The optical properties of the strained wurtzite GaN are investigated theoretically within the nearest neighbor tight-binding method. The piezoelectric effect is also taken into account. The empirical rule has been used in the strained band-structure calculation. The results show that the excitonic transition energies are anisotropic in the c-plane in a high electronic concentration system and have a 60 degrees periodicity, which is in agreement with experiment. (C) 2008 American Institute of Physics. [DOI: 10.1063/1.3001937]
Resumo:
Spin splitting of the AlyGa1-yAs/GaAs/AlxGa1-xAs/AlyGa1-yAs (x not equal y) step quantum wells (QWs) has been theoretically investigated with a model that includes both the interface and the external electric field contribution. The overall spin splitting is mainly determined by the interface contribution, which can be well manipulated by the external electric field. In the absence of the electric field, the Rashba effect exists due to the internal structure inversion asymmetry (SIA). The electric field can strengthen or suppress the internal SIA, resulting in an increase or decrease of the spin splitting. The step QW, which results in large spin splitting, has advantages in applications to spintronic devices compared with symmetrical and asymmetrical QWs. Due to the special structure design, the spin splitting does not change with the external electric field.
Resumo:
Using the effective-mass Hamiltonian for an arbitrary direction wurtzite semiconductor on the basis of k.p theory, we investigate the strain effects on the transition energies and optical properties in the R-plane ([1012]-oriented plane) GaN. The results show that (1) the transition energies decrease with the biaxial strains changing from -0.5 to 0.5%; and (2) giant optical anisotropy appears in the R-plane which is significantly affected by the biaxial strains. We clarify the relation between the strains and the polarization properties. Finally, we discuss the application of these properties to the R-plane GaN based devices. (c) 2009 The Japan Society of Applied Physics
Resumo:
By the method of finite difference, the anisotropic spin splitting of the AlxGa1-xAs/GaAs/AlyGa1-yAs/AlxGa1-xAs step quantum wells (QWs) are theoretically investigated considering the interplay of the bulk inversion asymmetry and structure inversion asymmetry induced by step quantum well structure and external electric field. We demonstrate that the anisotropy of the total spin splitting can be controlled by the shape of the QWs and the external electric field. The interface related Rashba effect plays an important effect on the anisotropic spin splitting by influencing the magnitude of the spin splitting and the direction of electron spin. The Rashba spin splitting presents in the step quantum wells due to the interface related Rashba effect even without external electric field or magnetic field.
Resumo:
Optical properties and surface structures of InAs/CaAs self-assembled quantum dots (QDs) grown on 2 nm In-0.2 Ga0.8As and x ML GaAs combined strain-buffer layer were investigated systematically by photoluminescence ( PL) and atomic force microscopy (AFM). The QD density increased from similar to 1.7 x 10(9) cm(-2) to similar to 3.8 x 10(9) cm(-1) due to the decreasing of the lattice mismatch. The combined layer was of benefit to increasing In incorporated into dots and the average height-to-width ratios, which resulted in the red-shift of the emission peaks. For the sample of x = 10 ML, the ground state transition is shifted to 1350 nm at room temperature.
Resumo:
We have demonstrated stable self-starting passive mode locking in a diode-end-pumped Nd:Gd-0.8-Y0.5VO4 laser by using an In0.25Ga0.75As absorber grown at low temperature (LT In0.25Ga0.75As absorber). An In0.25Ga0.75As single-quantum-well absorber, which was grown directly on the GaAs buffer by use of the metal-organic chemical-vapor deposition technique, acts simultaneously as a passive mode-locking device and as an output coupler. Continuous-wave mode-locked pulses were obtained at 1063.5 nm. We achieved a pulse duration of 2.6 ps and an average output power of 2.15 W at a repetition rate of 96.4 MHz. (c) 2005 Optical Society of America.
Resumo:
The electrical and structural properties of Mg delta-doped GaN epilayers grown by MOCVD were investigated. Compared to uniform Mg-doping GaN layers, it has been shown that the delta-doping (delta-doping) process could suppress the dislocation density and enhance the p-type performance. The influence of pre-purge step on the structural properties of GaN was also investigated. The hole concentration of p-GaN decreases when using a pre-purge step. These results can be explained convincingly using a simple model of impurity incorporation under Ga-free growth condition. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
High-performance violet light-emitting diodes (LEDs) with InGaN/AlInGaN multiple quantum well (MQW) active regions were grown by metal organic chemical vapor deposition (MOCVD). The interface flatness of the InGaN/AlInGaN MQWs and the emission efficiency of the LED are firstly improved with increasing Al content in the AlInGaN barrier layer, and then degraded as Al content increases further, being optimal when Al content is 0.12. Similarly, the result is optimized if the indium content is approximately 2.5% in the AlInGaN barrier layer. The mechanisms which have influences on the radiative efficiency when the Al content increases are discussed. A high output power of 7.3 mW for the violet LED at 20 mA current has been achieved. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The magnetic semiconductor GdxSi1-x was prepared by low-energy dual ion-beam epitaxy. GdxSi1-x shows excellent magnetic properties at room temperature. A high magnetic moment of 10 mu(B) per Gd atom is observed. The high atomic magnetic moment is interpreted as being a result of the RKKY mechanism. The indirect exchange interaction between ions is strong at large distances due to the low state density of the carriers in the magnetic semiconductor.
