959 resultados para Surface roughness (Ra)
Resumo:
This work is an example of the improvement on quantitative fractography by means of digital image processing and light microscopy. Two techniques are presented to investigate the quantitative fracture behavior of Ti-4Al-4V heat-treated alloy specimens, under Charpy impact testing. The first technique is the Minkowski method for fractal dimension measurement from surface profiles, revealing the multifractal character of Ti-4Al-4V fracture. It was not observed a clear positive correlation of fractal values against Charpy energies for Ti-4Al-4V alloy specimens, due to their ductility, microstructural heterogeneities and the dynamic loading characteristics at region near the V-notch. The second technique provides an entire elevation map of fracture surface by extracting in-focus regions for each picture from a stack of images acquired at successive focus positions, then computing the surface roughness. Extended-focus reconstruction has been used to explain the behavior along fracture surface. Since these techniques are based on light microscopy, their inherent low cost is very interesting for failure investigations.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
In this work we have developed a way to grow Fe/MgO(100) monocrystals by magnetron sputtering DC. We investigated the growing in a temperature range among 100 oC and 300 oC. Structural and magneto-crystalline properties were studied by different experimental techniques. Thickness and surface roughness of the films were investigated by atomic force microscopy, while magneto-crystalline properties were investigated by magneto-optical Kerr effect and ferromagnetic resonance. Our results show that as we increase the deposition temperature, the magneto-crystalline anisotropy of the films also increases, following the equation of Avrami. The best temperature value to make a film is 300 oC. As the main result, we built a base of magnetoresistence devices and as an aplication, we present measurements of Fe/Cr/Fe trilayer coupling. In a second work we investigated the temperature dependence of the first three interlayer spacings of Ag(100) surface using low energy electron diffraction. A linear expansion model of crystal surface was used and the values of Debye temperatures of the first two layers and thermal expansion coefficient were determinated. A relaxation of 1% was found for Ag(100) surface and these results are matched with faces (110) and (111) of the silver. iv
Resumo:
Objective:This study evaluated the in vitro adherence of pathogenic micro-organisms, Candida albicans, Staphylococcus aureus and Pseudomonas aeruginosa, to soft lining materials and their inhibitory effect on these micro-organisms.Materials and Methods:To measure adherence, specimens of Molloplast B and Ufi Gel P were inoculated [107 colony-forming units per millimetre (cfu/ml)] with TSB media containing the micro-organisms. To determine the number of micro-organisms in the 10-2-10-5 dilutions, 25 mu l of the suspension were transferred to plates of selective media. Colony counts of each specimen were quantified (cfu/ml). The surface roughness was measured with a perfilometer to assess the relationship between the adherence of micro-organisms and surface roughness of each material. For the inhibition test, specimens of materials were placed in agar plates inoculated individually with the micro-organisms. After 48 h, the inhibition zones around the specimens were measured.Results:None of the materials exhibited inhibition zones. The number of cfu/ml of S. aureus and P. aeruginosa were significantly greater than C. albicans for both materials. The Ufi Gel P exhibited greater adherence of C. albicans than Molloplast B. No correlation was observed between the adherence of micro-organisms and surface roughness.Conclusion:The surface roughness of the materials is not the only factor governing micro-organism adherence.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Background: Chemical modification of implant surface is typically associated with surface topographic alterations that may affect early osseointegration. This study investigates the effects of controlled surface alterations in early osseointegration in an animal model.Methods: Five implant surfaces were evaluated: 1) alumina-blasting, 2) biologic blasting, 3) plasma, 4) microblasted resorbable blasting media (microblasted RBM), and 5) alumina-blasting/acid-etched (AB/AE). Surface topography was characterized by scanning electron microscopy and optical interferometry, and chemical assessment by x-ray photoelectron spectroscopy. The implants were placed in the radius of six dogs, remaining 2 and 4 weeks in vivo. After euthanization, specimens were torqued-to-interface failure and non-decalcified - processed for histomorphologic bone-implant contact, and bone area fraction-occupied evaluation. Statistical evaluation was performed by one-way analysis of variance (P < 0.05) and post hoc testing by the Tukey test.Results: The alumina-blasting surface presented the highest average surface roughness and mean root square of the surface values, the biologic blasting the lowest, and AB/AE an intermediate value. The remaining surfaces presented intermediate values between the biologic blasting and AB/AE. The x-ray photoelectron spectroscopy spectra revealed calcium and phosphorus for the biologic blasting and microblasted RBM surfaces, and the highest oxygen levels for the plasma, microblasted RBM, and AB/AE surfaces. Significantly higher torque was observed at 2 weeks for the microblasted RBM surface (P < 0.04), but no differences existed between surfaces at 4 weeks (P > 0.74). No significant differences in bone-implant contact and bone area fraction-occupied values were observed at 2 and 4 weeks.Conclusion: The five surfaces were osteoconductive and resulted in high degrees of osseointegration and biomechanical fixation. J Periodontol 2011;82:742-750.