The variation in the electrical resistivity of the chalcogenide glasses Ge15Te85-x has been studied as a function of high pressure for pressures up to 8.5GPa. All the samples studied undergo a semi-conductor to metallic transition in a continuous manner at pressures between 1.5-2.5GPa. The transition pressure at which the samples turn metallic increases with increase in percentage of Indium. This increase is a direct consequence of the increase in network rigidity with the addition of Indium. At a constant pressure of 0.5GPa, the normalized resistivity shows some signature of the existence of the intermediate phase. Samples recovered after a pressure cycle remain amorphous suggesting that the semi-conductor to metallic transition arises from a reduction of the band gap due to pressure or the movement of the Fermi level into the conduction or valence band.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The electrical resistivity of bulk semiconducting amorphous TlxSe100-x alloys with 0 ≤ x ≤ 25 has been investigated up to a pressure of 14 GPa and down to liquidnitrogen temperature by use of a Bridgman anvil device. All the glasses undergo a discontinuous pressure-induced semiconducting-to-metal transition. X-ray diffraction studies on the pressure-recovered samples show that the high-pressure phase is the crystalline phase. The pressure-induced crystalline products are identified to be a mixture of Se having a hexagonal structure with a = 4·37 Aring and c = 4·95 Aring and TlSe having a tetragonal structure with a = 8·0 Aring and c = 7·0 Aring

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Electrical resistivity of bulk amorphous Al23T77 samples has been studied as a function of pressure (up to 80 kbar) and temperature (down to 77 K). At atmospheric pressure the temperature dependence of resistivity obeys the relation = π0 exp(δE/RT) with two activation energies. In the temperature range 300 K T > 234 K the activation energy is 0.58 eV and for 234 >T 185 K the value is δE = 0.30 ev. The activation energy has been measured as a function of pressure. The electrical resistivity decreases exponentially with the increase of pressure and at 70 kbar pressure the electrical behaviour of the sample shows a metallic nature with a positive temperature coefficient. The high pressure phase of the sample is found to be a crystalline hexagonal phase.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

High pressure studies of 35Cl NQR in the hexachlorocyclophosphazene N3P3Cl6 and in the K- and T-forms of octachlorocyclophospha.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Auto-ignition temperature of polystyrene, poly(vinyl chloride) and carboxy terminated polybutadiene has been measured at various oxygen pressures (1-28 atm) in a high pressure differential thermal analysis assembly at a heating rate of 10°C/min. The exothermic peak appears between 250-350°C in polystyrene and poly(vinyl chloride) and between 150-200°C for carboxy terminated polybutadiene. Ignition appears to be controlled by in situ forma tion and degradation of polymeric peroxides. Inverse dependence of ignition temperature on oxygen pressure is explained by the rate equation which con siders that ignition of a particular sample, of a fixed geometry, occurs when gasification rate reaches a unique critical value.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The pressure and temperature dependence of the electrical resistivity of bulk glassy Ge20Te80 is reported. The effect of annealing is also studied. The glass undergoes a polymorphous or congruent crystallization under high pressures. The high pressure phase is found to have fcc structure with Image . Under thermal treatment the glass undergoes the double stage crystallization. The sample annealed at the first crystallization temperature shows a pressure induced semiconductor-to-metal transition at 4.0 GPa pressure and the crystalline Ge20Te80 samples show the transition at 7 GPa pressure.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The resistivity of selenium-doped n-InP single crystal layers grown by liquid-phase epitaxy with electron concentrations varying from 6.7 x 10$^18$ to 1.8 x 10$^20$ cm$^{-3}$ has been measured as a function of hydrostatic pressure up to 10 GPa. Semiconductor-metal transitions were observed in each case with a change in resistivity by two to three orders of magnitude. The transition pressure p$_c$ decreased monotonically from 7.24 to 5.90 GPa with increasing doping concentration n according to the relation $p_c = p_o [1 - k(n/n_m)^a]$, where n$_m$ is the concentration (per cubic centimetre) of phosphorus donor sites in InP atoms, p$_o$ is the transition pressure at low doping concentrations, k is a constant and $\alpha$ is an exponent found experimentally to be 0.637. The decrease in p$_c$ is considered to be due to increasing internal stress developed at high concentrations of ionized donors. The high-pressure metallic phase had a resistivity (2.02-6.47) x 10$^{-7}$ $\Omega$ cm, with a positive temperature coefficient dependent on doping.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The pressure dependence of the electrical of the electrical resistivity of bulk GeSe2 glass shows a semiconductor-to-metal transition at 7 GPa pressure. The high pressure phase is examined using he x-ray diffractometer and is found to be crystalline, with a face-centered cubic structure having a =4.06A. The electrical conductivity has also been studied as a function of temperature at various pressures.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The effect of pressure on the electrical resistivity of bulk Si20Te80 glass has been studied up to a pressure of 8 GPa. A discontinuous transition occurs at a pressure of 7 GPa. The X-ray diffraction studies on the pressure quenched sample show that the high pressure phase is crystalline with hexagonal structure (c/a = 1.5). On heating, the high pressure hexagonal phase has on exothermic decomposition atT = 586 K into two crystalline phases, which are the stable phases tellurium and SiTe2 obtained by simple heating of the glass.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The electrical resistivity of layerd crystalline GeSe has been investigated up to a pressure of 100 kbar and down to liquid-nitrogen temperature by use of a Bridgman anvil device. A pressure-induced first-order phase transition has been observed in single-crystal GeSe near 6 GPa. The high-pressure phase is found to be quenchable and an x-ray diffraction study of the quenched material reveals that it has the face-centered-cubic structure. Resistivity measurements as a function of pressure and temperature suggest that the high-pressure phase is metallic.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

