1000 resultados para UNDOPED SEMIINSULATING GAAS
Resumo:
Local vibrational modes(LVMs) in tenths of InP samples reveal clearly existence of complexes related to hydrogen. Complexes of vacancy at indium site with one to four hydrogen atom(s) and isolated hydrogen or hydrogen dimers and complexes of hydrogen with various impurities and intrinsic defects are investigated by FTIR. Especially hydrogen related complexes between various transition metals and hydrogen or hydrogen related complexes between hydrogen with point defects. New LVMs related to hydrogen will be reported in this paper. Dynamical formation mechanism of defects in the annealed nominally undoped semiinsulating InP obtained by high pressure, high temperature annealing of ultra purity materials is proposed. Hydrogen can acts as actuator for antistructure defects production. Structural, electronic and vibrational properties of LVMs related to hydrogen as well as their temperature effects are discussed.
Resumo:
Low noise field effect transistors and analogue switch integrated circuits (ICs) have been fabricated in semi-insulating gallium arsenide (SI-GaAs) wafers grown in space by direct ion-implantation. The electrical behaviors of the devices and the ICs have surpassed those fabricated in the terrestrially grown SI-GaAs wafers. The highest gain and the lowest noise of the transistors made from space-grown SI-GaAs wafers are 22.8 dB and 0.78 dB, respectively. The threshold back-gating voltage of the ICs made from space-grown SI-GaAs wafers is better than 8.5 V The con-elation between the characterizations of materials and devices is studied systematically. (C) 2002 COSPAR. Published by Elsevier Science Ltd. All rights reserved.
Resumo:
ZnTe doped with high concentrations of oxygen has been proposed in previous works as an intermediate band (IB) material for photovoltaic applications. The existence of extra optical transitions related to the presence of an IB has already been demonstrated in this material and it has been possible to measure the absorption coefficient of the transitions from the valence band (VB) to the IB. In this study, we present the first measurement of the absorption coefficient associated with transitions from the IB to the conduction band (CB) in ZnTeO. The samples used are 4-mum-thick ZnTe layers with or without O in a concentration ~10 19 cm -3, which have been grown on semiinsulating GaAs substrates by molecular beam epitaxy (MBE). The IB-CB absorption coefficient peaks for photon energies ~0.4 eV. It is extracted from reflectance and transmittance spectra measured using Fourier transform infrared (FTIR) spectroscopy. Under typical FTIR measurement conditions (low light intensity, broadband spectrum), the absorption coefficient in IB-to-CB transitions reaches 700 cm -1. This is much weaker than the one observed for VB-IB absorption. This result is consistent with the fact that the IB is expected to be nearly empty of electrons under equilibrium conditions in ZnTe(O).
Resumo:
We investigate the dependence of the differential reflection on the structure parameters of quantum dot (QD) heterostructures in pump-probe reflection measurements by both numerical simulations based on the finite-difference time-domain technique and theoretical calculations based on the theory of dielectric films. It is revealed that the value and sign of the differential reflection strongly depend on the thickness of the cap layer and the QD layer. In addition, a comparison between the carrier dynamics in undoped and p-doped InAs/GaAs QDs is carried out by pump-probe reflection measurements. The carrier capture time from the GaAs barrier into the InAs wetting layer and that from the InAs wetting layer into the InAs QDs are extracted by appropriately fitting differential reflection spectra. Moreover, the dependence of the carrier dynamics on the injected carrier density is identified. A detailed analysis of the carrier dynamics in the undoped and p-doped QDs based on the differential reflection spectra is presented, and its difference with that derived from the time-resolved photoluminescence is discussed. (C) 2008 American Institute of Physics.
Resumo:
We have fabricated 1.3-mu m InAs-GaAs quantum-dot (QD) lasers with and without p-type modulation doping and their characteristics have been investigated. We find that introducing p-type doping in active regions can improve the temperature stability of 1.3-mu m InAs-GaAs QD lasers, but it does not, increase the saturation modal gain of the QD lasers. The saturation modal gain obtained from the two types of lasers is identical (17.5 cm(-1)). Moreover, the characteristic temperature increases as cavity length increases for the two types of lasers, and it improves more significantly for the lasers with p-type doping due to their higher gain.
