180 resultados para Substrate temperature


Relevância:

70.00% 70.00%

Publicador:

Resumo:

InAs layers were grown on GaAs by molecular beam epitaxy (MBE) at substrate temperature 450 and 480 degrees C, and the surface morphology was studied with scanning electron microscopy (SEM). We have observed a high density of hexagonal deep pits for samples grown at 450 degrees C, however, the samples grown at 480 degrees C have smooth surface. The difference of morphology can be explained by different migration of cations which is temperature dependent. Cross-sectional transmission electron microscopy (XTEM) studies showed that the growth temperature also affect the distributions of threading dislocations in InAs layers because the motion of dislocations is kinetically limited at lower temperature. (C) 1998 Elsevier Science B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Atomic force microscopy and photoluminescence spectroscopy (PL) has been used to study asymmetric bilayer InAs quantum dot (QD) structures grow by molecular-beam epitaxy on GaAs (001) substrates. The two InAs layers were separated by a 7-nm-thick GaAs spacer layer and were grown at different substrate temperature. We took advantage of the intrinsic nonuniformity of the molecular beams to grow the seed layer with an average InAs coverage of 2.0 ML. Then the seed layer thickness could be divided into three areas: below, around and above the critical thickness of the 2D-3D transition along the 11101 direction of the substrate. Correspondingly, the nucleation mechanisms of the upper InAs layer (UIL) could be also divided into three areas: temperature-controlled, competition between temperature-controlled and strain-induced, and strain-induced (template-controlled) nucleation. Small quantum dots (QDs) with a large density around 5 x 10(10) cm(-2) are found in the temperature-controlled nucleation area. The QD size distributions undergo a bimodal to a unimodal transition with decreasing QD densities in the strain-induced nucleation area, where the QD densities vary following that of the seed layer (templating effect). The optimum QD density with the UIL thickness fixed at 2.4 ML is shown to be around 1.5 x 10(10) cm(-2), for which the QD size distribution is unimodal and PL emission peaks at the longest wavelength. The QDs in the in-between area exhibit a broad size distribution with small QDs and strain-induced large QDs coexisting.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Ge composition dependence on the Ge cell temperature has been studied during the growth of Si1-xGex by disilane and solid Ge molecular beam epitaxy at a substrate temperature of 500 degrees C. It is found that the composition x increases and then saturates when the Ge cell temperature increases, which is different from the composition-dependent behavior in growth at high temperature as well as in growth by molecular beam epitaxy using disilane and germane. The enhanced hydrogen desorption from a Ge site alone cannot account for this abnormal composition-variation behavior. We attribute this behavior to the increase of rate constant of H desorption on a Si site when the Ge cell temperature increases.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The growth of highly lattice-mismatched InAs0.3Sb0.7 films on (100) GaAs Substrates by magnetron Sputtering has been investigated and even epitaxial lnAs(0.3)Sb(0.7) films have been successfully obtained. A strong effect of the growth conditions on the film structure was observed, revealing that there was a growth mechanism transition from three-dimensional nucleation growth to epitaxial layer-by-layer growth mode when increasing the substrate temperature. A qualitative explanation for that transition was proposed and the critical conditions for the epitaxial layer-by-layer growth mode were also discussed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Bulk single crystals b-FeSi2, as a new photoelectric and thermoelectric material, has been successfully grown using chemical vapor transport technique by using iodine as transport agent in a sealed ampoule. The effects of crystal growth condition on quality and morphologies of the single crystals were studied. Both needle-like and grain-like single crystals were gained. By changing substrate temperature, tetrahedral high quality a-FeSi2 single crystals were also obtained.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Gadolinium oxide thin films have been prepared on silicon (100) substrates with a low-energy dual ion-beam epitaxial technique. Substrate temperature was an important factor to affect the crystal structures and textures in an ion energy range of 100-500 eV. The films had a monoclinic Gd2O3 structure with preferred orientation ((4) over bar 02) at low substrate temperatures. When the substrate temperature was increased, the orientation turned to (202), and finally, the cubic structure appeared at the substrate temperature of 700 degreesC, which disagreed with the previous report because of the ion energy. The AES studies found that Gadolinium oxide shared Gd2O3 structures, although there were a lot of oxygen deficiencies in the films, and the XPS results confirmed this. AFM was also used to investigate the surface images of the samples. Finally, the electrical properties were presented. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Structural and optical properties were investigated for ZnO films grown on (100) and (001) gamma-LiAlO2 (LAO) substrates by pulsed laser deposition method. According XRD results, it is intuitionistic that (100) LAO is suitable for fabricating high quality ZnO film, while (001) LAO is unsuitable. The FWHM of XRD, stress in film and FWHM of UV PL spectra for ZnO films on (100) LAO show a decreasing with increasing substrate temperature from 300 to 600 degrees C. ZnO film fabricated at 600 degrees C has the greatest grain size, the smallest stress (0.47 Gpa) and PL FWHM value (similar to 85 meV). This means that the substrate temperature of 600 degrees C is optimum for ZnO film deposited on (100) LAO. Moreover, it was found that the UV PL spectra intensity of ZnO film is not only related to the grain size and stoichiometric, but also depends on the stress in the film.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Lattice-matched (Delta(a/a) = 1.8-3.4%) (001) LiGaO2 substrates have been employed for the first time to grow ZnO thin films by pulsed-laser deposition at 350-650 degrees C with oxygen partial pressure of 20Pa. XRD shows that a highly c-axis-oriented ZnO film can be deposited on (001) LiGaO2 substrate at 500 degrees C. AFM images reveal the surfaces of as-deposited ZnO films are smooth and root-mean-square values are 6.662, 5.765 and 6.834 nm at 350, 500 and 650 degrees C, respectively. PL spectra indicate only near-band-edge UV emission appears in the curve of ZnO film deposited at 500 degrees C. The deep-level emission of ZnO film deposited at 650 degrees C probably results from Li diffusion into the film. All the results illustrate substrate temperature plays a pretty important role in obtaining ZnO film with a high quality on LiGaO2 substrate by pulsed-laser deposition. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

