888 resultados para Silica incorporation
Novel triplexing-filter design using silica-based direction coupler and an arrayed waveguide grating
Resumo:
A new triplexing filter based on a silica direction coupler and an arrayed waveguide grating is presented. Using a combination of a direction coupler and an arrayed waveguide grating, a 1310-nm channel is multiplexed and 1490- and 1550-nm channels are demultiplexed for fiber-to-the-home. The direction coupler is used to coarsely separate the 1310-nm channel from the 1490- and 1550-nm channels. Subsequently, an arrayed waveguide grating is used to demultiplex the 1490- from 1550-nm channel. The simulated spectra show the 1-dB bandwidth of 110 nm for the 1310-nm channel and 20 and 20.5 nm for the 1490- and 1550-nm channels. The insertion loss is only 0.15 dB for 1310 nm and 5 dB for 1490 and 1550 nm. The crosstalk between the 1490- and 1550-nm channels was less than -35 dB. (C) 2009 Society of Photo-Optical Instrumentation Engineers. [DOI 10.1117/1.3065508]
Resumo:
Silica-based 64-channel arrayed waveguide gratings (AWGs) with double functions and 0.4 nm (50 GHz) channel spacing have been designed and fabricated. On the same component, Gauss and flat-top output response spectra are obtained simultaneously. The test results show that when the insertion loss ranges from 3.5 dB to 6 dB,the crosstalk is better than -34 dB, the 1 dB bandwidth is 0.12 nm, the 3 dB bandwidth is 0,218 nm, and the polarization-dependent loss (PDL) is less than 0.5 dB for Gauss response. When the insertion loss ranges,from 5.8 dB to 7.8 dB, the crosstalk is better than -30 dB, the 1 dB bandwidth is 0.24 nm, the 3 dB bandwidth is 0.33 nm, and the PDL is less than 0.2 dB for flat-top response.
Resumo:
The composite films of the nanocrystalline GaAs1-xSbx-SiO2 have been successfully deposited on glass and GaSb substrates by radio frequency magnetron co-sputtering. The 10K photoluminescence (PL) properties of the nanocrystalline GaAs1-xSbx indicated that the PL peaks of the GaAs1-xSbx nanocrystals follow the quantum confinement model very closely. Optical transmittance spectra showed that there is a large blue shift of optical absorption edge in nanocrystalline GaAs1-xSbx-SiO2 composite films, as compared with that of the corresponding bulk semiconductor, which is due to the quantum confinement effect.
Resumo:
This work demonstrates the condition optimization during liquid phase deposition (LPD) Of SiO2/GaAs films. LPD method is further applied to form Al2O3 films on semiconductors with poison-free materials. Proceeding at room temperature with inexpensive equipment, LPD of silica and alumina films is potentially serviceable in microelectronics and related spheres.
Resumo:
The preparation of metal alloy and monoelemental nanoclusters in silica by Ag, Cu ion sequential implantation and annealing in selected oxidizing or reducing atmosphere is studied. The formation of metastable Ag-Cu alloy is verified in the as-implanted samples by optical absorption spectra, selected area electron diffraction and energy dispersive spectrometer spectrum. The alloy is discomposed at elevated annealing temperature in both oxidizing and reducing atmospheres. The different effects of annealing behaviors on the Ag Cu alloy nanoclusters are investigated. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
This paper presents a detailed study on the effects of carbon incorporation and substrate temperature on structural, optical, and electrical properties of p-type nanocrystalline amorphous silicon films. A p-nc-SiC: H thin film with optical gap of 1.92 eV and activation energy of 0.06 eV is obtained through optimizing the plasma parameters. By using this p-type window layer, single junction diphasic nc-SiC : H/a-Si : H solar cells have been successfully prepared with a V-oc of 0.94 eV.