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Objectives: To evaluate the influence of different protocols for resin cement removal during cementation on biofilm formation.Methods: Twenty-eight ceramic blocks, which were injected under pressure, were placed over enamel blocks obtained from freshly extracted bovine incisors. The ceramic blocks were cemented to the enamel blocks using a dual-cured resin cement and the excess resin was removed according to the experimental group: TS: Teflon spatula; BR: brush; BR+: brush and polishing; SB+: scalpel blade and polishing. After autoclaving, the samples were colonised by incubation in a sucrose broth suspension standardised with Streptococcus mutans in microaerophilic stove. Specimens were quantitatively analysed for bacterial adherence at the adhesive interface using confocal laser scanning microscopy and counting the colony forming units, and qualitatively analysed using SEM. The roughness (Ra/Rz/RSm) was also analysed. Data were analysed by 1-way ANOVA and Tukey's test (5%).Results: The roughness values ranged from 0.96 to 1.69 mu m for Ra (p > 0.05), from 11.59 to 22.80 mu m for Rz (p = 0.02 < 0.05) and from 293.2 to 534.3 mu m for RSm (p = 0.00). Bacterial adhesion varied between 1,974,000 and 2,814,000 CFU/ml (p = 0.00). Biofilm mean thickness ranged from 0.477 and 0.556 mu m (p > 0.05), whilst the biovolume values were between 0.388 and 0.547 mu m(3)/mu m(2) (p = 0.04). Lower values for roughness, bacterial adhesion, biofilm thickness and biovolume were found with BR, whilst TS presented the highest values for most of the parameters. SEM images confirmed the quantitative values.Conclusions: The restoration margin morphology and interface roughness affects bacterial accumulation. The brush technique promoted less bacterial colonisation at the adhesive interface than did the other removal methods.Clinical significance: The brush technique seems to be a good option for removing the excess resin cement after adhesive cementation in clinical practice, as indicated by its better results with lower bacterial colonisation. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Ferroelectric SrBi4Ti4O15 thin films were successfully prepared on a Pt(111)/Ti/SiO2/Si(100) substrate for the first time by spin coating, using the polymeric precursor method. X-ray diffraction patterns of the films indicate that they are polycrystalline in nature. Atomic force microscopy (AFM) analyses showed that the surface of these films is smooth, dense and crack-free with low surface roughness (6.4 nm). At room temperature and at a frequency of 1 MHz, the dielectric constant and the dissipation factor were, respectively, 150 and 0.022. The C-V characteristics of perovskite thin film prepared at low temperature show normal ferrolectric behaviour. The remanent polarization and coercive field for the films deposited were 5.4 mu C/cm(2) and 8 5 kV/cm, respectively. All the capacitors showed good polarization fatigue characteristics at least up to 1 x 10(10) bipolar pulse cycles indicating that SrBi4Ti4O15 thin films can be a promising material for use in nonvolatile memories. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Polymeric precursor solution (Pechini method) was used to deposit LiNbO3 thin films by spin-coating on (100) silicon substrates. X-ray diffraction data of thin films showed that the increase of oxygen flow promotes a preferred orientation of (001) LiNbO3 planes parallel to the substrate surface. Surface roughness and grain size, observed by atomic force microscopy, change also with oxygen flow.
Resumo:
Ferroelectric Pb1-xCaxTiO3 (x = 0.24) thin films were formed on a Pt/Ti/SiO2/Si substrate by the polymeric precursor method using the dip-coating technique for their deposition. Characterization of the films bq X-ray diffraction showed a perovskite single phase with a tetragonal structure after annealing at 700 degreesC. Atomic force microscopy (AFM) analyses showed that the film had a smooth and crack-free surface with low surface roughness. In addition, the PCT thin film had a granular structure with an 80 nm grain size. The thickness of the films observed by the scanning electron microscopy (SEM) is 550 nm and there is a good adhesion between the film and substrate. For the electrical measurements metal-ferroelectric-metal of the type capacitors were obtained, where the thin films showed good dielectric and ferroelectric properties. The dielectric constant and dissipation factor at 1 kHz and measured at room temperature were found to be 457 and 0.03. respectively. The remanent polarization and coercive field for the: deposited films were P-r = 17 muC/cm(2) and E-c = 75 kV/cm, respectively. Moreover. The 550-nm-thick film showed a current density in the order of 10(-8) A/cm(2) at the applied voltage of 2 V. The high values of the thin film's dielectric properties are attributed to its excellent microstructural quality and the chemical homogeneity obtained by the polymeric precursor method. (C) 2001 Elsevier science Ltd. All rights reserved.