999 resultados para Crystal quality
Resumo:
ZnO films are prepared on glass substrates by pulsed laser deposition (PLD) at different oxygen pressures, and the effects of oxygen pressure on the structure and optoelectrical properties of as-grown ZnO films are investigated. The results show that the crystallite size and surface roughness of the films increase, but the carrier concentration and optical energy gap E-g decrease with increasing oxygen pressure. Only UV emission is found in the photoluminescence (PL) spectra of all the samples, and its intensity increases with oxygen pressure. Furthermore, there are marked differences in structure and properties between the films grown at low oxygen pressures (0.003 and 0.2 Pa) and the films grown at high oxygen pressures (24 and 150 Pa), which is confirmed by the fact that the crystallite size and UV emission intensity markedly increase, but the carrier concentration markedly decreases as oxygen pressure increases from 0.2 to 24 Pa. These results show that the crystal quality, including the microstructural quality and stoichiometry proportion, of the prepared ZnO films improves as oxygen pressure increases, particularly from 0.2 to 24 Pa.
Resumo:
ZnO thin films were prepared by pulsed laser deposition (PLD) on glass substrates with growth temperature from room temperature (RT) to 500 degrees C. The effects of substrate temperature on the structural and optical properties of ZnO films have been investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission spectra, and RT photoluminescence (PL) measurements. The results showed that crystalline and (0 0 2)-oriented ZnO films were obtained at all substrate temperatures. As the substrate temperature increased from RT to 500 degrees C, the ratio of grain size in height direction to that in the lateral direction gradually decreased. The same grain size in two directions was obtained at 200 degrees C, and the size was smallest in all samples, which may result in maximum E, and E-0 of the films. UV emission was observed only in the films grown at 200 degrees C, which is probably because the stoichiometry of ZnO films was improved at a suitable substrate temperature. It was suggested that the UV emission might be related to the stoichiometry in the ZnO film rather than the grain size of the thin film. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Highly c-axis oriented ZnO thin films were deposited on Si substrates by the pulsed laser deposition (PLD) method. At different growth temperatures, 200 nm silver films as the contact metal were deposited on the ZnO thin films. The growth temperatures have great influence on the crystal quality of Ag films. Current-voltage characteristics were measured at room temperature. The Schottky contacts between Ag and ZnO thin films were successfully obtained when silver electrodes were deposited at 150A degrees C and 200A degrees C. Ohmic contacts were formed while the growth temperatures were lower than 150A degrees C or higher than 200A degrees C. After analysis, the forming of Ag/ZnO Schottky contacts was shown to be dependent on the appearance of the p-type inversion layer at the interface between Ag and ZnO layers.
Resumo:
Well-aligned Zn1-xMgxO nanorods and film with Mg-content x from 0 to 0.051 have been successfully synthesized by metal organic chemical vapor deposition (MOCVD) without any catalysts. The characterization results showed that the diameters and lengths of the nanorods were in the range of 20-80 nm and 330-360 nm, which possessed wurtzite structure with a c-axis growth direction. As the increase of Mg precursor flows into the growth chamber, the morphology of Zn1-xMgxO evolves from nanorods to a film with scale-like surface and the height of the nanorods and the film was almost identical, it is suggested that the growth rate along the c-axis was hardly changed while the growth of six equivalent facets of the type {1 0 (1) over bar 0} of the Zn1-xMgxO has been improved. Photoluminescence and Raman spectra show that the products have a good crystal quality with few oxygen vacancies. With the Mg incorporation, multiple-phonon scattering become weak and broad, and the intensities of all observed vibrational modes decrease. And the ultraviolet near-band-edge emission shows a clear blueshift (x=0.051, as much as 90 meV) and slightly broadening compared with that of pure ZnO nanorods. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
We investigate the molecular beam epitaxy growth of GaSb films on GaAs substrates using AlSb buffer layers. Optimization of AlSb growth parameter is aimed at obtaining high GaSb crystal quality and smooth GaSb surface. The optimized growth temperature and thickness of AlSb layers are found to be 450 degrees C and 2.1 nm, respectively. A rms surface roughness of 0.67 nm over 10 x 10 mu m(2) is achieved as a 0.5 mu m GaSb film is grown under optimized conditions.
