Resumo:
Neutron-irradiated high-resistivity silicon detectors have been subjected to elevated temperature annealing (ETA). It has been found that both detector full depletion voltage and leakage current exhibit abnormal annealing (or ''reverse annealing'') behaviour for highly irradiated detectors: increase with ETA. Laser induced current measurements indicate a net increase of acceptor type space charges associated with the full depletion voltage increase after ETA. Current deep level transient spectroscopy (I-DLTS) and thermally stimulated current (TSC) data show that the dominant effect is the increase of a level at 0.39 eV below the conduction band (E(c) - 0.39 eV) or a level above the valence band (E(v) + 0.39 eV). Candidates tentatively identified for this level are the singly charged double vacancy (V-V-) level at E(c) - 0.39 eV, the carbon interstitial-oxygen interstitial (C-i-O-i) level at E(v) + 0.36 eV, and/or the tri-vacancy-oxygen center (V3O) at E(v) + 0.40 eV.
Resumo:
Current based microscopic defect analysis methods such as current deep level transient spectroscopy (I-DLTS) and thermally stimulated current (TSC) have been further developed in accordance with the need for the defect analysis of highly irradiated (Phi(n) > 10(13) n/cm(2)) high resistivity silicon detectors. The new I-DLTS/TSC system has a temperature range of 8 K less than or equal to T less than or equal to 450 K and a high sensitivity that can detect a defect concentration of less than 10(10)/cm(3) (background noise as low as 10 fA). A new filling method using different wavelength laser illumination has been applied, which is more efficient and suitable than the traditional voltage pulse filling. It has been found that the filling of a defect level depends on such factors as the total concentration of free carriers generated or injected, the penetration length of the laser (laser wavelength), the temperature at which the filling is taking place, as well as the decay time after the filling (but before the measurement). The mechanism of the defect filling can be explained by the competition between trapping and detrapping of defect levels, possible capture cross section temperature dependence, and interaction among various defect levels in terms of charge transferring. Optimum defect filling conditions have been suggested for highly irradiated high resistivity silicon detectors.
Resumo:
Experimental study of the reverse annealing of the effective concentration of ionized space charges (N-eff, also called effective doping or impurity concentration) of neutron irradiated high resistivity silicon detectors fabricated on wafers with various thermal oxides has been conducted at room temperature (RT) and elevated temperature (ET). Various thermal oxidations with temperatures ranging from 975 degrees C to 1200 degrees C with and without trichlorethane (TCA), which result in different concentrations of oxygen and carbon impurities, have been used. It has been found that, the RT annealing of the N-eff is hindered initially (t < 42 days after the radiation) for detectors made on the oxides with high carbon concentrations, and there was no carbon effect on the long term (t > 42 days after the radiation) N-eff reverse annealing. No apparent effect of oxygen on the stability of N-eff has been observed at RT. At elevated temperature (80 degrees C), no significant difference in annealing behavior has been found for detectors fabricated on silicon wafers with various thermal oxides. It is apparent that for the initial stages (first and/or second) of N-eff reverse annealing, there may tie no dependence on the oxygen and carbon concentrations in the ranges studied.
Resumo:
We present photoluminescence studies on highly dense two-dimensional electron gases in selectively Si delta-doped GaAs/In0.18Ga0.82As/Al0.25Ga0.75As quantum wells (N(s) = 4.24 x 10(12) cm-2). Five well-resolved photoluminescence lines centered at 1.4194, 1.4506, 1.4609, 1.4695 and 1.4808 eV were observed, which are attributed to the subband excition emission. The subband separations clearly exhibit the feature of a typical quantum well with triangle and square potential. These very intensive and sharp luminescence peaks with linewidths of 2.2 to 3.5 meV indicate the high quality of the structures. Their dependence on the excitation intensity and temperatures are also discussed.
Numerical analysis of four-wave-mixing based multichannel wavelength conversion techniques in fibers
Resumo:
We numerically investigate four-wave-mixing (FWM) based multichannel wavelength conversion for amplitude-modulated signals, phase-modulated signals, together with mixed amplitude and phase modulated signals. This paper also discusses the influence of stimulated Brillouin scattering (SBS) effects on high-efficiency FWM-based wavelength conversion applications. Our simulation results show that DPSK signals are more suitable for FWM-based multichannel wavelength conversion because the OOK signals will suffer from the inevitable datapattern-dependent pump depletion. In future applications, when the modulation format is partially upgraded from OOK to DPSK, the influence of OOK signals on the updated DPSK signals must be considered when using multichannel wavelength conversion. This influence becomes severe with the increase of OOK channel number. It can be concluded that DPSK signals are more appropriate for both transmission and multichannel wavelength conversion,especially in long haul and high bit-rate system.
Resumo:
We solve the single mode coupled rate equations by computer, simulate the behavior of a gain switch of an AlGalnP red light semiconductor laser diode, and find the characteristic of FWHM of pulses changing with the amplitude of modulation signal, the bias current, and the modulated frequency. On this basis, we conduct experiments. The experiment results accord with the simulations well.
Resumo:
This paper presents an LC VCO with auto-amplitude control (AAC), in which pMOS FETs are used,and the varactors are directly connected to ground to widen the linear range of Kvco. The AAC circuitry adds little noise to the VCO but provides it with robust performance over a wide temperature and carrier frequency range.The VCO is fabricated in a chartered 50GHz 0.35μm SiGe BiCMOS process. The measurements show that it has - 127. 27dBc/Hz phase noise at 1MHz offset and a linear gain of 32.4MHz/V between 990MHz and 1.14GHz.The whole circuit draws 6. 6mA current from 5V supply.
Resumo:
A passive mode-locked diode-pumped self-frequency-doubling Yb:YAB laser with a low modulation depth semiconductor saturable absorber mirror operating at 374 MHz is demonstrated. The measured pulse duration is 1.98 ps at the wavelength of 1044 nm. The maximum average power reaches 45 mW.
Resumo:
The band structure of 2D photonic crystals (PCs) and localized states resulting from defects are analyzed by finite-difference time-domain (FDTD) technique and Pade approximation. The effect of dielectric constant contrast and filling factor on photonic bandgap (PBG) for perfect PCs and localized states in PCs with point defects are investigated. The resonant frequencies and quality factors are calculated for PCs with different defects. The numerical results show that it is possible to modulate the location, width and number of PBGs and frequencies of the localized states only by changing the dielectric constant contrast and filling factor.
Resumo:
Both the vertical cavity surface emitting diodes and detectors are fabricated by using the epitaxial wafer with resonant cavity structure. Their characteristics are analyzed. The light emitters have high spectral purity of 4.8nm and high electroluminescence intensity of 0.7mW while injection current is 50mA. A 1*16 array of surface emitting light device is tested on line by probes and then used for module. The light detectors have wavelength selectivity and space selectivity. The required difference in input mirror reflectivity between emitters and detectors can easily be achieved though varying the numbers of top DBR period by etching.