932 resultados para oligomeric and polymeric thiophenes
Resumo:
CaBi4Ti4O15 thin films were deposited by the polymeric precursor method and crystallized in a domestic microwave oven and conventional furnace. The films obtained for microwave energy are well-adhered, homogeneous and with good specularity, when treated at 700 degrees C for 10 min. The microstructure and the structure of the films can be tuned by adjusting the crystallization conditions. When microwave oven is employed, the films presented bigger grains with mean grain size around 80 nm. For comparison, films were also prepared by the conventional furnace at 700 degrees C for 2 h. (C) 2007 Elsevier Masson SAS. All rights reserved.
Resumo:
Nanocrystalline Al(2)O(3)powders have been synthesized by the polymeric precursor method. A study of the evolution of crystalline phases of obtained powders was accomplished through X-ray diffraction, micro-Raman spectroscopy and refinement of the structures through the Rietveld method. The results obtained allow the identification of three steps on the gamma-Al2O3 to alpha-Al2O3 phase transition. The single-phase alpha-Al2O3 Powder was obtained after heat-treatment at 1050 degrees C for 2 h. A study of the morphology of the particles was accomplished through measures of crystallite size, specific surface area and transmission electronic microscopy. The particle size is closely related to gamma-Al2O3 to alpha-Al2O3 phase transition. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Thin films of lithium niobate were deposited on (100) silicon by the polymeric precursor method (Pechini method). Annealing in static air was performed at 500degreesC for 3 h. The films obtained were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. Electrical characterization of the films pointed to ferroelectricity via hysteresis loop. The dielectric constant, dissipation factor and resistance were measured in the frequency region from 10 Hz to 10 MHz. At 1 MHz, the dielectric constant was 46 and the dissipation factor was 0.043. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Disordered and crystalline Ba0.45Sr0.55TiO3 (BST) powder processed at low temperature was synthesized by the polymeric precursor method. The single-phase perovskite structure of the ceramics was identified by the Raman and X-ray diffraction techniques. Photoluminescence at room temperature was observed only in a disordered BST sample. Increasing the calcination time intensified the photoluminescence (PL), which reached its maximum value in the sample heat treated at 300 degrees C for 30 h. This emission may be correlated with the structural disorder. Periodic ab initio quantum-mechanical calculations using the CRYSTAL98 program can yield important information regarding the electronic and structural properties of crystalline and disordered solids. The experimental and theoretical results indicate the presence of intermediary energy levels in the band gap. This is ascribed to the break in symmetry, which is responsible for visible photoluminescence in the material's disordered state at room temperature. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Polymeric precursor solution (Pechini method) was used to deposit LiNbO3 thin films by spin-coating on (100) silicon substrates. X-ray diffraction data of thin films showed that the increase of oxygen flow promotes a preferred orientation of (001) LiNbO3 planes parallel to the substrate surface. Surface roughness and grain size, observed by atomic force microscopy, change also with oxygen flow.