Resumo:
The growth direction of ZnO thin films grown by metal-organic chemical vapor deposition (MOCVD) is modulated by pretreatment of (001) SMO3 (STO) substrates. ZnO films show a-oriented smooth surface with epitaxial relationship of < 001 > ZnO//< 110 > STO on as-received SfO, and c-axis columnar growth with < 010 > ZnO//< 110 > STO on etched STO, respectively. The orientation alteration of ZnO films is supposed to be caused by the change of STO surface polarity. In addition, the c-ZnO films exhibit an enhanced photoluminescence (PL) intensity due to the improved crystal quality, while the blueshift of PL peak is attributed to the smaller tensile strain. These results show that high quality c-ZnO, which is essential for electronic and optoelectronic device applications, can be grown on (001) SfO by MOCVD. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Sapphire substrates were nano-patterned by inductive coupled plasma etching process. Nonpolar a-plane GaN films were grown on planar and nano-patterned r-plane sapphire substrates by metal organic chemical vapor deposition. The anisotropic characteristic and the crystalline quality of the a-plane GaN films were studied through XRD rocking curves. The cross section and surface morphologies of the a-plane GaN films were studied using SEM and AFM measurements, respectively. The crystal quality and surface flatness of the nonpolar a-plane GaN were greatly improved through the usage of the nano-patterned r-plane sapphire substrates. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
ZnO film of 8 mu m thickness was grown on a sapphire (0 0 1) substrate with a GaN buffer layer by a novel growth technique called metal-source vapor phase epitaxy (MVPE). The surface of ZnO film measured by scanning electron microscope (SEM) is smooth and shows many regular hexagonal features. The full width at half maximum (FWHM) of ZnO(0 0 2) and (1 0 2) omega-scan rocking curves are 119 and 202 arcsec, corresponding a high crystal quality. The status of the strain in ZnO thick film was particularly analyzed by X-ray diffraction (XRD) omega-20 scanning. The results show that the strain in ZnO film is compressive, which is also supported by Raman scattering spectroscopy. The compressive strain can solve the cracking problem in the quick growth of ZnO thick film. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
High-density and uniform well-aligned ZnO sub-micron rods are synthesized on the silicon substrate over a large area. The morphology, and structure of the ZnO sub-micron rods are investigated by x-ray diffraction, transmission electron microscopy and Raman spectra. It is found that the ZnO sub-micron rods are of high crystal quality with the diameter in the range of 400-600 nm and the length of several micrometres long. The optical properties were studied bill photoluminescence spectra. The results show that the intensity of the ultraviolet emission at 3.3 eV is rather high, meanwhile the deep level transition centred at about 2.38 eV is weak. The free exciton emission could also be observed at low, temperature, which implies the high optical quality of the ZnO sub-micron rods. This growth technique provides one effective way to fabricate the high crystal quality ZnO nanowires array, which is very important for potential applications in the new-type optoelectronic nanodevices.
Resumo:
GaN epilayers were grown on Si(111) substrate by metalorganic chemical vapor deposition. By using the Al-rich AlN buffer which contains Al beyond stoichiometry, crack-free GaN epilayers with 1 mum thickness were obtained. Through x-ray diffraction (XRD) and secondary ion mass spectroscopy analyses, it was found that a lot of Al atoms have diffused into the under part of the GaN epilayer from the Al-rich AlN buffer, which results in the formation of an AlxGa1-xN layer at least with 300 nm thickness in the 1 mum thick GaN epilayer. The Al fraction x was estimated by XRD to be about 2.5%. X-ray photoelectron spectroscopy depth analysis was also applied to investigate the stoichiometry in the Al-rich buffer before GaN growth. It is suggested that the underlayer AlxGa1-xN originated from Al diffusion probably provides a compressive stress to the upper part of the GaN epilayer, which counterbalances a part of tensile stress in the GaN epilayer during cooling down and consequently reduces the cracks of the film effectively. The method using the Al diffusion effect to form a thick AlGaN layer is really feasible to achieve the crack-free GaN films and obtain a high crystal quality simultaneously. (C) 2004 American Institute of Physics.
