992 resultados para 128-799A
Resumo:
This paper reports a new method for detection of ROS scavengers including superoxide dismutase, ascorbic acid and glutathione based on a 'probe' of peroxidase-oxidase biochemical oscillator. The oscillation period and amplitude change with different concentrations of scavengers. The linear ranges of superoxide dismutase, ascorbic acid and glutathione are respectively 1.56 x 10(-4)-1.56 x 10(-3) mg mL(-1), 1.75 x 10(-7) -1.75 x 10(-5) mol L-1 and 9.38 x 10(-7) -7.5 x 10(-5) mol L-1. The selectivity, linearity and precision for superoxide dismutase, ascorbic acid, and glutathione are presented and discussed. The results compared well with other standard methods for determination of superoxide dismutase, ascorbic acid and glutathione. Some possible steps in the overall reaction mechanisms are discussed.
Resumo:
InN nanostructures with and without GaN capping layers were grown by using metal-organic chemical vapor deposition. Morphological, structural, and optical properties were systematically studied by using atomic force microscopy, X-ray diffraction (XRD) and temperature-dependent photoluminescence (PL). XRD results show that an InGaN structure is formed for the sample with a GaN capping layer, which will reduce the quality and the IR PL emission of the InN. The lower emission peak at similar to 0.7 eV was theoretically fitted and assigned as the band edge emission of InN. Temperature-dependent PL shows a good quantum efficiency for the sample without a GaN capping layers; this corresponds to a lower density of dislocations and a small activation energy.
Resumo:
A diode-pumped Nd:GdVO4 laser mode-locked by a semiconductor saturable absorber and output coupler (SESAOC) is passively stabilized to suppress Q-switched mode-locking. A phase mismatched 131130 second-harmonic generation (SHG) crystal is used for passive stabilization. The continuous wave mode-locking (CWML) threshold is reduced and the pulse width is compressed. The pulse width is 6.5 ps as measured at the repetition rate of 128 MHz. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
AlGaN-based resonant-cavity-enhanced (RCE) p-i-n photodetectors (PDs) for operating at the wavelength of 330 nm were designed and fabricated. A 20.5-pair AlN/Al0.3Ga0.7N distributed Bragg reflector (DBR) was used as the back mirror and a 3-pair AlN/Al0.3Ga0.7N DBR as the front one. In the cavity is a p-GaN/i-GaN/n-Al0.3Ga0.7N structure. The optical absorption of the RCE PD structure is at most 59.8% deduced from reflectance measurement. Selectively enhanced by the cavity effect, a response peak of 0.128 A/W at 330 nm with a half-peak breadth of 5.5 nm was obtained under zero bias. The peak wavelength shifted 15 nm with the incident angle of light increasing from 0 degrees to 60 degrees.
Resumo:
The InGaNAs(Sb)/(GaNAs)/GaAs quantum wells (QWs) emitting at 1.3-1.55 mu m have been grown by molecular beam epitaxy (MBE). The parameters of the radio frequency (RF) such as RF power and flow rate are optimized to reduce the damages from the ions or energetic species. The growth temperature is carefully controlled to prevent the phase segregation and strain relaxation. The effects of Sb on the wavelength and quality are investigated. The GaNAs barrier is used to extend the wavelength and reduce the strain. A 1.5865 mu m InGaNAs(Sb)/GaNAs SQW edge emitting laser lasing at room temperature at continuous wave operation mode is demonstrated. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Intrinsic nanocrystalline silicon films (nc-Si:H) were prepared by plasma enhanced chemical vapor deposition (PECVD) method. Films' microstructures and characteristics were studied with Raman spectroscopy and Atom Force Microscope (AFM). The electronic conductivity of nc-Si:H films was found to be 4.9 x 10(0)Omega(-1) cm(-1), which was one order of magnitude higher than the reported 10(-3)-10(-1)Omega(-1)cm(-1). And PIN solar cells with nc-Si:H film as intrinsic thin-layer (ITO/n(+)-nc-Si:H/i-nc-Si:H/p-c-Si/Ag) were researched. The cell's performances were measured, the open-circuit voltage V-oc was 534.7 mV, short-circuit current I-sc was 49.24 mA (3 cm(2)) and fill factor FF was 0.4228. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Surface micro-roughness, surface chemical properties, and surface wettability are three important aspects of wafer surfaces during a wafer cleaning process, which determine the bonding quality of ordinary direct wafer bonding. In this study, InP wafers are divided into four groups and treated by different chemical processes. Subsequently, the characteristics of the treated InP surfaces are carefully studied by X-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM), and contact angle measurements. The optimal wafer treatment method for wafer bonding is determined by comparing the results of the processes as a whole. This optimization is later evaluated by a scanning electronic microscope (SEM), and the ridge waveguide 1.55 mu m Si-based InP/InGaAsP multi-quantum-well laser chips are also fabricated. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Using non-identical quantum wells as the active material, a new distributed-feed back laser is fabricated with period varied Bragg grating. The full width at half maximum of 115 nm is observed in the amplified spontaneous emission spectrum of this material, which is flatter and wider than that of the identical quantum wells. Two wavelengths of 1.51 mu m and 1.53 mu m are realized under different work conditions. The side-mode suppression ratios of both wavelengths reach 40 dB. This device can be used as the light source of coarse wavelength division multiplexer communication systems.