Resumo:
PLZT thin films were prepared by a dip coating process using Pechini's method, also known as polymeric precursor method. The PLZT solution was obtained from a mixture of the individual cation solutions and the process to prepare each solution is based on metallic citrate polymerization. The viscosity of the PLZT solution was adjusted at 40 cP while the ionic concentration was adjusted at 0.1 M. PLZT solutions were deposited on silicon (100) and platinum coated silicon (100) substrates with withdrawal speed at 5 mm/min. The coated substrates were thermally treated with a heating rate of 1 degreesC/min up to 300 degreesC and 5 degreesC/min up to 650 degreesC in order to obtain homogeneous and cracks free films. The influence of oxygen flow on crystallization and morphology of PLZT (9/65/35) thin film is discussed. (C) 2002 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
Thin films of lithium niobate were deposited on Pt/Ti/SiO2 (111) substrates by spin coating from the polymeric precursor method (Pechini process). Annealing in static air was performed at 500 degreesC for 3 h. The obtained films were characterized by X-ray diffraction and atomic force microscopy. The dielectric constant, dissipation factor and resistance were measured in frequency region from 10 Hz to 10 MHz and the hysteresis loop was obtained. The influence of number of layers on crystallization, morphology and properties of LiNbO3 thin films is discussed. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Visible photoluminescence (PL) was observed for the first time at room temperature in structurally disordered calcium strontium tungstate powder, Ca0.60Sr0.40WO4 (CSW), obtained by the polymeric precursor method. The PL behavior of CSW powders has been analyzed as a function of the disorder rate, based on experimental and theoretical studies. Quantum mechanical theory based on density functional theory at the B3LYP level has been employed to study the electronic structure of two periodic models representing both crystalline and disordered powders. Their electronic structures have been analyzed in terms of density of states, band dispersion and charge densities. The calculations indicate a break in symmetry when passing from crystalline to disordered models, creating localized electronic levels above the valence band. Moreover, a negative charge transfer process takes place from the [WO3] cluster to the [WO4] cluster. The polarization induced by the break in symmetry and the existence of localized levels favors the creation of trapped holes and electrons, originating the PL phenomenon. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Synthesis and characterization of antimony tartrate used as a precursor of ceramic powders obtained by Pechini's method were carried out. Antimony tartrate was chosen as a substitute for the antimony citrate commonly used in this chemical processing, because of difficulties in preparing the citrate. FTIR and TGA/DTA analysis showed that antimony tartrate, H-2[Sb-2(C4H2O6)(2)]. forms a polymeric structure. The procedure described indicates that the antimony chelate obtained is adequate for Pechini's method.
Resumo:
The correlation between experimental data and theoretical calculations have been investigated to explain the photoluminescence at room temperature of Ba(Ti0.75Zr0.25)O-3 (BTZ) thin films prepared by the polymeric precursor method. The degree of structural order-disorder was investigated by X-ray diffraction, Fourier transform infrared spectroscopy, ultraviolet-visible absorption spectroscopy and photoluminescence (PL) measurements. First-principles quantum mechanical calculations based on density functional theory (B3LYP level) were employed to study the electronic structure of ordered and deformed asymmetric models. The electronic properties are analyzed and the relevance of the present theoretical and experimental results on the PL behavior is discussed. The presence of localized electronic levels and a charge gradient in the band gap due to a break in symmetry, are responsible for the PL in disordered BTZ lattice. (c) 2007 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Thin films of lithium niobate were deposited on the Pt/Ti/SiO2 (111) substrates by spin coating from the polymeric precursor method (Pechini process). Annealing in static air and oxygen atmosphere was performed at 500 degreesC for 3 h. The films obtained were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. The dielectric constant and dissipation factor were measured in frequency region from 10 Hz to 10 MHz. Electrical characterization of the films pointed to ferroelectricity via hysteresis loop. The influence of oxygen atmosphere on crystallization, morphology and properties of LiNbO3 thin films is discussed. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), with x ranging from 0 to 0.75 was grown on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution and spin-coating method. The dielectric constant of highly doped bismuth titanate was equal to 148 while dielectric losses remained low (tan delta = 0.0018), and the films showed well-saturated polarization-electric field curves (2P(r) = 40.6 muC/cm(2) and V-c = 0.99 V). The leakage current densities improve for the lanthanum-doped system. For five-layered BLT films with x = 0.75, a charge storage density of 35 fC/mum(2) and a thickness of 320 nm were found. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Ca(Zr0.05Ti0.95)O-3 (CZT) thin films were prepared by the polymeric precursor method by spin-coating process. The films were deposited on Pt(1 1 1)/Ti/SiO2/Si(1 0 0) substrates and annealed at 650 degrees C for 2,4, and 6 It in oxygen atmosphere. Structure and morphology of the CZT thin films were characterized by the X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FT-IR), atomic force microscopy (AFM) and field-emission scanning electron microscopy (FEG-SEM). XRD revealed that the film is free of secondary phases and crystallizes in the orthorhombic structure. The annealing time influences the grain size, lattices parameter and in the film thickness. (c) 2006 Elsevier B.V. All rights reserved.