Resumo:
Ultrafine powders of (Ti1-xSnx)O2, 0
Resumo:
Nanocrystalline TiO2 was synthesized using the microwave plasma technique and characterized using X-ray diffraction, transmission electron microscopy, scanning electron microscopy, laser particle size analyzer, UV-vis spectroscopy and BET surface area analyzer. The synthesized TiO2 powder crystallized in anatase phase and the crystallite sizes were in nanometers. The photocatalytic activity of the compound was determined and compared against the activity of the commercial Degussa P-25 TiO2 catalyst. The degradation rates of the dyes were found to be higher over the synthesized TiO2 as compared to that over commercial Degussa P-25 TiO2.
Resumo:
La2-xNiO4, La2-xSrxNiO4 and related layered nickelates have been investigated for possible presence of superconductivity. While there is clear onset of diamagnetism around 20 K in many of these nickelates, we do not, however, find any anomaly in the electrical resistivity, magnetoresistance or thermopower around 20 K. High energy spectroscopic studies show Ni to be in the 2+ oxidation state accompanied by a substantial proportion of oxygen holes.
Resumo:
This communication describes the voltage‐current characteristics in the breakdown region of p‐n junctions made on polycrystalline silicon of large grain size. The observed soft breakdown characteristics have been explained by taking into account the effect of curvature of the junction near the grain boundaries.
Resumo:
Current-voltage (I–U) characteristics of MOS structures on polycrystalline silicon are investigated. A model based on the carrier transport through the traps in the oxide is described to explain the I–U characteristics.Es werden Strom-Spannungs(I–U)-Charakteristiken von MOS-Strukturen auf polykristallinem Silizium untersucht. Ein Modell zur Erklärung der I–U-Charakteristiken wird beschrieben, das auf dem Ladungstransport über Oxidtraps beruht.
Resumo:
Sintered, polycrystalline ZnO ceramics with copper as the only additive exhibit highly nonlinear current‐voltage characteristics. Increasing nonlinearity index (α=4–45) with Cu concentration of 0.01–1 mol % is also variable with respect to ceramic processing methods. Incorporation of Cu in the ZnO lattice is indicated from the electron probe microanalysis and the photoluminescence spectra. Cu acceptors are compensated by holes in the grain boundary layers, whereas the concentration of intrinsic donors is higher in the grain interior. The presence of positive charges leads to thinning of the depletion region, resulting in nonlinear characteristics.
Resumo:
The photocatalytic degradation of nitrobenzene and substituted nitrobenzenes under UV exposure was investigated with combustion synthesized nano-TiO2 and commercial TiO2 catalyst, Degussa P-25. The experimental data indicated that the photodegradation kinetics was first order. The photocatalytic degradation rates were considerably higher when catalyzed with combustion synthesized TiO2 compared to that of Degussa P-25. The degradation rate coefficients followed the order: 1-chloro,14-dinitrobenzene similar or equal to 4-nitrophenot > 2-nitrophenol > 1-chloro.4-nitrobenzene > 3-niti-ophenol > 2,4-dinitrophenol > 1-chloro,2-nitrobenzene > nitrobenzene > 1,3-dinitrobenzene. Plausible mechanisms and reasons for the observation of the above order are discussed.
Resumo:
The ultrasonic degradation of two dyes, Rhodamine B (C28H31ClN2O3) and Rhodamine Blue (C28H32N2O3), were studied in the absence of catalyst and in the presence of two catalysts (combustion-synthesized anatase TiO2 and commercial Degussa P-25 TiO2. The rate of degradation of catalyzed reaction was higher than that obtained with in the absence of the catalysts. Among the catalysts, combustion-synthesized anatase TiO2 degraded the dyes faster when compared to the degradation with commercial Degussa P-25 catalyst. A Langmuir-Hinshelwood kinetic model was developed and the kinetic rate parameters were determined. The effect of other operating parameters, such as initial concentration, pH, temperature, and power intensity, was also investigated. The degradation rate increased with decreasing pH, increasing temperature, and higher intensity.
