949 resultados para Polymeric Materials
Resumo:
Stoichiometric Ba1-xSrxTiO3 (BST; x = 0.4) thin films were prepared by the polymeric precursor method. High quality polycrystalline films of BST with low roughness (approximate to 3 nm) were obtained from a Pt/Ti/SiO2/Si substrate deposited by spin-coating technique. Microstructure and morphological evaluation were done using grazing incident X-ray diffraction (GIXRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). Grazing incident angle XRD characterization of these films showed that BST phase crystallizes at 600 degrees C from an inorganic amorphous matrix. No intermediate crystalline phase was identified. A linear relationship between roughness and grain size was observed. (C) 2000 Elsevier B.V. B.V. All rights reserved.
Resumo:
The influence of niobia addition on the phase formation and dielectric properties of Pb(Zr0.45Ti0.55)O-3 powder prepared from polymeric precursor was analyzed. The weight fraction and unit-cell volume of the tetragonal phase decreased, and the mass fraction of the rhombohedral phase increased, with increasing niobia concentration. The rhombohedral unit-cell volume increased up to 5 mol% of added Nb and then decreased. Small amounts of pyrochlore and tetragonal zirconia phases were observed in PZT powder with more than 10 mol% Nb. These results were interpreted as an indication that the Nb ion was substituted for the zirconium ion in the tetragonal phase. For sintered PZT samples at 1100 degrees C, no free-zirconia phase was observed. The dielectric constant increased with the niobia addition up to 5 mol% and decreased for higher concentrations. The Curie temperature decreased with niobia addition up to 10 mol% before the formation of pyrochlore phase. (C) 2000 Elsevier B.V. Ltd. All rights reserved.
Resumo:
The 9.5/65/35 PLZT was prepared from the polymeric precursors (the Pechini and partial oxalate process) and by sintering in two stages in an oxygen atmosphere. After thermal treatment at 400 degreesC, the powders were calcinated and sintered at 1200 degreesC with slow heating and cooling rates. The second stage of sintering consisted of hot pressing at the same temperature in oxygen atmosphere. After calcination of PLZT powders obtained by both methods, as well as after sintering of PLZT obtained by Pechini process, the paraelectric cubic phase was formed. After sintering of PLZT obtained by partial oxalate procedure, small tetragonality of crystal structure was observed. After hot pressing PLZT was pseudocubic. SEM microstructural analyses were carried out of the sintering and hot pressed samples and indicated the small grain size less than 2 mum. (C) 2001 Elsevier B.V. B.V. All rights reserved.
Resumo:
Pure barium strontium titanate powder, with Ba/Sr ratio of 80/20 was prepared by the polymeric precursor method (also called Pechini process). The powder was obtained after a calcination at 800 degreesC for 8 h and characterized by XRD, IR, BET and SEM. The requirements to avoid barium carbonate as a secondary phase are presented and discussed in detail. (C) 2003 Elsevier B.V. All rights reserved.
Microwave synthesis of calcium bismuth niobate thin films obtained by the polymeric precursor method
Resumo:
The crystal structure, surface morphology and electrical properties of layered perovskite calcium bismuth niobate thin films (CaBi2Nb2O9-CBN) deposited on platinum coated silicon substrates by the polymeric precursor method have been investigated. The films were crystallized in a domestic microwave and in a conventional furnace. X-ray diffraction and atomic force microscopy analysis confirms that the crystallinity and morphology of the films are affected by the different annealing routes. Ferroelectric properties of the films were determined with remanent polarization P-r and a drive voltage V-c of 4.2 mu C/cm(2) and 1.7 V for the film annealed in the conventional furnace and 1.0 mu C/cm(2) and 4.0 V for the film annealed in microwave furnace, respectively. A slight decay after 10(8) polarization cycles was observed for the films annealed in the microwave furnace indicating a reduction of the domain wall mobility after interaction of the microwave energy with the bottom electrode. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Lithium tantalate (LiTaO3) thin films with 50:50 stoichiometry were deposited on silicon (100) substrates with two layers by the spin coating method using a polymeric organic solution. In order to study the influence of preannealing on the crystallinity, microstructure, grain size and roughness of the final film, two annealing procedures, slow preannealing and fast preannealing, were used. X-ray diffraction (XRD) results showed that LiTaO3 thin films are polycrystalline. It was observed by scanning electron microscopy (SEM) that the thin film, which had been thermally treated using slow preannealing, was characterized by a dense and homogeneous surface. The atomic force microscopy (AFM) studies showed that the roughness is strongly influenced by preannealing temperature. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
We report the successful deposition of CaBi2Nb2O9 (CBN) thin films on platinum coated silicon substrates by polymeric precursor method. The CBN thin films exhibited good structural, dielectric and CBN/Pt interface characteristics. The leakage current of the capacitor structure was around 0.15 A cm(-2) at an applied electric field of 30 kV cm(-1). The capacitance-voltage measurements indicated good ferroelectric polarization switching characteristics. The typical measured small signal dielectric constant and the dissipation factor at a frequency of 100 kHz were 90 and 0.053, respectively. The remanent polarization and the drive voltage values were 4.2 C cm(-2) and 1.7 V at an applied voltage of 10 V. No significant fatigue was observed at least up to 10(8) switching cycles. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Amorphous LiNbO3 thin films processed by polymeric precursor method exhibited efficient luminescence at room temperature. The films were deposited on silicon substrates and treated at 200degreesC for different times. The photoluminescence emission yield decreases with the increase of the treatment time and disappears for crystalline films. A theoretical-experimental study was performed on amorphous and crystalline materials to understand the influence of the defects on the photoluminescence properties. The theoretical band gap obtained by the difference of energy between the HOMO and LUMO levels is larger for crystalline structure when compared with amorphous material. This result, which is in agreement with experimental band gaps obtained from optical measurements, revealed the emergence of new electronic levels for the amorphous material, which are localized in the wide band gap of the crystalline structure. These new electronic levels may explain the photoluminescence observed at room temperature for LiNbO3 amorphous films.