An irreversible pressure induced semiconductor-to-metal transition in bulk Ge20Te80 glass is observed at about 5 GPa pressure. The high pressure phase has a face centered cubic structure with a lattice constant 6.42 A° as deduced by X-ray diffraction studies on the pressure quenched samples. The temperature and pressure dependence of the electrical resistivity confirms the observed transition to be a semiconductor-to-metal transition. The temperature dependence of thermo electric power is also reported.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Eclogites and their retrogressed equivalents from the eastern unit of the Glenelg-Attadale Inlier in NW Scotland preserve much microstructural evidence that indicates that very high-pressure/temperature eclogite facies conditions were reached, and followed by decompression and hydration during exhumation. Rutile exsolution in garnet and quartz exsolution in omphacite and titanite formed through mineral reactions during high P-T peak metamorphism. Isochemical phase diagrams modeled for samples from three different locations indicate that the outer part of the eastern unit preserves a peak metamorphic condition of c. 850-1000 degrees C at 18-25 kbar, whereas the central part has a similar pressure (c. 23 kbar), but a lower temperature (c. 670 degrees C). Due to the limitations in the phase diagram calculations the estimated P-T conditions represent the minimum conditions attained by the peak metamorphic assemblage, and the pre-exsoived peak assemblage probably stabilized at a higher pressure. This observation is strongly supported by the presence of exsolution microstructures. The present results demonstrate that the eastern unit experienced very high P-T conditions during peak metamorphism and a tight clockwise P-T trajectory and provide the first indication of possible ultrahigh-pressure metamorphism in the Glenelg eclogites. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Effect of disorder on the electrical resistance near the superconducting transition temperature in the paracoherence region of high temperature YBa2CU3O7-delta (YBCO) thin film superconductor is reported. For this, c-axis oriented YBa2Cu3O7-delta thin films having superconducting transition width varying between 0.27 K and 6 K were deposited using laser ablation and high pressure oxygen sputtering techniques. Disorder in these films was further created by using 100 MeV oxygen and 200 MeV silver ions with varying fluences. It is observed that the critical exponent in the paracoherence region for films with high transition temperature and small transition width is in agreement with the theoretically predicted value (gamma = 1.33) and is not affected by disorder, while for films with lower transition temperature and larger transition width the value of exponent is much larger as compared to that theoretically predicted and it varies from sample to sample and usually changes with disorder induced by radiation. This difference in the behaviour of the exponent has been explained on the basis of differences in the strength of weak links and the transition between temperatures T. and T, is interpreted as a percolation like transition with disorder. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Details of a simple and convenient high-pressure cell for continuous-wave, wide-line nuclear magnetic resonance investigation at high pressures and low temperatures are described. Experimental results obtained with the cell at 14*108 Pa and 77K for ammonium iodide are presented briefly.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

High pressure electrical resistivity measurements were carried out on GexSe100-x (0 less-than-or-equal-to x less-than-or-equal-to 40) glasses at ambient and low temperatures using the Bridgman anvil system. All the melt quenched glasses show a discontinuous glassy semiconductor to crystalline metal transition at high pressures. The high pressure phases of Ge-Se samples do not correspond to any of the equilibrium phases of the system. Additionally, the variation of transition pressure (P(T)), ambient resistivity (rho0) and the activation energy (DELTAE(t)) with composition, exhibit a change in behaviour at x = 20 and 33. The unusual variations observed in these glasses are discussed in the light of chemical and percolation thresholds occurring in the glassy system.