Resumo:
Molybdenum-doped TiO2 organic-inorganic hybrid nanoparticles were synthesized under mild hydrothermal conditions by in situ surface modification using n-butylamine. This was carried out at 150 degrees C at autogeneous pressure over 18 h. n-Butylamine was selected as a surfactant since it produced nanoparticles of the desired size and shape. The products were characterized using powder X-ray diffraction, Fourier transform infrared spectrometry, dynamic light-scattering spectroscopy, UV-Vis spectroscopy and transmission electron microscopy. Chemical oxygen demand was estimated in order to determine the photodegradation efficiency of the molybdenum-doped TiO2 hybrid nanoparticles in the treatment of pharmaceutical effluents. It was found that molybdenum-doped TiO2 hybrid nanoparticles showed higher photocatalytic efficiency than untreated TiO2 nanoparticles.
Resumo:
This paper reports the variations in impedance with frequency of metal‐oxide‐semiconductor (MOS) structures on polycrystalline silicon. The origin of these impedance‐frequency characteristics are qualitatively explained. These characteristics indicate that the MOS structure on polycrystalline silicon can be exploited to realize voltage controlled filters.
Resumo:
Experimental evidence that phosphorus in silicon is neutralized by hydrogenation is presented by measuring changes in sheet resistance and Hall mobility carrier in heavily phosphorus‐doped polycrystalline films.
Resumo:
PbSnS2 thin film has been prepared for the first time by spray pyrolysis technique on FTO substrate at 570K. The preliminary optical and structural characteristics of the film have been reported. The optical studies showed that the value of the fundamental absorption edge lies at 1.47eV and a low energy absorption band tail has been observed. The prepared film is p- type electrical conductivity, polycrystalline in nature and has an orthorhombic crystal structure. The value of an average grain size of the film is 350Å.
Resumo:
The ultrasonic degradation of two dyes, Rhodamine B (C28H31ClN2O3) and Rhodamine Blue (C28H32N2O3), were studied in the absence of catalyst and in the presence of two catalysts (combustion-synthesized anatase TiO2 and commercial Degussa P-25 TiO2. The rate of degradation of catalyzed reaction was higher than that obtained with in the absence of the catalysts. Among the catalysts, combustion-synthesized anatase TiO2 degraded the dyes faster when compared to the degradation with commercial Degussa P-25 catalyst. A Langmuir-Hinshelwood kinetic model was developed and the kinetic rate parameters were determined. The effect of other operating parameters, such as initial concentration, pH, temperature, and power intensity, was also investigated. The degradation rate increased with decreasing pH, increasing temperature, and higher intensity.
Resumo:
Based on in-situ Mossbauer and X-ray diffraction studies, it is shown that in the Fe/TiO2 catalyst, the anatase-rutile transformation of the TiO2 support is facilitated by the Fe2+ ions formed during the reduction. The transformation occurs at lower temperatures in Th/TiO2 and Cu/TiO2 compared to pure TiO2. In general, the transformation of anatase to rutile seems to occur at or below the temperature (approximately 770 K) at which strong-metal-support-interaction manifests itself.
Resumo:
In-situ EXAFS studies of sulphided Mo/TiO2 catalysts have shown that at low Mo loadings (2–4 wt%), an active species with a short Mo-S distance of 2.25 Å is formed, while on Mo/TiO2 with high Mo loadings as well as on Mo/gamma-Al2O3, bulk MoS2 (Mo-S, 2.42 Å) is formed. The species with the short Mo-S distance has Mo in an oxidation state close to 6 + and is likely to result from the sulphidation of the tetrahedral molybdate species present in the oxidic precursor at low Mo loadings. The calcination temperature of the oxidic precursor appears crucial, a high calcination temperature of 973 K favouring the formation of MoS3 on sulphidation, and a low calcination temperature of 623 K favouring MoS2.