ZnO nanoparticles were synthesized in ethanolic solution using a sol-gel method. The structural and optical properties were investigated by X-ray diffraction, transmission electron microscopy, UV absorption, and photoluminescence. After annealing at 200 degrees C, the particle size is increased and the peak of defect luminescence in the visible region is changed. A yellow emission was observed in the as-prepared sample and a green emission in the annealed sample. The change of the visible emission is related to oxygen defects. Annealing in the absence of oxygen would increase oxygen vacancies. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The Hamiltonian in the framework of eight-band effective-mass approximation of the zinc-blende nanowires and nanorods in the presence of external homogeneous magnetic field is given in the cylindrical coordinate. The electronic structure, optical properties, magnetic energy levels, and g factors of the nanowires and nanorods are calculated. It is found that the electron states consist of many hole-state components, due to the coupling of the conduction band and valence band. For the normal bands which are monotone functions of |k(z)|, long nanorods can be modeled by the nanowires, the energy levels of the nanorods approximately equal the values of the energy band E(k(z)) of the nanowires with the same radius at a special k(z), where k(z) is the wave vector in the wire direction. Due to the coupling of the states, some of the hole energy bands of the nanowires have their highest points at k(z)=0. Especially, the highest hole state of the InSb nanowires is not at the k(z)=0 point. It is an indirect band gap. For these abnormal bands, nanorods can not be modeled by the nanowires. The energy levels of the nanorods show an interesting plait-like pattern. The linear polarization factor is zero, when the aspect ratio L/2R is smaller than 1, and increases as the length increases. The g(z) and g(x) factors as functions of the k(z), radius R and length L are calculated for the wires and rods, respectively. For the wires, the g(z) of the electron ground state increases, and the g(z) of the hole ground state decreases first, then increases with the k(z) increasing. For the rods, the g(z) and g(x) of the electron ground state decrease as the R or the L increases. The g(x) of the hole ground state decreases, the g(z) of the hole ground state increases with the L increasing. The variation of the g(z) of the wires with the k(z) is in agreement with the variation of the g(z) of the rods with the L.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

InAs quantum dots (QDs) were grown on In0.15Ga0.85As strained layers by molecular beam epitaxy on GaAs (0 0 1) substrates. Atomic force microscopy and transmission electron microscopy study have indicated that In0.15Ga0.85As ridges and InAs QDs formed at the inclined upside of interface misfit dislocations (MDs). By testifying the MDs are mixed 60 degrees dislocations and calculating the surface stress over them when they are 12-180 nm below the surface, we found the QDs prefer nucleating on the side with tensile stress of the MDs and this explained why the ordering of QDs is weak when the InGaAs layer is relatively thick. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Zinc oxide flower-like bunches were directly synthesized on indium-doped tin oxide (ITO) glass substrates through a simple chemical bath deposition process. By adjusting precursor concentration, other morphologies ( spindles and rods) were also obtained. All of them are hexagonal and single crystalline in nature and grow along the [ 0001] crystallographic direction. The possible growth mechanisms for these nano- and microcrystals were proposed. It was revealed that both the inherent highly anisotropic structure of ZnO and the precursor concentration play crucial roles in determining final morphologies of the products. In addition, vibrational properties of ZnO crystals with different morphologies were investigated by Raman spectroscopy.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Self-assembled InAs quantum dots (QDs) are grown on vicinal GaAs (100) substrates by using metal-organic chemical vapour deposition (MOCVD). An abnormal temperature dependence of bimodal size distribution of InAs quantum dots is found. As the temperature increases, the density of the small dots grows larger while the density of the large dots turns smaller, which is contrary to the evolution of QDs on exact GaAs (100) substrates. This trend is explained by taking into account the presence of multiatomic steps on the substrates. The optical properties of InAs QDs on vicinal GaAs(100) substrates are also studied by photoluminescence (PL). It is found that dots on a vicinal substrate have a longer emission wavelength, a narrower PL line width and a much larger PL intensity.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

High (42.5%) indium content GaInNAs/GaAs quantum wells with room temperature emission wavelength from 1.3 mu m to 1.5 mu m range were successfully grown by Radio Frequency Plasma Nitrogen source assisted Molecular Beam Epitaxy. The growth parameters of plasma power and N-2 How rate were optimized systematically to improve the material quality. Photoluminescence and transmission electron microscopy measurements showed that the optical and crystal quality of the 1.54 mu m GaInNAs/GaAs QWs was kept as comparable as that in 1.31 mu m.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Al0.38Ga0.62N/AIN/GaN HEMT structures have been grown by metal-organic chemical vapor deposition (MOCVD) on 2-inch sapphire substrates. Samples with AIN growth time of 0s (without AIN interlayer), 12, 15, 18 and 24s are characterized and compared. The electrical properties of two-dimensional electron gas (2DEG) are improved by introducing AIN interlayers. The AIN growth time in the range of 12-18s, corresponding to the AIN thickness of 1-1.5 nm, is appropriate for the design of Al0.38Ga0.62N/AIN/GaN HEMT structures. The lowest sheet resistance of 277 Omega sq(-1) and highest room temperature 2DEG mobility of 1460 cm(2)V(-1) s(-1) are obtained on structure with AIN growth time of 12s. The structure with AIN growth time of 15s exhibits the highest 2DEG concentration of 1.59 x 10(13) cm(-2) and the smallest RMS surface roughness of 0.2 nm. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The growth of InAs quantum dots on vicinal GaAs (100) Substrates was systematically studied using low-pressure metalorganic chemical vapor deposition (MOCVD). The dots showed a clear bimodal size distribution on vicinal substrates. The way of evolution of this bimodal size distribution was studied as a function of growth temperature, InAs layer thickness and InAs deposition rate. The optical properties of dots grown on vicinal substrates were also studied by photoluminescence (PL). It was found that, compared with dots on exact substrates, dots on vicinal substrates had better optical properties such as a narrower PL line width, a longer emission wavelength, and a larger PL intensity. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Sb-doped and undoped ZnO thin films were deposited on Si (100) substrates by radio frequency (RF) magnetron sputtering. X-ray diffraction (XRD) and scanning electron microscopy (SEM) analyses revealed that all the films had polycrystalline wurtzite structure and c-axis preferred orientation. Room temperature Hall measurements showed that the as-grown films were n-type and conducting (rho similar to 1-10 Omega cm). Annealing in a nitrogen ambient at 400 degrees C for 1 h made both samples highly resistive (rho > 10(3) Omega cm). Increasing the annealing temperature up to 800 C, the resistivity of the ttndoped ZnO film decreased gradually, but it increased for the Sb-doped ZnO film. In the end, the Sb-doped ZnO film annealed at 800 C became semi-insulating with a resistivity of 10(4)Omega cm. In addition, the effects of annealing treatment and Sb-doping on the structural and electrical properties are discussed. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

