201 resultados para X-ray test
Resumo:
Cubic GaN was grown on GaAs(100) by low pressure metal organic chemical vapor deposition (MOCVD). X-ray diffraction, scanning electron microscope (SEM) and photoluminescence (PL) spectra were performed to characterize the quality of the GaN film. The PL spectra of cubic GaN thin films being thicker than 1.5 mu m were reported. Triple-crystal diffraction to analyze orientation distributions and strain of the thin films was also demonstrated.
Resumo:
Periodicity fluctuations of layer thickness and composition in a superlattice not only decrease the intensity, they also broaden the width of the satellite peaks in the x-ray diffraction pattern. In this letter, we develop a method that is dependent on the width of satellite peaks to assess periodicity fluctuations of a superlattice quickly. A linear relation of the magnitude of fluctuations, peak width and peak order has been derived from x-ray diffraction kinematical theory. By means of this method, periodicity fluctuations in strained (GaNAs)(1)(GaAs)(m) superlattices grown on GaAs substrates by molecular beam epitaxy have been studied. Distinct satellite peaks indicate that the superlattices are of high quality. The N composition of 0.25 and its fluctuation of 20% in a strained GaNxAs1-x monolayer are obtained from simulations of the measured diffraction pattern. The x-ray simulations and in situ observation results of reflection high-energy electron diffraction are in good agreement. (C) 1999 American Institute of Physics. [S0003-6951(99)00828-1].
Resumo:
We presented a series of symmetric double crystal X-ray diffraction (DCXD) measurements, (0 0 4), (2 2 0) and (2 - 2 0) diffraction, to investigate the strain relaxation in an InAs film grown on a GaAs(0 0 1) substrate. The strain tensor and rotation tensor were calculated according to the DCXD results. It is found that the misfit strain is relaxed nearly completely and the strain relaxation caused a triclinic deformation in the epilayer. The lattice parameter along the [1 1 0] direction is a little longer than that along the [1 - 1 0] direction. Furthermore, a significant tilt, 0.2 degrees, towards the [1 1 0] direction while a very slight one: 0.002 degrees, towards [1 - 1 0] direction were discussed. This anisotropic strain relaxation is attributed to the asymmetric distribution of misfit dislocations, which is also indicated by the variation of the full-width at half-maximum (FWHM) of (0 0 4) diffraction along four azimuth angles. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
A series of GaAs/InAs/GaAs samples were studied by double crystal X-ray diffraction and the X-ray dynamic theory was used to analyze the X-ray diffraction results. As the thickness of InAs layer exceeds 1.7 monolayer, 3-dimensional InAs islands appear. Pendellosung fringes shifted. A multilayer structure model is proposed to describe the strain status in the InAs islands of the sample and a good agreement is obtained between the experimental and theoretical curves.
Resumo:
X-ray photoelectron spectroscopy has been used to measure the valence band offset of the ZnO/BaTiO3 heterojunction grown by metal-organic chemical vapor deposition. The valence band offset (VBO) is determined to be 0.48 +/- 0.09 eV, and the conduction band offset (CBO) is deduced to be about 0.75 eV using the band gap of 3.1 eV for bulk BaTiO3. It indicates that a type-II band alignment forms at the interface, in which the valence and conduction bands of ZnO are concomitantly higher than those of BaTiO3. The accurate determination of VBO and CBO is important for use of semiconductor/ferroelectric heterojunction multifunctional devices.
Resumo:
The influence of band bending and polarization on the valence band offset measured by x-ray photoelectron spectroscopy (XPS) is discussed, and a modification method based on a modified self-consistent calculation is proposed to eliminate the influence and thus increasing the precision of XPS. Considering the spontaneous polarization at the surfaces and interfaces and the different positions of Fermi levels at the surfaces, we compare the energy band structures of Al/Ga-polar AlN/GaN and N-polar GaN/AlN heterojunctions, and give corrections to the XPS-measured valence band offsets. Other AlN/GaN heterojunctions and the piezoelectric polarization are also introduced and discussed in this paper.
