127 resultados para Ferroelectric films
Resumo:
Detailed room temperature micro-Raman scattering, X-ray diffraction, atomic force microscopy and specular reflectance infrared Fourier transform spectroscopy studies were carried out on soft chemical by processed Pb1-xBaxTiO3 thin films. The micro-Raman spectra pointed the existence of a stable tetragonal ferroelectric phase in the entire composition range (0 < x <= 1). The infrared reflectance spectra showed that the frequency of several peaks decreases as the Ba2+ concentration increases. These features are correlated to a decrease in the tetragonal distortion of the TiO6 octahedra as the Ba2+ concentration increases. Furthermore, as x increases from 0.70 to 1.0, the Raman spectrum shows an evolution towards the well-known Raman spectrum of the tetragonal BaTiO3. Therefore, we demonstrated that the combination of solid solution PbTiO3-BaTiO3 with a grain size in the order of 30-40 nm supports the tetragonal ferroelectric phase at room temperature. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Strontium bismuth tantalate thin films were prepared on several substrates (platinized silicon (PvTi/SiO2/Si), n-type (100)-oriented and p-type (111)-oriented silicon wafers, and fused silica) by the solution deposition method. The resin was obtained by the polymeric precursor method, based on the Pechini process, using strontium carbonate, bismuth oxide, and tantalum ethoxide as starting reagents. Characterizations by XRD and SEM were performed for structural and microstructural evaluations. The electrical measurements, carried on the MFM configuration, showed P-r values of 6.24 muC/cm(2) and 31.5 kV/cm for the film annealed at 800 degreesC. The film deposited onto fused silica and treated at 700 degreesC presented around 80 % of transmittance.
Resumo:
Pb1-xCaxTiO3 (0.10less than or equal toxless than or equal to0.40) thin films on Pt/Ti/SiO2/Si(100) substrates were prepared by the soft solution process and their characteristics were investigated as a function of the calcium content (x). The structural modifications in the films were studied using x-ray diffraction and micro-Raman scattering techniques. Lattice parameters calculated from x-ray data indicate a decrease in lattice tetragonality with the increasing content of calcium in these films. Raman spectra exhibited characteristic features of pure PbTiO3 thin films. Variations in the phonon mode wave numbers, especially those of lower wave numbers, of Pb1-xCaxTiO3 thin films as a function of the composition corroborate the decrease in tetragonality caused by the calcium doping. As the Ca content (x) increases from 0.10 to 0.40, the dielectric constant at room temperature abnormally increased at 1 kHz from 148 to 430. Also calcium substitution decreased the remanent polarization and coercive field from 28.0 to 5.3 muC/cm(2) and 124 to 58 kV/cm, respectively. These properties can be explained in terms of variations of phase transition (ferroelectric-paraelectric), resulting from the substitution the lead site of PbTiO(3)for the nonvolatile calcium. (C) 2002 American Institute of Physics.
Resumo:
SrBi2(Ta0.5Nb0.5)(2)O-9 (SBTN) thin films were obtained by polymeric precursor method on Pt/Ti/SiO2/Si(1 0 0) substrates. The film is dense and crack-free after annealing at 700 degrees C for 2 h in static air. Crystallinity and morphological characteristic were examined by X-ray diffraction (XRD), field emission scanning electron microscopy (FEG-SEM) and atomic force microscopy (AFM). The films displayed rounded grains with a superficial roughness of 3.5 nm. The dielectric permittivity was 122 with loss tangent of 0.040. The remanent polarization (P-r) and coercive field (E-c) were 5.1 mu C/cm(2) and 96 kV/cm, respectively. (C) 2007 Published by Elsevier B.V.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Dielectric and Raman scattering experiments were performed on polycrystalline Pb(1-x)Ba(x)TiO(3) thin films (x=0.40 and 0.60) as a function of temperature. The dielectric study on single phase compositions revealed that a diffuse-type phase transition occurred upon transformation of the cubic paraelectric to the tetragonal ferroelectric phase in all thin films, which showed a broadening of the dielectric peak. Diffusivity was found to increase with increasing barium contents in the composition range under study. In addition, the temperature dependence of Raman scattering spectra was investigated through the ferroelectric phase transition. The temperature dependence of the phonon frequencies was used to characterize the phase transitions. Raman modes persisted above the tetragonal to cubic phase transition temperature, although all optical modes should be Raman inactive. The origin of these modes was interpreted as a breakdown of the local cubic symmetry by chemical disorder. The lack of a well-defined transition temperature and the presence of broadbands in some temperature intervals above the paraferroelectric phase transition temperature suggest a diffuse-type phase transition. (C) 2008 American Institute of Physics.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
LiNbO3 thin films were prepared from polymeric precursor method by dip coating. The precursor films, deposited on Si(111) substrates, were heat-treated from 400°C to 900°C in order to study the heat treatment influence on the crystallinity and microstructure of the final film. The X-ray diffraction patterns showed, in particular, that these films crystallize at low temperature (450°C) and present no preferential orientation. The scanning electron microscopy studies showed that the film microstructure is strongly influenced by the annealing temperature. © 1997 Trans Tech Publications.
