985 resultados para GAAS QUANTUM-WELLS
Resumo:
Low-temperature electroluminescence (EL) is observed in n-type modulation-doped AlGaAs/InGaAs/GaAs quantum well samples by applying a positive voltage between the semitransparent Au gate and alloyed Au–Ge Ohmic contacts made on the top surface of the samples. We attribute impact ionization in the InGaAs QW to the observed EL from the samples. A redshift in the EL spectra is observed with increasing gate bias. The observed redshift in the EL spectra is attributed to the band gap renormalization due to many-body effects and quantum-confined Stark effect.
Resumo:
We present photoluminescence and reflectance spectra of GaAs/Al-x Ga-1-x As quantum wells in a magnetic field for the Faraday geometry. The photoluminescence peaks recorded are among the most intense and narrow reported to date. This has allowed us to study the behavior of closely spaced bound exciton lines under a magnetic field. Several new features including magnetic field induced splitting of the bound exciton emission peaks are reported.
Resumo:
The photoluminescence study of Fermi-edge singularity (FES) in modulation-doped pseudomorphic AlxGa1-xAs/InyGa1-yAs/GaAs quantum well (QW) heterostructures is presented. In the above QW structures the optical transitions between n = 1 and n = 2 electronic subband to the n = 1 heavy hole subband (E-11 and E-21 transitions, respectively) are observed with FES appearing as a lower energy shoulder to the E-21 transition. The observed FES is attributed to the Fermi wave vector in the first electronic subband under the conditions of population of the second electronic subband. The FES appears at about 10 meV below E-21 transition around 4.2 K. Initially it gets stronger with increasing temperature and becomes a distinct peak at about 20 K. Further increase in temperature quenches FES and reaches the base line at around 40 K.
Resumo:
High-indium-content InxGa1-xAs/GaAs single/multi-quantum well (SQW/MQW) structures have been systematically investigated. By optimizing the molecular-beam epitaxy growth conditions, the critical thickness of the strained In0.475Ga0.525As/GaAs QWs is raised to 7 nm, which is much higher than the value given by the Matthews and Blakeslee model. The good crystalline quality of the strained InGaAs/GaAs MQWs is proved by x-ray rocking curves. Photoluminescence measurements show that an emission wavelength of 1.25 mum at room temperatures with narrower full width at half maximum less than 30 meV can be obtained. The strain relaxation mechanism is discussed using the Matthews-Blakeslee model. (C) 2004 American Institute of Physics.
Resumo:
Photoluminescence (PL) spectra of the GaInNAs/GaAs single quantum well (SQW) with different N compositions are carefully studied in a range of temperatures and excitation power densities. The anomalous S-shape temperature dependence of the PL peak is analysed based on the competition and switching-over between the peaks related to N-induced localized states and the peak related to interband excitonic recombination. It is found that with increasing N composition, the localized energy increases and the turning point of the S-shape temperature dependence occurs at higher temperature, where the localized carriers in the bandtail states obtain enough thermal activation energy to be dissociated and delocalized. The rapid thermal annealing (RTA) effectively reduces the localized energy and causes a decrease of the switching-over temperature.
Resumo:
High structural and optical quality 1.3 mu m GaInNAs/GaAs quantum well (QW) samples with higher (42.5%) indium content were successfully grown by molecular-beam epitaxy. The cross-sectional transmission electron microscopy measurements reveal that there are no structural defects in such high indium content QWs. The room-temperature photoluminescence peak intensity of the GaIn0.425NAs/GaAs (6 nm/20 nm) 3QW is higher than, and the full width at half maximum is comparable to, that of In0.425GaAs/GaAs 3QW, indicating improved optical quality caused by strain compensation effect of introducing N to the high indium content InGaAs epilayer. (C) 2005 American Institute of Physics.
Resumo:
High-quality GaNAs/GaAs quantum wells with high substitutional N concentrations, grown by molecular-beam epitaxy, are demonstrated using a reduced growth rate in a range of 0.125-1 mu m/h. No phase separation is observed and the GaNAs well thickness is limited by the critical thickness. Strong room-temperature photoluminescence with a record long wavelength of 1.44 mu m is obtained from an 18-nm-thick GaN0.06As0.94/GaAs quantum well. (C) 2005 American Institute of Physics.
Resumo:
Optical properties of highly strained GaInAs/GaAs quantum wells (QWs) grown by molecular beam epitaxy with Sb assistance are investigated. The samples grown by Sb incorporation and Sb pre-deposition methods display high room-temperature photoluminescence (PL) intensity at extended long wavelength. This result is explained by the surfactant effects of Sb during the growth of GaInAs/GaAs QW systems. An abnormal S-shaped temperature dependence of the PL peak position is found in the In0.42Ga0.58As/GaAs triple QWs sample grown with Sb pre-deposition. By investigating the transmission electron microscope images and time-resolved PL spectra, it is found that the S-shaped temperature dependence of the PL peak position originates from the exciton localization effect brought by the Sb-rich clusters on the QW interface.