ZnO thin films were grown on (0001)LiNbO3 substrates by the MOCVD technique. The substrate temperatures during growth were changed from 400 to 600 degrees C. The X-ray diffraction (XRD) pattern of the ZnO film showed a strong [002] reflection peak, and the peak intensity was dependent on substrate temperature. The ZnO columnar grains were highly oriented along the (002) direction when the film processing temperature was 600 degrees C. The optical transmission and PL results also indicated that highest crystalline quality of the ZnO films could be obtained at elevated temperatures. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

ZnO thin films were grown on single-crystal gamma-LiAlO2 (LAO) and sapphire (0001) substrate by pulsed laser deposition (PLD). The structural, optical and electrical properties of ZnO films were investigated. The results show that LAO is more suitable for fabricating ZnO films than sapphire substrate and the highest-quality ZnO film was attained on LAO at the substrate temperature of 550 degrees C. However, when the substrate temperature rises to 700 degrees C, lithium would diffuse from the substrate (LAO) into ZnO film which makes ZnO film on LAO becomes polycrystalline without preferred orientation, the stress in ZnO film increases dominantly and the resistivity of the film decreases exponentially. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Nonpolar a-plane (1 1 2 0) ZnO films are fabricated on (3 0 2)gamma-LiAlO2 substrate by pulsed laser deposition. When substrate temperature is low, c-plane ZnO is dominant. As growth temperature increases to similar to 500 degrees C, pure (1 1 2 0)-oriented ZnO film can be obtained. The X-ray rocking curve of a-plane ZnO film broadens sharply when growth temperature is up to similar to 650 degrees C; such a broadening may be related to the anisotropic lateral growth rate of (1 12 0)-oriented ZnO grains. Atomic force microscopy reveals the surface morphology changes of ZnO films deposited at different temperatures. Raman spectra reveal that a compressive stress exists in the a-plane ZnO film. (C) 2007 Published by Elsevier B.V.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

用脉冲激光淀积法(PLD)在(111)面SrTiO3衬底上外延生长ZnO单晶薄膜。样品分别在衬底温度为350℃、500℃、600℃下外延生长。X射线衍射(XRD)的结果表明,所得的ZnO单晶薄膜结晶性能好,只出现(002)和(004)两个衍射峰,(002)峰的半高宽度(FWHM)为0.23°。在荧光光谱中我们只观察到来源于带边激子跃迁的强UV发射,并且随着生长温度的升高,紫外峰的强度逐渐增强。样品的SEM图像表明所得ZnO薄膜表面平整,晶粒均匀。衬底温度为600℃时,所得到的ZnO薄膜结构完整,晶粒尺寸最

Relevância:

60.00% 60.00%

Publicador:

Resumo:

利用激光脉冲沉积(PLD)技术在(302)γ-LiAIO2衬底上成功生长了非极性的a面(112^-0)γZnO薄膜.衬底温度为350℃时,薄膜是混合取向(a向和C向),以c面ZnO为主,且晶粒尺寸分布很宽;提高温度达500℃,薄膜变为单一的(1120)取向,摇摆曲线半高宽O.65^o,晶粒尺寸分布趋窄,利用偏振透射谱可以明显看出其面内的各向异性.衬底温度650℃下制备的样品晶粒继续长大,虽然摇摆曲线半高宽变大,但光致发光谱(PL)带边发射峰半高宽仅为105meV,比在350℃,500℃下制备的样品小1/5

Relevância:

60.00% 60.00%

Publicador:

Resumo:

ZrO2采用X射线衍射(XRD)技术分析了不同充氧条件和沉积温度对ZrO2溥膜组成结构的影响,并对不同工艺下制备的薄膜的表面粗糙度和激光损伤阈值进行了测量。结果发现随着氧压的升高,ZrO2溥膜将由单斜相多晶态逐渐转变为非晶态结构,而随着基片温度的增加,溥膜将由非晶态逐渐转变为单斜相多晶态。同时发现随着氧压升高晶粒尺寸减小,而随着沉积温度增加,晶粒尺寸增大。氧压增加时工艺对表面粗糙度有一定程度的改善,而沉积温度升高,工艺对表面粗糙度的改善不明显。晶粒尺寸大小变化与表面粗糙度变化存在对应关系。激光损伤测量表明

Relevância:

60.00% 60.00%

Publicador:

Resumo:

用直流磁控溅射法制备透明导电锡掺杂氧化铟(ITO)薄膜,靶材为ITO陶瓷靶,组分为m(In2O3):m(SnO2)=9∶1。运用分光光度计、四探针测试仪研究了基底温度对薄膜透过率、电阻率的影响,并用X射线衍射(XRD)仪对薄膜进行结构分析。计算了晶面间距和晶粒尺寸,分析了薄膜的力学性质。实验结果表明,在实验设备条件下,直流磁控溅射ITO陶瓷靶制备ITO薄膜时,适当的基底温度(200℃)能在保证薄膜85%以上高可见光透过率下,获得最低的电阻率,即基底温度有个最佳值。薄膜的结晶度随着基底温度的提高而提高。