The effect of pressure on the electrical resistivity of amorphous n-type (GeSe3.5)100�xBix been studied in a Bridgeman anvil system up to a pressure of 90 kbar down to liquid nitrogen temperature. A continuous amorphous semiconductor to metal-like solid transition in the undoped GeSe3.5 is observed at room temperature. Incorporation of Bi in the GeSe3.5 network is found to significantly disturb the behaviour of the resistivity with pressure. With increasing Bi concentration a much broader variation in resistivity with pressure is observed. The temperature dependence of the resistivity and activation energy at different pressures is also measured and they are found to be composition dependent. Results are discussed in the light of the Phillips Model of ordered clusters in chalcogenide semiconductors.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Electrical properties of deep defects induced in n-silicon by -particles of about 10 MeV energy at a dose of 1014 and 1015 cm-2 are studied by DLTS. The levels at Ec -0.18 eV, Ec -0.26 eV, and Ec -0.48 eV are identified as A center, V2 (=/-) and V2 (-/0) on the basis of activation energy, electron capture cross section, and annealing behavior. Two other irradiation related levels at Ec -0.28 eV and Ec -0.51 eV could not be related to any known center.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The polymerization of methyl methacrylate initiated by a mixed ligand complex. [NN-ethylenebis(salicylideneiminato)](benzoylacetonato)cobalt(III) has been studied in bulk and in benzene at 70° and 80°. The rate of polymerization is proportional to (concentration of the chelate)Image and the monomer exponent is close to 1.5. The activation energy and the kinetic and transfer constants are evaluated. A free radical mechanism has been proposed.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

A correlation has been established between the heat of depolymerization (DeltaH) of vinyl polymers for going from solid polymer state to gaseous monomer state and the activation energy (E) of degradation. On this basis it has been shown that the rate controlling step in the degradation lies in the initiation step. Attempt has been made to correlate theE and DeltaH with glass transition temperature (Tg) and melting temperature (Tm) of the polymers.[/ p]

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The behavior of cupric dipivaloylmethide in vinyl polymerization systems was investigated with a view to understanding the mechanism of polymerization initiation. Results of polymerization reactions together with spectral investigation data are presented. Polymerization in the presence of the chelate proceeds through a free-radical process. The corresponding kinetic and transfer constants and activation energy values suggest a normal propagation step. With the help of spectral data an attempt is made to suggest a plausible mechanism of initiation.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The thermal degradation of polystyrene peroxide was carried out using differential scanning calorimetry. The activation energy (E) was found to be 136 kJ mole–1 at all extents of decomposition. TheE value was found to correspond to-O-O-dissociation. The order of reaction was found to decrease from 2 to 1 as the decomposition progresse.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Thermal polymerization of acrylamide has been followed by the DSC technique, and the activation energy (E) values at different stages of the fraction polymerized (a) have been determined from the exotherm of the thermograms obtained. The trend of variation of E with agr shows that E remains constant up to agr = 0.5 and decreases with a further increase in agr. A close look at the composite nature of the exotherms, agr-t, and agr-T curves shows that the polymerization of acrylamide involves two processes. The first process is the formation of linear polyacrylamide and the second is the simultaneous cross-linking of the linear chains together with the formation of linear polyacrylamide. Experiments such as NH3 detection by differential thermal analysis techniques and annealing studies have been made to shed further light on the polymerization process.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Thermal decomposition of ethyl and isopropyl amine perchlorates has been studied by methods such as DTA, TG, isothermal weight loss measurements and the decomposition products have been analyzed in a mass spectrometer. Activation energy values for thermal decomposition have been calculated fromagr-t plots. The proton transfer dissociation mechanism proposed for the thermal decomposition of ammonium perchlorate (AP) has been extended to explain the decomposition products of these twosubstituted amine perchlorates.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

