The mineral arsentsumebite Pb2Cu(AsO4)(SO4)(OH), a copper arsenate-sulfate hydroxide of the brackebuschite group has been characterised by Raman spectroscopy. The brackebuschite mineral group are a series of monoclinic arsenates, phosphates and vanadates of the general formula A2B(XO4)(OH,H2O), where A may be Ba, Ca, Pb, Sr, while B may be Al, Cu2+,Fe2+, Fe3+, Mn2+, Mn3+, Zn and XO4 may be AsO4, PO4, SO4,VO4. Bands are assigned to the stretching and bending modes of SO42- AsO43- and HOAsO3 units. Raman spectroscopy readily distinguishes between the two minerals arsentsumebite and tsumebite. Raman bands attributed to arsenate are not observed in the Raman spectrum of tsumebite. Phosphate bands found in the Raman spectrum of tsumebite are not found in the Raman spectrum of arsentsumebite. Raman spectroscopy readily distinguishes the two minerals tsumebite and arsentsumebite.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Some minerals are formed which show poorly defined X-ray diffraction patterns. Vibrational spectroscopy offers one of the few methods for the assessment of the structure of the oxyanions in such minerals. Among this group of minerals is mallestigite with formula Pb3Sb5+(SO4)(AsO4)(OH)6•3H2O. The objective of this research is to determine the molecular structure of the mineral mallestigite using vibrational spectroscopy. Raman and infrared bands are attributed to the AsO43- , SO42- and water stretching vibrations. Mallestigite is a mineral formed in ancient waste dumps such as occurs at Mallestiger, Carinthia, Austria and as such is a mineral of archaeological significance.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In order to mimic the chemical reactions in cave systems, the analogue of the mineral stercorite H(NH4)Na(PO4)•4H2O has been synthesised. X-ray diffraction of the stercorite analogue matches the stercorite reference pattern. A comparison is made with the vibrational spectra of synthetic stercorite analogue and the natural Cave mineral. The mineral in nature is formed by the reaction of bat guano chemicals on calcite substrates. A single Raman band at 920 cm-1 (Cave) and 922 cm-1 (synthesised) defines the presence of hydrogen phosphate in the mineral. In the synthetic stercorite analogue, additional bands are observed and are attributed to the dihydrogen and phosphate anions. The vibrational spectra of synthetic stercorite only partly match that of the natural stercorite. It is suggested that natural stercorite is more pure than that of synthesised stercorite. Antisymmetric stretching bands are observed in the infrared spectrum at 1052, 1097, 1135 and 1173 cm-1. Raman spectroscopy shows the stercorite mineral is based upon the hydrogen phosphate anion and not the phosphate anion. Raman and infrared bands are found and assigned to PO43-, H2O, OH and NH stretching vibrations. Raman spectroscopy shows the synthetic analogue is similar to the natural mineral. A mechanism for the formation of stercorite is provided.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fibre composite structures have become the most attractive candidate for civil engineering applications. Fibre reinforced plastic polymer (FRP) composite materials have been used in the rehabilitation and replacement of the old degrading traditional structures or build new structures. However, the lack of design standards for civil infrastructure limits their structural applications. The majority of the existing applications have been designed based on the research and guidelines provided by the fibre composite manufacturers or based on the designer’s experience. It has been a tendency that the final structure is generally over-designed. This paper provides a review on the available studies related to the design optimization of fibre composite structures used in civil engineering such as; plate, beam, box beam, sandwich panel, bridge girder, and bridge deck. Various optimization methods are presented and compared. In addition, the importance of using the appropriate optimization technique is discussed. An improved methodology, which considering experimental testing, numerical modelling, and design constrains, is proposed in the paper for design optimization of composite structures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of this research is to determine the molecular structure of the mineral hidalgoite PbAl3(AsO4)(SO4)(OH)6 using vibrational spectroscopy. The mineral is found in old mine sites. Observed bands are assigned to the stretching and bending vibrations of (SO4)2- and (AsO4)3- units, stretching and bending vibrations of hydrogen bonded (OH)- ions and Al3+-(O,OH) units. The approximate range of O-H...O hydrogen bond lengths is inferred from the Raman and infrared spectra. Values of 2.6989 Å, 2.7682 Å, 2.8659 Å were obtained. The formation of hidalgoite may offer a mechanism for the removal of arsenic from the environment.