Generation of 1.5–12ns width-tunable 532nm pulses by adopting laser-induced plasma shutter technique
Resumo:
The annealing effects of sapphire substrates on the quality of epitaxial ZnO films grown by dc reactive magnetron sputtering were studied. The atomic steps formed on (0001) sapphire (alpha-Al2O3) substrates surface by annealing at high temperature were analyzed by atomic force microscopy. Their influence on the growth of ZnO films was examined by X-ray diffraction and photoluminescence measurements. Experimental results indicate that the film quality is strongly affected by annealing treatment of the sapphire substrate surface. The optimum annealing temperature of sapphire substrates for ZnO grown by magnetron sputtering is 1400 degrees C for 1 h in air.
Resumo:
Aluminum nitride (AlN) films were prepared on gamma-LiAlO2 substrates by radio frequency (rf) magnetron sputtering. The influence of substrate temperature (T-s) and nitrogen (N-2) concentration on film growth was investigated. The X-ray diffraction (XRD) results reveal that highly c-axis oriented AlN films can be obtained in the temperature range from room temperature (RT) to 300 degrees C. A smoother surface and a crystalline quality decrease with increasing N-2 concentration have been observed by XRD and atomic force microscopy (AFM) for the films deposited at lower substrate temperature. On the contrary, the degradation of the surface smoothness and the higher crystalline quality can be observed for the films deposited at a higher substrate temperature with N-2-rich ambient. The growth mechanism which leads to different crystalline quality of the films is discussed. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Optical properties and microstructure of Ag film on glass substrate with Cr intermediate layer were studied by using spectrophotometer and XRD. The spectra results showed that introducing Cr intermediate layer reduced the surface roughness and promoted the reflectivity of Ag film. The XRD analysis showed that the crystalline grains increased and the stress decreased. The adhesion was also improved by using the tape test method. (c) 2006 Published by Elsevier B.V.
Resumo:
The single-sided and dual-sided high reflective mirrors were deposited with ion-beam sputtering (IBS). When the incident light entered with 45 degrees, the reflectance of p-polarized light at 1064 nm exceeded 99.5%. Spectrum was gained by spectrometer and weak absorption of coatings was measured by surface thermal lensing (STL) technique. Laser-induced damage threshold (LIDT) was determined and the damage morphology was observed with Lecia-DMRXE microscope simultaneously. The profile of coatings was measured with Mark III-GPI digital interferometer. It was found that the reflectivity of mirror exceeded 99.9% and its absorption was as low as 14 ppm. The reflective bandwidth of the dual-sided sample was about 43 nm wider than that of single-sided sample, and its LIDT was as high as 28 J/cm2, which was 5 J/cm2 higher than that of single-sided sample. Moreover, the profile of dual-sided sample was better than that of substrate without coatings.
Resumo:
A series of silver films with different thickness were prepared under identical conditions by direct current magnetron sputtering. The optical properties of the silver films were measured using spectrophotometric techniques and the optical constants were calculated from reflection and transmission measurements made at near normal incidence. The results show that the optical properties and constants are affected by films' thickness. Below the critical thickness of 17 nm at which Ag film forms a continuous film, the optical properties and constants vary significantly as the thickness of films increases and then tends to a stable value which is reached at 41 nm. X-ray diffraction measurements were carried out to examine the structure and stress evolution of the Ag films as a function of films' thickness. It was found that the interplanar distance of (111) orientation decreases when the film thickness increases and tends to be close to that of bulk material. The compressive strains also decrease with increasing thickness. (C) 2007 Published by Elsevier B.V.
Resumo:
Zirconia films were prepared by e-beam evaporation, and oxygen plasma treatment was used to modify film properties. Spectrophotometry, x-ray diffractometry (XRD), and atomic force microscopy were used to characterize refractive index, extinction coefficient, rnicrostructure, and surface roughness, respectively. The experimental results indicate that both refractive index and extinction coefficient of the films were reduced slightly after oxygen plasma treatment, with the decrease of intrinsic stress and surface roughness. From XRD spectra, the intensity decrease of the T(110) diffraction peak was clearly observed after the treatment, which was caused by the restructuring of the film atoms. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
It is demonstrated with powerful evidence that the extraordinary transmission of a metallic grating is undoubtedly due to the excitation of standing surface plasma waves in the Fabry-Perot like resonator. This is the first time that the strong standing waves set up in the groove of a sub-wavelength double-layer grating (SWDG) for the surface plasma waves have been reported. Moreover, about 90% transmission is gained with an SWDG, more easily fabricated than ordinary metallic gratings, in the first peak of transmission spectrum.
Resumo:
A study on the layer structure of W/C multilayers deposited by magnetron sputtering is reported. In the study, soft x-ray resonant reflectivity and hard x-ray grazing incidence reflectivity of the W/C multilayers were measured. The imperfections at the interface such as interdiffusion and formation of compounds were dealt with by two methods. On analyzing the experimental results, we found that the incorporation of an interlayer was a more suitable method than the traditional statistical method to describe the layer structure of a W/C system we fabricated. The optical constants of each layer at a wavelength of 4.48 nm were also obtained from the analysis. Copyright (C) 2008 John Wiley & Sons, Ltd.