320 resultados para crystal structure and surface morphology
Resumo:
Carbon films with an open-ended structure were obtained by mass-selected ion-beam deposition technique at 800degreesC. Raman spectra show that these films are mainly sp(2)-bonded. In our case, threshold ion energy of 140 eV was found for the formation of such surface morphology. High deposition temperature and ion-beam current density are also responsible for the growth of this structure. Additionally, the growth mechanism of the carbon films is discussed in this article. It was found that the ions sputtered pits on the substrate in the initial stage play a key role in the tubular surface morphology. (C) 2002 American Vacuum Society.
Resumo:
Multi-sheet InGaN/GaN quantum dots (QDs) were grown successfully by surface passivation processing and low-temperature growth in metalorganic chemical vapor deposition. This method based on the principle of increasing the energy barrier of adatom hopping by surface passivation and low-temperature growth, is quite different from present methods. The InGaN quantum dots in the first layer of about 40-nm-wide and 15-nm-high grown by this method were revealed by atomic force microscopy. The InGaN QDs in upper layer grew bigger. To our knowledge, the current-voltage characteristics of multi-sheet InGaN/GaN QDs were measured for the fist time. Two kinds of resonance-tunneling-current features were observed which were attributed to the low-dimensional localization effect. Some current peaks only appeared in positive voltage for sample due to the non-uniformity of the QDs in the structure. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Carbon films were deposited by mass-selected ion beam technique with ion energies 50-200eV at a substrate temperature from room temperature to 80 degreesC,. For the energies used, smooth diamond-like carbon films were deposited at room temperature. When the substrate temperature was 600 degreesC,rough graphitic films were produced. But highly oriented carbon tubes were observed when the energies were larger than 140eV at 800 degreesC. They were perpendicular to the surface and parallel to each other. preferred orientation of graphite basic plane was observed by high-resolution electron microscopy. Shallow ion implantation and stress are responsible for this orientation.
Resumo:
CdS nanoparticies were prepared in air and their stability by air annealing was studied. A small change in crystal structure and particle size was observed by air annealing, but a rapid reduction in fluorescence was found. Through investigation, it is revealed that it is the surface change or reconstruction rather than the variation of the size or structure that decreases the fluorescence. The emission of the particles consists with two peaks which are dependent on the excitation energy. The two peaks are considered to be arisen from "two" different sizes of nanoparticles and may be explained in terms of selectively excited photoluminescence. Finally we discuss why the discrete state of nanoparticles are able to be resolved in the photoluminescence excitation spectrum, but could not be differentiated in the absorption spectrum.
Resumo:
The surface morphology of GaN grown by MOCVD on GaN/Si template was studied. Rough morphology and deep pinhole defects on some surface areas of the samples were observed and studied. The formation of rough morphology is possibly related to Ga-Si alloy produced due to poor thermal stability of template at high temperature. The deep pinhole defects generated are deep down to the surface of MBE-grown GaN/Si template. The stress originated from the large thermal expansion coefficient difference between GaN and Si may be related to the formation of the pinhole defects. The surface morphology of the GaN can be improved by optimizing the GaN/Si template and decreasing the growth temperature.
Resumo:
We demonstrate a novel oxide confined GaAs-based photonic crystal vertical cavity surface emitting laser (PC-VCSEL) operating at a wavelength of 850 nm based on coherent coupling. A ring-shaped light-emitting aperture is added to the conventional PC-VCSEL, and coherent coupling is achieved between the central defect aperture and the ring-shaped light-emitting aperture. Measurements show that under the continuous-wave (CW) injected current of 20 mA, a high power of 2 mW is obtained, and the side mode suppression ratio (SMSR) is larger than 20 dB. The average divergence angle is 4.2 degrees at the current level of 20 mA. Compared with the results ever reported, the divergence angle is reduced.
Resumo:
In this work we investigate the structural properties of symmetrically strained (GaIn)As/GaAs/Ga(PAs)/GaAs superlattices by means of x-ray diffraction, reciprocal-space mapping, and x-ray reflectivity. The multilayers were grown by metalorganic vapor-phase epitaxy on (001) GaAs substrates intentionally off-oriented towards one of the nearest [110] directions. High-resolution triple-crystal reciprocal-space maps recorded for different azimuth angles in the vicinity of the (004) Bragg diffraction clearly show a double periodicity of the x-ray peak intensity that can be ascribed to a lateral and a vertical periodicity occurring parallel and perpendicular to the growth surface. Moreover, from the intensity modulation of the satellite peaks, a lateral-strain gradient within the epilayer unit cell is found, varying from a tensile to a compressive strain. Thus, the substrate off-orientation promotes a lateral modulation of the layer thickness (ordered interface roughness) and of the lattice strain, giving rise to laterally ordered macrosteps. In this respect, contour maps of the specular reflected beam in the vicinity of the (000) reciprocal lattice point were recorded in order to inspect the vertical and lateral interface roughness correlation, A semiquantitative analysis of our results shows that the interface morphology and roughness is greatly influenced by the off-orientation angle and the lateral strain distribution. Two mean spatial wavelengths can be determined, one corresponding exactly to the macrostep periodicity and the other indicating a further interface waviness along the macrosteps. The same spatial periodicities were found on the surface by atomic-force-microscopy images confirming the x-ray results and revealing a strong vertical correlation of the interfaces up to the outer surface.
Resumo:
AlGa1-xAs/GaAs heterostructures have been grown by two different liquid phase epitaxy (LPE) modes, i.e. the supercooled and melt-etch methods, for the fabrication of highly efficient solar cells. Typical structural characteristics observed under a transmission electron microscope (TEM), an Auger energy spectrometer (AES) and corresponding device parameters were presented. The results indicated that the P+PNN+ configuration grown by the melt-etch method could be used to produce high performance, large area solar cells with effectively reducing the defects of the substrate and improving the minority carrier collection by forming a compositionally graded region in the window layer.
Resumo:
In this paper, we have prepared of a topography/chemical composition gradient polystyrene (PS) surface, i.e., an orthogonal gradient surface, to investigate the relationship between surface wettability and surface structure and chemical composition. The prepared surface shows a one-dimensional gradient in wettability in the x, y, and diagonal directions, including hydrophobic to hydrophilic, superhydrophobic to hydrophobic, superhydrophobic to superhydrophilic gradients, and so forth.