A mono-oxygenase catalysing the conversion of 2-ethyl-4-thioisonicotinamide (ethionamide) into its sulphoxide was purified from guinea-pig liver homogenates. The enzyme required stoicheiometric amounts of oxygen and NADPH for the sulphoxidation reaction. The purified protein is homogeneous by electrophoretic, antigenic and chromatographic criteria. The enzyme has mol.wt. 85000 and it contains 1g-atom of iron and 1mol of FAD per mol, but not cytochrome P-450. The enzyme shows maximal activity at pH7.4 in a number of different buffer systems and the Km values calculated for the substrate and NADPH are 6.5×10-5m and 2.8×10-5m respectively. The activation energy of the reaction was calculated to be 36kJ/mol. Under optimal conditions, the molecular activity of the enzyme (mol of substrate oxidized/min per mol of enzyme) is calculated to be 2.1. The oxygenase belongs to the class of general drug-metabolizing enzymes and it may act on different compounds which can undergo sulphoxidation. The mechanism of sulphoxidation was shown to be mediated by superoxide anions.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Transparent glasses in the composition BaO-0.5Li(2)O-4.5B(2)O(3) (BLBO) were fabricated via the conventional melt-quenching technique. X-ray powder diffraction combined with differential scanning calorimetric (DSC) studies carried out on the as-quenched samples confirmed their amorphous and glassy nature, respectively. The crystallization behavior of these glasses has been studied by isothermal and nonisothermal methods using DSC. Crystallization kinetic parameters were evaluated from the Johnson-Mehl-Avrami equation. The value of the Avrami exponent (n) was found to be 3.6 +/- 0.1, suggesting that the process involves three-dimensional bulk crystallization. The average value of activation energy associated with the crystallization of BLBO glasses was 317 +/- 10 kJ/mol. Transparent glass-ceramics were fabricated by controlled heat-treatment of the as-quenched glasses at 845 K/40 min. The dielectric constants for BLBO glasses and glass-ceramics in the 100 Hz-10 MHz frequency range were measured as a function of the temperature (300-925 K). The electrical relaxation and dc conductivity characteristics were rationalized using electric modulus formalism. The imaginary part of the electric modulus spectra was modeled using an approximate solution of the Kohlrausch-Williams-Watts relation. The temperature-dependent behavior of stretched exponent (beta) was discussed for the as-quenched and heat-treated BLBO glasses.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The polymerization of methyl methacrylate initiated by a mixed ligand complex. [NN′-ethylenebis(salicylideneiminato)](benzoylacetonato)cobalt(III) has been studied in bulk and in benzene at 70° and 80°. The rate of polymerization is proportional to (concentration of the chelate)1/2 and the monomer exponent is close to 1.5. The activation energy and the kinetic and transfer constants are evaluated. A free radical mechanism has been proposed.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Polymerization of methyl methacrylate in the presence of a mixed ligand complex, [N,N-ethylenebis(salicylideneiminato)](acetylacetonato)cobalt(III) in benzene was studied. The rate of polymerization was proportional to the square root of the concentration of the chelate and the monomer exponent was 1.67 and 1.69 at 60 and 70°C, respectively. The activation energy and the kinetic and transfer constants were evaluated. A free-radical mechanism has been proposed.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The electrical activation energy and optical band-gap of GeSe and GeSbSe thin films prepared by flash evaporation on to glass substrates have been determined. The conductivities of the films were found to be given by Image , the activation energy Ea being 0.53 eV and 0.40 eV for GeSe and GeSbSe respectively. The optical absorption constant α near the absorption edge could be described by Image from which the optical band-gaps E0 were found to be 1.01 eV for GeSe and 0.67 eV for GeSbSe at 300°K. At 110°K the corresponding values of E0 were 1.07 eV and 0.735 eV respectively. The significance of these values is discussed in relation to those of other amorphous semiconductors.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Differential scanning calorimetric studies on ammonium perchlorate have been carried out. The enthalpy values for the phase transition endotherm and the two exotherms have been reported in the present communication. A new method has been developed for the estimation of kinetic parameters from DSC the mograms. The values for activation energy as calculated by the above method for low temperature and high temperature exotherms are in close agreement with literature values. The present studies also confirm the presence of small exothermic peaks at the initial stages of high temperature exotherm. Explanation for the same has been given.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The explosive sensitivity of methylammonium perchlorates has been investigated by differential thermal analysis, thermogravimetric analysis, mass spectrometry and explosion delay experiments. The decomposition temperature of these compounds increases in the order CH3NH3ClO4>(CH3)2NH2ClO4>(CH3)3NHClO4. The activation energy shows the reverse order, indicating thereby that the stability increases with increasing substitution. Mass spectrometric investigation, however, suggests an increasing reactivity with increasing substitution. A possible explanation for such behaviour is proposed. It appears that explosion delay is correlated with thermal decomposition and impact sensitivity.