22 resultados para Intercritical annealing


Relevância:

60.00% 60.00%

Publicador:

Resumo:

Austenitization with lower temperature and intercritical annealing were introduced in the treatment of a maraging steel with a composition of Fe–12.94Ni–1.61Al–1.01Mo–0.23Nb (wt.%). Scanning electron microscopy was employed to study the microstructure after austenitization at 950 °C and intercritical annealing, followed by aging at 485 and 600 °C. X-ray diffraction (XRD) analysis was applied to evaluate the formation of retained or reverted austenite. Thermodynamic calculation was employed to calculate equilibrium phase mole fractions. Hardness and Charpy impact toughness of the steel were measured. Intercritical annealing treatments did not result in significant increase of hardness either before or after aging. The Charpy impact toughness of the alloy in aged condition was enhanced after austenitization at 950 °C. No austenite was observed in XRD. However, suspected reverted austenite was found after austenitization at 950 °C followed by aging at 600 °C for 4 h. Relationships among heat treatment, microstructure and mechanical properties are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly--lactide (PLLA) is one of the most significant members of a group of polymers regarded as bioabsorbable. Degradation of PLLA proceeds through hydrolysis of the ester bonds in the polymer chains and is influenced significantly by the polymer's molecular weight and crystallinity. To evaluate the effects of processing and sterilisation on these properties, PLLA pellets were either compression moulded or extruded, subjected to annealing at 120°C for 4 h and sterilised by ethylene oxide (EtO) gas. Procedures were used to evaluate the mechanical properties, molecular weight and crystallinity. Upon processing, the crystallinity of the material fell from 61% for the PLLA pellets to 12% and 20% for the compressed and extruded components, respectively. After annealing, crystallinity increased to 43% for the compression-moulded material and 40% for the extruded material. Crystallinity further increased upon EtO sterilisation. A slight decrease in molecular weight was observed for the extruded material through processing, annealing and sterilisation. Young's modulus generally increased with increasing crystallinity, and extension at break and tensile strength decreased. The results from this investigation suggest that PLLA is sensitive to processing and sterilisation, altering properties critical to its degradation rate.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Future read heads in hard disc storage require high conformal coatings of metal magnetic layers over high aspect ratio profiles. This paper describes pioneering work on the use of MOCVD for the deposition of cobalt layers. While pure cobalt layers could be deposited at 400C their magnetic properties are poor. It was found that the magnetic properties of the layers could be significantly enhanced with an optimised rapid thermal anneal. This work was sponsored by Seagate Technology and led to a follow up PhD studentship on the co-deposition of cobalt and iron by MOCVD.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sputtered silicon is investigated as a bonding layer for transfer of pre-processed silicon layers to various insulating substrates. Although the material appears suitable for low temperature processing, previous work has shown that gas trapped in the pores of the sputtered material is released at temperatures above 350 degrees C and further increases of temperature lead to destruction of any bonded interface. Pre-annealing at 1000 degrees C before bonding drives out gas and/or seals the surface, but for device applications where processing temperatures must be kept below about 300 degrees C, this technique cannot be used. In the current work, we have investigated the effect of excimer laser-annealing to heat the sputtered silicon surface to high temperature whilst minimising heating of the underlying substrate. Temperature profile simulations are presented and the results of RBS, TEM and AFM used to characterise the annealed layers. The results verify that gases are present in the sub-surface layers and suggest that while sealing of the surface is important for suppression of the out-diffusion of gases, immediate surface gas removal may also play a role. The laser-annealing technique appears to be an effective method of treating sputtered silicon, yielding a low roughness surface suitable for wafer bonding, thermal splitting and layer transfer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The university course timetabling problem involves assigning a given number of events into a limited number of timeslots and rooms under a given set of constraints; the objective is to satisfy the hard constraints (essential requirements) and minimize the violation of soft constraints (desirable requirements). In this study we employed a Dual-sequence Simulated Annealing (DSA) algorithm as an improvement algorithm. The Round Robin (RR) algorithm is used to control the selection of neighbourhood structures within DSA. The performance of our approach is tested over eleven benchmark datasets. Experimental results show that our approach is able to generate competitive results when compared with other state-of-the-art techniques.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The phase structure evolution of high impact polypropylene copolymer (IPC) during molten-state annealing and its influence on crystallization behaviour were studied. An entirely different architecture of the IPC melt was observed after being annealed, and this architecture resulted in variations of the crystallization behaviour. In addition, it was found that the core-shell structure of the dispersed phase was completely destroyed and the sizes of the dispersed domains increased sharply after being annealed at 200 degrees C for 200 min. Through examination of the coarseness of the phase morphology using phase contrast microscopy (PCM), it was found that a co-continuous structure and an abnormal 'sea-island' structure generally appeared with an increase in annealing time. The original matrix PP component appeared as a dispersed phase, whereas the copolymer components formed a continuous 'sea-island' structure. This change is ascribed to the large tension induced by solidification at the phase interface and the great content difference between the components. When the temperature was reduced the structure reverted to its original form. With increasing annealing time, the spherulite profiles became more defined and the spherulite birefringence changed from vague to clear. Overall crystallization rates and nucleation densities decreased, but the spherulite radial growth rates remained almost constant, indicating that molten-state annealing mainly affects the nucleation ability of IPC, due to a coarsened microstructure and decreased interface area. (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The results of a study of the variation in photocatalytic activity of TiO2, as measured by its ability to photomineralise 4-chlorophenol, as a function of temperature used to anneal the TiO2, are reported. Heat treatment of the TiO2 leads to a marked decrease in its photocatalytic activity at annealing temperatures above 600-degrees-C. This decrease is associated with a concomitant drop in the specific surface area of the TiO2, owing to particle sintering, rather than the anatase to rutile transformation, which occurs largely at temperatures above 700-degrees-C. There is a reasonable correlation between photocatalytic activity and the surface area of the aggregate particles in the dispersions of the different heat-treated TiO2 samples.