Resumo:
We have grown MnxGe1-x films (x=0, 0.06, 0.1) on Si (001) substrates by magnetron cosputtering, and have explored the resulting structural, morphological, electrical and magnetic properties. X-ray diffraction results show there is no secondary phase except Ge in the Mn0.06Ge0.94 film while new phase appears in the Mn0.1Ge0.9 film. Nanocrystals are formed in the Mn0.06Ge0.94 film, determined by field-emission scanning electron microscopy. Hall measurement indicates that the Mn0.06Ge0.94 film is p-type semiconductor and hole carrier concentration is 6.07 X 10(19) cm(-3) while the MnxGe1-x films with x=0 has n-type carriers. The field dependence of magnetization was measured using alternating gradient magnetometer, and it has been indicated that the Mn0.06Ge0.94 film is ferromagnetic at room temperature. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
A quantum waveguide theory is proposed for hole transport in the mesoscopic structures, including the band mixing effect. We found that due to the interference between the 'light' hole and 'heavy' wave, the transmission and reflection coefficients oscillate more irregularly as a function of incident wave vector geometry parameters. Furthermore conversion between the heavy hole and light hole states occurs at the intersection. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
The structural characteristic of cubic GaN (C-GaN) nucleation layers on GaAs(0 0 1) substrates by metalorganic chemical vapor deposition was in detail investigated first by X-ray diffraction (XRD) measurements, using a Huber five-circle diffractometer and an intense synchrotron X-ray source. The XRD results indicate that the C-GaN nucleation layers are highly crystallized. Phi scans and pole figures of the (1 1 1) reflections give a convincing proof that the GaN nucleation layers show exactly cubic symmetrical structure. The GaN(1 1 1) reflections at 54.74degrees in chi are a measurable component, however (002) components parallel to the substrate surface are not detected. Possible explanations are suggested. The pole figures of {1 0 (1) over bar 0} reflections from H-GaN inclusions show that the parasitic H-GaN originates from the C-GaN nucleation layers. The coherence lengths along the close-packed [1 1 1] directions estimated from the (1 1 1) peaks are nanometer order of magnitude. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Tb3+-doped zinc oxide nanocrystals with a hexagonal wurzite structure were successfully prepared by reaction between Zn-O-Tb precursors and LiOH in ethanol. Good incorporation of Tb3+ in ZnO nanocrystals is proved by XRD, FTIR, PL and PLE measurements. The presence of acetate complexes to zinc atoms on particle surfaces is disclosed by FTIR results. Emission from both Tb3+ ions and surface states in ZnO matrix, as well as their correlation were observed. The luminescence mechanism is discussed. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Self-assembled InAs QD dot-in-a-well (DWELL) structures were grown on GaAs substrate by MBE system, and heterojunction modulation-doped field effect transistor (MODFET) was fabricated. The optical properties of the samples show that the photoluminescence of InAs/GaAs self-assembled quantum dot (SAQD) is at 1.265 mu m at 300 K. The temperature-dependence of the abnormal redshift of InAs SAQD wavelength with the increasing temperature was observed, which is closely related with the inhomogeneous size distribution of the InAs quantum dot. According to the electrical measurement, high electric field current-voltage characteristic of the MODFET device were obtained. The embedded InAs QD of the samples can be regard as scattering centers to the vicinity of the channel electrons. The transport property of the electrons in GaAs channel will be modulated by the QD due to the Coulomb interaction. It has been proposed that a MODFET embedded with InAs QDs presents a novel type of field effect photon detector.
Resumo:
We present lateral intersubband photocurrent (PC) study on self-assembled InAs/InAIAs/InP(001) nanostructures in normal incidence. With the help of interband excitation, a broad PC signal has been observed in the photon energy range of 150-630 meV arising from the bound-to-continuum intersubband absorption in the InAs nanostructures. The large linewidth of the intersubband PC signal is due to the size inhomogeneity of the nanostructures. With the increase of the interband excitation the intersubband PC signal firstly increases with a redshift of PC peak and reaches its maximum, then decreases with no peak shift. The increase and redshift of the PC signal at low excitation level can be explained by the state filling effect. However, the decrease of PC signal at high excitation level may be due to the change of the mobility and lifetime of the electrons. The intersubband PC signal decreases when the temperature is increased, which can be explained by the decrease of the mobility and lifetime of the electrons and the thermal escape of electrons.
Resumo:
Morphology evolution of high-index (331)A surfaces during molecular beam epitaxy (MBE) growth have been investigated in order to uncover their unique physic properties and fabricate spatially ordered low dimensional nanostructures. Atomic Force Microscope (AFM) measurements have shown that the step height and terrace width of GaAs layers increase monotonically with increasing substrate temperature in conventional MBE. However, this situation is reversed in atomic hydrogen-assisted MBE, indicating that step bunching is partly suppressed. We attribute this to the reduced surface migration length of Ga adatoms with atomic hydrogen. By using the step arrays formed on GaAs (331)A surfaces as the templates, we fabricated laterally ordered InGaAs self-aligned nanowires.