X-ray diffraction and Rutherford backscattering/channeling were used to characterize the crystalline quality of an InN layer grown on Al2O3(0001) Using metal-organic chemical-vapor deposition. A full width at half maximum of 0.27 degrees from an InN(0002) omega scan and a minimum yield of 23% from channeling measurements show that this 480-nm-thick InN layer grown at low temperature (450 degrees C) has a relatively good crystalline quality. High-resolution x-ray diffraction indicates that the InN layer contains a small fraction of cubic InN, besides the predominant hexagonal phase. From this InN sample, the lattice constants a=0.353 76 nm and c=0.570 64 nm for the hexagonal InN and a=0.4986 nm for the cubic InN were determined independently. 2 theta/omega-chi mapping and a pole figure measurement revealed that the crystallographic relationship among the cubic InN, the hexagonal InN, and the substrate is: InN[111]parallel to InN[0001]parallel to Al2O3[0001] and InN{110}parallel to InN{1120}parallel to Al2O3{1010}, and that the cubic InN is twinned. Photoluminescence measurements indicate that the band-gap energy of this sample is approximately 0.82 eV. (c) 2006 American Vacuum Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

It is found that both methods using either continuous Sb supply or pre-deposition of a very thin Sb layer are efficient for the Sb-assisted molecular beam epitaxy growth of highly strained InGaAs/GaAs quantum wells (QWs). The emission of QWs is extended to long wavelength close to 1.25 mu m with high luminescence efficiency at room temperature. The influence of rapid thermal annealing (RTA) on the photoluminescence intensity critically depends on the annealing temperature and duration for highly strained QWs. A relatively low RTA temperature of 700 degrees C with a short duration of 10 s is suggested for optimizing the annealing effect. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The band structures of wurtzite ZnO are calculated using the empirical pseudopotential method (EPM). The 8 parameters of the Zn and O atom pesudopotential form factors with Schluter's formula are obtained. The effective mass parameters are extracted by using k.p Hamiltonian to fit the EPM results. The calculated band edge energies (E-g, E-A, E-B, and E-C) at Gamma point are in good agreement with experimental results. The ordering of ZnO at the top of valence band is found to be A(Gamma(7))-B(Gamma(9))-C(Gamma(7)) due to a negative spin-orbit (SO) splitting. Based on the band parameters obtained, the valence hole subbands of wurzite ZnO/MgxZn1-xO tensile-strained quantum wells (QWs) with different well widths and Mg compositions are calculated using 6-band k.p method. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

InAs was deposited by molecular beam epitaxy (MBE) on a GaAs substrate with an intentional temperature gradient from centre to edge. Two-dimensional (2D) to three-dimensional (3D) morphology evolution was found along the direction in which the substrate temperature was decreasing. Quantum dots (QDs) with density as low as similar to 8 x 10(6) cm(-2) were formed in some regions. We attribute the morphological evolution to the temperature-dependent desorption of deposited indium and the intermixing between deposited indium and gallium from the buffer.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Quasi-continuous-wave operation of GaAs/AlGaAs quantum-cascade lasers with high average optical power is demonstrated. Double X-ray diffraction has been used to investigate the quality of the epitaxial material. The compositional gradients and the interface quality are controlled effectively. The corrected average power of per facet about 17 mW and temperature tuning coefficient of the gain peak about 0.91 nm/K from 83 K to 140 K is achieved in pulse operation. Best value of threshold current density is less than 3.0 kA/cm(2) at 83 K. (C) 2005 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The growth of highly lattice-mismatched InAs0.3Sb0.7 films on (100) GaAs Substrates by magnetron Sputtering has been investigated and even epitaxial lnAs(0.3)Sb(0.7) films have been successfully obtained. A strong effect of the growth conditions on the film structure was observed, revealing that there was a growth mechanism transition from three-dimensional nucleation growth to epitaxial layer-by-layer growth mode when increasing the substrate temperature. A qualitative explanation for that transition was proposed and the critical conditions for the epitaxial layer-by-layer growth mode were also discussed. (c) 2005 Elsevier B.V. All rights reserved.