982 resultados para metalorganic chemical vapor deposition
Resumo:
The effects of in situ annealing treatment in the initial growth stage and In-doping during growth of the GaN on the material properties were investigated. GaN was grown by LP-MOVPE. In situ annealing reduced the full-width at half-maximum (FWHM) of X-ray rocking curves and reduced etch pit density of GaN films. It improved the optical properties of the epilayer. Undoped and In-doped GaN films of initial growth stage were investigated. It was found that morphology and optical properties were improved in In-doped samples. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Micro-Raman measurements were carried out to investigate the microstructure of amorphous silicon-nitrogen alloy (a-SiNx:H) samples with different N contents prepared by plasma enhanced chemical vapor deposition (PECVD). Resonant Raman effect was discovered by using 647.1- and 514.5-nm excitation wavelengths. The frequency of TO mode downshifts with increasing photon energy without varying its width, while LO mode expands to a great extent. The frequency-dependent shift of TO band is explained by heterogeneous structure model and quantum confinement model, and the width expansion of LO mode may be related to the overlapping of LA and LO bands. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
As reported by other authors, we have also observed that the Si growth rate decreases with increasing phosphine (PH3) flow rate in gas source-Si molecular beam epitaxy using phosphorous (P) as a n-type dopant. Why small quantity PH3 can affect Si growth rate? Up to now, the quantitative characterization of PH3 flow influence on Si growth rate is little known. In this letter, the PH, influence will be analyzed in detail and a model considering strong P surface segregation and its absorption of hydrogen will be proposed to characterize the effect. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Phosphor-doped nano-crystalline silicon ((n))nc-Si:H) films are successfully grown on the p-type (100) oriented crystal silicon ((p) c-Si) substrate by conventional plasma-enhanced chemical vapor deposition method. The films are obtained using high H-2 diluted SiH4 as a reaction gas source and using PH3 as the doping gas source of phosphor atoms. Futhermore, the heterojunction diodes are also fabricated by using (n)nc-Si:H films and (p)c-Si substrate. I-V properties are investigated in the temperature range of 230-420K. The experimental results domenstrate that (n)nc-Si:H/(p) c-Si heterojunction is a typical abrupt heterojunction having good rectifing and temperature properties. Carrier transport mechanisms are tunneling - recombination model at forward bias voltages. In the range of low bias voltages ( V-F< 0.8 V), the current is determined by recombination at the (n)nc-Si:H side of the space charge region, while the current becomes tunneing at higher bias voltages( V-F>1.0 V). The present heterojunction has high reverse breakdown voltage ( > - 75 V) and low reverse current (approximate to nA).
Resumo:
In this paper, we conduct a theoretical analysis of the design, fabrication, and performance measurement of high-power and high-brightness strained quantum-well lasers emitting at 0.98 mum, The material system of interest consists of an Al-free InGaAs-InGaAsP active region and AlGaAs cladding layers. Some key parameters of the laser structure are theoretically analyzed, and their effects on the laser performance are discussed. The laser material is grown by metal-organic chemical vapor deposition and demonstrates high quality with low-threshold current density, high internal quantum efficiency, and extremely low internal loss. High-performance broad-area multimode and ridge-waveguide single-mode laser devices are fabricated. For 100-mum-wide stripe lasers having a cavity length of 800 mum, a high slope efficiency of 1.08 W-A, a low vertical beam divergence of 34 degrees, a high output power of over 4.45 W, and a very high characteristic temperature coefficient of 250 K were achieved. Lifetime tests performed at 1.2-1.3 W (12-13 mW/mum) demonstrates reliable performance. For 4-mum-wide ridge waveguide single-mode laser devices, a maximum output power of 394 mW and fundamental mode power up to 200 mW with slope efficiency of 0.91 mW/mum are obtained.
Resumo:
The hydrogenated amorphous SiOx films (a-SiOx:H) with various oxygen contents have been prepared using plasma enhanced chemical vapor deposition technique. The films were implanted with erbium and annealed by rapid thermal annealing. An intense photoluminescence (PL) of Er at 1.54 mum has been observed at 77 K and at room temperature. The PL intensity depends strongly on both the oxygen content of the film and the rapid thermal annealing temperature and reaches its maximum if the ratio of O/Si in the film is approximately equal to 1.0 at 77 K and to 1.76 at room temperature. The microstructure of the film also has strong influences on the PL intensity. The PL intensity at 250 K is slightly more than a half of that at 15 K. It means that the temperature quenching effect of the PL intensity is very weak.
Resumo:
By mass-selected low energy ion beam deposition, amorphous carbon film was obtained. X-ray diffraction, Raman and Auger electron spectroscopy depth line shape measurements showed that such carbon films contained diamond particles. The main growth mechanism is subsurface implantation. Furthermore, it was indicated in a different way that ion bombardment played a decisive role in bias enhanced nucleation of chemical vapor deposition diamond.