Resumo:
Long-wavelength high indium content InxGa1-xAs/GaAs single/multi quantum wells (QWs) structures have been successfully grown by molecular beam epitaxy. It is evidenced by X-ray measurements that the critical thickness of the well width of InxGa1-xAs/GaAs QWs with an indium content x of 47.5% can be raised up to 7nm without strain relation. 1.25μ m photoluminescence (PL) emission is obtained from the QWs with narrower full-width at half maximum (FWHM) less than 30meV. Our results are important basements which are useful for further fabricating GaAs-based long-wavelength devices. © 2005 Elsevier B.V. All rights reserved.
Resumo:
The InGaNAs(Sb)/(GaNAs)/GaAs quantum wells (QWs) emitting at 1.3-1.55 mu m have been grown by molecular beam epitaxy (MBE). The parameters of the radio frequency (RF) such as RF power and flow rate are optimized to reduce the damages from the ions or energetic species. The growth temperature is carefully controlled to prevent the phase segregation and strain relaxation. The effects of Sb on the wavelength and quality are investigated. The GaNAs barrier is used to extend the wavelength and reduce the strain. A 1.5865 mu m InGaNAs(Sb)/GaNAs SQW edge emitting laser lasing at room temperature at continuous wave operation mode is demonstrated. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
A resonant-cavity enhanced reflective optical modulator is designed and frabricated, with three groups of three highly strained InGaAS/GaAs quantum wells in the cavity, for the low voltage and high contrast ratio operation. The quantum wells are positioned in antinodes of the optical standing wave. The modulator is grown in a single growth step in an molecular beam epitaxy system, using GaAs/AIAs distributed Bragg reflectors as both the top and bottom mirrors. Results show that the reflection device has a modulation extinction of 3 dB at -4.5 V bias.
Resumo:
The nonradiative recombination effect on carrier dynamics in GaInNAs/GaAs quantum wells is studied by time-resolved photoluminescence (TRPL) and polarization-dependent TRPL at various excitation intensities. It is found that both recombination dynamics and spin relaxation dynamics strongly depend on the excitation intensity. Under moderate excitation intensities the PL decay curves exhibit unusual non-exponential behaviour. This result is well stimulated by a rate equation involving both the radiative and non-radiative recombinations via the introduction of a new parameter of the effective concentration of nonradiative recombination centres in the rate equation. In the spin dynamics study, the spin relaxation also shows strong excitation power dependence. Under the high excitation power an increase of spin polarization degree with time is observed. This new finding provides a useful hint that the spin process can be controlled by excitation power in GaInNAs systems.
Resumo:
We investigate the effect of rapid thermal annealing on InGaNAs/GaAs quantum wells. At optimized annealing temperatures and times, the greatest enhancement of the photoluminescence intensity is obtained by a special two-step annealing process. To identify the mechanism affecting the material quality during the rapid thermal annealing, differential temperature analysis is applied, and temperature- and power-dependent photoluminescence is carried out on the samples annealed under different conditions. Our experiment reveals that some composition redistribution or other related ordering process may occur in the quantum-well layer during annealing. Annealing at a lower temperature for a long time primarily can remove defects and dislocations while annealing at a higher temperature for a short time primarily homogenizes the composition in the quantum wells.
Resumo:
High (42.5%) indium content GaInNAs/GaAs quantum wells with room temperature emission wavelength from 1.3 mu m to 1.5 mu m range were successfully grown by Radio Frequency Plasma Nitrogen source assisted Molecular Beam Epitaxy. The growth parameters of plasma power and N-2 How rate were optimized systematically to improve the material quality. Photoluminescence and transmission electron microscopy measurements showed that the optical and crystal quality of the 1.54 mu m GaInNAs/GaAs QWs was kept as comparable as that in 1.31 mu m.
Resumo:
It is found that both methods using either continuous Sb supply or pre-deposition of a very thin Sb layer are efficient for the Sb-assisted molecular beam epitaxy growth of highly strained InGaAs/GaAs quantum wells (QWs). The emission of QWs is extended to long wavelength close to 1.25 mu m with high luminescence efficiency at room temperature. The influence of rapid thermal annealing (RTA) on the photoluminescence intensity critically depends on the annealing temperature and duration for highly strained QWs. A relatively low RTA temperature of 700 degrees C with a short duration of 10 s is suggested for optimizing the annealing effect. (c) 2005 Elsevier B.V. All rights reserved.