995 resultados para Deposition temperatures


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The growth and fabrication of GaN/InGaN multiple quantum well (MQW) light emitting diodes ( LEDs) on ( 100) beta-Ga2O3 single crystal substrates by metal-organic chemical vapour deposition (MOCVD) technique are reported. x-ray diffraction (XRD) theta-2 theta. scan spectroscopy is carried out on the GaN buffer layer grown on a ( 100) beta-Ga2O3 substrate. The spectrum presents several sharp peaks corresponding to the ( 100) beta-Ga2O3 and ( 004) GaN. High-quality ( 0002) GaN material is obtained. The emission characteristics of the GaN/InGaN MQW LED are measurement. The first green LED on beta-Ga2O3 with vertical current injection is demonstrated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nonpolar a-plane (1120) ZnO thin films have been fabricated on gamma-LiAlO2 (302) substrates via the low-pressure metal-organic chemical vapor deposition. An obvious intensity variation of the E-2 mode in the Raman spectra indicates that there exhibits in-plane optical anisotropy in the a-plane ZnO thin films. Highly-oriented uniform grains of rectangular shape can be seen from the atomic force microscopy images, which mean that the lateral growth rate of the thin films is also anisotropic. It is demonstrated experimentally that a buffer layer deposited at a low temperature (200 degrees C) can improve the structural and optical properties of the epilayer to a large extent. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Non-polar (1 (1) over bar 00)m-plane ZnO thin film has been prepared on gamma-LiAlO2 (100)substrate via the low pressure metal organic chemical vapor deposition. Obvious intensity variation of the E-2 mode in the polarized Raman spectra and the absorption edge shift in the polarized optical transmission spectra indicate that the m-plane film exhibits optical anisotropy, which have applications in certain optical devices, such as the UV modulator and polarization-dependent beam switch. From the atomic force microscopy images, highly-oriented uniform-sized grains of rectangular shape were observed. (c) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 coatings are prepared on fused silica with conventional electron beam evaporation deposition. After annealed at different temperatures for four hours, the spectra and XRD patterns of TiO2 thin film are obtained. XRD patterns reveal that only anatase phase can be observed in TiO2 coatings regardless of the different annealing temperatures, and with the increasing annealing temperature, the grain size gradually increases. The relationship between the energy gap and microstructure of anatase is determined and discussed. The quantum confinement effect is observed that with the increasing grain size of TiO2 thin film, the band gap energy shifts from 3.4 eV to 3.21 eV. Moreover, other possible influence of the TiO2 thin-film microstructure, such as surface roughness and thin film absorption, on band gap energy is also expected.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 coatings were prepared on fused silica with conventional electron beam evaporation deposition. After TiO2 thin films were annealed at different temperatures for 4 h, several properties were investigated by X-ray diffraction (XRD), spectrometer.. photoelectron spectroscopy (XPS) and AFM. It was found that with the annealing temperature increasing, the transmittance of TiO2 coatings decreased, and the cutoff wavelength shifted to long wavelength in near ultraviolet band. Especially, when coatings were annealed at high temperature, the optical loss is very serious, which can be attributed to the scattering and the absorption of TiO2 coatings. XRD patterns revealed that only anatase phase was observed in TiO2 coatings regardless of the different annealing temperatures. XPS results indicated that the fine chemical shift of TiO2 2p(1/2) should be attributed to existence of oxygen vacancies around Ti+4 ion. The investigation on surface morphology by AFM showed that the RMS of titania thin films gradually increases from less than 0.40 nm to 5.03 nm and it should be ascribed to the growth of titanium dioxide grain size with the increase of annealing temperature. (C) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Graded-index ZrO2 films has been fabricated on K9 glass by glancing angle deposition. Because the index mismatch at the interface has been reduced, the film results in wideband high-transmission antireflection. From 400nm to 1200nm, the film reflection is lower than 0.8% and the lowest value is 0.2% at 432nm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The temperature of water in a river system affects fish in various ways; it has an influence on feeding habits, movement and metabolism. All fish vary in their ability to tolerate fluctuations in temperature, but those that live in a reasonably stable environment are more sensitive to major changes (tropical fish) than are salmon which can tolerate abrupt changes. The body temperature of the majority of fish differs from that of the surrounding water by only 0.5 to 1.0 degrees, and changes in temperature can, in many cases, be a signalling factor for some process, for example spawning, migration or feeding. It has been found, after monitoring the activity in 2,623 salmon in the River Lune, that they live in a water temperature of 0-17 degrees. Whilst salmon ova can develop in a temperature range of 0-12 degrees, spawning takes place within a much closer range, and these tolerances will be found in the Report. This report offers data and analysis of fish movement correlated to water temperature for the years 1964/65.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Some results of an investigation on the layer thickness uniformity of glancing angle deposition are presented. A zirconia monolayer has been deposited by glancing angle deposition to analyze the layer thickness uniformity. The experimental results indicate that the thickness variation over the substrate is less than 0. 1%, which is considered as good uniformity. It is found that the non-uniformity of experimental results is larger than that of the theoretical results. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The glancing angle deposition (GLAD) technique was used to deposit ZnS films by electron beam evaporation method. The cross sectional scanning electron microscopy (SEM) image illustrated a highly orientated microstructure composed of slanted column. The atomic force microscopy (APM) analysis indicated that incident flux angle had significant effects on the nodule size and surface roughness. Under identical nominal thickness, the actual thickness of the GLAD films is related to the incident flux angle. The refractive index and in-plane birefringence of the GLAD ZnS films were discussed, and the maximum bireffingence Delta n = 0.036 was obtained at incident flux angle of alpha = 80 degrees. Therefore, the glancing angle deposition technique is a promising way to create a columnar structure with enhanced birefringent property. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 thin films were prepared on BK7 glass substrates by electron beam evaporation deposition method. The influence of deposition rate varying from 1.2 to 6.3 nm s(-1) on surface morphology and other properties of ZrO2 films were examined. With increasing deposition rate, the surface defect density increased. The decrease in half width at full maximum in X-ray diffraction pattern with deposition rate indicates an increase in crystal dimension with increasing deposition rate. Electron beam deposited ZrO2 films are known to be inhomogeneous. From the change of the peak transmittance value, it can be deduced that the inhomogeneity of ZrO2 films strengthened gradually with increasing deposition rate. The type of surface defects changed from nodules to craters when the deposition rate was high enough.