Resumo:
The magnetic/nonmagnetic p-n junction was prepared by implanting gadolinium into the n-type silicon with low-energy dual-ion-beam epitaxy technology. The magnetic layer GdxSi1-x shows excellent magnetic properties at room temperature. High magnetic moment 10mu(B) per Gd atom is observed, which is interpreted by RKKY mechanism. Magnetic/nonmagnetic p-n junctions show rectifying behaviour, but no magnetoresistance is observed.
Resumo:
Semiconducting gadolinium silicide GdxSi samples were prepared by mass-analyzed low-energy dual ion beam epitaxy technique. Auger electron spectroscopy depth profiles indicate that the gadolinium ions are implanted into the single-crystal silicon substrate and formed 20 nm thick GdxSi film. X-ray double-crystal diffraction measurement shows that there is no new phase formed. The XPS spectra show that one type of silicon peaks whose binding energy is between that of silicide and silicon dioxide, and the gadolinium peak of binding energy is between that of metal Gd and Gd2O3. All of these results indicate that an amorphous semiconductor is formed. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Tunnel-regenerated multiple-active-region (TRMAR) light-emitting diodes (LEDs) with high quantum efficiency and high brightness have been proposed and fabricated. We have proved experimentally that the efficiency of the electrical luminescence and the on-axis luminous intensity of such TRMAR LEDs scaled linearly approximately with the number of the active regions. The on-axis luminous intensity of such TRMAR LEDs with only 3 mum GaP current spreading layer have exceeded 5 cd at 20 mA dc operation under 15 degrees package. The high-quantum-efficiency and high-brightness LEDs under the low injection level were realized. (C) 2001 American Institute of Physics.
Resumo:
A novel semiconductor laser structure is put forward to resolve the major difficulties of high power laser diodes. In this structure, several active regions are cascaded by tunnel junctions to form a large optical cavity and to achieve super high efficiency. This structure can solve the problems of catastrophic optical damage of facet, thermal damage and poor light beam quality effectively. Low-pressure metalorganic chemical vapor deposition method is adopted to grow the novel semiconductor laser structures, which are composed of Si:GaAs/C:GaAs tunnel junctions, GaAs/InGaAs strain quantum well active regions. External differential quantum efficiency as high as 2.2 and light power output of 2.5 W per facet (under 2A drive current) are achieved from an uncoated novel laser device with three active regions.
Raman-forbidden mode and oxygen ordering in Bi2Sr2-xLaxCuO6+gamma single crystals annealed in oxygen
Resumo:
A Raman-forbidden phonon mode at about 840 cm(-1) is observed popularly on the surface of pun and La-doped Bi2Sr2-xLaxCuO6+y (0 less than or equal to x less than or equal to 0.8) single crystals annealed in oxygen. A remarkable excitation dependence of this additional line is found. Based on the properties of the structure of the Bi-O layer with excess oxygen atoms and the similarity in the appearance of the Raman-forbidden modes between RBa2Cu3Ox (R = Y, Nd, Gd, Pr) and Bi2Sr2-xLaxCuO6+y systems, we attribute the manifestation of this additional line to the ordering of the interstitial oxygen in the Bi-O layers. Our results provide Raman evidences for confirming that the ordering of the movable oxygen may exist universally in high-temperature superconductors.
Resumo:
A systematic study of syntheses and magnetic properties of the Nd-3 Fe29-xCrx (x=4.5, 4.7, 5.0, and 5.5) compounds has been performed. The single-phase compounds of Nd3Fe29-xCrx can be formed in the range 4.5 less than or equal to x less than or equal to 5.5. The Curie temperature Tc, the saturation magnetization M-S at 4.2 K, the anisotropy field H-A at 4.2 K and room temperature, and the intra-sublattice exchange coupling parameter j(FeFe) at 4.2 K for the Nd3Fe29-xCrx compounds decrease with increasing Cr composition from x=4.5 to 5.5, respectively. Nitrogenation and carbonation, unlike hydrogenation, result mainly in improvements of the Curie temperature, the saturation magnetization and the anisotropy field at 4.2 K and room temperature for the Nd3Fe29-xCrx compounds compared with their parent compounds.