877 resultados para diode-pump laser
Resumo:
By using a semiconductor saturable-absorber output coupler as a mode-locking device, we experimentally realized the operation of a diode-pumped passively mode-locked Nd:YVO4 laser. Stable laser pulses with duration of 2.3 ps were generated at the output power of about 1 W. With increasing the pump power to 9 W, the maximum mode-locked power of 1.7 W was obtained, which corresponds to a slope conversion efficiency of 44% and optical-to-optical conversion efficiency of 19%.
Resumo:
We report on a diode- pumped CW passively mode locked ceramic Nd: YAG laser with SESAM ( semiconductor saturable absorber mirror), wavelength 1064nm. At a pump power of 7.6w, the pulse width was estimated to be similar to 8.3ps with repetition rate similar to 130MHz and the average output power was 1.59w. To our knowledge, this was the first demonstration that ceramic Nd: YAG was used for diode pumped CW passively mode locking. (C) 2005 Optical Society of America.
Resumo:
Passive mode locking of a diode-pumped Nd:GdVO4 laser was demonstrated using In0.25Ga0.75As as saturable absorber as well as output coupler. The pulse width was measured to be about 16 ps with a repetition rate of 146 MHz. The average output power was 120 mW with pump power of 6 W. To our knowledge, this is the first demonstration on a passively mode-locked Nd:GdVO4 laser by using an In0.25Ga0.75As output coupler. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
We have demonstrated a passively Q-switched and mode-locked Nd:YVO4 laser with an intracavity composite semiconductor saturable absorber (ICSSA). Stable Q-switched and mode-locked pulses with Q-switched envelope pulse duration of 180 ns and pulse repetition rate of 72KHz have been obtained. The maximum average output power was 1.45W at 8W incident pump power. The repetition rate of the mode-locked pulses inside the Q-switched envelope was 154 MHz. Experimental results revealed that this ICSSA was suitable for Q-switched and mode-locked solid-state lasers. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
A diode-pumped passively Q-switched mode-locked (QML) Nd:GdVO4 laser with a low temperature GaAs (LT-GaAs) saturable absorber is presented. The maximal Q-switched mode-locked average output power was 798 mW with the Q-switched envelop having a repetition rate of 125 kHz. The mode-locked pulse trains inside the Q-switched pulse envelope had a repetition rate of similar to 750 MHz. The laser properties of the operational parameters on the pump power were also investigated experimentally.
Resumo:
We have demonstrated a self-staring passively continuous-wave mode-locked diode end-pumped Nd:YLF laser with a semiconductor saturable absorber mirror of single-quantum-well (In0.25Ga0.75As) grown by metal-organic chemical-vapor deposition technique at low temperature. The saturable absorber was used as nonlinear absorber and output coupler simultaneously. Stable pulse duration of 3 ps has been achieved at the repetition rate of 98 MHz. The average output power was 530 mW at 1053 nm under the incident pump power of 10 W, corresponding to the peak power of 1.8 kW and pulse energy of 5.4 nJ.
Resumo:
A simple cw mode-locked solid-state laser, which is end-pumped by a low-power laser diode, was demonstrated by optimizing the laser-mode size inside the gain medium. The optimum ratio between mode and pump spot sizes inside the laser crystal was estimated for a cw mode-locked laser, taking into account the input pump power. Calculation and experiment have shown that the optimum ratio was about 3 when the pump power is 2 W, which is different from the value regularly used in passively mode-locked solid-state lasers. This conclusion is also helpful in increasing the efficiency of high-power ultrashort lasers. (C) 2006 Society of Photo-Optical Instrumentation Engineers.
Resumo:
We have demonstrated an efficient and compact passively Q-switched and mode-locked (QML) 1064 nm Nd:YVO4 laser by using a low temperature grown GaAs (LT-GaAs) saturable absorber as well as an output coupler. Stable QML with envelope duration as short as 10 ns and Q-switched repetition rate of 36 kHz was obtained. It is the shortest envelope duration as far as we know, and it is so short that it can be used as Q-switching pulses directly. At 6.9 W of the incident pump power, average output power of 1.24 W was achieved and the corresponding peak power and energy of a single Q-switched pulse were 3.44 kW and 34.4 mu J, respectively. The mode-locked pulses inside the Q-switched pulse envelope had a repetition rate of 780 MHz. (C) 2005 Elsevier B.V. All rights reserved.
Resumo:
A passively Q-switched Yb: YAG microchip laser has been constructed by using a doped GaAs as the saturable absorber as well as the output coupler. At 13.5 W of pump power the device produces high-quality 3.4 muJ 52 ns pulses at 1030nm with a pulse repetition rate of 7.8kHz in a TEM00-mode.