Resumo:
Glass ionomer cements (GICs) are largely employed in Dentistry for several applications, such as luting cements for the attachment of crowns, bridges, and orthodontic brackets as well as restorative materials. The development of new glass systems is very important in Dentistry to improve of the mechanical properties and chemical stability. The aim of this study is the preparation of two glass systems containing niobium in their compositions for use as GICs. Glass systems based on the composition SiO2,Al2O3-Nb2O5-CaO were prepared by chemical route at 700degreesC. The XRD and DTA results confirmed that the prepared materials are glasses. The structures of the obtained glasses were compared to commercial material using FTIR, Al-27 and Si-29 MAS-NMR. The analysis of FTIR and MAS-NMR spectra indicated that the systems developed and commercial material are formed by SiO4 and AlO4 linked tetrahedra. These structures are essential to get the set time control and to have cements. These results encourage further applications of the experimental glasses in the formation of GICs. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
SnO2-based materials are used as sensors, catalysts and in electro-optical devices. This work aims to synthesize and characterize the SnO2/Sb2O3-based inorganic pigments, obtained by the polymeric precursor method, also known as Pechini method (based on the metallic citrate polymerization by means of ethylene glycol). The precursors were characterized by thermogravimetry (TG) and differential thermal analysis (DTA). After characterization, the precursors were heat-treated at different temperatures and characterized by X-ray diffraction. According to the TG/DTA curves basically two-step mass loss process was observed: the first one is related to the dehydration of the system; and the second one is representative to the combustion of the organic matter. Increase of the heat treatment temperature from 500 to 600 degrees C and 700 degrees C resulted higher crystallinity of the formed product.
Resumo:
This study includes Ca-PZT in the morphotropic phase boundary, MPB process combining the Pechini method, (ZT) and the Partial oxalate method (Ca-PZT) by obtaining single phase particles of ZT phase with a high specific surface area (similar to 110 m(2)/g at 550 degrees C) and narrow particle size distribution. Lead and calcium oxalates were precipitated onto the ZT particle surface and reacted to a solid state interface ZT/Ca-PZT/PbO-CaO. A deviation of a coexistence region from F-T- and F-R-phases to F-R-phase (Zr rich region) was observed. Strong surface area reduction occurs by Ca-PZT crystallization at about 700 degreesC, and demonstrated high sinterability (2.40 m(2)/g - 350 nm) with apparent densities near to 99.9%. Different processing methods did not demonstrate superior results. Studies of calcined powder shows a high sinterability of powder calcined 3 h at 700 degrees C and sintered 3 h at 1000 degreesC coming up to 99.8% of relative density. (C) 2001 Kluwer Academic Publishers.
Resumo:
High-quality (Pb, La)TiO3 ferroelectric thin films were successfully prepared on a Pt(111)/Ti/SiO2/Si(100) substrate for the first time by spin coating, using the polymeric precursor method. The X-ray diffraction patterns show that the films are polycrystalline in nature. This method allows for low temperature (500 degrees C) synthesis, a high quality microstructure and superior dielectric properties. The effects on the microstructure and electrical properties were studied by changing the La content. The films annealed at 500 degreesC have a single perovskite phase with only a tetragonal or pseudocubic structure. As the La content is increased, the dielectric constant of PLT thin films increases from 570 up to 1138 at room temperature. The C-V and P-E characteristics of perovskite thin films prepared at a low temperature show normal ferroelectric behavior, representing the ferroelectric switching property. The remanent polarization and coercive field of the films deposited decreased due to the transformation from the ferroelectric to the paraelectric phase with an increased La content. (C) 2001 Kluwer Academic Publishers.
Resumo:
Pure and Nb doped PbZr0.4Ti0.603 thin films was prepared by the polymeric precursor method and deposited by spin coating on Pt/Ti/SiO2/Si (100) substrates and annealed at 700 degreesC. The films are oriented in (1 1 0) and (1 0 0) direction. The electric properties of PZT thin films show strong dependence of the crystallographic orientation. The P-E hysteresis loops for the thin film with composition PbZr0.39Ti0.6Nb0.103 showed good saturation, with values for coercive field (E-c) equal to 60 KV cm(-1) and for remanent polarization (P-r) equal to 20 muC cm(-2). The measured dielectric constant (epsilon) is 1084 for this film. These results show good potential for application in FERAM. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
The (1 1 7) and (0 0 1 0)-oriented Bi4Ti3O12 thin films were fabricated on Pt/Ti/SiO2/Si substrates by using a polymeric precursor solution under appropriate crystallization conditions. Atomic force microscopy and scanning electron microscopy showed relatively large grains, which is typical for this system. The capacitance dependence on voltage is strongly non-linear, confirming the ferroelectric properties of the films resulting from the domain switching. The (1 1 7)-oriented films exhibited a higher remanent polarization (23.7 μ C cm(-2)) than the (0 0 1 0)-oriented films (11.8 μ C cm(-2)). Fatigue tests revealed that the temperature of thermal treatment and degree of orientation affect the performance of the device. © 2005 Elsevier B.V. All rights reserved.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)