Resumo:
X-ray photoelectron spectroscopy has been used to measure the valence band offset (VBO) at the GaN/Ge heterostructure interface. The VBO is directly determined to be 1.13 +/- 0.19 eV, according to the relationship between the conduction band offset Delta E-C and the valence band offset Delta E-V : Delta E-C = E-g(GaN) - E-g(Ge) - Delta E-V, and taking the room-temperature band-gaps as 3.4 and 0.67 eV for GaN and Ge, respectively. The conduction band offset is deduced to be 1.6 +/- 0.19 eV, which indicates a type-I band alignment for GaN/Ge. Accurate determination of the valence and conduction band offsets is important for the use of GaN/Ge based devices.
Valence band offset of MgO/TiO2 (rutile) heterojunction measured by X-ray photoelectron spectroscopy
Resumo:
The valence band offset (VBO) of MgO/TiO2 (rutile) heterojunction has been directly measured by Xray photoelectron spectroscopy. The VBO of the heterojunction is determined to be 1.6 +/- 0.3 eV and the conduction band offset (CBO) is deduced to be 3.2 +/- 0.3 eV, indicating that the heterojunction exhibits a type-I band alignment. These large values are sufficient for MgO to act as tunneling barriers in TiO2 based devices. The accurate determination of the valence and conduction band offsets is important for use of MgO as a buffer layer in TiO2 based field-effect transistors and dye-sensitized solar cells.
Resumo:
X-ray photoelectron spectroscopy has been used to measure the valence band offset (VBO) of the w-InN/h-BN heterojunction. We find that it is a type-II heterojunction with the VBO being -0.30 +/- A 0.09 eV and the corresponding conduction band offset (CBO) being 4.99 +/- A 0.09 eV. The accurate determination of VBO and CBO is important for designing the w-InN/h-BN-based electronic devices.
Resumo:
The characteristics of K alpha X-ray sources generated by p-polarized femtosecond laser-solid interactions are experimentally studied in the relativistic regime. By use of knife-edge image technique and a single-photon-counting X-ray CCD camera, we obtaine the source size, the spectrum and the conversion efficiency of the Ka X-ray sources. The experimental results show that the conversion efficiency of Ka photons reaches an optimum value of 7.08 x 10(-6)/sr at the laser intensity of 1.6 x 10(18) W/cm(2), which is different from the Reich's simulation results (Reich et al., 2000 Phys. Rev. Lett. 84 4846). We find that about 10% of laser energy is converted into the forward hot electrons at the laser intensity of 1.6 x 10(18) W/cm(2).
Resumo:
We present a novel X-ray frame camera with variable exposure time that is based on double-gated micro-channel plates (MCP). Two MCPs are connected so that their channels form a Chevron-MCP structure, and four parallel micro-strip lines (MSLs) are deposited on each surface of the Chevron-MCP. The MSLs on opposing surfaces of the Chevron-MCP are oriented normal to each other and subjected to high voltage. The MSLs on the input and output surfaces are fed high voltage pulses to form a gating action. In forming two-dimensional images, modifying the width of the gating pulse serves to set exposure times (ranging from ps to ms) and modifying the delay between each gating pulse serves to set capture times. This prototype provides a new tool for high-speed X-ray imaging, and this paper presents both simulations and experimental results obtained with the camera.
Resumo:
The composition and stain distributions in the InGaN epitaxial films are jointly measured by employing various x-ray diffraction (XRD) techniques, including out-of-plane XRD at special planes, in-plane grazing incidence XRD, and reciprocal space mapping (RSM). It is confirmed that the measurement of (204) reflection allows a rapid access to estimate the composition without considering the influence of biaxial strain. The two-dimensional RSM checks composition and degree of strain relaxation jointly, revealing an inhomogeneous strain distribution profile along the growth direction. As the film thickness increases from 100 nm to 450 nm, the strain status of InGaN films gradually transfers from almost fully strained to fully relaxed state and then more in atoms incorporate into the film, while the near-interface region of InGaN films remains pseudomorphic to GaN.