Resumo:
The surface reaction mechanism of Si1-xGex/Si growth using SiH4 and GeH4 in UHV/CVD system was studied. The saturated adsorption and desorption of SiH4 from Si(1 0 0) surface was investigated with the help of TPD and RHEED, and it was found that all the 4 hydrogen atoms of one SiH4 molecule were adsorbed to the Si surface, which meant that the dissociated adsorption ratio was proportional to 4 power of surface vacancies. The analysis of the reaction of GeH4 was also done. A new surface reaction kinetic model on Si1-xGex/Si epitaxial growth under UHV conditions by SiH4/GeH4 was proposed based on these studies. The predictions of the model were verified by the experimental results. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
We have studied the effect of rapid thermal annealing (RTA) on GaInNAs/GaAs quantum wells (QWs) grown by molecular-beam epitaxy using a dc plasma as the N source. It was found that RTA at low temperature (LT, 650 degrees C) and high temperature (HT, 900 degrees C) could both improve the QW quality significantly. To clarify the mechanism of quality improvement by RTA, a magnetic field perpendicular to the path of the N plasma flux was applied during the growth of the GaInNAs layers for the sake of comparison. It was found that LT-RTA mainly removed dislocations at interfaces related to the ion bombardment, whereas, HT-RTA further removed dislocations originating from the growth. LT-RTA caused only a slight blueshift of photoluminescence peak wavelength, probably due to defect-assisted interdiffusion of In-Ga at the QW interfaces. The blueshift caused by HT-RTA, on the other hand, was much larger. It is suggested that this is due to the fast defect-assisted diffusion of N-As at the QW interfaces. As defects are removed by annealing, the diffusion of In-Ga at interfaces would be predominant. (C) 2000 American Institute of Physics. [S0003- 6951(00)01535-7].
Resumo:
A constant amount of Ge was deposited on strained GexSi1-x layers of approximately the same thickness but with different alloy compositions, ranging from x = 0.06 to x = 0.19. From their atomic-force-microscopy images, we found that both the size and density of Ge islands increased with the Ge composition of the strained layer. By conservation of mass, this implies that these islands must incorporate material from the underlying strained layer. (C) 2000 American Institute of Physics. [S0003-6951(00)03529-4].
Resumo:
Hydrogenated amorphous SiOx films are fabricated via plasma enhanced chemical vapor deposition technique. After erbium implantation and rapid thermal annealing, photoluminescence (PL) are measured at 77 K and room temperature (RT), respectively. We observed the strong PL at 1.54 mu m at RT. The 1.54 mu m PL intensity changes with the variation of concentration of oxygen. The most intense PL at 77 K in a-SiOx:H (Er) corresponds to O/Si = 1.0 and at RT to O/Si = 1.76. Based on our results, we propose that Er ions contributed to PL come from O-rich region in the film. Er ions in Si-rich region have no relation with FL. Temperature dependence of the intensity of the 1.54 mu m line of the Er3+ transition displays a very weak temperature quenching in Er-doped hydrogenated amorphous Si. The PL intensity at 250 K is a little more one half of that at 15 K.
Resumo:
We have studied the growth of GaInNAs by a plasma-assisted molecular-beam epitaxy (MBE). It was found that the N-radicals were incorporated into the epitaxial layer like dopant atoms. In the range of 400-500 degrees C, the growth temperature (T-g) mainly affected the crystal quality of GaInNAs rather than the N concentration. The N concentration dropped rapidly when T-g exceeded 500 degrees C. Considering N desorption alone is insufficient to account for the strong falloff of the N concentration with T-g over 500 degrees C, the effect of thermally-activated N surface segregation must be taken into account. The N concentration was independent of the arsenic pressure and the In concentration in GaInNAs layers, but inversely proportional to the growth rate. Based on the experimental results, a kinetic model including N desorption and surface segregation was developed to analyze quantitatively the N incorporation in MBE growth. (C) 2000 American Institute of Physics. [S0003-6951(00)00928-1].
Resumo:
We report on the strong blue-violet photoluminescence (PL) at room temperature from the large-scale highly aligned boron carbonitride (BCN) nanofibers synthesized by bias-assisted hot filament chemical vapor deposition. The photoluminescence peak wavelength shifts in the range of 470-390 nm by changing the chemical composition of the BCN nanofibers, which shows an interesting blue and violet-light-emitting material with adjustable optical properties. The mechanism for the shift of the PL peaks at room temperature is also discussed. (C) 2000 American Institute of Physics. [S0003-6951(00)04427-2].
Resumo:
Raman scattering measurement has been used to study the residual strains in the thin 3C-SiC/Si(001) epilayers with a variation of film thickness from 0.1 to 1.2 mu m. which were prepared by chemical vapor deposition (CVD)growth. Two methods have been exploited to figure our the residual strains and the exact LO bands. The final analyzing results show that residual strains exist in the 3C-SiC epilayers. The average stress is 1.3010 GPa, and the relative change of the lattice constant is 1.36 parts per thousand. Our measurements also show that 3C-SiC phonons are detectable even for the samples with film thickness in the range of 0.1 to 0.2 mu m. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
Resumo:
Nanocrystalline silicon (nc-Si) embedded SiO2 matrix has been formed by annealing the SiOx films fabricated by plasma-enhanced chemical vapor deposition (PECVD) technique. Absorption coefficient and photoluminescence of the films have been measured at room temperature. The experimental results show that there is an "aUrbach-like" b exponential absorption in the spectral range of 2.0-3.0 eV. The relationship of (alpha hv)(1/2) proportional to(hv - E-g) demonstrates that the luminescent nc-Si have an indirect band structure. The existence of Stokes shift between photoluminescence and absorption edge indicates that radiative combination can take place not only between electron states and hole states but also between shallow trap states of electrons and holes. (C) 2000 Elsevier Science B.V. All rights reserved.