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Some minerals are colloidal and show no X-ray diffraction patterns. Vibrational spectroscopy offers one of the few methods for the assessment of the structure of these types of mineral. Among this group of minerals is pitticite simply described as Fe, AsO4, SO4, H2O. The objective of this research is to determine the molecular structure of the mineral pitticite using vibrational spectroscopy. Raman microscopy offers a useful method for the analysis of such colloidal minerals. Raman and infrared bands are attributed to the , and water stretching vibrations. The Raman spectrum is dominated by a very intense sharp band at 983 cm−1 assigned to the symmetric stretching mode. A strong Raman band at 1041 cm−1 is observed and is assigned to the antisymmetric stretching mode. Low intensity Raman bands at 757 and 808 cm−1 may be assigned to the antisymmetric and symmetric stretching modes. Raman bands observed at 432 and 465 cm−1 are attributable to the doubly degenerate ν2(SO4)2- bending mode.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The emissions to water from a 1.9 kW two-stroke outboard engine were investigated in the laboratory and in the field, with the primary objective being to characterise and quantify the pollutants that remain within the water column. The emission rates of polycyclic aromatic hydrocarbons (PAHs) and volatile organic compounds (VOCs) were determined for the engine when using a mineral and an equivalent environmentally adapted lubricant (EAL). A comparison of the emission rates was conducted between the results from the fresh and sea water tests. The results showed that there was little difference in the emission rates of these pollutants when either of the lubricants was used in both the fresh and sea water. A further set of tests were done to find out the effect on pH of water due to the underwater emissions and these tests were done using both mineral and environmentally adapted lubricant. The results showed that the type of lubricant does not have any effect on the change in pH of the water.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structures of two hydrated proton-transfer compounds of 4-piperidinecarboxamide (isonipecotamide) with the isomeric heteroaromatic carboxylic acids indole-2-carboxylic acid and indole-3-carboxylic acid, namely 4-carbamoylpiperidinium indole-2-carboxylate dihydrate (1) and 4-carbamoylpiperidinium indole-3-carboxylate hemihydrate (2) have been determined at 200 K. Crystals of both 1 and 2 are monoclinic, space groups P21/c and P2/c respectively with Z = 4 in cells having dimensions a = 10.6811(4), b = 12.2017(4), c = 12.5456(5) Å, β = 96.000(4)o (1) and a = 15.5140(4), b = 10.2908(3), c = 9.7047(3) Å, β = 97.060(3)o (2). Hydrogen-bonding in 1 involves a primary cyclic interaction involving complementary cation amide N-H…O(carboxyl) anion and anion hetero N-H…O(amide) cation hydrogen bonds [graph set R22(9)]. Secondary associations involving also the water molecules of solvation give a two-dimensional network structure which includes weak water O-H…π interactions. In the three-dimensional hydrogen-bonded structure of 2, there are classic centrosymmetric cyclic head-to-head hydrogen-bonded amide-amide interactions [graph set R22(8)] as well as lateral cyclic amide-O linked amide-amide extensions [graph set R24(8)]. The anions and the water molecule, which lies on a twofold rotation axis, are involved in secondary extensions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The mineral schlossmacherite (H3O,Ca)Al3(AsO4,PO4,SO4)2(OH)6 , a multi-cation-multi-anion mineral of the beudantite mineral subgroup has been characterised by Raman spectroscopy. The mineral and related minerals functions as a heavy metal collector and is often amorphous or poorly crystalline, such that XRD identification is difficult. The Raman spectra are dominated by an intense band at 864 cm-1, assigned to the symmetric stretching mode of the AsO43- anion. Raman bands at 809 and 819 cm-1 are assigned to the antisymmetric stretching mode of AsO43- . The sulphate anion is characterised by bands at 1000 cm-1 (ν1), and at 1031, 1082 and 1139 cm-1 (ν3). Two sets of bands in the OH stretching region are observed: firstly between 2800 and 3000 cm-1 with bands observed at 2850, 2868, 2918 cm-1 and secondly between 3300 and 3600 with bands observed at 3363, 3382, 3410, 3449 and 3537 cm-1. These bands enabled the calculation of hydrogen bond distances and show a wide range of H-bond distances.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Shattuckite Cu5(SiO3)4(OH)2 is a copper hydroxy silicate and is commonly known as a ‘healing’ mineral. Three shattuckite mineral samples from three different origins were analysed by Raman spectroscopy. Some Raman bands are common in the spectra of the minerals. Raman bands at around 890, 1058 and 1102 are described as the ν3 –SiO3 antisymmetric stretching vibrations. The Raman band at 670 cm-1 is assigned to the ν4 bending modes of the -SiO3 units and the band at around 785 cm-1is due to Si-O-Si chain stretching mode. Raman (and infrared) spectroscopy proves that water is in the molecular structure of shattuckite; thus the formula is better written as Cu5(SiO3)4(OH)2•xH2O.