Resumo:
We report an end-pumped and passive mode-locking all-solid-state laser. The laser consists of a Nd:GdVO4 crystal and a linear resonator with a semiconductor saturable absorber mirror that yield mode locking. We achieved stable continuous-wave mode locking with an 8-ps pulse duration at a 154-MHz repetition rate. The average output power was 600 mW with 4 W of pump power. To our knowledge this is the first report of the use of a Nd:GdVO4 crystal for mode locking with a semiconductor saturable absorber mirror. (C) 2003 Optical Society of America.
Resumo:
Two semiconductor saturable absorber mirrors (SESAMs), of which one is coated with 50% reflection film on the top and the other is not, were contrastively studied in passively mode-locked solid-state lasers which were pumped by low output power laser diode (LD). Experiments have shown that reducing the modulation depth of SESAM by coating partial reflection film, whose reflectivity is higher than that between SESAM and air interface, is an effective method to get continuous wave (CW) mode-locking instead of Q-switched mode-locking (QML) in low power pumped solid-state lasers. A simple Nd:YVO4 laser pumped by low power LD, in which no water-cooling system was used, could obtain CW mode-locking by the 50% reflector coated SESAM with average output power of ~ 20 mW
Resumo:
Polymethyl methacrylate (PMMA) optical fibres are fabricated by a preform drawing process. The Raman spectra of PMMA fibres are recorded using a diode pumped solid state laser emitting at 532 nm and a CCD-spectrograph in the 400–3800 cm−1 range. The variation of the Raman intensity with the length of the optical fibre is studied. Investigations are carried out on the variation of FWHM of the Raman peak at 2957 cm−1 with the length of the optical fibre and pump power. The differential scattering cross section and gain coefficient of the Raman peak at 2957 cm−1 in PMMA are calculated in relation to that of toluene.
Resumo:
Polymethyl methacrylate (PMMA) optical fibres are fabricated by a preform drawing process. The Raman spectra of PMMA fibres are recorded using a diode pumped solid state laser emitting at 532 nm and a CCD-spectrograph in the 400–3800 cm−1 range. The variation of the Raman intensity with the length of the optical fibre is studied. Investigations are carried out on the variation of FWHM of the Raman peak at 2957 cm−1 with the length of the optical fibre and pump power. The differential scattering cross section and gain coefficient of the Raman peak at 2957 cm−1 in PMMA are calculated in relation to that of toluene
Resumo:
In this paper we investigate the energy transfer processes in TM3+/Er3+ doped telluride glass pumped at the commercial diode laser pump wavelength similar to 800 nm. Tailoring the rare-earths content in the glass matrix, seven main energy transfer channels within the doping range considered were identified, A 6-fold enhancement of the Er3+ visible frequency upconversion fluorescence at similar to 660 nm is observed due to the inclusion of Tm3+ ions. This is evidence of the relevant contribution of the route Er-1(I-4(11/2)) + Er-2(I-4(13/2)) -> Er-1(I-4(15/2)) + Er-2(F-4(9/2)) to the process. Energy migration among pumped I-4(9/2) level reducing the efficiency of the upconversion emission rate (H-3(11/2), S-4(3/2), and F-4(9/2)) is observed for Er3+ above 1.5 wt%. The rate equations regarding the observed energy transfer routes are determined and a qualitative analysis of the observed processes is reported. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Through the use of Transient Diode Laser Absorption Spectroscopy (TDLAS), the rate coefficient for the vibrational relaxation of N2O (ν2) by O(3P) at room temperature (32 ºC)) was determined to be (1.51 ± 0.11)x10-12 cm3molecule-1sec-1. A Q-switched, frequency quadrupled (266 nm) Nd:YAG laser pulse was used as the pump for this experiment. This pulse caused the photodissociation of O3 into O2 and O atoms.Excited oxygen (O(1D)) was collisionally quenched to ground state (O(3P)) by Ar and/or Xe. Photodissociation also caused a temperature jump within the system, exciting the ν2 state of N2O molecules. Population in the ν2 state was monitored through a TDLASobservation of a ν3 transition. Data were fit using a Visual Fortran 6.0 Global Fitting program. Analysis of room temperature data taken using only Ar to quench O atoms to the ground state gave the same rate coefficient as analysis of data taken using an Ar/Xe mixture, suggesting Ar alone is a sufficient bath gas. Experimentation was alsoperformed at -27 ºC and -82 ºC for a temperature dependence analysis. A linear regression analysis gave a rate coefficient dependence on temperature of ... for the rate coefficient of the vibrational relaxation of N2O (ν2) by atomic oxygen.