Resumo:
We have studied the influence of the growth temperature of the high-temperature (HT) AIN buffer layer on the properties of the GaN epilayer which was grown on Si(111) substrate by metalorganic chemical vapor deposition (MOCVD). It was found that the crystal quality of the GaN epilayer strongly depends on the growth temperature of the HT-AIN buffer. The growth temperature of the AIN buffer to obtain high-quality GaN epilayers lies in a narrow window of several tens of degrees. When the temperature is lower than a certain temperature range, the appearance of AIN polycrystals results in the deterioration of the crystal quality of the AIN buffer layer, which is greatly disadvantageous to the coalescence of the GaN epilayer. Although the AIN buffer's crystal quality is improved as the growth temperature increases, the Si outdiffusion from the substrate is also enhanced when the temperature is higher than a certain temperature range, which will demolish the subsequent growth of the GaN epilayer. Therefore, there exists an optimum growth temperature range of the AIN buffer around 1080degreesC for the growth of high-quality GaN epilayers. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
GaN nanowires have been grown with and without In as an additional source. The effects of In surfactant on the crystal quality and photoluminescence property of GaN nanowires are reported for the first time. X-ray diffraction, field emission scanning electron microscopy, high-resolution transmission electron microscopy, energy-dispersive x-ray spectroscopy, and photoluminescence measurements are employed to analyse the products. The results show that introducing a certain amount of In surfactant during the growth process can improve the crystal quality of the GaN nanowires, and enhance the photolurainescence of them. In addition, the as-prepared GaN nanowires have the advantage of being easy to be separated, which will benefit the subsequent nanodevice fabrication.
Resumo:
We have investigated the effect of the thickness and layer number of the low-temperature A1N interlayer (LT-A1N IL) on the stress relaxation and the crystal quality of GaN epilayers grown on Si (111) substrate by metalorganic chemical vapor deposition. It is found that the stress decreases with the increase of the LT-AIN IL thickness, but the crystal quality of the GaN epilayer goes worse quickly when the LT-AIN IL thickness is larger than 16 nm. This is because the increase of the LT-AIN IL thickness will increase the coalescence thickness of its upper GaN layer, which sensitively affects the crystal quality of the epilayer. Using multiple LT-AIN ILs is an effective method not only to reduce the stress, but also to improve the crystal quality of the GaN epilayer. With the increase of the interlayer number, the probability that dislocations are blocked increases and the probability that dislocations are produced at interfaces decreases. Thus, dislocations in the most upper part of GaN are reduced, resulting in the improvement of the crystal quality. Finally, it is suggested that when the total thickness of the epilayer is fixed, both the thickness and the number of the LT-AIN IL should be carefully designed to reduce the stress and improve the crystal quality of the epilayer simultaneously. (c) 2004 Elsevier B.V.. All rights reserved.
Resumo:
Two-dimensional ZnO nanowall networks were grown on ZnO-coated silicon by thermal evaporation at low temperature without catalysts or additives. All of the results from scanning electronic spectroscope, X-ray diffraction and Raman scattering confirmed that the ZnO nanowalls were vertically aligned and c-axis oriented. The room-temperature photoluminescence spectra showed a dominated UV peak at 378 nm, and a much suppressed orange emission centered at similar to 590 nm. This demonstrates fairly good crystal quality and optical properties of the product. A possible three-step, zinc vapor-controlled process was proposed to explain the growth of well-aligned ZnO nanowall networks. The pre-coated ZnO template layer plays a key role during the synthesis process, which guides the growth direction of the synthesized products. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
A new AlGaN/AlN/GaN high electron mobility transistor (HEMT) structure using a compositionally step-graded AlGaN barrier layer is grown on sapphire by metalorganic chemical vapour deposition (MOCVD). The structure demonstrates significant enhancement of two-dimensional electron gas (2DEG) mobility and smooth surface morphology compared with the conventional HEMT structure with high Al composition AlGaN barrier. The high 2DEG mobility of 1806 cm(2)/Vs at room temperature and low rms surface roughness of 0.220 nm for a scan area of 5 mu m x 5 mu m are attributed to the improvement of interfacial and crystal quality by employing the step-graded barrier to accommodate the large lattice mismatch stress. The 2DEG sheet density is independent of the measurement temperature, showing the excellent 2DEG confinement of the step-graded structure. A low average sheet resistance of 314.5 Omega/square, with a good resistance uniformity of 0.68%, is also obtained across the 50 mm epilayer wafer. HEMT devices are successfully fabricated using this material structure, which exhibits a maximum extrinsic transconductance of 218 mS/mm and a maximum drain current density of 800 mA/mm.