Resumo:
Flexible and free-standing films of piezoelectric composites made up of lead zirconate titanate (PZT) ceramic powder dispersed in a castor oil-based polyurethane (PU) matrix were obtained by spin coating and characterized as materials for sensor applications. The piezoelectric coefficients d 31 and d 33 were measured with the usual technique. The piezoelectric charge constant d 33 yields values up to ≤24 pC/N, even at lower PZT content (33 vol%). Some desirable properties like piezoelectricity, flexibility and good mechanical resistance show this new material to be a good alternative for use as sensors and actuators.
Resumo:
Polycrystalline SrBi2Nb2O9-layered ferroelectric thin films were synthesized on Pt/Ti/SiO2/Si substrate using the polymeric precursors solution. The dip-coated films were specular and crack-free and crystallized during firing at 700 °C. Single-, double-, and triple-layered films were obtained by several dips in the deposition solution, and the influence of crystallization between each dip was studied. Microstructure and morphological evaluation were followed by grazing incident x-ray diffraction (GIXRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). Multilayered films obtained using the intermediate-crystallized layer route present a dense microstructure with spherical grains, with a preferential orientation in the 〈215〉 direction; films obtained using the intermediate-amorphous layer route are polycrystalline and present elongated grains around 250 nm in size.
Resumo:
Polymeric precursor solution was used to deposit LiNbO3 thin films by dip coating on sapphire substrates. The effects of processing variables, such as heat treatment conditions and number of deposited layers, on crystallinity and morphology of the final films were investigated. X-ray diffraction patterns show the oriented growth of the films. The rocking curves, obtained around the (006) LiNbO3 peak, revealed that the shape peak and the FWHM value were influenced by the processing variables. According to these parameters, some films presented very homogeneous dense and smooth surfaces, as shown by the SEM and AFM studies.
Resumo:
The effects of heat-treatment temperature on LiNbO3 thin films prepared by the polymeric precursor method were investigated. The precursor solution was deposited on Si(111) substrates by dip coating. X-ray diffraction and thermal analyses revealed that the crystallization process occurred at a low temperature (420 °C) and led to films with no preferential orientation. High-temperature treatments promoted formation of the LiNb3O8 phase. Scanning electron microscopy, coupled with energy dispersive spectroscopy analyses, showed that the treatment temperature also affected the film microstructure. The surface texture - homogeneous, smooth, and pore-free at low temperature - turned into an `islandlike' microstructure for high-temperature treatments.
Resumo:
Strontium barium niobate (SBN) thin films were crystallized by conventional electric furnace annealing and by rapid-thermal annealing (RTA) at different temperatures. The average grain size of films was 70 nm and thickness around 500 nm. Using x-ray diffraction, we identified the presence of polycrystalline SBN phase for films annealed from 500 to 700 °C in both cases. Phases such as SrNb2O6 and BaNb2O6 were predominantly crystallized in films annealed at 500 °C, disappearing at higher temperatures. Dielectric and ferroelectric parameters obtained from films crystallized by conventional furnace and RTA presented essentially the same values.
Resumo:
Strontium bismuth tantalate thin films were prepared on several substrates (platinized silicon (Pt/Ti/SiO 2 /Si), n -type (100)-oriented and p -type (111)-oriented silicon wafers, and fused silica) by the solution deposition method. The resin was obtained by the polymeric precursor method, based on the Pechini process, using strontium carbonate, bismuth oxide, and tantalum ethoxide as starting reagents. Characterizations by XRD and SEM were performed for structural and microstructural evaluations. The electrical measurements, carried on the MFM configuration, showed P r values of 6.24 μC/cm 2 and 31.5 kV/cm for the film annealed at 800 C. The film deposited onto fused silica and treated at 700 C presented around 80% of transmittance. © 2002 Taylor & Francis.
Resumo:
Recently, piezoelectric cellular polypropylene (PP) was proposed as a new type of quasi-ferroelectric. The observed hysteresis of the charge density as a function of the electric field could be explained as field-dependent charging inside the gas-filled voids. Interestingly enough, the measurable poling behavior of the macroscopic dipoles formed by charges that are trapped at the internal void surfaces is phenomenologically completely identical to the cooperative poling behavior of microscopic molecular dipoles in ferroelectric polymers. Therefore, it can be assumed that charge separation (or charge redistribution) and subsequent trapping in cellular PP is a rather fast switching process. In order to examine the poling dynamics, we developed an experimental setup for pulsed poling. High-voltage pulses with a duration of 45 μs (FWHM) were applied in direct contact to two-side metallized cellular PP films. The pulsed poling yields piezoelectricity in the cellular PP. We study and discuss the dependence of the resulting piezoelectricity on the poling field. We also characterize the charge separation during application of higher electric poling fields of up to -10 kV in direct contact to the two-side metallized films for longer times.