Pure barium strontium titanate powder, with Ba/Sr ratio of 80/20 was prepared by the polymeric precursor method (also called Pechini process). The powder was obtained after a calcination at 800 degreesC for 8 h and characterized by XRD, IR, BET and SEM. The requirements to avoid barium carbonate as a secondary phase are presented and discussed in detail. (C) 2003 Elsevier B.V. All rights reserved. |
| Formato |
217-221 |
| Identificador |
http://dx.doi.org/10.1016/S1044-5803(03)00095-0 Materials Characterization. New York: Elsevier B.V., v. 50, n. 2-3, p. 217-221, 2003. 1044-5803 http://hdl.handle.net/11449/37139 10.1016/S1044-5803(03)00095-0 WOS:000186249900021 |
| Idioma(s) |
eng |
| Publicador |
Elsevier B.V. |
| Relação |
Materials Characterization |
| Direitos |
closedAccess |
| Palavras-Chave | #BST #polymeric precursor #Pechini #microstructure #BET |
| Tipo |
info:eu-repo/semantics/article |