Resumo:
The effect of Al incorporation on the AlGaN growth by metalorganic chemical vapor deposition is investigated. With the increase of trimethylalluminum (TMAl) flux, the crystal quality becomes worse, and the epilayer surface becomes rougher. An interesting phenomenon is that the growth rate of AlGaN decrease with increasing TMAl flux, which is opposite to the AlN growth rate dependence on the TMAl flux. All these effects are attributed to the different properties of At atoms due to the higher bond strength of Al-N compared with Ga-N, which lead to lower surface mobility and stronger competitive ability of Al atoms during the growth. The enhancement of the surface mobility of Al is especially important for improving the quality of AlGaN. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The GaSb and Ga0.62In0.38Sb nanocrystals were embedded in the SiO2 films by radio-frequency magnetron co-sputtering and were grown on GaSb and Si substrates at different temperatures. We present results on the 10K excitonic photoluminescence (PL) properties of nanocrystalline GaSb and Ga0.62In0.38Sb as a function of their size. The measurements show that the PL of the GaSb and Ga0.62In0.38Sb nanocrystallites follows the quantum confinement model very closely. By using deconvolution of PL spectra, origins of structures in PL were identified. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
We investigated the effects of concomitant In- and N-incorporation on the photoluminescence (PL) of GaInNAs grown by molecular beam epitaxy. In comparison with the N-free GaInAs epilayer, the PL spectra of the GaInNAs epilayer exhibit an anomalous S-shape temperature dependence of dominant luminescence peak. Through further careful inspection, two PL peaks are clearly discerned and are associated with the interband excitonic recombinations and excitons bound to N-induced isoelectronic impurity states, respectively. By comparing the PL spectra of GaInNAs/ GaAs quantum wells (QWs) with those of In-free GaNAs/GaAs QWs grown under similar conditions, it is found that the concomitant In- and N-incorporation reduces the density of impurities and has an effect to improve the intrinsic optical transition of GaInNAs, but also enhance the N-induced clustering effects. At last, we found that rapid thermal annealing can significantly reduce the density of N-induced impurities. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
In this study, we first present the process of the melt epitaxial (ME) growth method, and the improvement of low-temperature electron mobility of the long-wavelength InAsSb epilayers grown by ME in a fused silica boat. The electrical properties were investigated by van der Pauw measurement at 300 and 77 K. It is seen that the electron mobility of the InAsSb samples grown by graphite boat decreased from 55,700 to 26,600 cm(2)/V s when the temperature was reduced from 300 to 77 K, while for the samples grown by fused silica boat, the electron mobility increased from 52,600 at 300 K to 54,400 cm(2)/V s at 77 K. The electron mobility of 54,400cm(2)/Vs is the best result, so far, for the InAsSb materials with cutoff wavelength of 8-12 mum at 77 K. This may be attributed to the reduction of the carbon contamination by using a fused silica boat instead of a graphite boat. (C) 2002 Elsevier Science B.V. All rights reserved.
Influence of dual incorporation of In and N on the luminescence of GaInNAs/GaAs single quantum wells
Resumo:
The optical properties of above- and below-band-edge transitions have been investigated by incorporating In atoms into GaNAs/GaAs single quantum wells. The experimental results show that with increasing In concentration the interband luminescence is improved and the luminescence intensity below the band edge in GaInNAs/GaAs decreases significantly. An interpretation is given that N atoms are preferable to form a covalent bond with In than with Ga atoms in a GaInNAs alloy, due to the compensation of the atomic-size difference between In and N atoms on the GaAs substrate. The photoreflectance spectra of the GaInNAs/GaAs single quantum well support the assignment of an intrinsic mechanism to the high-energy luminescence peak. (C) 2000 American Institute of Physics. [S0003- 6951(00)01752-6].
Resumo:
We have studied the growth of GaInNAs by a plasma-assisted molecular-beam epitaxy (MBE). It was found that the N-radicals were incorporated into the epitaxial layer like dopant atoms. In the range of 400-500 degrees C, the growth temperature (T-g) mainly affected the crystal quality of GaInNAs rather than the N concentration. The N concentration dropped rapidly when T-g exceeded 500 degrees C. Considering N desorption alone is insufficient to account for the strong falloff of the N concentration with T-g over 500 degrees C, the effect of thermally-activated N surface segregation must be taken into account. The N concentration was independent of the arsenic pressure and the In concentration in GaInNAs layers, but inversely proportional to the growth rate. Based on the experimental results, a kinetic model including N desorption and surface segregation was developed to analyze quantitatively the N incorporation in MBE growth. (C) 2000 American Institute of Physics. [S0003-6951(00)00928-1].
Resumo:
A new-style silica planar lightwave circuit (PLC) hybrid integrated triplexer, which can demultiplex 1490-nm download data and 1550-nm download analog signals, as well as transmit 1310-nm upload data, is presented. It combines SiO2 arrayed waveguide gratings (AWGs) with integrated photodetectors (PDs) and a high performance laser diode (LD). The SiO2 AWGs realize the three-wavelength coarse wavelength-division multiplexing (CWDM). The crosstalk is less than 40 dB between the 1490- and 1550-nm channels, and less than 45 dB between 1310- and 1490- or 1550-nm channels. For the static performances of the integrated triplexer, its upload output power is 0.4 mW, and the download output photo-generated current is 76 A. In the small-signal measurement, the upstream 3-dB bandwidth of the triplexer is 4 GHz, while the downstream 3-dB bandwidths of both the analog and digital sections reach 1.9 GHz.
Resumo:
InGaN/GaN heterostructures have been deposited onto (0 0 0 1) sapphire by our home-made low pressure MOVPE with different growth parameters. It has been noted that the indium incorporation depends by a complex way on a number of factors. In this work, the effect of substrate temperature, trimethylindium input flow and V/III ratio on the indium incorporation has been investigated. Finally, by optimizing the growth parameters, we made a series of single-phase InGaN samples with indium content from 10% up to 45%.