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Innovation processes are rarely smooth and disruptions often occur at transition points were one knowledge domain passes the technology on to another domain. At these transition points communication is a key component in assisting the smooth hand over of technologies. However for smooth transitions to occur we argue that appropriate structures have to be in place and boundary spanning activities need to be facilitated. This paper presents three case studies of innovation processes and the findings support the view that structures and boundary spanning are essential for smooth transitions. We have explained the need to pass primary responsibility between agents to successfully bring an innovation to market. We have also shown the need to combine knowledge through effective communication so that absorptive capacity is built in process throughout the organisation rather than in one or two key individuals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Kinoite Ca2Cu2Si3O10(OH)4 is a mineral named after a Jesuit missionary. Raman and infrared spectroscopy have been used to characterise the structure of the mineral. The Raman spectrum is characterised by an intense sharp band at 847 cm-1 assigned to the ν1 (A1g) symmetric stretching vibration. Intense sharp bands at 951, 994 and 1000 cm-1 are assigned to the ν3 (Eu, A2u, B1g) SiO4 antisymmetric stretching vibrations. Multiple ν2 SiO4 vibrational modes indicate strong distortion of the SiO4 tetrahedra. Multiple CaO and CuO stretching bands are observed. Raman spectroscopy confirmed by infrared spectroscopy clearly shows that hydroxyl units are involved in the kinoite structure. Based upon the infrared spectra, it is proposed that water is also involved in the kinoite structure. Based upon vibrational spectroscopy, the formula of kinoite is defined as Ca2Cu2Si3O10(OH)4•xH2O.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: In vitro investigations have demonstrated the importance of the ribcage in stabilising the thoracic spine. Surgical alterations of the ribcage may change load-sharing patterns in the thoracic spine. Computer models are used in this study to explore the effect of surgical disruption of the rib-vertebrae connections on ligament load-sharing in the thoracic spine. Methods: A finite element model of a T7-8 motion segment, including the T8 rib, was developed using CT-derived spinal anatomy for the Visible Woman. Both the intact motion segment and the motion segment with four successive stages of destabilization (discectomy and removal of right costovertebral joint, right costotransverse joint and left costovertebral joint) were analysed for a 2000Nmm moment in flexion/extension, lateral bending and axial rotation. Joint rotational moments were compared with existing in vitro data and a detailed investigation of the load sharing between the posterior ligaments carried out. Findings: The simulated motion segment demonstrated acceptable agreement with in vitro data at all stages of destabilization. Under lateral bending and axial rotation, the costovertebral joints were of critical importance in resisting applied moments. In comparison to the intact joint, anterior destabilization increases the total moment contributed by the posterior ligaments. Interpretation: Surgical removal of the costovertebral joints may lead to excessive rotational motion in a spinal joint, increasing the risk of overload and damage to the remaining ligaments. The findings of this study are particularly relevant for surgical procedures involving rib head resection, such as some techniques for scoliosis deformity correction.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thermogravimetry combined with evolved gas mass spectrometry has been used to characterise the mineral ardealite and to ascertain the thermal stability of this ‘cave’ mineral. The mineral ardealite Ca2(HPO4)(SO4)•4H2O is formed through the reaction of calcite with bat guano. The mineral shows disorder and the composition varies depending on the origin of the mineral. Thermal analysis shows that the mineral starts to decompose over the temperature range 100 to 150°C with some loss of water. The critical temperature for water loss is around 215°C and above this temperature the mineral structure is altered. It is concluded that the mineral starts to decompose at 125°C, with all waters of hydration being lost after 226°C. Some loss of sulphate occurs over a broad temperature range centred upon 565°C. The final decomposition temperature is 823°C with loss of the sulphate and phosphate anions.