Resumo:
Photoreflectance (PR) has been used to study surface electronic properties (electric field, Fermi level pinning, and density of surface states) of undoped-n(+) (UN+) GaAs treated in the solution of ammonium sulfide in isopropanol. Complex Fourier transformation (CFT) of PR spectra from passivated surface shows that the sulfur overlay on GaAs surface makes no contribution to Franz-Keldysh oscillations (FKOs). The barrier height measured by PR is derived from surface states directly, rather than the total barrier height, which includes the potentials derived from Ga-S and As-S dipole layers. Comparing with native oxidated surface, the passivation leads to 80 meV movement of surface Fermi level towards the conduction band minimum, and reduction by more than one order in density of surface states. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
Self-assembled InAs quantum dots (QDs) have been fabricated by depositing 1.6, 1.8, 2.0 and 2.5 monolayer (ML) InAs on surfaces of the undoped-n(+) (UN+) type GaAs structure. Room temperature contactless electroreflectance (CER) was employed to study the built-in electric field and the surface Fermi level pinning of these QD-covered UN+ GaAs samples. The CER results show that 1.6 ML InAs QDs on GaAs do not modify the Fermi level, whereas for samples with more than 1.6 ML InAs coverage, the surface Fermi level is moved to the valence band maximum of GaAs by about 70 meV (which is independent of the InAs deposition thickness) compared to bare GaAs. It is concluded that the modification of InAs coverage on the Fermi level on the GaAs surface is due to the QDs, rather than to the wetting layer. (C) 2003 American Institute of Physics.
Resumo:
technique, on both semi-insulating and semi-conducting CraAs substrates with (100) orientation, offset by 2° towards (110) direction. Systematic variation of As/Ga was performed to gain an understanding of growth process, type of formation and other related physical properties. The films were characterized by using the variety of techniques, such as SEM, EDAX, HRTEM, XRD, and PL. Optical and electrical properties of undoped CyaAs epilayers are presented with reference to the growth conditions and AsH3/TMGa ratio. Photoluminescence measurements of GaAs epilayers were recorded at 4.2K and shows the emission of free exciton and confirmed their high purity. The dominant residual impurities in GaAs are presented by using PL. Finally, electrochemical depth profiling exhibited almost homogeneous background carrier distribution and excellent abruptness between the thin GaAs epilayer and substrate.
Resumo:
We report an experimental and theoretical study of maximum modal gain of p-doped 1.3 mu m InAs/GaAs quantum dot (QD) lasers. The maximum modal gain of the QD laser with five stacks of QDs is as high as 17.5 cm(-1) which is the same as that of the undoped laser with identical structures. The expression of the maximum modal gain is derived and it is indicated that p-doping has no effect to the maximum modal gain. We theoretically calculated the maximum modal gain of the QD lasers and the result is in a good agreement with the experimental data. Furthermore, QDs with lower height or smaller aspect ratio are beneficial to achieving a greater maximum modal gain that leads to lower threshold current density and higher differential modal gain, which is good for the application of p-doped 1.3 mu m InAs/GaAs QD lasers in optical communications systems.
Resumo:
Quantum-confined Stark effect and built-in dipole moment in self-assembled InAs/GaAs quantum dots (QDs), which are grown at relative low temperature (460degreesC) and embedded in GaAs p-i-n structure, have been studied by dc-biased electroreflectance. Franz-Keldysh oscillations from the undoped GaAs layer are used to determine the electric field under various bias voltages. Stark shift of -34 meV for the ground-state interband transition of the QDs is observed when the electric field increases from 105 to 308 kV/cm. The separation of the electron and hole states in the growth direction of 0.4 nm, corresponding to the built-in dipole moment of 6.4x10(-29) C m, is determined. It is found that the electron state lies above that of the hole, which is the same as that predicted by theoretical calculations for ideal pyramidal InAs QDs. (C) 2004 American Institute of Physics.
Resumo:
A series of 1-mu m-thick undoped In0.53Ga0.47As with different substrate growth temperature (T-g) or different beam flux pressure (BFP) of As were grown on lattice-matched semi-insulating InP (001) substrates by molecular beam epitaxy (MBE). Van der Pauw Hall measurements were carried out for these In0.53Ga0.47As samples. The residual electron concentration decreased with increasing temperature from 77 to 140 K, but increased with increasing temperature from 140 to 300 K. Rapid thermal annealing (RTA) can reduce the residual electron concentration. The residual electron mobility increased with increasing temperature from 77 to 300 K. All these electrical properties are associated with As antisite defects. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
We have investigated the photoluminescence mapping characteristics of semi-insulating (SI) InP wafers obtained by annealing in iron phosphide ambience (FeP2-annealed). Compared with as-grown Fe-doped and undoped SI InP wafers prepared by annealing in pure phosphorus vapour (P-annealed), the FeP2-annealed ST InP wafer has been found to exhibit a better photoluminescence uniformity. Radial Hall measurements also show that there is a better resistivity uniformity on the FeP2-annealed Sl InP wafer. When comparing the distribution of deep levels between the annealed wafers measured by optical transient Current spectroscopy, we find that the incorporation of iron atoms into the Sl InP Suppresses the formation of a few defects. The correlation observed in this study implies that annealing in iron phosphorus ambience makes Fe atoms diffuse uniformly and occupy the indium site in the Sl InP lattice. As it stands, we believe that annealing undoped conductive InP in iron phosphide vapour is an effective means to obtain semi-insulating InP wafers with superior uniformity.