InGaAsP QWs by Impurity Free Vacancy Diffusion Using SiO_2 Encapsulation
Resumo:
Experiment on quantum well intermixing (QWI) of InGaAsP QWs by impurity free vacancy diffusion (IFVD) using SiO_2 encapsulation is reported. A maximum band gap wavelength blue-shift as large as 200nm is realized. Furthermore, an FP laser blue-shifted 21nm by QWI is fabricated with characteristics comparable with the asgrown one.
Resumo:
Properties of Fe-doped semi-insulating (SI) InP with different iron concentrations are studied by using Hall effect, current-voltage (I-V), photoluminescence spectroscopy (PL) and photocurrent spectroscopy (PC) measurements. I-V characteristics of SI InP strongly depend on Fe doping concentration. Fe doping concentration also influences optical properties and defective formation in as-grown SI InP. Band-gap narrowing phenomenon and defects in Fe doped SI InP are studied using PI and PC.
Resumo:
The photoluminescence from ZnS1-xTex alloy with 0 < x < 0.3 was investigated under hydrostatic pressure up to 7 GPa. Two peaks were observed in the alloys with x < 0.01, which are related to excitons bound to isolated Te isoelectronic impurities (Te-1 centers) and Te pairs (Te-2 centers), respectively. Only the Te-2 related emissions were observed in the alloys with 0.01 < x < 0.03. The emissions in the alloys with 0.03 < x < 0.3 are attributed to the excitons bound to the Te-n (n greater than or equal to 3) cluster centers. The pressure coefficient of the Te-1 related peak is 89(4) meV/GPa, about 40% larger than that of the band gap of ZnS. On the other hand, the pressure coefficient of the Te-2 related emissions is only 52(4) meV/GPa, about 15% smaller than that of the ZnS band gap. A simple Koster-Slater model has been used to explain the different pressure behavior of the Te-1 and Te-2 centers. The pressure coefficient of the Te-3 centers is 62(2) meV/GPa. Then the pressure coefficients of the Te-n centers decrease rapidly with further increasing Te composition.
Resumo:
Photoluminescence (PL) of strained SiGe/Si multiple quantum wells (MQW) with flat and undulated SiGe well layers was studied at different temperature. With elevated temperature from 10K, the no-phonon (NP) peak of the SiGe layers in the flat sample has firstly a blue shift due to the dominant transition converting from bound excitons (BE) to free excitons (FE), and then has a red shift when the temperature is higher than 30K because of the narrowing of the band gap. In the undulated sample, however, monotonous blue shift was observed as the temperature was elevated from 10 K to 287 K. The thermally activated electrons, confined in Si due to type-II band alignment, leak into the SiGe crest regions, and the leakage is enhanced with the elevated temperature. It results in a blue shift of the SiGe luminescence spectra.
Resumo:
A series of systematic experiments on the growth of high quality GaNAs strained layers on GaAs (001) substrate have been carried out by using DC active Nz plasma, assisted molecular beam epitaxy. The samples of GaNAs between 3 and 200 nm thick were evaluated by double crystal X-ray diffraction (XRD) and photoluminescence (PL) measurements. PL and XRD measurements for these samples are in good agreement. Some material growth and structure parameters affecting the properties of GaNAs/GaAs heterostructure were studied; they were: (1) growth temperature of GaNAs epilayer; (2) electrical current of active N-2 plasma; (3) Nz flow rate; (4) GaNAs growth rate; (5) the thickness of GaNAs strained layer. XRD and PL measurements showed that superlattice with distinct satellite peaks up to two orders and quantum well structure with intensity at 22 meV Fourier transform infrared spectroscopy (FWHM) can be achieved in molecular beam epitaxy (MBE) system. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
Resumo:
We have measured photoluminescence of ZnSxTe1-x alloys (x > 0.7) at 300 K and under hydrostatic pressure up to 7 GPa. The spectra contain only a broad emission band under excitation of the 406.7 nm line. Its pressure coefficients are 47, 62 and 45 meV/GPa for x = 0.98, 0.92 and 0.79 samples, which are about 26%, 7% and 38% smaller than that of the band gap in the corresponding alloys. The Stokes shifts between emission and absorption of the bands were calculated by fitting the pressure dependence of the emission intensity, being 0.29, 0.48 and 0.13 eV for the three samples, respectively. The small pressure coefficient and large Stokes shift indicate that the emission band observed in our samples may correspond to the Te isoelectronic center in the ZnSxTe1-x alloy.